374 Polypropylene/Red Mud Polymer Composites: Effects of Powder Size on Mechanical and Thermal Properties
Authors: Munir Tasdemir
Abstract:
Polymer/clay composites have received great attention in the past three decades owing to their light weight coupled with significantly better mechanical and barrier properties than the corresponding neat polymer resins. An investigation was carried out on the effects of red mud powder size and ratio on the mechanical and thermal properties of polypropylene /red mud polymer composites. Red mud, in four different concentrations (0, 10, 20 and 30 wt %) and three different powder size (180, 63 and 38 micron) were added to PP to produce composites. The mechanical properties, including the elasticity modulus, tensile & yield strength, % elongation, hardness, Izod impact strength and the thermal properties including the melt flow index, heat deflection temperature and vicat softening point of the composites were investigated. The structures of the composites were investigated by scanning electron microscopy and compared to mechanical and thermal properties as a function of red mud powder content and size.Keywords: polypropylene, powder, red mud, mechanical properties
Procedia PDF Downloads 304373 Hedonic Pricing Model of Parboiled Rice
Authors: Roengchai Tansuchat, Wassanai Wattanutchariya, Aree Wiboonpongse
Abstract:
Parboiled rice is one of the most important food grains and classified in cereal and cereal product. In 2015, parboiled rice was traded more than 14.34 % of total rice trade. The major parboiled rice export countries are Thailand and India, while many countries in Africa and the Middle East such as Nigeria, South Africa, United Arab Emirates, and Saudi Arabia, are parboiled rice import countries. In the global rice market, parboiled rice pricing differs from white rice pricing because parboiled rice is semi-processing product, (soaking, steaming and drying) which affects to their color and texture. Therefore, parboiled rice export pricing does not depend only on the trade volume, length of grain, and percentage of broken rice or purity but also depend on their rice seed attributes such as color, whiteness, consistency of color and whiteness, and their texture. In addition, the parboiled rice price may depend on the country of origin, and other attributes, such as certification mark, label, packaging, and sales locations. The objectives of this paper are to study the attributes of parboiled rice sold in different countries and to evaluate the relationship between parboiled rice price in different countries and their attributes by using hedonic pricing model. These results are useful for product development, and marketing strategies development. The 141 samples of parboiled rice were collected from 5 major parboiled rice consumption countries, namely Nigeria, South Africa, Saudi Arabia, United Arab Emirates and Spain. The physicochemical properties and optical properties, namely size and shape of seed, colour (L*, a*, and b*), parboiled rice texture (hardness, adhesiveness, cohesiveness, springiness, gumminess, and chewiness), nutrition (moisture, protein, carbohydrate, fat, and ash), amylose, package, country of origin, label are considered as explanatory variables. The results from parboiled rice analysis revealed that most of samples are classified as long grain and slender. The highest average whiteness value is the parboiled rice sold in South Africa. The amylose value analysis shows that most of parboiled rice is non-glutinous rice, classified in intermediate amylose content range, and the maximum value was found in United Arab Emirates. The hedonic pricing model showed that size and shape are the key factors to determine parboiled rice price statistically significant. In parts of colour, brightness value (L*) and red-green value (a*) are statistically significant, but the yellow-blue value (b*) is insignificant. In addition, the texture attributes that significantly affect to the parboiled rice price are hardness, adhesiveness, cohesiveness, and gumminess. The findings could help both parboiled rice miller, exporter and retailers formulate better production and marketing strategies by focusing on these attributes.Keywords: hedonic pricing model, optical properties, parboiled rice, physicochemical properties
Procedia PDF Downloads 306372 Consolidation of Carbonyl Nickel Powders by Hot Pressing
Authors: Ridvan Yamanoglu, Ismail Daoud
Abstract:
In the current study, carbonyl nickel powders were sintered by uniaxial hot pressing technique. Loose starting powders were poured directly into a graphite die with a 15.4 mm inner diameter. Two graphite punches with an outer diameter of 15 mm were inserted into the die; then the powders were sintered at different sintering temperatures, holding times and pressure conditions. The sintered samples were polished and examined by optical microscopy. Hardness and bending behavior of the sintered samples were investigated in order to determine the mechanical properties of the sintered nickel samples. To carried out the friction properties of the produced samples wear tests were studied using a pin on disc tribometer. Load and distance were selected as wear test parameters. The fracture surface of the samples after bending test was also carried out by using scanning electron microscopy.Keywords: nickel powder, sintering, hot press, mechanical properties
Procedia PDF Downloads 142371 Effect of Cr2O3 on Mechanical Properties of Aluminum Produced Powder Metallurgy
