Search results for: microstructure inspection
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 1130

Search results for: microstructure inspection

1010 Gas Tungsten Arc Welded Joints of Cast Al-Mg-Sc Alloy

Authors: K. Subbaiah, C. V. Jeyakumar, S. R. Koteswara Rao

Abstract:

Cast Aluminum-Magnesium-Scandium alloy was Gas Tungsten Arc (GTA) welded, and the microstructure and mechanical properties of the joint and its component parts were examined and analyzed. The global joint fractured in the base metal, and thus possessed slightly greater tensile strength than the base metal. These results clearly show that Gas Tungsten Arc welding is an optimum / suitable welding process for cast Aluminum-Magnesium-Scandium alloys.

Keywords: cast Al-Mg-Sc alloy, GTAW, microstructure, mechanical properties

Procedia PDF Downloads 381
1009 Remanufacturing and Integrity Assessment of a 27-Year-Old 25kV Gas Insulated Switchgear: A Comprehensive Study on Dismantling, Inspection, and Testing

Authors: Yechan Kim, Bonhyuk Ku, Minkyung Jung, Hyoungku Kang

Abstract:

This study presents the remanufacturing of a 25kV gas insulated switchgear (GIS) that operated indoors for 27 years before being decommissioned due to aging. The research involved a detailed process of dismantling, visual inspection, component-wise examination, and various testing methodologies to assess the equipment's condition. The focus was on evaluating the GIS's integrity and feasibility for remanufacturing. The results highlight the potential of remanufacturing in extending the life of electrical power equipment, offering insights into the best practices, challenges, and technical considerations of such an undertaking. This contributes to a sustainable approach in the power industry, emphasizing the reuse and restoration of aging equipment.

Keywords: remanufacturing, dismantling, gas insulated switchgear, sustainability, life extension

Procedia PDF Downloads 44
1008 Clustering-Based Threshold Model for Condition Rating of Concrete Bridge Decks

Authors: M. Alsharqawi, T. Zayed, S. Abu Dabous

Abstract:

To ensure safety and serviceability of bridge infrastructure, accurate condition assessment and rating methods are needed to provide basis for bridge Maintenance, Repair and Replacement (MRR) decisions. In North America, the common practices to assess condition of bridges are through visual inspection. These practices are limited to detect surface defects and external flaws. Further, the thresholds that define the severity of bridge deterioration are selected arbitrarily. The current research discusses the main deteriorations and defects identified during visual inspection and Non-Destructive Evaluation (NDE). NDE techniques are becoming popular in augmenting the visual examination during inspection to detect subsurface defects. Quality inspection data and accurate condition assessment and rating are the basis for determining appropriate MRR decisions. Thus, in this paper, a novel method for bridge condition assessment using the Quality Function Deployment (QFD) theory is utilized. The QFD model is designed to provide an integrated condition by evaluating both the surface and subsurface defects for concrete bridges. Moreover, an integrated condition rating index with four thresholds is developed based on the QFD condition assessment model and using K-means clustering technique. Twenty case studies are analyzed by applying the QFD model and implementing the developed rating index. The results from the analyzed case studies show that the proposed threshold model produces robust MRR recommendations consistent with decisions and recommendations made by bridge managers on these projects. The proposed method is expected to advance the state of the art of bridges condition assessment and rating.

Keywords: concrete bridge decks, condition assessment and rating, quality function deployment, k-means clustering technique

Procedia PDF Downloads 197
1007 Effects of Al on Microstructure and Magnetic Properties of (Nd,Pr)-(Fe,Co)-B Alloys Prepared by Mechanical Alloying

Authors: Rahim Sabbaghizadeh, Mansor Hashim, Nooshin Shourcheh

Abstract:

Nanocrystalline Nd8Pr2Fe79-xCo5B6Alx (x=0, 1, 2, 3) magnets were prepared by mechanical alloying and respective heat treatment, and the effects of the addition of Al on the microstructure and magnetic properties of Nd-Fe-Co-B alloy were studied. The changes in the nanostructure and magnetic properties were examined by X-Ray diffraction, combined with Field Emission Scanning electron microscopy (FeSEM) and vibrating sample magnetometer (VSM). Addition of Al was found to be effective for improving the coercivity and the hysteresis squareness in Nd–Fe–Co–B magnets without decreasing much the remanent magnetization.

