Search results for: iron phosphate
1419 Study of Divalent Phosphate Iron-Oxide Precursor Recycling Technology
Authors: Shinn-Dar Wu
Abstract:
This study aims to synthesize lithium iron phosphate cathode material using a recycling technology involving non-protective gas calcination. The advantages include lower cost and easier production than traditional methods that require a large amount of protective gas. The novel technology may have extensive industrial applications. Given that the traditional gas calcination has a large number of protection free Fe3+ production, this study developed a precursor iron phosphate (Fe2+) material recycling technology and conducted related tests and analyses. It focused on flow field design of calcination and new technology as well as analyzed the best conditions for powder calcination combination. The electrical properties were determined by button batteries and exhibited a capacity of 118 mAh/g (The use of new materials synthesis, capacitance is about 122 mAh/g). The cost reduced to 50% of the original.Keywords: lithium battery, lithium iron phosphate, calcined technology, recycling technology
Procedia PDF Downloads 4811418 Oxygen-Tolerant H₂O₂ Reduction Catalysis by Iron Phosphate Coated Iron Oxides
Authors: Chia-Ting Chang, Chia-Yu Lin
Abstract:
We report on the decisive role of iron phosphate (FePO₄), formed in-situ during the electrochemical characterization, played in the electrocatalytic activity, especially its oxygen tolerance of iron oxides towards H₂O₂ reduction. Iron oxides studied including, Nanorod arrays (NRs) of β-FeOOH, γ-Fe₂O₃, α-Fe₂O₃, α-Fe₂O₃ nanosheets (α-Fe₂O₃NS), α-Fe₂O₃ nanoparticles (α-Fe₂O₃NP), were synthesized using chemical bath deposition. The nanostructure was controlled simply by adjusting the composition of precursor solution and reaction duration for CBD process, whereas the crystal phase was controlled by adjusting the annealing temperature. It was found that iron phosphate (FePO₄) was deposited in-situ onto the surface of this nanostructured α-Fe₂O₃ during the electrochemical pretreatment in the phosphate electrolyte, and both FePO₄ and α-Fe₂O₃ showed the activity in catalysing the electrochemical reduction of H₂O₂. In addition, the interaction/compatibility between deposited FePO₄ and iron oxides has a decisive effect on the overall electrocatalytic activity of the resultant electrodes; FePO₄ only showed synergetic effect on the overall electrocatalytic activity of α-Fe₂O₃NR and α-Fe2O₃NS. Both α-Fe₂O₃NR and α-Fe₂O₃NS showed two reduction peaks in phosphate electrolyte containing H₂O₂, one being pH-dependent and related to the electrocatalytic properties of FePO₄, and the other one being pH-independent and only related to the intrinsic electrocatalytic properties of α-Fe₂O₃NR and α-Fe₂O₃NS. However, all iron oxides showed only one pH-independent reductive peak in non-phosphate electrolyte containing H₂O₂. The synergesitic catalysis exerted by FePO₄ with α-Fe₂O₃NR or α-Fe₂O₃NS providing additional oxygen-insensitive active site for H₂O₂ reduction, which allows their applications to electrochemical detection of H₂O₂ without the interference of O₂ involving in oxidase-catalyzed chemical processes.Keywords: H₂O₂ reduction, Iron oxide, iron phosphate, O₂ tolerance
Procedia PDF Downloads 4151417 Acid Mine Drainage Remediation Using Silane and Phosphate Coatings
Authors: M. Chiliza, H. P. Mbukwane, P Masita, H. Rutto
Abstract:
Acid mine drainage (AMD) one of the main pollutants of water in many countries that have mining activities. AMD results from the oxidation of pyrite and other metal sulfides. When these metals gets exposed to moisture and oxygen, leaching takes place releasing sulphate and Iron. Acid drainage is often noted by 'yellow boy,' an orange-yellow substance that occurs when the pH of acidic mine-influenced water raises above pH 3, so that the previously dissolved iron precipitates out. The possibility of using environmentally friendly silane and phosphate based coatings on pyrite to remediate acid mine drainage and prevention at source was investigated. The results showed that both coatings reduced chemical oxidation of pyrite based on Fe and sulphate release. Furthermore, it was found that silane based coating performs better when coating synthesis take place in a basic hydrolysis than in an acidic state.Keywords: acid mine drainage, pyrite, silane, phosphate
Procedia PDF Downloads 3421416 Removal and/or Recovery of Phosphates by Precipitation as Ferric Phosphate from the Effluent of a Municipal Wastewater Treatment Plant
Authors: Kyriaki Kalaitzidou, Athanasia Tolkou, Christina Raptopoulou, Manassis Mitrakas, Anastasios Zouboulis
Abstract:
