1032 Effect of Different Carbon Fabric Orientations on the Fracture Properties of Carbon Fabric Reinforced Polymer Composites

Authors: S. F. Halim, H. F. Naguib, S. N. Lawandy, R. S. Hegazy, M. N. Baheg

Abstract:

The main drawbacks of the traditional carbon fabric reinforced epoxy resin (CFRP) are low strain failure, delamination between composites layers, and low impact resistance due to the brittleness of epoxy resin. The aim of this study is to enhance the fracture properties of the CFRP composites laminates via the variation of composite's designs. A series of composites were fabricated in which bidirectional (00/900) carbon fabric (CF) layers were laid inside the resin matrix with orientation codes as F1 [(00, 900)/ (00, 900)], F2 [(900, 00)/ (00, 900)] and F3 [(00,900)/ (900, 00). The mechanical and dynamic properties of the composites were estimated. In addition, the morphology of samples surface was examined by scanning electron microscope (SEM) after impact fracture. The results revealed that the CFRP properties could be tailored fitting specific applications by controlling the fabric orientation inside the CFRP composite design. F2 orientation [(900, 00)/ (00.900)] showed the highest tensile and flexural strength values. On the other hand, the impact strength values of composites were in the order F1 > F2 > F3. The storage modulus, loss modulus, and glass transition temperature Tg values obtained from the dynamic mechanical analysis (DMA) examination was in the order F1 > F2 > F3. The variation in the properties of the composite was clearly explained by the SEM micrographs as the failure of F3 orientation properties was referred to as the complete breakage of the CF layers upon fracture.

Keywords: carbon fiber, CFRP, composites, epoxy resins, flexural strength

Procedia PDF Downloads 98
1031 Laser-TIG Welding-Brazing for Dissimilar Metals between Aluminum Alloy and Steel

Authors: Xiangfang Xu, Bintao Wu, Yugang Miao, Duanfeng Han

Abstract:

Experiments were conducted on 5A06 aluminum alloy and Q235 steel using the laser-TIG hybrid heat source welding-brazing method to realize the reliable connection of Al/Fe dissimilar metals and the welding characteristics were analyzed. It was found that the joints with uniform seam and high tensile strength could be obtained using such a method, while the welding process demanded special welding parameters. Spectrum measurements showed that the Al and Fe atoms diffused more thoroughly at the brazing interface and formed a 3μm-thick intermetallic compound layer at the Al/Fe joints brazed connection interface. Shearing tests indicated that the shearing strength of the Al/Fe welding-brazed joint was 165MPa. The fracture occurred near the melting zone of aluminum alloy, which belonged to the mixed mode with the ductile fracture as the base and the brittle fracture as the supplement.

Keywords: Al/Fe dissimilar metals, laser-TIG hybrid heat source, shearing strength, welding-brazing method

Procedia PDF Downloads 358
1030 Knowledge and Capabilities of Primary Caregivers in Providing Quality Care for Elderly Patients with Post- Operative Hip Fracture, Songklanagarind Hospital

Authors: Manee Hasap, Mongkolchai Hasap, Tasanee Nasae

Abstract:

The purpose of this study was to evaluate the primary caregivers’ knowledge and capabilities for providing quality care to be hospitalized post-hip fracture surgery elderly patients. The theoretical framework of the study was derived from the concepts of dependent care agency in Orem’s Self-Care theory, and family care provision for the elderly and chronically ill patients. 59 subjects were purposively selected. The subjects were primary caregivers of post-operated hip fracture elderly patients who had been admitted to the Orthopaedic Ward of Songklanagarind Hospital. Demographic data of the caregivers and patients were collected by non-participant observation using the evaluation and recording forms. The reliability of caregivers’ knowledge measurement (0.86) was obtained by KR-20 and that of caregivers’ capabilities for post-operative care evaluation form (0.97) obtained from 2 observers by interrater reliability. The data were analyzed using descriptive statistic, which were frequency, percentage, mean, and standard deviation. The result of this study indicated that elderly patients with post-hip fracture surgery had many pre-discharge self care limitations. Approximately, 75% of the caregivers had knowledge to respond to patient’s essential needs at a high level, while the rest (25%) had this knowledge a moderate level. For observation, 57.63% of the subjects had capabilities in care practice at a moderate level; 28.81% had capabilities in care practice at a high level, while 13.56% had at a low level. The result of this study can be used as basic information for patients and caregivers capabilities developing plan especially, providing patients’ activities, accident surveillance and complications prevention for a good life quality of elderly patients after hip surgery both hospitalization and rehabilitation at home.

Keywords: care givers’ knowledge, care givers’ capabilities, elderly hip fracture patients, patients

Procedia PDF Downloads 529
1029 Evaluation of Bone and Body Mineral Profile in Association with Protein Content, Fat, Fat-Free, Skeletal Muscle Tissues According to Obesity Classification among Adult Men

Authors: Orkide Donma, Mustafa M. Donma

Abstract:

Obesity is associated with increased fat mass as well as fat percentage. Minerals are the elements, which are of vital importance. In this study, the relationships between body as well as bone mineral profile and the percentage as well as mass values of fat, fat-free portion, protein, skeletal muscle were evaluated in adult men with normal body mass index (N-BMI), and those classified according to different stages of obesity. A total of 103 adult men classified into five groups participated in this study. Ages were within 19-79 years range. Groups were N-BMI (Group 1), overweight (OW) (Group 2), first level of obesity (FLO) (Group 3), second level of obesity (SLO) (Group 4) and third level of obesity (TLO) (Group 5). Anthropometric measurements were performed. BMI values were calculated. Obesity degree, total body fat mass, fat percentage, basal metabolic rate (BMR), visceral adiposity, body mineral mass, body mineral percentage, bone mineral mass, bone mineral percentage, fat-free mass, fat-free percentage, protein mass, protein percentage, skeletal muscle mass and skeletal muscle percentage were determined by TANITA body composition monitor using bioelectrical impedance analysis technology. Statistical package (SPSS) for Windows Version 16.0 was used for statistical evaluations. The values below 0.05 were accepted as statistically significant. All the groups were matched based upon age (p > 0.05). BMI values were calculated as 22.6 ± 1.7 kg/m2, 27.1 ± 1.4 kg/m2, 32.0 ± 1.2 kg/m2, 37.2 ± 1.8 kg/m2, and 47.1 ± 6.1 kg/m2 for groups 1, 2, 3, 4, and 5, respectively. Visceral adiposity and BMR values were also within an increasing trend. Percentage values of mineral, protein, fat-free portion and skeletal muscle masses were decreasing going from normal to TLO. Upon evaluation of the percentages of protein, fat-free portion and skeletal muscle, statistically significant differences were noted between NW and OW as well as OW and FLO (p < 0.05). However, such differences were not observed for body and bone mineral percentages. Correlation existed between visceral adiposity and BMI was stronger than that detected between visceral adiposity and obesity degree. Correlation between visceral adiposity and BMR was significant at the 0.05 level. Visceral adiposity was not correlated with body mineral mass but correlated with bone mineral mass whereas significant negative correlations were observed with percentages of these parameters (p < 0.001). BMR was not correlated with body mineral percentage whereas a negative correlation was found between BMR and bone mineral percentage (p < 0.01). It is interesting to note that mineral percentages of both body as well as bone are highly affected by the visceral adiposity. Bone mineral percentage was also associated with BMR. From these findings, it is plausible to state that minerals are highly associated with the critical stages of obesity as prominent parameters.