Keywords: mechanical alloying, nanocrystalline, Nd-Fe-B, vibrating sample magnetomete

Procedia PDF Downloads 489
1006 Effect of Stirrup Corrosion on Concrete Confinement Strength

Authors: Mucip Tapan, Ali Ozvan, Ismail Akkaya

Abstract:

This study investigated how the concrete confinement strength and axial load carrying capacity of reinforced concrete columns are affected by corrosion damage to the stirrups. A total of small-scale 12 test specimens were cast for evaluating the effect of stirrup corrosion on confinement strength of concrete. The results of this study show that the stirrup corrosion alone dramatically decreases the axial load carrying capacity of corroded reinforced concrete columns. Recommendations were presented for improved inspection practices which will allow estimating concrete confinement strength of corrosion-damaged reinforced concrete bridge columns.

Keywords: bridge, column, concrete, corrosion, inspection, stirrup reinforcement

Procedia PDF Downloads 422
1005 A Review on Application of Waste Tire in Concrete

Authors: M. A. Yazdi, J. Yang, L. Yihui, H. Su

Abstract:

The application of recycle waste tires into civil engineering practices, namely asphalt paving mixtures and cementbased materials has been gaining ground across the world. This review summarizes and compares the recent achievements in the area of plain rubberized concrete (PRC), in details. Different treatment methods have been discussed to improve the performance of rubberized Portland cement concrete. The review also includes the effects of size and amount of tire rubbers on mechanical and durability properties of PRC. The microstructure behaviour of the rubberized concrete was detailed.

Keywords: waste rubber aggregates, microstructure, treatment methods, size and content effects

Procedia PDF Downloads 299
1004 Geometric Calibration of Computed Tomography Equipment

Authors: Chia-Hung Liao, Shih-Chieh Lin

Abstract:

X-ray computed tomography (CT) technology has been used in the electronics industry as one of the non-destructive inspection tools for years. The key advantage of X-ray computed tomography technology superior to traditional optical inspection is the penetrating characteristics of X-rays can be used to detect defects in the interior of objects. The objective of this study is to find a way to estimate the system geometric deviation of X-ray CT equipment. Projection trajectories of the characteristic points of standard parts were tracked, and ways to calculate the deviation of various geometric parameters of the system will be proposed and evaluated. A simulation study will be conducted to first find out the effects of system geometric deviation on projected trajectories. Then ways to estimate geometric deviation with collected trajectories will be proposed and tested through simulations.

Keywords: geometric calibration, X-ray computed tomography, trajectory tracing, reconstruction optimization

Procedia PDF Downloads 80
1003 Effect of Forging Pressure on Mechanical Properties and Microstructure of Similar and Dissimilar Friction Welded Joints (Aluminium, Copper, Steel)

Authors: Sagar Pandit

Abstract:

The present work focuses on the effect of various process parameters on the mechanical properties and microstructure of joints produced by continuous drive friction welding and linear friction welding. An attempt is made to investigate the feasibility of obtaining an acceptable weld joint between similar as well as dissimilar components and the microstructural changes have also been assessed once the good weld joints were considered (using Optical Microscopy and Scanning Electron Microscopy techniques). The impact of forging pressure in the microstructure of the weld joint has been studied and the variation in joint strength with varying forge pressure is analyzed. The weld joints were obtained two pair of dissimilar materials and one pair of similar materials, which are listed respectively as: Al-AA5083 & Cu-C101 (dissimilar), Aluminium alloy-3000 series & Mild Steel (dissimilar) and High Nitrogen Austenitic Stainless Steel pair (similar). Intermetallic phase formation was observed at the weld joints in the Al-Cu joint, which consequently harmed the properties of the joint (less tensile strength). It was also concluded that the increase in forging pressure led to both increment and decrement in the tensile strength of the joint depending on the similarity or dissimilarity of the components. The hardness was also observed to possess maximum as well as minimum values at the weld joint depending on the similarity or dissimilarity of workpieces. It was also suggested that a higher forging pressure is needed to obtain complete joining for the formation of the weld joint.

