Search results for: starch industry
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 5363

Search results for: starch industry

5363 Physicochemical Characteristics of Rice Starch Chainat 1 Variety by Physical Modification

Authors: Orose Rugchati, Sarawut Wattanawongpitak

Abstract:

The Chainat 1 variety (CN1) of rice, which generally has high amylose starch, is distributed in the lower part of Northern Thailand. CN1 rice starch can be used in both food and non-food products. In this research, the CN1 rice starch from the wet-milling process was prepared by Pre-Gelatinization (Heat-Moisture Treatments, HMT) under different conditions: percentage of moisture contents (20% and 30%) and duration time in minutes (0, 30, 60, and 90) at a specific temperature 110°C. The physicochemical characteristics of CN1 rice starch modification, such as amylose content, viscosity, swelling, and solubility property, were evaluated and compared with native CN1 rice starch. The results showed that modification CN1 rice starch tends to have some characteristics better than native starch. The appearance color and starch granule of modified CN1 by HMT have more effective characteristics than native starch when increased duration time. The duration time and moisture content are significant factors to the CN1 starch characteristic by HMT. Moreover, physical modification of CN1 starch by HMT can be described as a modified rice starch providing in many applications and the advantage of biodegradability development.

Keywords: physicochemical characteristics, physical modification, pre-gelatinization, Heat-Moisture Treatments, rice starch, Chainat 1 variety (CN1)

Procedia PDF Downloads 123
5362 Horse Chestnut Starch: A Noble Inedible Feedstock Source for Producing Thermoplastic Starch (TPS)

Authors: J. Castaño, S. Rodriguez, C. M. L. Franco

Abstract:

Starch isolated from non-edible A. hippocastanum seeds was characterized and used for preparing starch-based materials. The apparent amylose content of the isolated starch was 33.1%. The size of starch granules ranged from 0.7 to 35µm, and correlated with the shape of granules (spherical, oval and irregular). The chain length distribution profile of amylopectin showed two peaks, at polymerization degree (DP) of 12 and 41-43. Around 53% of branch unit chains had DP in the range of 11-20. A. hippocastanum starch displayed a typical C-type pattern and the maximum decomposition temperature was 317°C. Thermoplastic starch (TPS) prepared from A. hippocastanum with glycerol and processed by melt blending exhibited adequate mechanical and thermal properties. In contrast, plasticized TPS with glycerol:malic acid (1:1) showed lower thermal stability and a pasty and sticky behavior, indicating that malic acid accelerates degradation of starch during processing.

Keywords: Aesculus hippocastanum L., amylopectin structure, thermoplastic starch, non-edible source

Procedia PDF Downloads 342
5361 X-Ray Diffraction and Crosslink Density Analysis of Starch/Natural Rubber Polymer Composites Prepared by Latex Compounding Method

Authors: Raymond Dominic Uzoh

Abstract:

Starch fillers were extracted from three plant sources namely amora tuber (a wild variety of Irish potato), sweet potato and yam starch and their particle size, pH, amylose, and amylopectin percentage decomposition determined accordingly by high performance liquid chromatography (HPLC). The starch was introduced into natural rubber in liquid phase (through gelatinization) by the latex compounding method and compounded according to standard method. The prepared starch/natural rubber composites was characterized by Instron Universal testing machine (UTM) for tensile mechanical properties. The composites was further characterized by x-ray diffraction and crosslink density analysis. The particle size determination showed that amora starch granules have the highest particle size (156 × 47 μm) followed by yam starch (155× 40 μm) and then the sweet potato starch (153 × 46 μm). The pH test also revealed that amora starch has a near neutral pH of 6.9, yam 6.8, and sweet potato 5.2 respectively. Amylose and amylopectin determination showed that yam starch has a higher percentage of amylose (29.68), followed by potato (22.34) and then amora starch with the lowest value (14.86) respectively. The tensile mechanical properties testing revealed that yam starch produced the best tensile mechanical properties followed by amora starch and then sweet potato starch. The structure, crystallinity/amorphous nature of the product composite was confirmed by x-ray diffraction, while the nature of crosslinking was confirmed by swelling test in toluene solvent using the Flory-Rehner approach. This research study has rendered a workable strategy for enhancing interfacial interaction between a hydrophilic filler (starch) and hydrophobic polymeric matrix (natural rubber) yielding moderately good tensile mechanical properties for further exploitation development and application in the rubber processing industry.