Keywords: bone, men, minerals, obesity

Procedia PDF Downloads 86
1028 The Ductile Fracture of Armor Steel Targets Subjected to Ballistic Impact and Perforation: Calibration of Four Damage Criteria

Authors: Imen Asma Mbarek, Alexis Rusinek, Etienne Petit, Guy Sutter, Gautier List

Abstract:

Over the past two decades, the automotive, aerospace and army industries have been paying an increasing attention to Finite Elements (FE) numerical simulations of the fracture process of their structures. Thanks to the numerical simulations, it is nowadays possible to analyze several problems involving costly and dangerous extreme loadings safely and at a reduced cost such as blast or ballistic impact problems. The present paper is concerned with ballistic impact and perforation problems involving ductile fracture of thin armor steel targets. The target fracture process depends usually on various parameters: the projectile nose shape, the target thickness and its mechanical properties as well as the impact conditions (friction, oblique/normal impact...). In this work, the investigations are concerned with the normal impact of a conical head-shaped projectile on thin armor steel targets. The main aim is to establish a comparative study of four fracture criteria that are commonly used in the fracture process simulations of structures subjected to extreme loadings such as ballistic impact and perforation. Usually, the damage initiation results from a complex physical process that occurs at the micromechanical scale. On a macro scale and according to the following fracture models, the variables on which the fracture depends are mainly the stress triaxiality ƞ, the strain rate, temperature T, and eventually the Lode angle parameter Ɵ. The four failure criteria are: the critical strain to failure model, the Johnson-Cook model, the Wierzbicki model and the Modified Hosford-Coulomb model MHC. Using the SEM, the observations of the fracture facies of tension specimen and of armor steel targets impacted at low and high incident velocities show that the fracture of the specimens is a ductile fracture. The failure mode of the targets is petalling with crack propagation and the fracture facies are covered with micro-cavities. The parameters of each ductile fracture model have been identified for three armor steels and the applicability of each criterion was evaluated using experimental investigations coupled to numerical simulations. Two loading paths were investigated in this study, under a wide range of strain rates. Namely, quasi-static and intermediate uniaxial tension and quasi-static and dynamic double shear testing allow covering various values of stress triaxiality ƞ and of the Lode angle parameter Ɵ. All experiments were conducted on three different armor steel specimen under quasi-static strain rates ranging from 10-4 to 10-1 1/s and at three different temperatures ranging from 297K to 500K, allowing drawing the influence of temperature on the fracture process. Intermediate tension testing was coupled to dynamic double shear experiments conducted on the Hopkinson tube device, allowing to spot the effect of high strain rate on the damage evolution and the crack propagation. The aforementioned fracture criteria are implemented into the FE code ABAQUS via VUMAT subroutine and they were coupled to suitable constitutive relations allow having reliable results of ballistic impact problems simulation. The calibration of the four damage criteria as well as a concise evaluation of the applicability of each criterion are detailed in this work.

Keywords: armor steels, ballistic impact, damage criteria, ductile fracture, SEM

Procedia PDF Downloads 287
1027 Optimization of the Numerical Fracture Mechanics

Authors: H. Hentati, R. Abdelmoula, Li Jia, A. Maalej

Abstract:

In this work, we present numerical simulations of the quasi-static crack propagation based on the variation approach. We perform numerical simulations of a piece of brittle material without initial crack. An alternate minimization algorithm is used. Based on these numerical results, we determine the influence of numerical parameters on the location of crack. We show the importance of trying to optimize the time of numerical computation and we present the first attempt to develop a simple numerical method to optimize this time.

Keywords: fracture mechanics, optimization, variation approach, mechanic

Procedia PDF Downloads 575
1026 Osteoarticular Manifestations and Abnormalities of Bone Metabolism in Celiac Disease

Authors: Soumaya Mrabet, Imen Akkari, Amira Atig, Elhem Ben Jazia

Abstract:

Introduction: Celiac disease (CD) is a chronic autoimmune inflammatory enteropathy caused by gluten. The clinical presentation is very variable. Malabsorption in the MC is responsible for an alteration of the bone metabolism. Our purpose is to study the osteoarticular manifestations related to this condition. Material and methods: It is a retrospective study of 41 cases of CD diagnosed on clinical, immunological, endoscopic and histological arguments, in the Internal Medicine and Gastroenterology Department of Farhat Hached Hospital between September 2005 and January 2016. Results: Osteoarticular manifestations were found in 9 patients (22%) among 41 patients presenting CD. These were 7 women and 2 men with an average age of 35.7 years (25 to 67 years). These manifestations were revelatory of CD in 3 cases. Abdominal pain and diarrhea were present in 6 cases. Inflammatory polyarthralgia of wrists and knees has been reported in 7 patients. Mechanical mono arthralgia was noted in 2 patients. Biological tests revealed microcytic anemia by iron deficiency in 7 cases, hypocalcemia in 5 cases, Hypophosphatemia in 3 cases and elevated alkaline phosphatases in 3 cases. Upper gastrointestinal endoscopy with duodenal biopsy found villous atrophy in all cases. In immunology, Anti-transglutaminase antibodies were positive in all patients, Anti-endomysium in 7 cases. Measurement of bone mineral density (BMD) by biphotonic X-ray absorptiometer with evaluation of the T-score and the Z-score was performed in Twenty patients (48.8%). It was normal in 7 cases (33%) and showed osteopenia in 5 patients (25%) and osteoporosis in 2 patients (10%). All patients were treated with a Gluten-free diet associated with vitamin D and calcium substitution in 5 cases. The evolution was favorable in all cases with reduction of bone pain and normalization of the phosphocalcic balance. Conclusion: The bone impact of CD is frequent but often asymptomatic. Patients with CD should be evaluated by the measurement of bone mineral density and monitored for calcium and vitamin D deficiencies.