Keywords: forging pressure, friction welding, mechanical properties, microstructure

Procedia PDF Downloads 84
1002 A Study on the Magnetic and Mechanical Properties of Nd-Fe-B Sintered Magnets According to Sintering Temperature

Authors: J. H. Kim, S. Y. Park, K. M. Lim, S. K. Hyun

Abstract:

The effect of sintering temperature on the magnetic and mechanical properties of Nd-Fe-B sintered magnets has been investigated in this study. The sintering temperature changed from 950°C to 1120°C. While remanence and hardness of the magnets increased with increasing sintering temperature, the coercivity first increased, and then decreased. The optimum magnetic and mechanical properties of the magnets were obtained at the sintering temperature of 1050°C. In order to clarify the reason for the variation on magnetic and mechanical properties of the magnets, we systematically analyzed the microstructure.

Keywords: magnetic and mechanical property, microstructure, permanent magnets, sintered Nd-Fe-B magnet

Procedia PDF Downloads 307
1001 Compare Hot Forming and Cold Forming in Rolling Process

Authors: Ali Moarrefzadeh

Abstract:

In metalworking, rolling is a metal forming process in which metal stock is passed through a pair of rolls. Rolling is classified according to the temperature of the metal rolled. If the temperature of the metal is above its recrystallization temperature, then the process is termed as hot rolling. If the temperature of the metal is below its recrystallization temperature, the process is termed as cold rolling. In terms of usage, hot rolling processes more tonnage than any other manufacturing process, and cold rolling processes the most tonnage out of all cold working processes. This article describes the use of advanced tubing inspection NDT methods for boiler and heat exchanger equipment in the petrochemical industry to supplement major turnaround inspections. The methods presented include remote field eddy current, magnetic flux leakage, internal rotary inspection system and eddy current.

Keywords: hot forming, cold forming, metal, rolling, simulation

Procedia PDF Downloads 498
1000 The Influence of Ni Elements on Mechanical Properties and Microstructure of Twinning Induced Plasticity (TWIP)

Authors: Yuksel Akinay, Fatih Hayat

Abstract:

The influence of Ni elements on mechanical properties and microstructure of twinning induced plasticity (TWIP) steels were investigated in this study. TWIP 1 (0,6C, 24Mn) and TWIP 2 (0,6C, 24Mn, 1Ni) high Mn TWIP (Twinning Induced Plasticity) steels were fabricated, and were annealed at 700°C, 800°C and 900°C for 150 minute and then air-cooled. The microstructures and mechanical properties of specimens were analysed to investigate influence of Ni element on TWIP steel. The carbide precipitations have seen in microstructure of TWIP 1 and TWIP 2 specimen annealed at 700 °C. However, the microstructures of TWIP 1 annealed at 800°C and 900°C are fully austenite and some grains are including annealing twins. However twining did not occur at TWIP 2 specimens annealed at 700 °C, 800 °C and 900 °C. TWIP 2 steel contains also Ni element differently from TWIP 1 steel. It can conclude that, Nickel (Ni) was restrained formation of twinning. The reversion of the tensile strength occurred between 700°C and 800°C because of the carbide precipitation hardening. Beside that, hardness value has decreased between 800 °C and 900 °C, which show a good agreement with the equilibrium dissolution temperature of M3C carbides. However, the results show that, carbide precipitations also are as strong barriers for the formation of twining. For this reason, twinning was not obtained at 700 °C.

Keywords: high manganese, heat treatment, SEM, TWIP steel, cold rolling, nickel

Procedia PDF Downloads 328
999 Retraction Free Motion Approach and Its Application in Automated Robotic Edge Finishing and Inspection Processes

Authors: M. Nemer, E. I. Konukseven

Abstract:

In this paper, a motion generation algorithm for a six Degrees of Freedom (DoF) robotic hand in a static environment is presented. The purpose of developing this method is to be used in the path generation of the end-effector for edge finishing and inspection processes by utilizing the CAD model of the considered workpiece. Nonetheless, the proposed algorithm may be extended to be applicable for other similar manufacturing processes. A software package programmed in the application programming interface (API) of SolidWorks generates tool path data for the robot. The proposed method significantly simplifies the given problem, resulting in a reduction in the CPU time needed to generate the path, and offers an efficient overall solution. The ABB IRB2000 robot is chosen for executing the generated tool path.