Keywords: natural rubber, fillers, starch, amylose, amylopectin, crosslink density

Procedia PDF Downloads 143
5360 Synthesis of Biopolymeric Nanoparticles of Starch for Packaging Reinforcement Applications

Authors: Yousof Farrag, Sara Malmir, Rebeca Bouza, Maite Rico, Belén Montero, Luís Barral

Abstract:

Biopolymers are being extensively studied in the last years as a replacement of the conventional petroleum derived polymers, especially in packaging industry. They are natural, biodegradable materials. However, the lack of good mechanical and barrier properties is a problem in the way of this replacement. One of the most abundant biopolymers in the nature is the starch, its renewable, biocompatible low cost polysaccharide, it can be obtained from wide variety of plants, it has been used in food, packaging and other industries. This work is focusing on the production a high yield of starch nanoparticles via nanoprecipitation, to be used as reinforcement filling of biopolymer packaging matrices made of different types of starch improving their mechanical and barrier properties. Wheat and corn starch solutions were prepared in different concentrations. Absolute ethanol, acetone and different concentrations of hydrochloric acid were added as antisolvents dropwise under different amplitudes of sonication and different speeds of stirring, the produced particles were analyzed with dynamic light scattering DLS and scanning electron microscope SEM getting the morphology and the size distribution to study the effect of those factors on the produced particles. DLS results show that we have nanoparticles using low concentration of corn starch (0.5%) using 0.1M HCl as antisolvent, [Z average: 209 nm, PDI: 0,49], in case of wheat starch, we could obtain nanoparticles [Z average: 159 nm, PDI: 0,45] using the same starch solution concentration together with absolute ethanol as antisolvent.

Keywords: biopolymers, nanoparticles, DLS, starch

Procedia PDF Downloads 296
5359 Characterization of Edible Film from Uwi Starch (Dioscorea alata L.)

Authors: Miksusanti, Herlina, Wiwin

Abstract:

The research about modification uwi starch (Dioscorea alata L) by using propylene oxide has been done. Concentration of propylene oxide were 6%(v/w), 8%(v/w), and 10%(v/w). The amilograf parameters after modification were characteristic breakdown viscosity 43 BU and setback viscosity 975 BU. The modification starch have edible properties according to FDA (Food and Drug Administration) which have degree of modification < 7%, degree of substitution < 0,1 and propylene oxide concentration < 10%(v/w). The best propylene oxide in making of edible film was 8 %( v/w). The starch control can be made into edible film with thickness 0,136 mm, tensile strength 20,4605 MPa and elongation 22%. Modification starch of uwi can be made into edible film with thickness 0,146 mm, tensile strength 25, 3521 Mpa, elongation 30% and water vapor transmission 7, 2651 g/m2/24 hours. FTIR characterization of uwi starch showed the occurrence of hydroxypropylation. The peak spectrum at 2900 cm-1 showed bonding of C-H from methyl group, which is characteristic for modification starch with hydroxypropyl. Characterization with scanning electron microscopy showed that modification of uwi starch has turned the granule of starch to be fully swallon.

Keywords: uwi starch, edible film, propylen oxide, modification

Procedia PDF Downloads 269
5358 Synthesis and Properties of Oxidized Corn Starch Based Wood Adhesive

Authors: Salise Oktay, Nilgun Kizilcan, Basak Bengu

Abstract:

At present, formaldehyde-based adhesives such as urea-formaldehyde (UF), melamine-formaldehyde (MF), melamine – urea-formaldehyde (MUF), etc. are mostly used in wood-based panel industry because of their high reactivity, chemical versatility, and economic competitiveness. However, formaldehyde-based wood adhesives are produced from non- renewable resources and also formaldehyde is classified as a probable human carcinogen (Group B1) by the U.S. Environmental Protection Agency (EPA). Therefore, there has been a growing interest in the development of environment-friendly, economically competitive, bio-based wood adhesives to meet wood-based panel industry requirements. In this study, like a formaldehyde-free adhesive, oxidized starch – urea wood adhesives was synthesized. In this scope, firstly, acid hydrolysis of corn starch was conducted and then acid thinned corn starch was oxidized by using hydrogen peroxide and CuSO₄ as an oxidizer and catalyst, respectively. Secondly, the polycondensation reaction between oxidized starch and urea conducted. Finally, nano – TiO₂ was added to the reaction system to strengthen the adhesive network. Solid content, viscosity, and gel time analyses of the prepared adhesive were performed to evaluate the adhesive processability. FTIR, DSC, TGA, SEM characterization techniques were used to investigate chemical structures, thermal, and morphological properties of the adhesive, respectively. Rheological analysis of the adhesive was also performed. In order to evaluate the quality of oxidized corn starch – urea adhesives, particleboards were produced in laboratory scale and mechanical and physical properties of the boards were investigated such as an internal bond, modulus of rupture, modulus of elasticity, formaldehyde emission, etc. The obtained results revealed that oxidized starch – urea adhesives were synthesized successfully and it can be a good potential candidate to use the wood-based panel industry with some developments.