Keywords: bone mineral density, celiac disease, osteoarticular manifestations, vitamin D and calcium

Procedia PDF Downloads 298
1025 Thermal Method Production of the Hydroxyapatite from Bone By-Products from Meat Industry

Authors: Agnieszka Sobczak-Kupiec, Dagmara Malina, Klaudia Pluta, Wioletta Florkiewicz, Bozena Tyliszczak

Abstract:

Introduction: Request for compound of phosphorus grows continuously, thus, it is searched for alternative sources of this element. One of these sources could be by-products from meat industry which contain prominent quantity of phosphorus compounds. Hydroxyapatite, which is natural component of animal and human bones, is leading material applied in bone surgery and also in stomatology. This is material, which is biocompatible, bioactive and osteoinductive. Methodology: Hydroxyapatite preparation: As a raw material was applied deproteinized and defatted bone pulp called bone sludge, which was formed as waste in deproteinization process of bones, in which a protein hydrolysate was the main product. Hydroxyapatite was received in calcining process in chamber kiln with electric heating in air atmosphere in two stages. In the first stage, material was calcining in temperature 600°C within 3 hours. In the next stage unified material was calcining in three different temperatures (750°C, 850°C and 950°C) keeping material in maximum temperature within 3.0 hours. Bone sludge: Bone sludge was formed as waste in deproteinization process of bones, in which a protein hydrolysate was the main product. Pork bones coming from the partition of meat were used as a raw material for the production of the protein hydrolysate. After disintegration, a mixture of bone pulp and water with a small amount of lactic acid was boiled at temperature 130-135°C and under pressure4 bar. After 3-3.5 hours boiled-out bones were separated on a sieve, and the solution of protein-fat hydrolysate got into a decanter, where bone sludge was separated from it. Results of the study: The phase composition was analyzed by roentgenographic method. Hydroxyapatite was the only crystalline phase observed in all the calcining products. XRD investigation was shown that crystallization degree of hydroxyapatite was increased with calcining temperature. Conclusion: The researches were shown that phosphorus content is around 12%, whereas, calcium content amounts to 28% on average. The conducted researches on bone-waste calcining at the temperatures of 750-950°C confirmed that thermal utilization of deproteinized bone-waste was possible. X-ray investigations were confirmed that hydroxyapatite is the main component of calcining products, and also XRD investigation was shown that crystallization degree of hydroxyapatite was increased with calcining temperature. Contents of calcium and phosphorus were distinctly increased with calcining temperature, whereas contents of phosphorus soluble in acids were decreased. It could be connected with higher crystallization degree of material received in higher temperatures and its stable structure. Acknowledgements: “The authors would like to thank the The National Centre for Research and Development (Grant no: LIDER//037/481/L-5/13/NCBR/2014) for providing financial support to this project”.

Keywords: bone by-products, bone sludge, calcination, hydroxyapatite

Procedia PDF Downloads 264
1024 Role of Vitamin D in Osseointegration of Dental Implant

Authors: Pouya Khaleghi

Abstract:

Dental implants are a successful treatment modality for restoring both function and aesthetics. Dental implant treatment has predictive results in the replacement of the lost teeth and has a high success rate even in the long term. The most important factor which is responsible for the positive course of implant treatment is the process of osseointegration between the implant structure and the host’s bone tissue. During recent years, many studies have focused on surgical and prosthetic factors, as well as the implant-related factors. However, implant failure still occurs despite the improvements that have led to the increased survival rate of dental implants, which suggests the possible role of some host-related risk factors. Vitamin D is a fat-soluble vitamin regulating calcium and phosphorus metabolism in tissues. The role of vitamin D in bone healing has been under investigation for several years. Vitamin D deficiency has also been associated with impaired and delayed callus formation and fractures healing; however, the role of vitamin D has not been clarified. Therefore, it is extremely important to study the phenomenon of a connection formed between bone tissue and the surface of a titanium implant and find correlations between the 25- hydroxycholecalciferol concentration in blood serum and the course of osseointegration. Because the processes of bone remodeling are very dynamic in the period of actual osseointegration, it is necessary to obtain the correct concentration of vitamin D3 metabolites in blood serum. In conclusion, the correct level of 25-hydroxycholecalciferol on the day of surgery and vitamin D deficiency treatment have a significant influence on the increase in the bone level at the implant site during the process of osseointegration assessed radiologically.

Keywords: implant, osseointegration, vitamin d, dental

Procedia PDF Downloads 141
1023 Risk of Fractures at Different Anatomic Sites in Patients with Irritable Bowel Syndrome: A Nationwide Population-Based Cohort Study

Authors: Herng-Sheng Lee, Chi-Yi Chen, Wan-Ting Huang, Li-Jen Chang, Solomon Chih-Cheng Chen, Hsin-Yi Yang

Abstract:

A variety of gastrointestinal disorders, such as Crohn’s disease, ulcerative colitis, and coeliac disease, are recognized as risk factors for osteoporosis and osteoporotic fractures. One recent study suggests that individuals with irritable bowel syndrome (IBS) might also be at increased risk of osteoporosis and osteoporotic fractures. Up to now, the association between IBS and the risk of fractures at different anatomic sites occurrences is not completely clear. We conducted a population-based cohort analysis to investigate the fracture risk of IBS in comparison with non-IBS group. We identified 29,505 adults aged ≥ 20 years with newly diagnosed IBS using the Taiwan National Health Insurance Research Database in 2000-2012. A comparison group was constructed of patients without IBS who were matched according to gender and age. The occurrence of fracture was monitored until the end of 2013. We analyzed the risk of fracture events to occur in IBS by using Cox proportional hazards regression models. Patients with IBS had a higher incidence of osteoporotic fractures compared with non-IBS group (12.34 versus 9.45 per 1,000 person-years) and an increased risk of osteoporotic fractures (adjusted hazard ratio [aHR] = 1.27, 95 % confidence interval [CI] = 1.20 – 1.35). Site specific analysis showed that the IBS group had a higher risk of fractures for spine, forearm, hip and hand than did the non-IBS group. With further stratification for gender and age, a higher aHR value for osteoporotic fractures in IBS group was seen across all age groups in males, but seen in elderly females. In addition, female, elderly, low income, hypertension, coronary artery disease, cerebrovascular disease, and depressive disorders as independent osteoporotic fracture risk factors in IBS patients. The IBS is considered as a risk factor for osteoporotic fractures, particularly in female individuals and fracture sites located at the spine, forearm, hip and hand.

Keywords: irritable bowel syndrome, fracture, gender difference, longitudinal health insurance database, public health

Procedia PDF Downloads 202
1022 A Method to Identify Areas for Hydraulic Fracturing by Using Production Logging Tools

Authors: Armin Shirbazo, Hamed Lamei Ramandi, Mohammad Vahab, Jalal Fahimpour

Abstract:

Hydraulic fracturing, especially multi-stage hydraulic fracturing, is a practical solution for wells with uneconomic production. The wide range of applications is appraised appropriately to have a stable well-production. Production logging tool, which is known as PLT in the oil and gas industry, is counted as one of the most reliable methods to evaluate the efficiency of fractures jobs. This tool has a number of benefits and can be used to prevent subsequent production failure. It also distinguishes different problems that occurred during well-production. In this study, the effectiveness of hydraulic fracturing jobs is examined by using the PLT in various cases and situations. The performance of hydraulically fractured wells is investigated. Then, the PLT is employed to gives more information about the properties of different layers. The PLT is also used to selecting an optimum fracturing design. The results show that one fracture and three-stage fractures behave differently. In general, the one-stage fracture should be created in high-quality areas of the reservoir to have better performance, and conversely, in three-stage fractures, low-quality areas are a better candidate for fracturing

Keywords: multi-stage fracturing, horizontal well, PLT, fracture length, number of stages

Procedia PDF Downloads 161
1021 Finite Element Analysis of Debonding Propagation in FM73 Joint under Static Loading

Authors: Reza Hedayati, Meysam Jahanbakhshi

Abstract:

In this work, Fracture Mechanics is used to predict crack propagation in the adhesive joining aluminum and composite plates. Three types of loadings and two types of glass-epoxy composite sequences: [0/90]2s and [0/45/-45/90]s are considered for the composite plate. Therefore, 2*3=6 cases are considered and their results are compared. The debonding initiation load, complete debonding load, crack face profile and load-displacement diagram have been compared for the six cases.

Keywords: adhesive joint, debonding, fracture, LEFM, APDL

Procedia PDF Downloads 562
1020 A Biomimetic Uncemented Hip Resurfacing Versus Various Biomaterials Hip Resurfacing Implants

Authors: Karima Chergui, Hichem Amrani, Hammoudi Mazouz, Fatiha Mezaache

Abstract:

Cemented femoral resurfacings have experienced a revival for younger and more active patients. Future developments have shown that the uncemented version eliminates failures related to cementing implants. A three-dimensional finite element method (FEM) simulation was carried out in order to exploit a new resurfacing prothesis design named MARMEL, proposed by a recent study with Co–Cr–Mo material, for comparing a hip uncemented resurfacing with a novel carbon fiber/polyamide 12 (CF/PA12) composite to other hip resurfacing implants with various bio materials. From FE analysis, the von Mises stress range for the Composite hip resurfacing was much lower than that in the other hip resurfacing implants used in this comparison. These outcomes showed that the biomimetic hip resurfacing had the potential to reduce stress shielding and prevent from bone fracture compared to conventional hip resurfacing implants.

Keywords: biomechanics, carbon–fibre polyamide 12, finite element analysis, hip resurfacing

Procedia PDF Downloads 297
1019 Effect of Institution Volume on Mortality and Outcomes in Osteoporotic Hip Fracture Care

Authors: J. Milton, C. Uzoigwe, O. Ayeko, B. Offorha, K. Anderson, R. G. Middleton

Abstract:

Background: We used the UK National Hip Fracture database to determine the effect of institution hip fracture case volume on hip fracture healthcare outcomes in 2019. Using logistic regression for each healthcare outcome, we compared the best performing 50 units with the poorest performing 50 units in order to determine if the unit volume was associated with performance for each particular outcome. Method: We analysed 175 institutions treating a total of 67,673 patients over the course of a year. Results: The number of hip fractures seen per unit ranged between 86 and 952. Larger units tendered to perform health assessments more consistently and mobilise patients more expeditiously post-operatively. Patients treated at large institutions had shorter lengths of stay. With regard to most other outcomes, there was no association between unit case volume and performance, notably compliance with the Best Practice Tariff, time to surgery, proportion of eligible patients undergoing total hip arthroplasty, length of stay, delirium risk, and pressure sore risk assessments. Conclusion: There is no relationship between unit volume and the majority of health care outcomes. It would seem that larger institutions tend to perform better at parameters that are dependent upon personnel numbers. However, where the outcome is contingent, even partially, on physical infrastructure capacity, there was no difference between larger and smaller units.

Keywords: institution volume, mortality, neck of femur fractures, osteoporosis

Procedia PDF Downloads 65
1018 Ilizarov's External Fixator. A Bone Regeneration Method Little Used in Africa. Our Experience of 20 Years in Cameroon.