Phosphate rock is the main source of phosphorous (P) in fertilizers and is essential for high crop yield in agriculture; currently, it is considered as a critical element, phasing scarcity. Chemical precipitation, which is a commonly used method of phosphorous removal from wastewaters, finds its significance in that phosphates may be precipitated in appropriate chemical forms that can be reused-recovered. Most often phosphorous is removed from wastewaters in the form of insoluble phosphate salts, by using salts (coagulants) of multivalent metal ions, most frequently iron, aluminum, calcium, or magnesium. The removal degree is affected by various factors, such as pH, chemical agent dose, temperature, etc. In this study, phosphate precipitation from the secondary (biologically treated) effluent of a municipal wastewater treatment plant is examined. Using chlorosulfate (FeClSO4) it was attempted to either remove and/or recover PO43-. Results showed that the use of Fe3+ can achieve residual concentrations lower than the commonly applied legislation limit of PO43- (i.e. 3 mg PO43-/L) by adding 7.5 mg/L Fe3+ in the secondary effluent with an initial concentration of about 10 mg PO43-/L and at pH range between 6 to 9. In addition, the formed sediment has a percentage of almost 24% PO43- content. Therefore, simultaneous removal and recovery of PO43- as ferric phosphate can be achieved, making it possible for the ferric phosphate to be re-used as a possible (secondary) fertilizer source.Keywords: ferric phosphate, phosphorus recovery, phosphorus removal, wastewater treatment
Procedia PDF Downloads 4841415 Effect of Iron Contents on Rheological Properties of Syndiotactic Polypropylene/iron Composites
Authors: Naveed Ahmad, Farooq Ahmad, Abdul Aal
Abstract:
The effect of iron contents on the rheological behavior of sPP/iron composites in the melt phase was investigated using a series of syndiotactic polypropylene/iron (sPP/iron) composite samples. Using the Advanced Rheometric Expansion System, studies with small amplitude oscillatory shear were conducted (ARES). It was discovered that the plateau modulus rose along with the iron loading. Also it was found that both entanglement molecular weight and packing length decrease with increase in iron loading.. This finding demonstrates how iron content in polymer/iron composites affects chain parameters and dimensions, which in turn affects the entire chain dynamics.Keywords: plateau modulus, packing lenght, polymer/iron composites, rheology, entanglement molecular weight
Procedia PDF Downloads 1611414 Reduction Behavior of Some Low-Grade Iron Ores for Application in Blast Furnace
Authors: Heba Al-Kelesh
Abstract:
Day after day, high-grade iron ores are consumed. Because of the strong global demand for iron and steel, it has necessitated the utilization of various low-grade iron ores, which are not suitable for direct exploitation in the iron industry. The low-grade ores cannot be dressed using traditional mineral processing methods because of complicated mineral compositions. The present work is aimed to investigate the reducibility of some Egyptian iron ores and concentrates by conditions emulate different blast furnace areas. Representative specimens are collected from El-Gedida–Baharia oasis, Eastern South Aswan, and Eastern desert-wadi Kareem (EDC). Some mineralogical and morphological characterizations are executed. The reactivity arrangement of green samples is Baharia>Aswan>EDC. The presence of magnetite decreased reactivity of EDC. The reducibility of the Aswan sample is lower than Baharia due to the presence of agglomerated metallic grain surrounded by semi-melted phases. Specimens are annealed at 1000ᵒC for 3 hours. After firing, the reducibility of Aswan becomes the lowest due to the formation of fayalite and calcium phosphate phases. The relative attitude for green and fired samples reduced at different conditions are studied. For thermal and top areas, the reactivity of fired samples is greater than green ones, which were confirmed by morphological examinations.Keywords: reducibility, low grade, iron industry, blast furnace
Procedia PDF Downloads 1271413 A Ratiometric Inorganic Phosphate Sensor Based on CdSe/ZnS QDs and Rhodamine 6G-Doped Nanofibers
Authors: Hong Dinh Duong, Jong Il Rhee
Abstract:
In this study, a ratiometric inorganic phosphate sensor was fabricated by a double layer of the rhodamine 6G-doped nanofibers and the CdSe/ZnS QDs-captured polymer. In which, CdSe/ZnS QDs with emission wavelengths of 595nm were synthesized and ligands on their surface were exchanged with mercaptopropionic acid (MPA). The synthesized MPA-QDs were combined with the mixture of sol-gel of 3-glycidoxypropyl trimethoxysilane (GPTMS), 3-aminopropyltrimethoxysilane (APTMS) and polyurethane (PU) to build a layer for sensing inorganic phosphate. Another sensing layer was of nanofibers doped R6G which were produced from poly(styrene-co-acrylonitrile) by electrospining. The ratio of fluorescence intensities between rhodamin 6G (R6G) and CdSe/ZnS QDs exposed at different phosphate concentrations was used for calculating a linear phosphate concentration range of 0-10mM.Keywords: nanofiber, QDs, ratiometric phosphate sensor, rhodamine 6G, sol-gel
Procedia PDF Downloads 4101412 The Effect of Application of Biological Phosphate Fertilizer (Fertile 2) and Triple Super Phosphate Chemical Fertilizers on Some Morphological Traits of Corn (SC704)
Authors: M. Mojaddam, M. Araei, T. Saki Nejad, M. Soltani Howyzeh
Abstract:
In order to study the effect of different levels of triple super phosphate chemical fertilizer and biological phosphate fertilizer (fertile 2) on some morphological traits of corn this research was carried out in Ahvaz in 2002 as a factorial experiment in randomized complete block design with 4 replications.) The experiment included two factors: first, biological phosphate fertilizer (fertile 2) at three levels of 0, 100, 200 g/ha; second, triple super phosphate chemical fertilizer at three levels of 0, 60, 90 kg/ha of pure phosphorus (P2O5). The obtained results indicated that fertilizer treatments had a significant effect on some morphological traits at 1% probability level. In this regard, P2B2 treatment (100 g/ha biological phosphate fertilizer (fertile 2) and 60 kg/ha triple super phosphate fertilizer) had the greatest plan height, stem diameter, number of leaves and ear length. It seems that in Ahvaz weather conditions, decrease of consumption of triple superphosphate chemical fertilizer to less than a half along with the consumption of biological phosphate fertilizer (fertile 2) is highly important in order to achieve optimal results. Therefore, it can be concluded that biological fertilizers can be used as a suitable substitute for some of the chemical fertilizers in sustainable agricultural systems.Keywords: biological phosphate fertilizer (fertile 2), triple super phosphate, corn, morphological traits