Authors: Yasin Akgul, Fazil Husem, Memis Isik
Abstract:
In this study, effect of content of chromium (III) oxide on production of Al/Cr203 alloys were investigated. Experimental procedure was started with mixturing of powders in the presence of absolute ethanol, vacuum distillation technique was used for evaporation, by ultrasonic bath and mechanic stirrer. Pressing procedure was achieved by hydrolic press that has 100 tons forcing for production of 25 mm diameter compact green billets. Green bodies were sintered at 600 °C in argon atmosphere. Scanning electron microscope (SEM) analysis for characterization of microstructure, compression test for determination of strength and Vickers test for measuring of hardness of sintered billets were done. End of the study is concluded that, enhancement of physical and mechanical properties is observed by increasing content of chromium (III) oxide.Keywords: aluminium, chromium (III) oxide, powder metallurgy, sintering
Procedia PDF Downloads 208370 Tower Crane Selection and Positioning on Construction Sites
Authors: Dirk Briskorn, Michael Dienstknecht
Abstract:
Cranes are a key element in construction projects as they are the primary lifting equipment and among the most expensive construction equipment. Thus, selecting cranes and locating them on-site is an important factor for a project's profitability. We focus on a site with supply and demand areas that have to be connected by tower cranes. There are several types of tower cranes differing in certain specifications such as costs or operating radius. The objective is to select cranes and determine their locations such that each demand area is connected to its supply area at minimum cost. We detail the problem setting and show how to obtain a discrete set of candidate locations for each crane type without losing optimality. This discretization allows us to reduce our problem to the classic set cover problem. Despite its NP-hardness, we achieve good results employing a standard solver and a greedy heuristic, respectively.Keywords: positioning, selection, standard solver, tower cranes
Procedia PDF Downloads 345369 Enhancement of Mechanical and Biological Properties in Wollastonite Bioceramics by MgSiO3 Addition
Authors: Jae Hong Kim, Sang Cheol Um, Jong Kook Lee
Abstract:
Strong and biocompatible wollastonite (CaSiO3) was fabricated by pressureless sintering at temperature range of 1250~ 1300 ℃ and phase transition of to β-wollastonite with an addition of MgSiO3. Starting pure α-wollastonite powder were prepared by solid state reaction, and MgSiO3 powder was added to α-wollastonite powder to induce the phase transition α to β-wollastonite over 1250℃. Sintered wollastonite samples at 1250℃ with 5 and 10 wt% MgSiO3 were α+β phase and β phase respectively, and showed higher densification rate than that of α or β-wollastonite, which are almost the same as the theoretical density. Hardness and Young’s modulus of sintered wollastonite were dependent on the apparent density and the amount of β-wollastonite. Young’s modulus (78GPa) of β-wollastonite added 10 wt% MgSiO3 was almost double time of sintered α-wollastonite. From the in-vitro test, biphasic (α+β) wollastonite with 5wt% MgSiO3 addition had good bioactivity in simulated body fluid solution.Keywords: β-wollastonite, high density, MgSiO3, phase transition
Procedia PDF Downloads 559368 Effect of Saturation and Deformation Rate on Split Tensile Strength for Various Sedimentary Rocks
Authors: D. K. Soni
Abstract:
A study of engineering properties of stones, i.e. compressive strength, tensile strength, modulus of elasticity, density, hardness were carried out to explore the possibility of optimum utilization of stone. The laboratory test results on equally dimensioned discs of the stone show a considerable variation in computed split tensile strength with varied rates of deformation. Hence, the effect of strain rate on the tensile strength of a sand stone and lime stone under wet and dry conditions has been studied experimentally using the split tensile strength test technique. It has been observed that the tensile strength of these stone is very much dependent on the rate of deformation particularly in a dry state. On saturation the value of split tensile strength reduced considerably depending upon the structure of rock and amount of water absorption.Keywords: sedimentary rocks, split tensile test, deformation rate, saturation rate, sand stone, lime stone
Procedia PDF Downloads 378367 Cold Metal Transfer Welding of Dissimilar Thickness 6061-T6 to 5182-O Aluminum Alloys
Authors: A. Elrefaei
Abstract:
The possibility of having sheets with different thicknesses and materials in one assembly facilitates the optimal material distribution within the final product and reduces the weight of the structure. Ability of joining process to assembly these different material combinations is always a challenge to the designer. In this study, 0.6 mm thick 6061-T6 and 2 mm thick 5182-O were robot CMT welded using ER5356 and ER4043 filler metals. The thermal effect of welding resulted in a loss of hardness in the 6061 HAZ. Joints welded by ER5356 filler metal were much higher in fracture load than joints welded by ER4043 and the elongation of joints welded by ER5356 was almost double its corresponding joints welded by ER4043 filler. Owing to the big difference in formability and thickness of base metals, the fracture in forming test occurred in the softened 6061 HAZ out from the weld centerline.Keywords: aluminum, CMT, mechanical, welding