Authors: Ibrahima Farikou, Kolontchang Gatchou Alberic Lionel, Tsiagadgui Jean Gustave, Ngo Yamben Marie-Ange, Handy Eone Daniel

Abstract:

Introduction: It was in 1956 that Ilizarov pioneered the concept of osteogenesis in distraction by the device that bears his name to help produce bone and soft tissue regeneration and bone consolidation. This technique is not widely used in Africa where, however, its applications are numerous (loss of bone substances, congenital or acquired malformations). Our goal is to bring the indications of Ilizarov's device back to our practice conditions. Methods: Our study was conducted in 2 hospitals over a period of 20 years. For the retrospective phase, this study included all complete usable records of patients operated on in the Ilizarov external fixator department, and for the prospective phase, all patients operated on in the departments with complete usable records. Our sample was consecutive and not exhaustive. Data were analyzed by SPSS software version 23.0. Results: A total of 52 patients were reviewed. The average age of our patients was 14.7 years. The sex ratio was 1.6 in favor of men. The lower limb was the most affected (49), with a predominance of the tibia (62.4%). The average elongation was 6.4 cm. Traumatic acquired pathologies (delayed union, malunion) represented 60.6%. The mean time to union was seven months. Correction of the limb length discrepancy or filling of loss of bone substance was obtained in 75% of cases. Functionally, 80.8% of the patients treated had regained autonomy at the end of treatment, but in 17.3% of the patients, pain and limping persisted. Conclusion: This technique should be popularized in Africa because the benefit that would accrue to patients is invaluable and would be an attractive alternative to many amputations sometimes carried out in Africa by despair.

Keywords: ilizarov, external fixator, limb lengthening, bone regeneration, africa

Procedia PDF Downloads 63
1017 To What Extent Does Physical Activity and Standard of Competition Affect Quantitative Ultrasound (QUS) Measurements of Bone in Accordance with Muscular Strength and Anthropometrics in British Young Males?

Authors: Joseph Shanks, Matthew Taylor, Foong Kiew Ooi, Chee Keong Chen

Abstract:

Introduction: Evidences of relationship between bone, muscle and standard of competition among young British population is limited in literature. The current literature recognises the independent and synergistic effects of fat free and fat mass as the stimulus for osteogenesis. This study assessed the extent to which physical activity (PA) and standard of competition (CS) influences quantitative ultrasound (QUS) measurements of bone on a cross-sectional basis accounting for muscular strength and anthropometrics in British young males. Methods: Pre-screening grouped 66 males aged 18-25 years into controls (n=33) and district level athletes (DLAs) (n=33) as well as low (n=21), moderate (n=23) and high (n=22) physical activity categories (PACs). All participants underwent QUS measurements of bone (4 sites, i.e. dominant distal radius (DR), dominant mid-shaft tibia (DT), non-dominant distal radius (NR) and non-dominant mid-shaft tibia (NT)), isokinetic strength tests (dominant and non-dominant knee flexion and extension) and anthropometric measurements. Results: There were no significant differences between any of the groups with respect to QUS measurements of bone at all sites with regards to PACs or CS. Significant higher isokinetic strength values were observed in DLAs than controls (p < 0.05), and higher than low PACs (p < 0.05) at 60o.s-1 of concentric and eccentric measurements. No differences in subcutaneous fat thickness were found between all the groups (CS or PACs). Percentages of body fat were significantly higher (p < .05) in low than high PACs and CS groups. There were significant positive relationships between non dominant radial speed of sound and fat free mass at both DR (r=0.383, p=0.001) and NR (r=0.319, p=0.009) sites in all participants. Conclusion: The present study findings indicated that muscular strength and body fat are closely related to physical activity level and standard of competition. However, bone health status reflected by quantitative ultrasound (QUS) measurements of bone is not related to physical activity level and standard of competition in British young males.

Keywords: bone, muscular strength, physical activity, standard of competition

Procedia PDF Downloads 487
1016 Fracture Behaviour of Functionally Graded Materials Using Graded Finite Elements

Authors: Mohamad Molavi Nojumi, Xiaodong Wang

Abstract:

In this research fracture behaviour of linear elastic isotropic functionally graded materials (FGMs) are investigated using modified finite element method (FEM). FGMs are advantageous because they enhance the bonding strength of two incompatible materials, and reduce the residual stress and thermal stress. Ceramic/metals are a main type of FGMs. Ceramic materials are brittle. So, there is high possibility of crack existence during fabrication or in-service loading. In addition, damage analysis is necessary for a safe and efficient design. FEM is a strong numerical tool for analyzing complicated problems. Thus, FEM is used to investigate the fracture behaviour of FGMs. Here an accurate 9-node biquadratic quadrilateral graded element is proposed in which the influence of the variation of material properties is considered at the element level. The stiffness matrix of graded elements is obtained using the principle of minimum potential energy. The implementation of graded elements prevents the forced sudden jump of material properties in traditional finite elements for modelling FGMs. Numerical results are verified with existing solutions. Different numerical simulations are carried out to model stationary crack problems in nonhomogeneous plates. In these simulations, material variation is supposed to happen in directions perpendicular and parallel to the crack line. Two special linear and exponential functions have been utilized to model the material gradient as they are mostly discussed in literature. Also, various sizes of the crack length are considered. A major difference in the fracture behaviour of FGMs and homogeneous materials is related to the break of material symmetry. For example, when the material gradation direction is normal to the crack line, even under applying the mode I loading there exists coupled modes I and II of fracture which originates from the induced shear in the model. Therefore, the necessity of the proper modelling of the material variation should be considered in capturing the fracture behaviour of FGMs specially, when the material gradient index is high. Fracture properties such as mode I and mode II stress intensity factors (SIFs), energy release rates, and field variables near the crack tip are investigated and compared with results obtained using conventional homogeneous elements. It is revealed that graded elements provide higher accuracy with less effort in comparison with conventional homogeneous elements.