Keywords: CAD-based tools, edge deburring, edge scanning, offline programming, path generation

Procedia PDF Downloads 263
998 Mechanical and Microstructural Properties of Rotary-Swaged Wire of Commercial-Purity Titanium

Authors: Michal Duchek, Jan Palán, Tomas Kubina

Abstract:

Bars made of titanium grade 2 and grade 4 were subjected to rotary forging with up to 2.2 true strain reduction in the cross-section from 10 to 3.81 mm. During progressive deformation, grain refinement in the transverse direction took place. In the longitudinal direction, ultrafine microstructure has not developed. It has been demonstrated that titanium grade 2 strengthens more than grade 4. The ultimate tensile strength increased from 650 MPa to 1040 MPa in titanium grade 4. Hardness profiles on the cross section in both materials show an increase in the centre of the wire.

Keywords: commercial-purity titanium, wire, rotary swaging, tensile test, hardness, modulus of elasticity, microstructure

Procedia PDF Downloads 214
997 Deformation and Crystallization in a 7075-T651 Friction Stir Weld

Authors: C. S. Paglia

Abstract:

The deformation and the crystallization in a 7075-T651 friction stir weld, in particular for regions directly in contact with the mechanical action of the rotating probe, have been investigated by means of optical microscopy. The investigation enabled to identify regions of the weld differently affected by the deformation caused by the welding process. The highly deformed grains in the horizontal direction close to the plate margin were indicative of shear movements along the horizontal plane, while highly deformed grains along the plate margin in the vertical direction were indicative of vertical shear movements of opposite directions, which superimposed the shear movement along the horizontal plane. The vertical shear movements were not homogeneous through the plate thickness. The microstructure indicated that after the probe passes, the grain growth may take place under static conditions. The small grains microstructure of the nugget region, formed after the main dynamic recrystallization process, develops to an equiaxed microstructure. A material transport influenced by the rotating shoulder was also observed from the trailing to the advancing side of the weld.

Keywords: AA7075-T651, friction stir welding, deformation, crystallization

Procedia PDF Downloads 98
996 Fabricating Sheets of Mg-Zn Alloys by Thermomechanical Process

Authors: Seok Hong Min, Tae Kwon Ha

Abstract:

In the present study, hot-rolled sheets of Mg-xZn alloy s(x=6, 8, and 10 weight percent) were produced by employing casting, homogenization heat treatment, hot rolling, and annealing processes subsequently. Effect of Zn addition on the microstructure and mechanical properties of Mg-Zn alloys were also investigated in each process. Through calculation of phase equilibria of Mg-Zn alloys, solution treatment temperature was decided as temperatures from 350 oC, where supersaturated solid solution can be obtained. After solution treatment, hot rolling was successfully conducted by reduction of 60%. Compression and tension tests were carried out at room temperature on the samples as-cast, solution treated, hot-rolled and recrystallized after rolling.

Keywords: Mg-Zn alloy, heat treatment, microstructure, mechanical properties, hot rolling

Procedia PDF Downloads 292
995 Performance of Visual Inspection Using Acetic Acid for Cervical Cancer Screening as Compared to HPV DNA Testingin Ethiopia: A Comparative Cross-Sectional Study

Authors: Agajie Likie Bogale, Tilahun Teklehaymanot, Getnet Mitike Kassie, Girmay Medhin, Jemal Haidar Ali, Nega Berhe Belay

Abstract:

Objectives: The aim of this study is to evaluate the performance of visual inspection using acetic acid compared with HPV DNA testing among women living with HIV in Ethiopia. Methods: Acomparative cross-sectional study was conducted to address the aforementioned objective. Data were collected from January to October 2021 to compare the performance of these two screening modalities. Trained clinicians collected cervical specimens and immediately applied acetic acid for visual inspection. The HPV DNA testing was done using Abbott m2000rt/SP by trained laboratory professionals in accredited laboratories. A total of 578 HIV positive women with age 25-49 years were included. Results: Test positivity was 8.9% using VIA and 23.3% using HPV DNA test. The sensitivity and specificity of the VIA test were 19.2% and 95.1%, respectively, while the positive and negative predictive values of the VIA test were 54.4% and 79.4%, respectively. The strength of agreement between the two screening methods was poor (k=0.184), and the area under the curve was 0.572. The burden of genetic distribution of high risk HPV16 was 3.8%, and mixed HPV16& other HR HPV was 1.9%. Other high risk HPV types were predominant in this study (15.7%). Conclusion: The high positivity result using HPV DNA testing compared with VIA, and low sensitivity of VIA are indicating that the implementation of HPV DNA testing as the primary screening strategy is likely to reduce cervical cancer cases and deaths of women in the country.