Procedia PDF Downloads 209366 A High Amylose-Content and High-Yielding Elite Line Is Favorable to Cook 'Nanhan' (Semi-Soft Rice) for Nursing Care Food Particularly for Serving Aged Persons
Authors: M. Kamimukai, M. Bhattarai, B. B. Rana, K. Maeda, H. B. Kc, T. Kawano, M. Murai
Abstract:
Most of the aged people older than 70 have difficulty in chewing and swallowing more or less. According to magnitude of this difficulty, gruel, “nanhan” (semi-soft rice) and ordinary cooked rice are served in general, particularly in sanatoriums and homes for old people in Japan. Nanhan is the name of a cooked rice used in Japan, having softness intermediate between gruel and ordinary cooked rice, which is boiled with intermediate amount of water between those of the latter two kinds of cooked rice. In the present study, nanhan was made in the rate of 240g of water to 100g of milled rice with an electric rice cooker. Murai developed a high amylose-content and high-yielding elite line ‘Murai 79’. Sensory eating-quality test was performed for nanhan and ordinary cooked rice of Murai 79 and the standard variety ‘Hinohikari’ which is a high eating-quality variety representative in southern Japan. Panelists (6 to 14 persons) scored each cooked rice in six items viz. taste, stickiness, hardness, flavor, external appearance and overall evaluation. Grading (-3 ~ +3) in each trait was performed, regarding the value of the standard variety Hinohikari as 0. Paddy rice produced in a farmer’s field in 2013 and 2014 and in an experimental field of Kochi University in 2015 and 2016 were used for the sensory test. According to results of the sensory eating-quality test for nanhan, Murai 79 is higher in overall evaluation than Hinohikari in the four years. The former was less sticky than the latter in the four years, but the former was statistically significantly harder than the latter throughout the four years. In external appearance, the former was significantly higher than the latter in the four years. In the taste, the former was significantly higher than the latter in 2014, but significant difference was not noticed between them in the other three years. There were no significant differences throughout the four years in flavor. Regarding amylose content, Murai 79 is higher by 3.7 and 5.7% than Hinohikari in 2015 and 2016, respectively. As for protein content, Murai 79 was higher than Hinohikari in 2015, but the former was lower than the latter in 2016. Consequently, the nanhan of Murai 79 was harder and less sticky, keeping the shape of grains as compared with that of Hinohikari, which may be due to its higher amylose content. Hence, the nanhan of Murai 79 may be recognized as grains more easily in a human mouth, which could make easier the continuous performance of mastication and deglutition particularly in aged persons. Regarding ordinary cooked rice, Murai 79 was similar to or higher in both overall evaluation and external appearance as compared with Hinohikari, despite its higher hardness and lower stickiness. Additionally, Murai 79 had brown-rice yield of 1.55 times as compared with Hinohikari, suggesting that it would enable to supply inexpensive rice for making nanhan with high quality particularly for aged people in Japan.Keywords: high-amylose content, high-yielding rice line, nanhan, nursing care food, sensory eating quality test
Procedia PDF Downloads 116365 Production of Hard Nickel Particle Reinforced Ti6Al4V Matrix Composites by Hot Pressing
Authors: Ridvan Yamanoglu
Abstract:
In the current study, titanium based composites reinforced by hard nickel alloy particles were produced. Powder metallurgical hot pressing technique was used for the fabrication of composite materials. The composites containing different ratio of hard nickel particles were sintered at 900 oC for 15 and 30 minutes under 50 MPa pressure. All titanium based composites were obtained under a vacuum atmosphere of 10-4 mbar to prevent of oxidation of titanium due to its high reactivity to oxygen. The microstructural characterization of the composite samples was carried out by optical and scanning electron microscopy. The mechanical properties of the samples were determined by means of hardness and wear tests. The results showed that when the nickel particle content increased the mechanical properties of the composites enhanced. The results are discussed in detail and optimum nickel particle content were determined.Keywords: titanium, composite, nickel, hot pressing
Procedia PDF Downloads 149364 Retention Properties of the Matrix Material Fe-Mn-Cu-Sn-C in Relation to Diamond Particles
Authors: Elżbieta Cygan-Bączek, Piotr Wyżga, Sławomir Cygan
Abstract:
In the presented work, the main goal was to investigate the retention properties, defined as the ability of the matrix material to hold diamond particles in relation to metallized (Ti, Si, Cr, Co, Cu, Ni) and non-metallized diamond crystals. For this purpose, diamond-impregnated specimens were tested for wear rate on abrasive sandstone using a test rig specially designed to simulate tool application conditions. The tests that involved 3- and 2-body abrasion ranked the alloys in different orders. The ability of the matrix to retain diamond crystals was determined using the electron microskopy (SEM, TEM). The specimens were also characterized by X-ray diffraction (XRD) and hardness. The conducted research has shown that Si and Ti metallized diamonds, apart from mechanical jamming in the matrix, are also connected in a metallurgical manner, ensuring the improvement of the retention properties of the matrix material.Keywords: diamond, metallic-diamond segments, retention, abrasive wear resistance