Keywords: finite element, fracture mechanics, functionally graded materials, graded element

Procedia PDF Downloads 149
1015 The Effects of Inferior Tilt Fixation on a Glenoid Components in Reverse Shoulder-Arthroplasty

Authors: Soo Min Kim, Soo-Won Chae, Soung-Yon Kim, Haea Lee, Ju Yong Kang, Juneyong Lee, Seung-Ho Han

Abstract:

Reverse total shoulder arthroplasty (RTSA) has become an effective treatment option for cuff tear arthropathy and massive, irreparable rotator cuff tears and indications for its use are expanding. Numerous methods for optimal fixation of the glenoid component have been suggested, such as inferior overhang, inferior tilt, to maximize initial fixation and prevent glenoid component loosening. The inferior tilt fixation of a glenoid component has been suggested, which is expected to decrease scapular notching and to improve the stability of a glenoid component fixation in reverse total shoulder arthroplasty. Inferior tilt fixation of the glenoid component has been suggested, which can improve stability and, because it provides the most uniform compressive forces and imparts the least amount of tensile forces and micromotion, reduce the likelihood of mechanical failure. Another study reported that glenoid component inferior tilt improved impingement-free range of motion as well as minimized the scapular notching. Several authors have shown that inferior tilt of a glenoid component reduces scapular notching. However, controversy still exists regarding its importance in the literature. In this study the influence of inferior tilt fixation on the primary stability of a glenoid component has been investigated. Finite element models were constructed from cadaveric scapulae and glenoid components were implanted with neutral and 10° inferior tilts. Most previous biomechanical studies regarding the effect of glenoid component inferior tilt used a solid rigid polyurethane foam or sawbones block, not cadaveric scapulae, to evaluate the stability of the RTSA. Relative micromotions at the bone-glenoid component interface, and the distribution of bone stresses under the glenoid component and around the screws were analyzed and compared between neutral and 10° inferior tilt groups. Contact area between bone and screws and cut surface area of the cancellous bone exposed after reaming of the glenoid have also been investigated because of the fact that cancellous and cortical bone thickness vary depending on the resection level of the inferior glenoid bone. The greater relative micromotion of the bone-glenoid component interface occurred in the 10° inferior tilt group than in the neutral tilt group, especially at the inferior area of the bone-glenoid component interface. Bone stresses under the glenoid component and around the screws were also higher in the 10° inferior tilt group than in the neutral tilt group, especially at the inferior third of the glenoid bone surface under the glenoid component and inferior scapula. Thus inferior tilt fixation of the glenoid component may adversely affect the primary stability and longevity of the reverse total shoulder arthroplasty.

Keywords: finite element analysis, glenoid component, inferior tilt, reverse total shoulder arthroplasty

Procedia PDF Downloads 269
1014 Improved Mechanical Properties and Osteogenesis in Electrospun Poly L-Lactic Ultrafine Nanofiber Scaffolds Incorporated with Graphene Oxide

Authors: Weili Shao, Qian Wang, Jianxin He

Abstract:

Recently, the applications of graphene oxide in fabricating scaffolds for bone tissue engineering have been received extensive concern. In this work, poly l-lactic/graphene oxide composite nanofibers were successfully fabricated by electrospinning. The morphology structure, porosity and mechanical properties of the composite nanofibers were characterized using different techniques. And mouse mesenchymal stem cells were cultured on the composite nanofiber scaffolds to assess their suitability for bone tissue engineering. The results indicated that the composite nanofiber scaffolds had finer fiber diameter and higher porosity as compared with pure poly l-lactic nanofibers. Furthermore, incorporation of graphene oxide into the poly l-lactic nanofibers increased protein adsorptivity, boosted the Young’s modulus and tensile strength by nearly 4.2-fold and 3.5-fold, respectively, and significantly enhanced adhesion, proliferation, and osteogenesis in mouse mesenchymal stem cells. The results indicate that composite nanofibers could be excellent and versatile scaffolds for bone tissue engineering.

Keywords: poly l-lactic, graphene oxide, osteogenesis, bone tissue engineering

Procedia PDF Downloads 279
1013 Horizontal Bone Augmentation Using Two Membranes at Dehisced Implant Sites: A Randomized Clinical Study

Authors: Monika Bansal

Abstract:

Background: Placement of dental implant in narrow alveolar ridge is challenging to be treated. GBR procedure is currently most widely used to augment the deficient alveolar ridges and to treat the fenestration and dehiscence around dental implants. Thus, the objectives of the present study were to evaluate as well as compare the clinical performance of collagen membrane and titanium mesh for horizontal bone augmentation at dehisced implant sites. Methods and material: Total 12 single edentulous implant sites with buccal bone deficiency in 8 subjects were equally divided and treated simultaneously with either of the two membranes and DBBM(Bio-Oss) bone graft. Primary outcome measurements in terms of defect height and defect width were made using a calibrated plastic periodontal probe. Re-entry surgery was performed to remeasure the augmented site and to remove Ti-mesh at 6th month. Independent paired t-tests for the inter-group comparison and student-paired t-tests for the intra-group comparison were performed. The differences were considered to be significant at p ≤ 0.05. Results: Mean defect fill with respect to height and width was 3.50 ± 0.54 mm (87%) and 2.33 ± 0.51 mm (82%) for collagen membrane and 3.83 ± 0.75 mm (92%) and 2.50 ± 0.54 mm (88%) for Ti-mesh group respectively. Conclusions: Within the limitation of the study, it was concluded that mean defect height and width after 6 months were statistically significant within the group without significant difference between them, although defect resolution was better in Ti-mesh.

Keywords: collagen membrane, dehiscence, dental implant, horizontal bone, augmentation, ti-mesh

Procedia PDF Downloads 80
1012 Geothermal Prospect Prediction at Mt. Ciremai Using Fault and Fracture Density Method

Authors: Rifqi Alfadhillah Sentosa, Hasbi Fikru Syabi, Stephen

Abstract:

West Java is a province in Indonesia which has a number of volcanoes. One of those volcanoes is Mt. Ciremai, located administratively at Kuningan and Majalengka District, and is known for its significant geothermal potential in Java Island. This research aims to assume geothermal prospects at Mt. Ciremai using Fault and Fracture Density (FFD) Method, which is correlated to the geochemistry of geothermal manifestations around the mountain. This FFD method is using SRTM data to draw lineaments, which are assumed associated with fractures and faults in the research area. These faults and fractures were assumed as the paths for reservoir fluids to reached surface as geothermal manifestations. The goal of this method is to analyze the density of those lineaments found in the research area. Based on this FFD Method, it is known that area with high density of lineaments located on Mt. Kromong at the northern side of Mt. Ciremai. This prospect area is proven by its higher geothermometer values compared to geothermometer values calculated at the south area of Mt. Ciremai.