Procedia PDF Downloads 4431411 A Highly Sensitive Dip Strip for Detection of Phosphate in Water
Authors: Hojat Heidari-Bafroui, Amer Charbaji, Constantine Anagnostopoulos, Mohammad Faghri
Abstract:
Phosphorus is an essential nutrient for plant life which is most frequently found as phosphate in water. Once phosphate is found in abundance in surface water, a series of adverse effects on an ecosystem can be initiated. Therefore, a portable and reliable method is needed to monitor the phosphate concentrations in the field. In this paper, an inexpensive dip strip device with the ascorbic acid/antimony reagent dried on blotting paper along with wet chemistry is developed for the detection of low concentrations of phosphate in water. Ammonium molybdate and sulfuric acid are separately stored in liquid form so as to improve significantly the lifetime of the device and enhance the reproducibility of the device’s performance. The limit of detection and quantification for the optimized device are 0.134 ppm and 0.472 ppm for phosphate in water, respectively. The device’s shelf life, storage conditions, and limit of detection are superior to what has been previously reported for the paper-based phosphate detection devices.Keywords: phosphate detection, paper-based device, molybdenum blue method, colorimetric assay
Procedia PDF Downloads 1701410 Using Morlet Wavelet Filter to Denoising Geoelectric ‘Disturbances’ Map of Moroccan Phosphate Deposit ‘Disturbances’
Authors: Saad Bakkali
Abstract:
Morocco is a major producer of phosphate, with an annual output of 19 million tons and reserves in excess of 35 billion cubic meters. This represents more than 75% of world reserves. Resistivity surveys have been successfully used in the Oulad Abdoun phosphate basin. A Schlumberger resistivity survey over an area of 50 hectares was carried out. A new field procedure based on analytic signal response of resistivity data was tested to deal with the presence of phosphate deposit disturbances. A resistivity map was expected to allow the electrical resistivity signal to be imaged in 2D. 2D wavelet is standard tool in the interpretation of geophysical potential field data. Wavelet transform is particularly suitable in denoising, filtering and analyzing geophysical data singularities. Wavelet transform tools are applied to analysis of a moroccan phosphate deposit ‘disturbances’. Wavelet approach applied to modeling surface phosphate “disturbances” was found to be consistently useful.Keywords: resistivity, Schlumberger, phosphate, wavelet, Morocco
Procedia PDF Downloads 4221409 Bioremediation Potentials of Some Indigenous Microorganisms Isolated from Auto Mechanic Workshops on Irrigation Water Used in Lokoja Kogi State of Nigeria
Authors: Emmanuel Ekpa, Adaji Andrew, Queen Opaluwa, Isreal Daraobong
Abstract:
Three (3) indigenous bacteria species (Bacillus spp, Acinectobacter spp and Moraxella spp) previously isolated from contaminated soil of some auto mechanic workshops were used for bioremediation studies on some irrigation water used at Sarkin-noma Fadama farms located in Lokoja Kogi State, Nigeria. This was done in order to investigate their bioremediation potentials using a simple pour plate method. The physicochemical parameters and heavy metal analysis (using AAS iCE 3000) of the irrigation water were performed before and after inoculation of the isolated organisms. Nitrate and phosphate concentration were found to be 10.56mg/L and 12.63mg/L prior to inoculation while iron and zinc were 0.9569mg/L and 0.2245mg/L respectively. Other physicochemical parameters were also observed to be high prior to inoculation. After the bioremediation test (inoculation with the isolated organisms), a nitrate and phosphate content of 2.53mg/L and 2.61mg/L were recorded respectively, iron and zinc gave 0.1694mg/L and 0.0174mg/L concentrations while other physicochemical parameters measured were also found to be lower in their respective values. The implication of this present study is that a number of carefully isolated indigenous bacteria species are capable of reducing the amount of heavy metal concentrations in water. Also, non-metallic contaminants like nitrate and phosphate are susceptible to bioremediation in the presence of such efficient system.Keywords: bioremediation, heavy metals, physicochemical parameters, Bacillus spp, Acinectobacter spp and Moraxella spp, AAS, spectrometer 3000
Procedia PDF Downloads 3381408 Enhancing Protein Incorporation in Calcium Phosphate Coating on Titanium by Rapid Biomimetic Co-Precipitation Technique
Authors: J. Suwanprateeb, F. Thammarakcharoen
Abstract:
Calcium phosphate coating (CaP) has been employed for protein delivery, but the typical direct protein adsorption on the coating led to low incorporation content and fast release of the protein from the coating. By using bovine serum albumin (BSA) as a model protein, rapid biomimetic co-precipitation between calcium phosphate and BSA was employed to control the distribution of BSA within calcium phosphate coating during biomimetic formation on titanium surface for only 6 h at 50 oC in an accelerated calcium phosphate solution. As a result, the amount of BSA incorporation and release duration could be increased by using a rapid biomimetic co-precipitation technique. Up to 43 fold increases in the BSA incorporation content and the increase from 6 h to more than 360 h in release duration compared to typical direct adsorption technique were observed depending on the initial BSA concentration used during co-precipitation (1, 10, and 100 microgram/ml). From X-ray diffraction and Fourier transform infrared spectroscopy studies, the coating composition was not altered with the incorporation of BSA by this rapid biomimetic co-precipitation and mainly comprised octacalcium phosphate and hydroxyapatite. However, the microstructure of calcium phosphate crystals changed from straight, plate-like units to curved, plate-like units with increasing BSA content.Keywords: biomimetic, Calcium Phosphate Coating, protein, titanium
Procedia PDF Downloads 3851407 Simultaneous Removal of Phosphate and Ammonium from Eutrophic Water Using Dolochar Based Media Filter
Authors: Prangya Ranjan Rout, Rajesh Roshan Dash, Puspendu Bhunia
Abstract:
With the aim of enhancing the nutrient (ammonium and phosphate) removal from eutrophic wastewater with reduced cost, a novel media based multistage bio filter with drop aeration facility was developed in this work. The bio filter was packed with a discarded sponge iron industry by product, ‘dolochar’ primarily to remove phosphate via physicochemical approach. In the multi stage bio-filter drop, aeration was achieved by the process of percolation of the gravity-fed wastewater through the filter media and dropping down of wastewater from stage to stage. Ammonium present in wastewater got adsorbed by the filter media and biomass grown on the filter media and subsequently, got converted to nitrate through biological nitrification in the aerobic condition, as realized by drop aeration. The performance of the bio-filter in treating real eutrophic wastewater was monitored for a period of about 2 months. The influent phosphate concentration was in the range of 16-19 mg/L, and ammonium concentration was in the range of 65-78 mg/L. The average nutrient removal efficiency observed during the study period were 95.2% for phosphate and 88.7% for ammonium, with mean final effluent concentration of 0.91, and 8.74 mg/L, respectively. Furthermore, the subsequent release of nutrient from the saturated filter media, after completion of treatment process has been undertaken in this study and thin layer funnel analytical test results reveal the slow nutrient release nature of spent dolochar, thereby, recommending its potential agricultural application. Thus, the bio-filter displays immense prospective for treating real eutrophic wastewater, significantly decreasing the level of nutrients and keeping the effluent nutrient concentrations at par with the permissible limit and more importantly, facilitating the conversion of the waste materials into usable ones.Keywords: ammonium removal, phosphate removal, multi-stage bio-filter, dolochar
Procedia PDF Downloads 1941406 Mineralogical Characteristics of Phosphates from the Djebel Onk Deposits: Treatment and Valorization of Co-Products
Authors: Samira Tlili, Amina Grairia, Sihem Benayache, Saida Bouyegh, Sabrina Ladjama, Abdelmoumen Guedri
Abstract:
Phosphorites from Djebel Onk Tebessa/Algeria deposit contain a CaO of 50-52 wt. % and P₂O₅ level of ≥ 30.20 wt. %. The microstructure revealed using a spectroscopy electronic microscope (SEM) consists of phosphate granules with an ovular form. In this investigation, we have identified phosphate with varying particle sizes using mineralogical methods. The phosphogypsum formed by the mineralization of natural phosphate has also been discovered. This co-product was formed during the attack on natural phosphates by sulfuric acid. This study demonstrated the effectiveness of the thermoanalytical technique of differential scanning calorimetry (DSC), X-ray diffraction, and EDS/MEB analysis. FTIR analyses also validated the identification of mineral phases with the observation of bands from structural phosphate groups.Keywords: phosphate, Djebel Onk deposit, mineralogy, valorization, phosphogypsum
Procedia PDF Downloads 231405 Influence of Iron Ore Mineralogy on Cluster Formation inside the Shaft Furnace
Authors: M. Bahgat, H. A. Hanafy, S. Lakdawala
Abstract:
Clustering phenomenon of pellets was observed frequently in shaft processes operating at higher temperatures. Clustering is a result of the growth of fibrous iron precipitates (iron whiskers) that become hooked to each other and finally become crystallized during the initial stages of metallization. If the pellet clustering is pronounced, sometimes leads to blocking inside the furnace and forced shutdown takes place. This work clarifies further the relation between metallic iron whisker growth and iron ore mineralogy. Various pellet sizes (6 – 12.0 & +12.0 mm) from three different ores (A, B & C) were (completely and partially) reduced at 985 oC with H2/CO gas mixture using thermos-gravimetric technique. It was found that reducibility increases by decreasing the iron ore pellet’s size. Ore (A) has the highest reducibility than ore (B) and ore (C). Increasing the iron ore pellet’s size leads to increase the probability of metallic iron whisker formation. Ore (A) has the highest tendency for metallic iron whisker formation than ore (B) and ore (C). The reduction reactions for all iron ores A, B and C are mainly controlled by diffusion reaction mechanism.Keywords: shaft furnace, cluster, metallic iron whisker, mineralogy, ferrous metallurgy