Keywords: cervical cancer screening, HPV DNA, VIA, Ethiopia

Procedia PDF Downloads 104
994 Alloying Effect on Hot Workability of M42 High Speed Steel

Authors: Jung-Ho Moon, Tae Kwon Ha

Abstract:

In the present study, the effect of Si, Al, Ti, Zr, and Nb addition on the microstructure and hot workability of cast M42 tool steels, basically consisting of 1.0C, 0.2Mn, 3.8Cr, 1.5W, 8.5Co, 9.2Mo, and 1.0V in weight percent has been investigated. Tool steels containing Si of 0.25 and 0.5 wt.%, Al of 0.06 and 0.12 wt.%, Ti of 0.3 wt.%, Zr of 0.3 wt.%, and Nb of 0.3 wt.% were cast into ingots of 140 mm´ 140 mm´ 330 mm by vacuum induction melting. After solution treatment at 1150°C for 1.5 hrs. followed by furnace cooling, hot rolling at 1180 °C was conducted on the ingots. Addition of titanium, zirconium and niobium was found to retard the decomposition of the eutectic carbides and result in the deterioration of hot workability of the tool steels, while addition of aluminium and silicon showed relatively well decomposed carbide structure and resulted in sound hot rolled plates.

Keywords: high speed steels, alloying elements, eutectic carbides, microstructure, hot workability

Procedia PDF Downloads 334
993 Microstructures and Mechanical Property of ti6al4v - a Comparison between Selective Laser Melting, Electron Beam Melting and Spark Plasma Sintering

Authors: Javad Karimi, Prashanth Konda Gokuldoss

Abstract:

Microstructural inhomogeneity in additively manufactured materials affects the material properties. The present study aims in minimizing such microstructural inhomogeneity in Ti6Al4V alloy fabricated using selective laser melting (SLM) from the gas atomized powder. A detailed and systematic study of the effect of remelting on the microstructure and mechanical properties of Ti6Al4V manufactured by SLM was compared with electron beam melting and spark plasma sintering.

Keywords: additive manufacturing, selective laser melting, Ti6Al4V, microstructure

Procedia PDF Downloads 139
992 Multi-Scale Damage Modelling for Microstructure Dependent Short Fiber Reinforced Composite Structure Design

Authors: Joseph Fitoussi, Mohammadali Shirinbayan, Abbas Tcharkhtchi

Abstract:

Due to material flow during processing, short fiber reinforced composites structures obtained by injection or compression molding generally present strong spatial microstructure variation. On the other hand, quasi-static, dynamic, and fatigue behavior of these materials are highly dependent on microstructure parameters such as fiber orientation distribution. Indeed, because of complex damage mechanisms, SFRC structures design is a key challenge for safety and reliability. In this paper, we propose a micromechanical model allowing prediction of damage behavior of real structures as a function of microstructure spatial distribution. To this aim, a statistical damage criterion including strain rate and fatigue effect at the local scale is introduced into a Mori and Tanaka model. A critical local damage state is identified, allowing fatigue life prediction. Moreover, the multi-scale model is coupled with an experimental intrinsic link between damage under monotonic loading and fatigue life in order to build an abacus giving Tsai-Wu failure criterion parameters as a function of microstructure and targeted fatigue life. On the other hand, the micromechanical damage model gives access to the evolution of the anisotropic stiffness tensor of SFRC submitted to complex thermomechanical loading, including quasi-static, dynamic, and cyclic loading with temperature and amplitude variations. Then, the latter is used to fill out microstructure dependent material cards in finite element analysis for design optimization in the case of complex loading history. The proposed methodology is illustrated in the case of a real automotive component made of sheet molding compound (PSA 3008 tailgate). The obtained results emphasize how the proposed micromechanical methodology opens a new path for the automotive industry to lighten vehicle bodies and thereby save energy and reduce gas emission.