Keywords: geothermal prospect, fault and fracture density, Mt. Ciremai, surface manifestation

Procedia PDF Downloads 323
1011 Numerical Simulation of Bio-Chemical Diffusion in Bone Scaffolds

Authors: Masoud Madadelahi, Amir Shamloo, Seyedeh Sara Salehi

Abstract:

Previously, some materials like solid metals and their alloys have been used as implants in human’s body. In order to amend fixation of these artificial hard human tissues, some porous structures have been introduced. In this way, tissues in vicinity of the porous structure can be attached more easily to the inserted implant. In particular, the porous bone scaffolds are useful since they can deliver important biomolecules like growth factors and proteins. This study focuses on the properties of the degradable porous hard tissues using a three-dimensional numerical Finite Element Method (FEM). The most important studied properties of these structures are diffusivity flux and concentration of different species like glucose, oxygen, and lactate. The process of cells migration into the scaffold is considered as a diffusion process, and related parameters are studied for different values of production/consumption rates.

Keywords: bone scaffolds, diffusivity, numerical simulation, tissue engineering

Procedia PDF Downloads 352
1010 Conservative Treatment Versus Percutaneous Wire Fixation in treatment of Distal Radial Fracture in Elderly

Authors: Abdelfatah Elsenosy, Mahmoud Ebrahim

Abstract:

Background: Distal radius fractures are commonly encountered in orthopedic practice, especially in elderly patients. A number of clinical papers have supported the idea that anatomic restoration of the distal end of the radius is essential to gain superior results. Aim and objectives: The aim of the study is to systematically review the literature for the management of distal end radius in elderly persons (conservative treatment versus percutaneous wire fixation) as regards radiological and functional outcomes. Subjects and methods: Studies were identified from the Medline, Cochrane, EMBASE, and Google Scholar databases were searched until 2019 using combinations of the following search terms: distal radius fracture, conservative treatment, non-operative treatment, and nonsurgical treatment, surgical treatment, operative, elderly, and older. Reference lists of relevant studies were manually searched. Results: There was no statistical significance difference between CI and PKF groups’ frequency of complication in all of the selected studies. Based on the results, we recommend more analysis regarding every parameter of the radiographic and functional results and specific complications related to each fixation need to be accomplished, which requires more Randomized controlled trials (RCTs) with high quality. Conclusion: Surgical treatment seems to be more effective distal radius fracture compared with conservative treatment when the radiographic outcomes were analyzed, and no significant differences were detected in the functional outcomes and complication rate.

Keywords: radius, fracture, surgical, RCTs, conservative, radiographic, outcomes, orthopedic

Procedia PDF Downloads 126
1009 A Simple Technique for Centralisation of Distal Femoral Nail to Avoid Anterior Femoral Impingement and Perforation

Authors: P. Panwalkar, K. Veravalli, M. Tofighi, A. Mofidi

Abstract:

Introduction: Anterior femoral perforation or distal anterior nail position is a known complication of femoral nailing specifically in pertrochantric fractures fixed with cephalomedullary nail. This has been attributed to wrong entry point for the femoral nail, nail with large radius of curvature or malreduced fracture. Left alone anterior perforation of femur or abutment of nail on anterior femur will result in pain and risk stress riser at distal femur and periprosthetic fracture. There have been multiple techniques described to avert or correct this problem ranging from using different nail, entry point change, poller screw to deflect the nail position, use of shorter nail or use of curved guidewire or change of nail to ensure a nail with large radius of curvature Methods: We present this technique which we have used in order to centralise the femoral nail either when the nail has been put anteriorly or when the guide wire has been inserted too anteriorly prior to the insertion of the nail. This technique requires the use of femoral reduction spool from the nailing set. This technique was used by eight trainees of different level of experience under supervision. Results: This technique was easily reproducible without any learning curve without a need for opening of fracture site or change in the entry point with three different femoral nailing sets in twenty-five cases. The process took less than 10 minutes even when revising a malpositioned femoral nail. Conclusion: Our technique of using femoral reduction spool is easily reproducible and repeatable technique for avoidance of non-centralised femoral nail insertion and distal anterior perforation of femoral nail.

Keywords: femoral fracture, nailing, malposition, surgery

Procedia PDF Downloads 95
1008 Thickness Effect on Concrete Fracture Toughness K1c

Authors: Benzerara Mohammed, Redjel Bachir, Kebaili Bachir

Abstract:

The cracking of the concrete is a more crucial problem with the development of the complex structures related to technological progress. The projections in the knowledge of the breaking process make it possible today for better prevention of the risk of the fracture. The breaking strength brutal of a quasi-fragile material like the concrete called Toughness, is measured by a breaking value of the factor of intensity of the constraints K1C for which the crack is propagated, it is an intrinsic property of material. Many studies reported in the literature treating of the concrete were carried out on specimens which are in fact inadequate compared to the intrinsic characteristic to identify. We started from this established fact, in order to compare the evolution of the parameter of toughness K1C measured by calling upon ordinary concrete specimens of three prismatics geometries different (10*10*84) cm³ and (5*20*120) cm³ &(12*20*120) cm³ containing from the side notches various depths simulating of the cracks was set up. The notches are carried out using triangular pyramidal plates into manufactured out of sheet coated placed at the centre of the specimens at the time of the casting, then withdrawn to leave the trace of a crack. The tests are carried out in 3 points bending test in mode 1 of fracture, by using the techniques of mechanical fracture. The evolution of the parameter of toughness K1C measured with the three geometries specimens gives almost the same results. They are acceptable and return in the beach of the results determined by various researchers (toughness of the ordinary concrete turns to the turn of the 1 MPa √m). These results inform us about the presence of an economy on the level of the geometrie specimen (5*20*120) cm³, therefore to use plates specimens later if one wants to master the toughness of this material complexes, astonishing but always essential that is the concrete.