Procedia PDF Downloads 4711404 Scanning Electrochemical Microscopy Studies of Magnesium-Iron Galvanic Couple
Authors: Akram Alfantazi, Tirdad Nickchi
Abstract:
Magnesium galvanic corrosion plays an important role in the commercialization of Mg alloys in the automobile industry. This study aims at visualizing the electrochemical activity of the magnesium surface being coupled with pure iron in sulfate-chloride solutions. Scanning electrochemical microscopy was used to monitor the chemical activity of the surface and the data was compared with the conventional corrosion results such as potentiodynamic polarization, linear polarization, and immersion tests. The SECM results showed that the chemical reactivity of Mg is higher than phosphate-permanganate-coated Mg. Regions in the vicinity of the galvanic couple boundary are very active in the magnesium phase and fully protected in the iron phase. Scanning electrochemical microscopy results showed that the conversion coating provided good corrosion resistance for magnesium in the short-term but fails at long-term testing.Keywords: corrosion, galvanic corrosion, magnesium, scanning electrochemical microscopy
Procedia PDF Downloads 2881403 Investigation of the Fading Time Effects on Microstructure and Mechanical Properties in Vermicular Cast Iron
Authors: Mehmet Ekici
Abstract:
In this study, the fading time affecting the mechanical properties and microstructures of vermicular cast iron were studied. Pig iron and steel scrap weighing about 12 kg were charged into the high-frequency induction furnace crucible and completely melted for production of vermicular cast iron. The slag was skimmed using a common flux. After fading time was set at 1. 3 and 5 minutes. In this way, three vermicular cast iron was produced that same composition but different phase structures. The microstructure of specimens was investigated, and uni-axial tensile test and the Charpy impact test were performed, and their micro-hardness measurements were done in order to characterize the mechanical behaviours of vermicular cast iron.Keywords: vermicular cast iron, fading time, hardness, tensile test and impact test
Procedia PDF Downloads 3491402 Bioavailability of Iron in Some Selected Fiji Foods using In vitro Technique
Authors: Poonam Singh, Surendra Prasad, William Aalbersberg
Abstract:
Iron the most essential trace element in human nutrition. Its deficiency has serious health consequences and is a major public health threat worldwide. The common deficiencies in Fiji population reported are of Fe, Ca and Zn. It has also been reported that 40% of women in Fiji are iron deficient. Therefore, we have been studying the bioavailability of iron in commonly consumed Fiji foods. To study the bioavailability it is essential to assess the iron contents in raw foods. This paper reports the iron contents and its bioavailability in commonly consumed foods by multicultural population of Fiji. The food samples (rice, breads, wheat flour and breakfast cereals) were analyzed by atomic absorption spectrophotometer for total iron and its bioavailability. The white rice had the lowest total iron 0.10±0.03 mg/100g but had high bioavailability of 160.60±0.03%. The brown rice had 0.20±0.03 mg/100g total iron content but 85.00±0.03% bioavailable. The white and brown breads showed the highest iron bioavailability as 428.30±0.11 and 269.35 ±0.02%, respectively. The Weetabix and the rolled oats had the iron contents 2.89±0.27 and 1.24.±0.03 mg/100g with bioavailability of 14.19±0.04 and 12.10±0.03%, respectively. The most commonly consumed normal wheat flour had 0.65±0.00 mg/100g iron while the whole meal and the Roti flours had 2.35±0.20 and 0.62±0.17 mg/100g iron showing bioavailability of 55.38±0.05, 16.67±0.08 and 12.90±0.00%, respectively. The low bioavailability of iron in certain foods may be due to the presence of phytates/oxalates, processing/storage conditions, cooking method or interaction with other minerals present in the food samples.Keywords: iron, bioavailability, Fiji foods, in vitro technique, human nutrition
Procedia PDF Downloads 5311401 Effects of Bacteria on Levels of AFM1 in Phosphate Buffer at Different Level of Energy Source
Authors: Ali M. Elgerbi, Obied A. Alwan, Al-Taher O. Alzwei, Abdurrahim A. Elouzi
Abstract:
The binding of AFM1 to bacteria in phosphate buffer solution depended on many factors such as: availability of energy, incubation period, species and strain of bacteria. Increase in concentration of sugar showed higher removal of AFM1 and faster than in phosphate buffer alone. With 1.0% glucose lactic acid bacteria and bifidobacteria showed toxin removal ranging from 7.7 to 39.7% whereas with 10.0% glucose the percentage removal was 21.8 to 45.4% at 96 hours of incubation.Keywords: aflatoxin M1, lactic acid bacteria, bifidobacteria , binding, phosphate buffer
Procedia PDF Downloads 5071400 Removal of Iron (II) from Wastewater in Oil Field Using 3-(P-Methyl) Phenyl-5-Thionyl-1,2,4-Triazoline Assembled on Silver Nanoparticles