Procedia PDF Downloads 102363 Performance Evaluation of Moringa Oleifera as Coagulant for Treating Abattoir Wastewater
Authors: Adesiji Adeolu Richard, Hassa Musa, Osita Evaritus Asogwa, Mary Oluwatobi Odekunle, Mangey Jarumi Akila
Abstract:
In this paper, extract from raw Moringa Oleifera seeds for the treatment of 40 liters of abattoir wastewater was studied for a period of ten (10) weeks. A completely randomized design with loading dosages of 10, 12, 14, 16, 18, and 20g of processed Moringa Oleifera seed was used in the treatment. A control sample (with no Moringa Oleifera treatment) was also included. The physical and chemical properties of abattoir wastewater were investigated before and after treatment. The turbidity value was reduced drastically after the treatments from 15.40 to 7.63 mg/l for 16g dosage in week 7. Total alkalinity, Total hardness, Conductivity, Calcium, and Biological Oxygen Demand were all found to be reduced in concentration within the second and fourth weeks of the experiment with 14 to 16g of Moringa Oleifera dosage. The results generally showed that 16g/500ml of Moringa Oleifera was able to treat abattoir wastewater after weeks of the experiment.Keywords: Moringa Oleifera, abattoir wastewater, turbidity, conductivity, pH
Procedia PDF Downloads 79362 Mechanical Properties of Nanocomposites Cobalt Matrix with Nano SiC Particles
Authors: Dhuha Albusalih, David Weston, Simon Gill
Abstract:
Nanocomposites Co-SiC with well dispersed nanoparticles and Co nano grain size has produced using Pulse Reverse Plating (PRP) and using anionic surfactant. Different particle contents of nanocomposites were produced by altering the plating parameters. The method allows great control over the level of nanoparticles in the coating, without changing bath chemistry. Examination by Scanning Electron Microscopy (SEM), Energy Dispersive Spectroscopy (EDX), TEM and X-Ray Diffraction (XRD) analysis was performed to characterize and study the strengthening mechanisms of these nanocomposites. The primary strengthening mechanisms were shown to be grain refinement and dispersion strengthening. Tribological performances of the produced electroplated nanocomposite Co-SiC coatings were examined. Results showed that the coating with the higher volume fraction (vol. %) of SiC and the smallest grain size has the higher hardness and low wear rate.Keywords: nanocomposites, pulse reverse plating, tribological performance of cobalt nanocomposites
Procedia PDF Downloads 280361 Correlation between Electromyographic and Textural Parameters for Different Textured Indian Foods Using Principal Component Analysis
Authors: S. Rustagi, N. S. Sodhi, B. Dhillon, T. Kaur
Abstract:
The objective of this study was to check whether there is any relationship between electromyographic (EMG) and textural parameters during food texture evaluation. In this study, a total of eighteen mastication variables were measured for entire mastication, per chew mastication and three different stages of mastication (viz. early, middle and late) by EMG for five different foods using eight human subjects. Cluster analysis was used to reduce the number of mastication variables from 18 to 5, so that principal component analysis (PCA) could be applied on them. The PCA further resulted in two meaningful principal components. The principal component scores for each food were measured and correlated with five textural parameters (viz. hardness, cohesiveness, chewiness, gumminess and adhesiveness). Correlation coefficients were found to be statistically significant (p < 0.10) for cohesiveness and adhesiveness while if we reduce the significance level (p < 0.20) then chewiness also showed correlation with mastication parameters.Keywords: electromyography, mastication, sensory, texture
Procedia PDF Downloads 318360 Development of Ferrous-Aluminum Alloys from Recyclable Material by High Energy Milling
Authors: Arnold S. Freitas Neto, Rodrigo E. Coelho, Erick S. Mendonça
Abstract:
This study aimed to obtain an alloy of Iron and Aluminum in the proportion of 50% of atomicity for each constituent. Alloys were obtained by processing recycled aluminum and chips of 1200 series carbon steel in a high-energy mill. For the experiment, raw materials were processed thorough high energy milling before mixing the substances. Subsequently, the mixture of 1200 series carbon steel and Aluminum powder was carried out a milling process. Thereafter, hot compression was performed in a closed die in order to obtain the samples. The pieces underwent heat treatments, sintering and aging. Lastly, the composition and the mechanical properties of their hardness were analyzed. In this paper, results are compared with previous studies, which used iron powder of high purity instead of Carbon steel in the composition.Keywords: Fe-Al alloys, high energy milling, metallography characterization, powder metallurgy
Procedia PDF Downloads 283359 Enhancing of Paraffin Wax Properties by Adding of Low Density Polyethylene (LDPE)
Authors: Siham Mezher Yousif, Intisar Yahiya Mohammed, Salma Nagem Mouhy
Abstract:
Low Density Polyethylene is a thermoplastic resin extracted from petroleum based, whereas the wax is an oily organic component that is contains of alkanes, ester, polyester, and hydroxyl ester. The purpose of this research is to find out the optimum conditions of the wax produced by inducing with LDPE. The experiments were carried out by mixing different percentages of wax and LDPE to produce different polymer/wax compositions, in which lower values of the penetration, thickness, and electrical conductivity are obtained with increasing of mixing ratio of LDPE/wax which showed results of 19 mm penetration, 692 micron thickness and 5.9 mA electrical conductivity for 90 wt % of LDPE/wax) maximum mixing ratio (. It’s found that the optimum results regarding penetration, enamel thickness, and electrical conductivity “according to the enamel hardness, insulation properties, and economic aspects” are 20 mm, 276 micron, and 6.2 mA respectively.Keywords: paraffin wax, low density polyethylene, blending, mixing ratio, bleaching
Procedia PDF Downloads 86358 Measurements of Physical Properties of Directionally Solidified Al-Si-Cu Ternary Alloy
Authors: Aynur Aker, Hasan Kaya
Abstract:
Al-12.6wt.%Si-2wt.%Cu ternary alloy of near eutectic composition was directionally solidified upward at a constant temperature gradient in a wide range of growth rates (V=8.25-165.41 µm/s). The microstructures (λ), microhardness (HV), tensile stress (σ) and electrical resistivity (ρ) were measured from directionally solidified samples. The dependence of microstructures, microhardness and electrical resistivity on growth rate (V) was also determined by statistical analysis. According to these results, it has been found that for increasing values of V, the values of HV, σ and ρ increase. Variations of electrical resistivity for casting Al-Si-Cu alloy were also measured at the temperature in range 300-500 K. The enthalpy (ΔH) and the specific heat (Cp) for the Al-Si-Cu alloy were determined by differential scanning calorimeter (DSC) from heating trace during the transformation from solid to liquid. The results obtained in this work were compared with the similar experimental results in the literature.Keywords: Al-Si-Cu alloy, microstructures, micro-hardness, tensile stress electrical resistivity, enthalpy
Procedia PDF Downloads 252357 Investigation Acute Toxicity and Bioaccumulation Mineral Mercury in Rutilus frisii Kutum
Authors: A. Gharaei, R. Karami
Abstract:
Rutilus frisii Kutum was exposed to various concentrations of mercuric chloride in water to determine its acute toxicity and bioaccumulation. We carried out ten treatments with three replicates and one control for each of the chemicals using the static O. E. C. D. method in 55-liter-tanks each containing 14 fingerlings. During the experiments, the average pH was recorded as 7.8, total hardness was measured to be 255 mg/l, the average water temperature was 27±1 degrees centigrade and dissolved oxygen was 7.2 mg/l. Mean LC50 values of Hgcl2 for juvenile R. frisii kutum with mean weight 1±0.2 gr were 0.102 and 0.86 mgHg/l at 24h and 96h, respectively. The bioaccumulation values during 24h in tissue, kidney, and gill were 1.55, 16.1, and 22.7 mgHg/l, respectively. So, these values during 96h were 2.8, 16.8, and 26.65 mgHg/l, respectively. The bioconcentration factors in tissue, kidney, and gill during 24h were 14.75, 153.39, and 216.11 and so during 96h were 33.8, 198.1, and 313.5 times. These results show that bioaccumulation was highest in the gill and then kidney and tissue, respectively. This study suggested that between mercury concentrations of water with bioaccumulation in tissue more than kidney and gill.Keywords: HgCl2, LC5096h, bioaccumulation, Rutilus frisii Kutum, Caspian Sea
Procedia PDF Downloads 541356 Formulation and Evaluation of Dispersible Tablet of Furosemide for Pediatric Use
Authors: O. Benaziz, A. Dorbane, S. Djeraba
Abstract:
The objective of this work is to formulate a dry dispersible form of furosemide in the context of pediatric dose adjustment. To achieve this, we have produced a set of formulas that will be tested in process and after compression. The formula with the best results will be improved to optimize the final shape of the product. Furosemide is the most widely used pediatric diuretic because of its low toxicity. The manufacturing process was chosen taking into account all the data relating to the active ingredient and the excipients used and complying with the specifications and requirements of dispersible tablets. The process used to prepare these tablets was wet granulation. Different excipients were used: lactose, maize starch, magnesium stearate and two superdisintegrants. The mode of incorporation of super-disintegrant changes with each formula. The use of super-disintegrant in the formula allowed optimization of the disintegration time. Prepared tablets were evaluated for weight, content uniformity, hardness, disintegration time, friability and in vitro dissolution test.Keywords: formulation, dispersible tablets, wet granulation, superdisintegrants, disintegration
Procedia PDF Downloads 317355 Review of Friction Stir Welding of Dissimilar 5000 and 6000 Series Aluminum Alloy Plates
Authors: K. Subbaiah
Abstract:
Friction stir welding is a solid state welding process. Friction stir welding process eliminates the defects found in fusion welding processes. It is environmentally friend process. 5000 and 6000 series aluminum alloys are widely used in the transportation industries. The Al-Mg-Mn (5000) and Al-Mg-Si (6000) alloys are preferably offer best combination of use in Marine construction. The medium strength and high corrosion resistant 5000 series alloys are the aluminum alloys, which are found maximum utility in the world. In this review, the tool pin profile, process parameters such as hardness, yield strength and tensile strength, and microstructural evolution of friction stir welding of Al-Mg alloys 5000 Series and 6000 series have been discussed.Keywords: 5000 series and 6000 series Al alloys, friction stir welding, tool pin profile, microstructure and properties
Procedia PDF Downloads 435354 Slurry Erosion Behaviour of Cryotreated SS316L Impeller Steel Used for Irrigation Pumps
Authors: Jagtar Singh, Kulwinder Singh
Abstract:
Slurry erosion is a type of erosion wherein material is removed from the target surface due to impingement of solid particles entrained in liquid medium. Slurry erosion performance of deep cryogenic treatment on impeller steel SS 316 L has been investigated. Slurry collected from an actual irrigation pump used as the abrasive media in an erosion test rig. An attempt has been made to study the effect of velocity of fluid and impingement angle by constant concentration (ppm) on the slurry erosion behavior of these cryotreated steels under different experimental conditions. The slurry erosion wear analysis of cryotreated and untreated steels was done. The slurry erosion performance of cryotreated SS 316L impeller steel has been found to superior to that of untreated steel. Metallurgical investigation, hardness as well as %age of carbide in both types of steel was also investigated.Keywords: deep cryogenic treatment, impeller, Irrigation pumps SS316L, slurry erosion
Procedia PDF Downloads 375353 Optimization of Process Parameters for Rotary Electro Discharge Machining Using EN31 Tool Steel: Present and Future Scope
Authors: Goutam Dubey, Varun Dutta
Abstract:
In the present study, rotary-electro discharge machining of EN31 tool steel has been carried out using a pure copper electrode. Various response variables such as Material Removal Rate (MRR), Tool Wear Rate (TWR), and Machining Rate (MR) have been studied against the selected process variables. The selected process variables were peak current (I), voltage (V), duty cycle, and electrode rotation (N). EN31 Tool Steel is hardened, high carbon steel which increases its hardness and reduces its machinability. Reduced machinability means it not economical to use conventional methods to machine EN31 Tool Steel. So, non-conventional methods play an important role in machining of such materials.Keywords: electric discharge machining, EDM, tool steel, tool wear rate, optimization techniques
Procedia PDF Downloads 177352 [Keynote Talk]: Determination of the Quality of the Machined Surface Using Fuzzy Logic
Authors: Dejan Tanikić, Jelena Đoković, Saša Kalinović, Miodrag Manić, Saša Ranđelović
Abstract:
This paper deals with measuring and modelling of the quality of the machined surface of the metal machining process. The average surface roughness (Ra) which represents the quality of the machined part was measured during the dry turning of the AISI 4140 steel. A large number of factors with the unknown relations among them influences this parameter, and that is why mathematical modelling is extremely complicated. Different values of cutting speed, feed rate, depth of cut (cutting regime) and workpiece hardness causes different surface roughness values. Modelling with soft computing techniques may be very useful in such cases. This paper presents the usage of the fuzzy logic-based system for determining metal machining process parameter in order to find the proper values of cutting regimes.Keywords: fuzzy logic, metal machining, process modeling, surface roughness
Procedia PDF Downloads 139351 Evaluation of Groundwater Quality and Its Suitability for Drinking and Agricultural Purposes Using Self-Organizing Maps
Authors: L. Belkhiri, L. Mouni, A. Tiri, T.S. Narany
Abstract:
In the present study, the self-organizing map (SOM) clustering technique was applied to identify homogeneous clusters of hydrochemical parameters in El Milia plain, Algeria, to assess the quality of groundwater for potable and agricultural purposes. The visualization of SOM-analysis indicated that 35 groundwater samples collected in the study area were classified into three clusters, which showed progressive increase in electrical conductivity from cluster one to cluster three. Samples belonging to cluster one are mostly located in the recharge zone showing hard fresh water type, however, water type gradually changed to hard-brackish type in the discharge zone, including clusters two and three. Ionic ratio studies indicated the role of carbonate rock dissolution in increases on groundwater hardness, especially in cluster one. However, evaporation and evapotranspiration are the main processes increasing salinity in cluster two and three.Keywords: groundwater quality, self-organizing maps, drinking water, irrigation water
Procedia PDF Downloads 231350 Spark Plasma Sintering of Aluminum-Based Composites Reinforced by Nanocrystalline Carbon-Coated Intermetallic Particles
Authors: B. Z. Manuel, H. D. Esmeralda, H. S. Felipe, D. R. Héctor, D. de la Torre Sebastián, R. L. Diego
Abstract:
Aluminum Matrix Composites reinforced with nanocrystalline Ni3Al carbon-coated intermetallic particles, were synthesized by powder metallurgy. Powder mixture of aluminum with 0.5-volume fraction of reinforcement particles was compacted by spark plasma sintering (SPS) technique and the compared with conventional sintering process. The better results for SPS technique were obtained in 520ºC-5kN-3min.The hardness (70.5±8 HV) and the elastic modulus (95 GPa) were evaluated in function of sintering conditions for SPS technique; it was found that the incorporation of these kind of reinforcement particles in aluminum matrix improve its mechanical properties. The densities were about 94% and 97% of the theoretical density. The carbon coating avoided the interfacial reaction between matrix-particle at high temperature (520°C) without show composition change either intermetallic dissolution.Keywords: aluminum matrix composites, intermetallics, spark plasma sintering, nanocrystalline
Procedia PDF Downloads 424349 Determination of Weathering at Kilistra Ancient City by Using Non-Destructive Techniques, Central Anatolia, Turkey
Authors: İsmail İnce, Osman Günaydin, Fatma Özer
Abstract:
Stones used in the construction of historical structures are exposed to various direct or indirect atmospheric effects depending on climatic conditions. Building stones deteriorate partially or fully as a result of this exposure. The historic structures are important symbols of any cultural heritage. Therefore, it is important to protect and restore these historical structures. The aim of this study is to determine the weathering conditions at the Kilistra ancient city. It is located in the southwest of the Konya city, Central Anatolia, and was built by carving into pyroclastic rocks during the Byzantine Era. For this purpose, the petrographic and mechanical properties of the pyroclastic rocks were determined. In the assessment of weathering of structures in the ancient city, in-situ non-destructive testing (i.e., Schmidt hardness rebound value, relative humidity measurement) methods were applied.Keywords: cultural heritage, Kilistra ancient city, non-destructive techniques, weathering
Procedia PDF Downloads 335348 Investigation of the Cognition Factors of Fire Response Performances Based on Survey
Authors: Jingjing Yan, Gengen He, Anahid Basiri
Abstract:
The design of an indoor navigation system for fire evacuation support requires not only physical feasibility but also a relatively thorough consideration of the human factors. This study has taken a survey to investigate the fire response performances (FRP) of the indoor occupants in age of 20s, virtually in an environment for their routine life, focusing on the aspects of indoor familiarity (spatial cognition), psychological stress and decision makings. For indoor familiarity, it is interested in three factors, i.e., the familiarity to exits and risky places as well as the satisfaction degree of the current indoor sign installation. According to the results, males have a higher average familiarity with the indoor exits while both genders have a relatively low level of risky place awareness. These two factors are positively correlated with the satisfaction degree of the current installation of the indoor signs, and this correlation is more evident for the exit familiarity. The integration of the height factor with the other two indoor familiarity factors can improve the degree of indoor sign satisfaction. For psychological stress, this study concentrates on the situated cognition of moving difficulty, nervousness, and speed reduction when using a bending posture during the fire evacuation to avoid smoke inhalation. The results have shown that both genders have a similar mid-level of hardness sensation. The females have a higher average level of nervousness, while males have a higher average level of speed reduction sensation. This study has assumed that the growing indoor spatial cognition can help ease the psychological hardness and nervousness. However, it only seems to be true after reaching a certain level. When integrating the effects from indoor familiarity and the other two psychological factors, the correlation to the sensation of speed change can be strengthened, based on a stronger positive correlation with the integrated factors. This study has also investigated the participants’ attitude to the navigation support during evacuation, and the majority of the participants have shown positive attitudes. For following the guidance under some extreme cases, i.e., changing to a longer path and to an alternative exit, the majority of the participants has shown the confidence of keeping trusting the guidance service. These decisions are affected by the combined influences from indoor familiarity, psychological stress, and attitude of using navigation service. For the decision time of the selected extreme cases, it costs more time in average for deciding to use a longer route than to use an alternative exit, and this situation is more evident for the female participants. This requires further considerations when designing a personalized smartphone-based navigation app. This study has also investigated the calming factors for people being trapped during evacuation. The top consideration is the distance to the nearest firefighters, and the following considerations are the current fire conditions in the surrounding environment and the locations of all firefighters. The ranking of the latter two considerations is very gender-dependent according to the results.Keywords: fire response performances, indoor spatial cognition, situated cognition, survey analysis
Procedia PDF Downloads 113347 Study the Effect of Sensitization on the Microstructure and Mechanical Properties of Gas Tungsten Arc Welded AISI 304 Stainless Steel Joints