Keywords: short fiber reinforced composite, structural design, damage, micromechanical modelling, fatigue, strain rate effect

Procedia PDF Downloads 86
991 Aging Effect on Mechanical Behavior of Duplex Stainless Steel

Authors: Jeonho Moon, Tae Kwon Ha

Abstract:

In the present study, the effect of Si, Al, Ti, Zr, and Nb addition on the microstructure and hot workability of cast M42 tool steels, basically consisting of 1.0 C, 0.2 Mn, 3.8 Cr, 1.5 W, 8.5 Co, 9.2 Mo, and 1.0 V in weight percent has been investigated. Tool steels containing Si of 0.25 and 0.5 wt.%, Al of 0.06 and 0.12 wt.%, Ti of 0.3 wt.%, Zr of 0.3 wt.%, and Nb of 0.3wt.% were cast into ingots of 140 mm x 140 mm x 330 mm by vacuum induction melting. After solution treatment at 1150 °C for 1.5 hr followed by furnace cooling, hot rolling at 1180 °C was conducted on the ingots. Addition of titanium, zirconium and niobium was found to retard the decomposition of the eutectic carbides and result in the deterioration of hot workability of the tool steels, while addition of aluminum and silicon showed relatively well decomposed carbide structure and resulted in sound hot rolled plates.

Keywords: duplex stainless steel, alloying elements, eutectic carbides, microstructure, hot workability

Procedia PDF Downloads 388
990 Cold Spray Fabrication of Coating for Highly Corrosive Environment

Authors: Harminder Singh

Abstract:

Cold spray is a novel and emerging technology for the fabrication of coating. In this study, coating is successfully developed by this process on superalloy surface. The selected coating composition is already proved as corrosion resistant. The microstructure of the newly developed coating is examined by various characterization techniques, for testing its suitability for high temperature corrosive conditions of waste incinerator. The energy producing waste incinerators are still running at low efficiency, mainly due to their chlorine based highly corrosive conditions. The characterization results show that the developed cold sprayed coating structure is suitable for its further testing in highly aggressive conditions.

Keywords: coating, cold spray, corrosion, microstructure

Procedia PDF Downloads 360
989 Hazardous Vegetation Detection in Right-Of-Way Power Transmission Lines in Brazil Using Unmanned Aerial Vehicle and Light Detection and Ranging

Authors: Mauricio George Miguel Jardini, Jose Antonio Jardini

Abstract:

Transmission power utilities participate with kilometers of circuits, many with particularities in terms of vegetation growth. To control these rights-of-way, maintenance teams perform ground, and air inspections, and the identification method is subjective (indirect). On a ground inspection, when identifying an irregularity, for example, high vegetation threatening contact with the conductor cable, pruning or suppression is performed immediately. In an aerial inspection, the suppression team is mobilized to the identified point. This work investigates the use of 3D modeling of a transmission line segment using RGB (red, blue, and green) images and LiDAR (Light Detection and Ranging) sensor data. Both sensors are coupled to unmanned aerial vehicle. The goal is the accurate and timely detection of vegetation along the right-of-way that can cause shutdowns.

Keywords: 3D modeling, LiDAR, right-of-way, transmission lines, vegetation

Procedia PDF Downloads 110
988 A Metallography Study of Secondary A226 Aluminium Alloy Used in Automotive Industries

Authors: Lenka Hurtalová, Eva Tillová, Mária Chalupová, Juraj Belan, Milan Uhríčik

Abstract:

The secondary alloy A226 is used for many automotive casting produced by mould casting and high pressure die-casting. This alloy has excellent castability, good mechanical properties and cost-effectiveness. Production of primary aluminium alloys belong to heavy source fouling of life environs. The European Union calls for the emission reduction and reduction in energy consumption, therefore, increase production of recycled (secondary) aluminium cast alloys. The contribution is deal with influence of recycling on the quality of the casting made from A226 in automotive industry. The properties of the casting made from secondary aluminium alloys were compared with the required properties of primary aluminium alloys. The effect of recycling on microstructure was observed using combination different analytical techniques (light microscopy upon black-white etching, scanning electron microscopy-SEM upon deep etching and energy dispersive X-ray analysis-EDX). These techniques were used for the identification of the various structure parameters, which was used to compare secondary alloy microstructure with primary alloy microstructure.

Keywords: A226 secondary aluminium alloy, deep etching, mechanical properties, recycling foundry aluminium alloy

Procedia PDF Downloads 515
987 Evaluation of Soil Stiffness and Strength for Quality Control of Compacted Earthwork

Authors: A. Sawangsuriya, T. B. Edil

Abstract:

Microstructure and fabric of soils play an important role on structural properties e.g. stiffness and strength of compacted earthwork. Traditional quality control monitoring based on moisture-density tests neither reflects the variability of soil microstructure nor provides a direct assessment of structural property, which is the ultimate objective of the earthwork quality control. Since stiffness and strength are sensitive to soil microstructure and fabric, any independent test methods that provide simple, rapid, and direct measurement of stiffness and strength are anticipated to provide an effective assessment of compacted earthen materials’ uniformity. In this study, the soil stiffness gauge (SSG) and the dynamic cone penetrometer (DCP) were respectively utilized to measure and monitor the stiffness and strength in companion with traditional moisture-density measurements of various earthen materials used in Thailand road construction projects. The practical earthwork quality control criteria are presented herein in order to assure proper earthwork quality control and uniform structural property of compacted earthworks.