Keywords: nano-TiO₂, corn starch, formaldehyde emission, wood adhesives

Procedia PDF Downloads 119
5357 Barrier Properties of Starch-Ethylene Vinyl Alcohol Nanocomposites

Authors: Farid Amidi Fazli

Abstract:

Replacement of plastics used in the food industry seems to be a serious issue to overcome mainly the environmental problems in recent years. This study investigates the hydrophilicity and permeability properties of starch biopolymer which ethylene vinyl alcohol (EVOH) (0-10%) and nanocrystalline cellulose (NCC) (1 -15%) were used to enhance its properties. Starch -EVOH nanocomposites were prepared by casting method in different formulations. NCC production by acid hydrolysis was confirmed by scanning electron microscopy. Solubility, water vapor permeability, water vapor transmission rate and moisture absorbance were measured on each of the nanocomposites. The results were analyzed by SAS software. The lowest moisture absorbance was measured in pure starch nanocomposite containing 8% NCC. The lowest permeability to water vapor belongs to starch nanocomposite containing 8% NCC and the sample containing 7.8% EVOH and 13% NCC. Also, the lowest solubility was observed in the composite contains the highest amount of EVOH. Applied Process resulted in production of bio films which have good resistance to water vapor permeability and solubility in water. The use of NCC and EVOH leads to reduced moisture absorbance property of the biofilms.

Keywords: starch, EVOH, nanocrystalline cellulose, hydrophilicity

Procedia PDF Downloads 389
5356 Characteristics of Oil-In-Water Emulsion Stabilized with Pregelatinized Waxy Rice Starch

Authors: R. Yulianingsih, S. Gohtani

Abstract:

Characteristics of pregelatinized waxy rice starch (PWR) gelatinized at different temperatures (65, 75, and 85 °C, abbreviated as PWR 65, 75 and 85 respectively) and their emulsion-stabilizing properties at different starch concentrations (3, 5, 7, and 9%) were studied. The yield stress and consistency index value of PWR solution increased with an increase in starch concentration. The pseudoplasticity of PWR 65 solution increased and that for both PWR 75 and 85 solution decreased with an increase in starch concentration. Small angle X-ray scattering (SAXS) profiles analyzed by Kratky Plot indicated that PWR 65 is natively unfolded particles while PWR 75 and 85 are the globular particles. The characteristics of emulsions stabilized with PWR were influenced by the temperature of gelatinization process and starch concentration. Elevated concentration of starch decreased the value of yield stress and increased the consistency index. PWR 65 produce stable emulsion to creaming at starch concentrations more than 5%, while PWR 85 is able to produce stable emulsion to both creaming and coalescence of droplets.

Keywords: emulsion, gelatinization temperature, rheology, small-angle X-ray scattering, waxy rice starch

Procedia PDF Downloads 135
5355 Characterization and Degradation Analysis of Tapioca Starch Based Biofilms

Authors: R. R. Ali, W. A. W. A. Rahman, R. M. Kasmani, H. Hasbullah, N. Ibrahim, A. N. Sadikin, U. A. Asli

Abstract:

In this study, tapioca starch which acts as natural polymer was added in the blend in order to produce biodegradable product. Low density polyethylene (LDPE) and tapioca starch blends were prepared by extrusion and the test sample by injection moulding process. Ethylene vinyl acetate (EVA) acts as compatibilizer while glycerol as processing aid was added in the blend. The blends were characterized by using melt flow index (MFI), fourier transform infrared (FTIR) and the effects of water absorption to the sample. As the starch content increased, MFI of the blend was decreased. Tensile testing were conducted shows the tensile strength and elongation at break decreased while the modulus increased as the starch increased. For the biodegradation, soil burial test was conducted and the loss in weight was studied as the starch content increased. Morphology studies were conducted in order to show the distribution between LDPE and starch.