Authors: Viranshu Kumar, Hitesh Arora, Pradeep Joshi
Abstract:
SS 304 is Austenitic stainless steel with Chromium and Nickel as basic constituents. It has excellent corrosion resistance properties and very good weldability. Austenitic stainless steels have superior mechanical properties at high temperatures and are used extensively in a range of applications. SS 304L has wide applications in various industries viz. Nuclear, Pharmaceutical, marine, chemical etc. due to its excellent applications and ease of joining this material has become very popular for fabrication as well as weld surfacing. Austenitic stainless steels have a tendency to form chromium depleted zones at the grain boundaries during welding and heat treatment, where chromium combines with available carbon in the vicinity of the grain boundaries, to produce an area depleted in chromium, and thus becomes susceptible to intergranular corrosion. This phenomenon is known as sensitization.Keywords: sensitization, SS 304, GTAW, mechanical properties, carbideprecipitationHAZ, microstructure, micro hardness, tensile strength
Procedia PDF Downloads 366346 Development of AA2024 Matrix Composites Reinforced with Micro Yttrium through Cold Compaction with Superior Mechanical Properties
Authors: C. H. S. Vidyasagar, D. B. Karunakar
Abstract:
In this present work, five different composite samples with AA2024 as matrix and varying amounts of yttrium (0.1-0.5 wt.%) as reinforcement are developed through cold compaction. The microstructures of the developed composite samples revealed that the yttrium reinforcement caused grain refinement up to 0.3 wt.% and beyond which the refinement is not effective. The microstructure revealed Al2Cu precipitation which strengthened the composite up to 0.3 wt.% yttrium reinforcement. Upon further increase in yttrium reinforcement, the intermetallics and the precipitation coarsen and their corresponding strengthening effect decreases. The mechanical characterization revealed that the composite sample reinforced with 0.3 wt.% yttrium showed highest mechanical properties like 82 HV of hardness, 276 MPa Ultimate Tensile Strength (UTS), 229 MPa Yield Strength (YS) and an elongation (EL) of 18.9% respectively. However, the relative density of the developed composites decreased with the increase in yttrium reinforcement.Keywords: mechanical properties, AA 2024 matrix, yttrium reinforcement, cold compaction, precipitation
Procedia PDF Downloads 123345 Characterization of Alloyed Grey Cast Iron Quenched and Tempered for a Smooth Roll Application
Authors: Mohamed Habireche, Nacer E. Bacha, Mohamed Djeghdjough
Abstract:
In the brick industry, smooth double roll crusher is used for medium and fine crushing of soft to medium hard material. Due to opposite inward rotation of the rolls, the feed material is nipped between the rolls and crushed by compression. They are subject to intense wear, known as three-body abrasion, due to the action of abrasive products. The production downtime affecting productivity stems from two sources: the bi-monthly rectification of the roll crushers and their replacement when they are completely worn out. Choosing the right material for the roll crushers should result in longer machine cycles, and reduced repair and maintenance costs. All roll crushers are imported from outside Algeria. This results in sometimes very long delivery times which handicap the brickyards, in particular in respecting delivery times and honored the orders made by customers. The aim of this work is to investigate the effect of alloying additions on microstructure and wear behavior of grey lamellar cast iron for smooth roll crushers in brick industry. The base gray iron was melted in an induction furnace with low frequency at a temperature of 1500 °C, in which return cast iron scrap, new cast iron ingot, and steel scrap were added to the melt to generate the desired composition. The chemical analysis of the bar samples was carried out using Emission Spectrometer Systems PV 8050 Series (Philips) except for the carbon, for which a carbon/sulphur analyser Elementrac CS-i was used. Unetched microstructure was used to evaluate the graphite flake morphology using the image comparison measurement method. At least five different fields were selected for quantitative estimation of phase constituents. The samples were observed under X100 magnification with a Zeiss Axiover T40 MAT optical microscope equipped with a digital camera. SEM microscope equipped with EDS was used to characterize the phases present in the microstructure. The hardness (750 kg load, 5mm diameter ball) was measured with a Brinell testing machine for both treated and as-solidified condition test pieces. The test bars were used for tensile strength and metallographic evaluations. Mechanical properties were evaluated using tensile specimens made as per ASTM E8 standards. Two specimens were tested for each alloy. From each rod, a test piece was made for the tensile test. The results showed that the quenched and tempered alloys had best wear resistance at 400 °C for alloyed grey cast iron (containing 0.62%Mn, 0.68%Cr, and 1.09% Cu) due to fine carbides in the tempered matrix. In quenched and tempered condition, increasing Cu content in cast irons improved its wear resistance moderately. Combined addition of Cu and Cr increases hardness and wear resistance for a quenched and tempered hypoeutectic grey cast iron.Keywords: casting, cast iron, microstructure, heat treating
Procedia PDF Downloads 80