Keywords: dynamic cone penetrometer, moisture content, quality control, relative compaction, soil stiffness gauge, structural properties

Procedia PDF Downloads 336
986 A Comparative Assessment of Industrial Composites Using Thermography and Ultrasound

Authors: Mosab Alrashed, Wei Xu, Stephen Abineri, Yifan Zhao, Jörn Mehnen

Abstract:

Thermographic inspection is a relatively new technique for Non-Destructive Testing (NDT) which has been gathering increasing interest due to its relatively low cost hardware and extremely fast data acquisition properties. This technique is especially promising in the area of rapid automated damage detection and quantification. In collaboration with a major industry partner from the aerospace sector advanced thermography-based NDT software for impact damaged composites is introduced. The software is based on correlation analysis of time-temperature profiles in combination with an image enhancement process. The prototype software is aiming to a) better visualise the damages in a relatively easy-to-use way and b) automatically and quantitatively measure the properties of the degradation. Knowing that degradation properties play an important role in the identification of degradation types, tests and results on specimens which were artificially damaged have been performed and analyzed.

Keywords: NDT, correlation analysis, image processing, damage, inspection

Procedia PDF Downloads 515
985 Directional Solidification of Al–Cu–Mg Eutectic Alloy

Authors: Yusuf Kaygısız, Necmetti̇n Maraşlı

Abstract:

Aluminum alloys are produced and used at various areas of industry and especially in the aerospace industry. The advantages of these alloys over traditional iron-based alloys are lightweight, corrosion resistance, and very good thermal and electrical conductivity. The aim of this work is to experimentally investigate the effect of growth rates on the eutectic spacings (λ), microhardness, tensile strength and electrical resistivity in Al–30wt.%Cu–6wt.%Mg eutectic alloy. Al–Cu–Mg eutectic alloy was directionally solidified at a constant temperature gradient (G=8.55 K/mm) with different growth rates, 9.43 to 173.3 µm/s by using a Bridgman-type furnace. The dependency of microstructure, microhardness, tensile strength and electrical resistivity for directionally solidified the Al-Cu-Mg eutectic alloy were investigated. Eutectic microstructure is consisting of regular Al2CuMg lamellar and Al2Cu rod phases with in the α (Al) solid solution matrix. The lamellar eutectic spacings were measured from transverse sections of the samples. It was found that the value of microstructures decrease with the increase the value the growth rates. The microhardness, tensile strength and electrical resistivity of the alloy also were measured from sample and relationships between them were experimentally analyzed by using regression analysis. According to present results, values tensile strength and electrical resistivity increase with increasing growth rates.

Keywords: directional solidification, aluminum alloys, microstructure, electrical properties, hardness test

Procedia PDF Downloads 264
984 Defect-Based Urgency Index for Bridge Maintenance Ranking and Prioritization

Authors: Saleh Abu Dabous, Khaled Hamad, Rami Al-Ruzouq

Abstract:

Bridge condition assessment and rating provide essential information needed for bridge management. This paper reviews bridge inspection and condition rating practices and introduces a defect-based urgency index. The index is estimated at the element-level based on the extent and severity of the different defects typical to the bridge element. The urgency index approach has the following advantages: (1) It facilitates judgment submission, i.e. instead of rating the bridge element with a specific linguistic overall expression (which can be subjective and used differently by different people), the approach is based on assessing the defects; (2) It captures multiple defects that can be present within a deteriorated element; and (3) It reflects how critical the element is through quantifying critical defects and their severity. The approach can be further developed and validated. It is expected to be useful for practical purposes as an early-warning system for critical bridge elements.