Authors: E. M. S. Azzam, S. A. Ahmed, H. H. Mohamed, M. A. Adly, E. A. M. Gad
Abstract:
In this work we prepared 3-(p-methyl) phenyl-5-thionyl-1,2,4-triazoline (C1). The nanostructure of the prepared C1 compound was fabricated by assembling on silver nanoparticles. The UV and TEM analyses confirm the assembling of C1 compound on silver nanoparticles. The effect of C1 compound on the removal of Iron (II) from Iron contaminated samples and industrial wastewater samples (produced water from oil processing facility) were studied before and after their assembling on silver nanoparticles. The removal of Iron was studied at different concentrations of FeSO4 solution (5, 14 and 39 mg/l) and field sample concentration (661 mg/l). In addition, the removal of Iron (II) was investigated at different times. The Prepared compound and its nanostructure with AgNPs show highly efficient in removing the Iron ions. Quantum chemical descriptors using DFT was discussed. The output of the study pronounces that the C1 molecule can act as chelating agent for Iron (II).Keywords: triazole derivatives, silver nanoparticles, iron (II), oil field
Procedia PDF Downloads 6581399 The Hydrolysis of Phosphate Esters Can Be Enhanced by Intramolecular Hydrogen Bonding
Authors: Mohamed S. Sasi
Abstract:
The research project aim is to study the hydrolysis of 8-diethylphosphate-1-naphthalenol with hydroxylamine in water. 8-diethylphosphate-1-naphthalenol, 1 was successfully synthesized and its rate of reaction with hydroxylamine was studied at 60°C. Pseudo first order behavior was observed. The rate of P-O cleavage of 1 at 60°C (7.43 x 10-3 M-1s-1) was found to be 178 fold and 7 fold slower than diethyl 8-dimethylamino-1-naphthyl phosphate, 3 at 60°C (1.32 M-1s-1) and diethyl 8-amino-1-naphthyl phosphate, 2 at 90 °C (5.5 x 10-2 M-1s-1) respectively. The rate of P-O cleavage of 1 with hydroxylamine was found to be faster than that of 4-chlorophenyl-1-cyclopropylphosphate triester, 5 where the reaction was too slow to observe at 60°C.Keywords: phosphate esters, intramolecular hydrogen bonding
Procedia PDF Downloads 4301398 Tricalcium Phosphate-Chitosan Composites for Tissue Engineering Applications
Authors: G. Voicu, C. D. Ghitulica, A. Cucuruz, C. Busuioc
Abstract:
In the field of tissue engineering, the compositional and microstructural features of the employed materials play an important role, with implications on the mechanical and biological behaviour of the medical devices. In this context, the development of calcium phosphate-natural biopolymer composites represents a choice of many scientific groups. Thus, tricalcium phosphate powders were synthesized by a wet method, namely co-precipitation, starting from high purity reagents. Moreover, the substitution of calcium with magnesium have been approached, in the 5-10 wt.% range. Afterwards, the phosphate powders were integrated into two types of composites with chitosan, different from morphological point of view. First, 3D porous scaffolds were obtained by a freeze-drying procedure. Second, uniform compact films were achieved by film casting. The influence of chitosan molecular weight (low, medium and high), as well as phosphate powder to polymer ratio (1:1 and 1:2) on the morphological properties, were analysed in detail. In conclusion, the reported biocomposites, prepared by a straightforward route are suitable for bone substitution or repairing applications.Keywords: bone reconstruction, chitosan, composite scaffolds, tricalcium phosphate
Procedia PDF Downloads 2441397 Synthesis and Characterization of Iron Modified Geopolymer and Its Resistance against Chloride and Sulphate
Authors: Noor-ul-Amin, Lubna Nawab, Sabiha Sultana
Abstract:
Geopolymer with different silica to alumina ratio with iron have been synthesized using sodium silicate, aluminum, and iron salts as a source of silica, alumina and iron source, and sodium/potassium hydroxide as an alkaline medium. The iron source will be taken from iron (III) salts and laterite clay samples. Laterite has been used as a natural source of iron in modified geopolymer. The synthesized iron modified geopolymer was submitted to the different aggressive environment, including chloride and sulphate solutions in different concentration. Different experimental techniques, including XRF, XRD, and FTIR, were used to study the bonding nature and effect of aggressive environment on geopolymer. The major phases formed during geopolymerization are sodalite (Na₄Al₃Si₃O₁₂Cl), albite (NaAlSi₃O₈), hematite (Fe₂O₃), and chabazite as confirmed from the XRD results. The resulting geopolymer showed greater resistance to sulphate and chloride as compared to the normal geopolymer.Keywords: modified geopolymer, laterite, chloride, sulphate
Procedia PDF Downloads 1561396 Synthesis of Bimetallic Fe/Cu Nanoparticles with Different Copper Loading Ratios
Authors: May Thant Zin, Josephine Borja, Hirofumi Hinode, Winarto Kurniawan
Abstract:
Nanotechnology has multiple and enormous advantages for all application. Therefore, this research is carried out to synthesize and characterize bimetallic iron with copper nano-particles. After synthesizing nano zero valent iron by reduction of ferric chloride by sodium borohydride under nitrogen purging environment, bimetallic iron with copper nanoparticles are synthesized by varying different loads of copper chloride. Due to different standard potential (E0) values of copper and iron, copper is coupled with iron at (Cu to Fe ratio of 1:5, 1:6.7, 1:10, 1:20). It is found that the resulted bimetallic Fe/Cu nanoparticles are composing phases of iron and copper. According to the diffraction patterns indicating the state of chemical combination of the bimetallic nanoparticles, the particles are well-combined and crystalline sizes are less than 1000 Ao (or 100 nm). Specifically, particle sizes of synthesized bimetallic Fe/Cu nanoparticles are ranging from 44.583 nm to 85.149 nm. Procedia PDF Downloads 4461395 High Phosphate-Containing Foods and Beverages: Perceptions of the Future Healthcare Providers on Their Harmful Effect in Excessive Consumption
Authors: ATM Emdadul Haque
Abstract:
Phosphorus is an essential nutrient which is regularly consumed with food and exists in the body as phosphate. Phosphate is an important component of cellular structures and needed for bone mineralization. Excessive accumulation of phosphate is an important driving factor of mortality in chronic renal failure patients; of relevance, these patients are usually provided health care by doctors, nurses, and pharmacists. Hence, this study was planned to determine the level of awareness of the future healthcare providers about the phosphate-containing foods and beverages and to access their knowledge on the harmful effects of excess phosphate consumption. A questionnaire was developed and distributed among the year-1 medical, nursing and pharmacy students. 432 medical, nursing and pharmacy students responded with age ranging from 18-24 years. About 70% of the respondents were female with a majority (90.7%) from Malay ethnicity. Among the respondents, 29.9% were medical, 35.4% were the pharmacy and 34.7% were nursing students. 79.2% students knew that phosphate was an important component of the body, but only 61.8% knew that consuming too much phosphate could be harmful to the body. Despite 97% of the students knew that carbonated soda contained high sugar, surprisingly 77% of them did not know the presence of high phosphate in the same soda drinks; in the similar line of observation, 67% did not know the presence of it in the fast food. However, it was encouraging that 94% of the students wanted to know more about the effects of phosphate consumption, 74.3% were willing to give up drinking soda and eating fast food, and 52% considered taking green coconut water instead of soda drinks. It is, therefore, central to take an educational initiative to increase the awareness of the future healthcare providers about phosphate-containing food and its harmful effects in excessive consumptions.Keywords: high phosphate containing foods and beverages, excessive consumption, future health care providers, phosphorus
Procedia PDF Downloads 3701394 Utilization of Sorghum and White Bean Flour for the Production of Gluten Free and Iron Rich Cookies
Authors: Tahra Elobeid, Emmerich Berghofer
Abstract:
The aim of this study is to find innovative approaches for the production of iron rich foods using natural iron sources. The vehicle used for fortification was sorghum whereas the iron fortificant was white bean. Fortified sorghum cookies were produced from five different mixtures; iron content, iron bioavailability, cookie texture and acceptability were measured. Cookies were prepared from the three fortified flours; 90% sorghum + 10% white bean (S9WB1), 75% sorghum + 25% white bean (S3WB1), 50% sorghum + 50% white bean (S1WB1) and 100% sorghum and 100% white bean. The functional properties gave good results in all the formulations. Statistical analysis of the iron content in the five different cookies showed that there was significant difference at the 95% confidence level (ANOVA). The iron content in all the recipes including the 100% sorghum improved, the increase ranging from 112% in 100% sorghum cookies to 476% in 100% white bean cookies. This shows that the increase in the amount of white bean used for fortification leads to the improvement of the iron content of cookies. The bioavailability of iron ranged from 21.3% in 100% sorghum to 28.6% in 100% white bean cookies. In the 100% sorghum cookies the iron bioavailability increased with reference to raw sorghum due to the addition of eggs. Bioavailability of iron in raw sorghum is 16.2%, therefore the percentage increase ranged from 5.1% to 28.6%. The cookies prepared from 10% white bean (S9WB1) scored the lowest 3.7 in terms of acceptability. They were the least preferred due to their somewhat soft texture. The 30% white bean cookies (S3WB1) gave results comparable to the 50% (S1WB1) and 100% white bean cookies. Cookies prepared with high percentage of white bean (50% and 100% white bean) gave the best results. Therefore cookie formulations from sorghum and white bean are successful in improving the iron status of anaemic individuals.Keywords: sorghum, white bean, iron content, bioavailable iron, cookies
Procedia PDF Downloads 4171393 Sintered Phosphate Cement for HLW Encapsulation
Authors: S. M. M. Nelwamondo, W. C. M. H. Meyer, H. Krieg
Abstract:
The presence of volatile radionuclides in high level waste (HLW) in the nuclear industry limits the use of high temperature encapsulation technologies (glass and ceramic). Chemically bonded phosphate cement (CBPC) matrixes can be used for encapsulation of low level waste. This waste form is however not suitable for high level waste due to the radiolysis of water in these matrixes. In this research, the sintering behavior of the magnesium potassium phosphate cement waste forms was investigated. The addition of sintering aids resulted in the sintering of these phosphate cement matrixes into dense monoliths containing no water. Experimental evidence will be presented that this waste form can now be considered as a waste form for volatile radionuclides and high level waste as radiation studies indicated no chemical phase transition or physical degradation of this waste form.Keywords: chemically bonded phosphate cements, HLW encapsulation, thermal stability, radiation stability
Procedia PDF Downloads 6381392 Assessment of the Physical and Chemical Characteristics of Ugbogui River, Edo State, Nigeria
Authors: Iyagbaye O. Rich, Omoigberale O. Michael, Iyagbaye A. Louis
Abstract:
The physical, chemical parameters and some trace contents of Ugbogui in Edo State, Nigeria were investigated from August 2015 to April 2016. Four stations were studied from upstream to downstream using standard methods. A total of thirty-three (33) physical and chemical characteristics and trace metal contents were examined; Air and water temperatures, depth, transparency, colour, turbidity, flow velocity, pH, total alkalinity, conductivity and dissolved solids etc. Other includes dissolved oxygen, oxygen saturation, biochemical oxygen demand, chloride, phosphate, sodium, nitrate, sulphate, potassium, calcium, magnesium, iron, lead, copper, zinc, nickel, cadmium, vanadium and chromium. Eleven (11) parameters exhibited clear seasonal variations. However, there were high significant differences (p < 0.01) in the values of depth, colour, total suspended solid, biochemical oxygen demand, chemical oxygen demand, chloride, bicarbonate, phosphate, sulphate, iron, manganese, zinc, copper, chromium and cadmium among the stations. The anthropogenic activities had negatively impacted at station 3 of the river, although most of the recorded values were still within permissible limits.Keywords: anthropogenic activities, Nigeria, permissible limits, physical and chemical parameters, trace metal, water quality
Procedia PDF Downloads 1271391 Prevalence of Overweight and Obesity in Iron-Deficient Iranian Teenagers Girls
Authors: Eftekhari M. H., Mozaffari-Khosravi H., Shidfar F.
Abstract:
Background: Many Iranian adolescent girls are iron deficient, but it is unclear whether the iron deficiency is associated with other nutritional risk indicators. Objective: we aimed to investigate the association between iron deficiency and weight status (measured as BMI) among a reprehensive sample of teenage girls. Methods: A cross-sectional study was performed in a region of southern I.R.Iran. One hundred eighty-seven iron-deficient participants (aged between 11 to 14) were selected by systematic random sampling among all students in grades 1 to 3 from high schools for girls. We assayed hemoglobin, hematocrit, serum ferritin, iron and total iron binding capacity and measured weight and height. Body mass index was calculated according to age and gender-specific BMI growth charts for children 2 to 20 years of age. Results: 13% were at risk for being overweight and 8.3% were overweight. The severity of iron deficiency increased as BMI increased from normal to at risk for overweight and overweight. Iron deficiency anemia was most prevalent among overweight adolescents than at risk for overweight and normal weight adolescents (28%, 18%, and 13%, respectively). Conclusions: The results of this study showed an inverse association of BMI with serum ferritin. Overweight adolescents demonstrated an increased prevalence of anemia. Because of the potentially harmful effects of iron deficiency, obese adolescents should be routinely screened and treated as necessary.Keywords: adolescent, over weight, iron deficiency, Iran
Procedia PDF Downloads 1401390 Phosphate Capture from Sewage by Hafnium-Modified Fe₃O₄@SiO₂ Superparamagnetic Nanoparticles: Adsorption Capacity, Selectivity, Reusability Analysis and Mechanistic Insights
Authors: Qian Zhao
Abstract:
With global increasing demand for phosphorus and intensively depleting reserves, it is urgent need to explore innovative approaches towards capturing phosphate from sewage, which is also an effective way to reduce phosphate contamination and avoid eutrophication of water bodies. In the present article, the superparamagnetic nano-sorbents containing Fe₃O₄ core and hafnium-modified MgAl/MgFe layered double hydroxides shell (abbreviated as MgAlHf-NP and MgFeHf-NP) was developed using a simple and low-cost synthesis protocol. The obtained Hf-coated nano-materials showed well-defined crystal structure and sufficient saturation magnetization and exhibited higher adsorption capacity for phosphate. Meanwhile, high selectivity was also confirmed since coexisting foreign anions and biomacromolecules showed little competitive effect on phosphate adsorption. The enhancement via doping with Hf should be explained by the stronger ligand complexation built by the pair of hard acid Hf ion and hard base phosphate that matched up the bonding preferences. Sufficient OH⁻ concentration and clear pH shift during the desorption/regeneration allowed for regeneration rate of higher than 90% after 5 cycles of adsorption desorption. This article attempts to provide a competitive candidate for phosphate-capture, which is highly effective, easily separable and repeatedly usable.Keywords: phosphate recovery, nanoparticles, superparamagnetic, adsorption, reusability
Procedia PDF Downloads 141