Keywords: elementary representative volume, concrete, fissure, toughness

Procedia PDF Downloads 191
1007 Stem Cell Fate Decision Depending on TiO2 Nanotubular Geometry

Authors: Jung Park, Anca Mazare, Klaus Von Der Mark, Patrik Schmuki

Abstract:

In clinical application of TiO2 implants on tooth and hip replacement, migration, adhesion and differentiation of neighboring mesenchymal stem cells onto implant surfaces are critical steps for successful bone regeneration. In a recent decade, accumulated attention has been paid on nanoscale electrochemical surface modifications on TiO2 layer for improving bone-TiO2 surface integration. We generated, on titanium surfaces, self-assembled layers of vertically oriented TiO2 nanotubes with defined diameters between 15 and 100 nm and here we show that mesenchymal stem cells finely sense TiO2 nanotubular geometry and quickly decide their cell fate either to differentiation into osteoblasts or to programmed cell death (apoptosis) on TiO2 nanotube layers. These cell fate decisions are critically dependent on nanotube size differences (15-100nm in diameters) of TiO2 nanotubes sensing by integrin clustering. We further demonstrate that nanoscale topography-sensing is feasible not only in mesenchymal stem cells but rather seems as generalized nanoscale microenvironment-cell interaction mechanism in several cell types composing bone tissue network including osteoblasts, osteoclast, endothelial cells and hematopoietic stem cells. Additionally we discuss the synergistic effect of simultaneous stimulation by nanotube-bound growth factor and nanoscale topographic cues on enhanced bone regeneration.

Keywords: TiO2 nanotube, stem cell fate decision, nano-scale microenvironment, bone regeneration

Procedia PDF Downloads 407
1006 Study and Analyze of Metallic Glasses for Biomedical Applications: From Soft to Bone Tissue Engineering

Authors: A. Monfared, S. Faghihi

Abstract:

Metallic glasses (MGs) are newcomers in the field of metals that show great potential for soft and bone tissue engineering due to the amorphous structure that endows unique properties. Up to now, various MGs based on Ti, Zr, Mg, Zn, Fe, Ca, and Sr in the form of a ribbon, bulk, thin-film, and powder have been investigated for biomedical purposes. This article reviews the compositions and biomedical properties of MGs as well as analyzes results in order to guide new approaches and future development of MGs.

Keywords: metallic glasses, biomaterials, biocompatibility, biocorrosion

Procedia PDF Downloads 181
1005 Analysis of the Plastic Zone Under Mixed Mode Fracture in Bonded Composite Repair of Aircraft

Authors: W. Oudad, H. Fikirini, K. Boulenouar

Abstract:

Material fracture by opening (mode I) is not alone responsible for fracture propagation. Many industrial examples show the presence of mode II and mixed mode I + II. In the present work the three-dimensional and non-linear finite element method is used to estimate the performance of the bonded composite repair of metallic aircraft structures by analyzing the plastic zone size ahead of repaired cracks under mixed mode loading. The computations are made according to Von Mises and Tresca criteria. The extension of the plastic zone which takes place at the tip of a crack strictly depends on many variables, such as the yield stress of the material, the loading conditions, the crack size and the thickness of the cracked component, The obtained results show that the presence of the composite patch reduces considerably the size of the plastic zone ahead of the crack. The effects of the composite orientation layup (adhesive properties) and the patch thickness on the plastic zone size ahead of repaired cracks were analyzed.

Keywords: crack, elastic-plastic, J integral, patch, plastic zone

Procedia PDF Downloads 412
1004 The Prognostic Values of Current Staging Schemes in Temporal Bone Carcinoma: A Real-World Evidence-Based Study

Authors: Minzi Mao, Jianjun Ren, Yu Zhao

Abstract:

Objectives: The absence of a uniform staging scheme for temporal bone carcinoma (TBC) seriously impedes the improvement of its management strategies. Therefore, this research was aimed to investigate the prognostic values of two currently applying staging schemes, namely, the modified Pittsburgh staging system (MPB) and Stell’s T classification (Stell-T) in patients with TBC. Methods: Areal-world single-institution retrospectivereview of patientsdiagnosed with TBC between2008 and 2019 was performed. Baseline characteristics were extracted, and patients were retrospectively staged by both the MPB and Stell-T classifications. Cox regression analyseswereconductedtocomparetheoverall survival (OS). Results: A total of 69 consecutive TBC patients were included in thisstudy. Univariate analysis showed that both Stell-T and T- classifications of the modified Pittsburgh staging system (MPB-T) were significant prognostic factors for all TBC patients as well as temporal bone squamous cell carcinoma (TBSCC, n=50) patients (P < 0.05). However, only Stell-T was confirmed to be an independent prognostic factor in TBSCC patients (P = 0.004). Conclusions: Tumor extensions, quantified by both Stell-T and MPB-T classifications, are significant prognostic factors for TBC patients, especially for TBSCC patients. However, only the Stell-T classification is an independent prognostic factor for TBSCC patients.

Keywords: modified pittsburgh staging system, overall survival, prognostic factor, stell’s T- classification, temporal bone carcinoma

Procedia PDF Downloads 100
1003 The Long-Term Effects of Immediate Implantation, Early Implantation and Delayed Implantation at Aesthetics Area

Authors: Xing Wang, Lin Feng, Xuan Zou, Hongchen liu

Abstract:

Immediate Implantation after tooth extraction is considered to be the ideal way to retain the alveolar bone, but some scholars believe the aesthetic effect in the Early Implantation case are more reliable. In this study, 89 patients were added to this retrospective study up to 5 years. Assessment indicators was including the survival of the implant (peri-implant infection, implant loosening, shedding, crowns and occlusal), aesthetics (color and fullness gums, papilla height, probing depth, X-ray alveolar crest height, the patient's own aesthetic satisfaction, doctors aesthetics score), repair defects around the implant (peri-implant bone changes in height and thickness, whether the use of autologous bone graft, whether to use absorption/repair manual nonabsorbable material), treatment time, cost and the use of antibiotics.The results demonstrated that there is no significant difference in long-term success rate of immediate implantation, early implantation and delayed implantation (p> 0.05). But the results indicated immediate implantation group could get get better aesthetic results after two years (p< 0.05), but may increase the risk of complications and failures (p< 0.05). High-risk indicators include gingival recession, labial bone wall damage, thin gingival biotypes, planting position and occlusal restoration bad and so on. No matter which type of implanting methods was selected, the extraction methods and bone defect amplification techniques are observed as a significant factors on aesthetic effect (p< 0.05).

Keywords: immediate implantation, long-term effects, aesthetics area, dental implants

Procedia PDF Downloads 330