Keywords: condition rating, deterioration, inspection, maintenance

Procedia PDF Downloads 422
983 Microstructural and Tribological Properties of Thermally Sprayed High Entropy Alloys Coating

Authors: Abhijith N. V., Abhijit Pattnayak, Deepak Kumar

Abstract:

Nowadays, a group of alloys, namely high entropy alloys (HEA), because of their excellent properties. However, the fabrication of HEAs requires multistage techniques, especially mill-ing, sieving, compaction, sintering, inert media, etc. These processes are laborious, costly, time-oriented, and unsuitable for commercial application. This study adopted a single-stage process-based HVOF thermal spray to develop HEA coating on SS304L substrates. The wear behavior of the deposited HEA coating was explored under different milling time durations (5h, 10h, and 15h, respectively). The effect of feedstock preparation, microstructure, surface chemistry, and mechanical and metallurgical properties on wear resistance was also investigated. The microstructure and composition of both coating and feedstock were evaluated by scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) analysis. Finally, the phase distribution was correlated by X-ray diffraction (XRD ) analysis. The results showed that 15h milled powder coating indicated better tribological than the base substrate and 5h,10h milled powder coating. A chemically stable Body Centered Cubic (BCC) solid solution phase was generated within the 15h milled powder-coated system, which resulted in superior tribological properties.

Keywords: high entropy alloys coating, wear mechanism, HVOF coating, microstructure

Procedia PDF Downloads 65
982 Root Cause Analysis of Surveillance Quality in Tanjung Priok Port to Prevent Epidemic Potential Disease as a Form of Bioterrorism Threat

Authors: Dina A. Amu, Fifi N. Afifah, Catur Rosidati, Tirton Nefianto

Abstract:

Indonesia was shaken up by the avian influenza cases that had caused the country suffered losses of millions of dollars. The avian influenza case had even been suspected as a bioterrorism attack since it was an uncommon case in epidemiology. Furthermore, this avian influenza virus is a high pathogenic one and Indonesia has the highest case of fatality rate in the world. Bioterrorism threats or epidemic potential disease outbreaks currently does not exist in Tanjung Priok port yet. However, the surveillance system enhancement on epidemic potential diseases should be taken as a prevention, especially because Indonesia is currently facing the ASEAN Economic Society (AES). Therefore, this research evaluates the health surveillance system which is organized by Control, Quarantine and Surveillance Department, Health Office of Tanjung Priok Port. This study uses qualitative-evaluative method which utilizes Urgency Seriousness Growth (USG) method to determine priority issues and Root Cause analysis to determine the cause of prior problem. The result of this research shows that the implementation of epidemic potential disease surveillance in Tanjung Priok port has not done in the best possible way. It is because the lack of time allocation and the succinctness of the check list of ship's environmental health inspection. Therefore, Health Ministry of Indonesia should recruit more employees at the health office of Tanjung Priok port, hold a simulation of ship's inspection and simplify the list for ship's environmental health inspection.

Keywords: surveillance, epidemic potential disease, port health, bioterrorism

Procedia PDF Downloads 338
981 Hardness and Microstructure of Rapidly Quenched Aluminum Alloys

Authors: Mehdi Ghatus

Abstract:

Two simple apparatus based on the hammer and anvil principle have been constructed and used to study the microstructure and micro-hardness characteristics of some AL-base alloys. Foils with thicknesses arranging from 20 µm up to 600 µm have been obtained. The cooling rate was estimated to be in the range 10^4 - 10^5 K/sec. Microstructure study of rapidly quenched Al-30% Si foils indicated that with decreasing the foil thickness the size of primary Si crystallites decreases in the whole investigated range (0.64-0.15 mm). However, the volume fraction of the primary Si crystals in the structure remained constant down to thickness the primary Si volume fraction started to decrease. Rapid quenching of Al- 14-16% Cu showed single phase cell structure. In foils up to 0.55 mm with decreasing the foil thickness the cell size decreases and micro-hardness increases particularly in foils below 0.3 mm in thickness. Isochronal annealing of theses foils show that the highly supersaturated Al-14-16% Cu solid solution decomposes readily at relatively low temperature and short time intervals. The maximum hardness is obtained after annealing at 100 °C for 30 minutes. However with decreasing the Cu content of the foils the precipitation process is largely delayed. Eight hours of annealing at 100 °C was not enough to achieve the maximum hardness in Al-4% Cu thin foils. The achieved hardness value was more than twice of the maximum hardness obtained in articles of similar composition but conventionally aged.

Keywords: aluminum, hardness, alloys, quenched aluminum

Procedia PDF Downloads 400