Keywords: biopolymers, degradable polymers, starch based polyethylene, injection moulding

Procedia PDF Downloads 252
5354 Characterization and Quantification of Relatives Amounts of Phosphorylated Glucosyl Residues in C6 and C3 Position in Banana Starch Granules by 31P-NMR

Authors: Renata Shitakubo, Hanyu Yangcheng, Jay-lin Jane, Fernanda Peroni Okita, Beatriz Cordenunsi

Abstract:

In the degradation transitory starch model, the enzymatic activity of glucan/water dikinase (GWD) and phosphoglucan/water dikinase (PWD) are essential for the granule degradation. GWD and PWD phosphorylate glucose molecules in the positions C6 and C3, respectively, in the amylopectin chains. This action is essential to allow that β-amylase degrade starch granules without previous action of α-amylase. During banana starch degradation, as part of banana ripening, both α- and β-amylases activities and proteins were already detected and, it is also known that there is a GWD and PWD protein bounded to the starch granule. Therefore, the aim of this study was to quantify both Gluc-6P and Gluc-3P in order to estimate the importance of the GWD-PWD-β-amylase pathway in banana starch degradation. Starch granules were isolated as described by Peroni-Okita et al (Carbohydrate Polymers, 81:291-299, 2010), from banana fruit at different stages of ripening, green (20.7%), intermediate (18.2%) and ripe (6.2%). Total phosphorus content was determinate following the Smith and Caruso method (1964). Gluc-6P and Gluc-3P quantifications were performed as described by Lim et al (Cereal Chemistry, 71(5):488-493, 1994). Total phosphorous content in green banana starch is found as 0.009%, intermediary banana starch 0.006% and ripe banana starch 0.004%, both by the colorimetric method and 31P-NMR. The NMR analysis showed the phosphorus content in C6 and C3. The results by NMR indicate that the amylopectin is phosphorylate by GWD and PWD before the bananas become ripen. Since both the total content of phosphorus and phosphorylated glucose molecules at positions C3 and C6 decrease with the starch degradation, it can be concluded that this phosphorylation occurs only in the surface of the starch granule and before the fruit be harvested.

Keywords: starch, GWD, PWD, 31P-NMR

Procedia PDF Downloads 427
5353 Impact of Heat Moisture Treatment on the Yield of Resistant Starch and Evaluation of Functional Properties of Modified Mung Bean (Vigna radiate) Starch

Authors: Sreejani Barua, P. P. Srivastav

Abstract:

Formulation of new functional food products for diabetes patients and obsessed people is a challenge for food industries till date. Starch is a certainly happening, ecological, reasonable and profusely obtainable polysaccharide in plant material. In the present scenario, there is a great interest in modifying starch functional properties without destroying its granular structure using different modification techniques. Resistant starch (RS) contains almost zero calories and can control blood glucose level to prevent diabetes. The current study focused on modification of mung bean starch which is a good source of legumes carbohydrate for the production of functional food. Heat moisture treatment (HMT) of mung starch was conducted at moisture content of 10-30%, temperature of 80-120 °C and time of 8-24 h.The content of resistant starch after modification was significantly increased from native starches containing RS 7.6%. The design combinations of HMT had been completed through Central Composite Rotatable Design (CCRD). The effects of HMT process variables on the yield of resistant starch was studied through Rapid Surface Methodology (RSM). The highest increase of resistant starch was found up to 34.39% when treated the native starch with 30% m.c at 120 °C temperature for 24 h.The functional properties of both native and modified mung bean starches showed that there was a reduction in the swelling power and swelling volume of HMT starches. However, the solubility of the HMT starches was higher than that of untreated native starch and also observed change in structural (scanning electron microscopy), X-Ray diffraction (XRD) pattern, blue value and thermal (differential scanning calorimetry) properties. Therefore, replacing native mung bean starch with heat-moisture treated mung bean starch leads to the development of new products with higher resistant starch levels and functional properties.

Keywords: Mung bean starch, heat moisture treatment, functional properties, resistant starch

Procedia PDF Downloads 169
5352 Optimal Consume of NaOH in Starches Gelatinization for Froth Flotation

Authors: André C. Silva, Débora N. Sousa, Elenice M. S. Silva, Thales P. Fontes, Raphael S. Tomaz

Abstract:

Starches are widely used as depressant in froth flotation operations in Brazil due to their efficiency, increasing the selectivity in the inverse flotation of quartz depressing iron ore. Starches market have been growing and improving in recent years, leading to better products attending the requirements of the mineral industry. The major source of starch used for iron ore is corn starch, which needs to be gelatinized with sodium hydroxide (NaOH) prior to use. This stage has a direct impact on industrials costs, once the lowest consumption of NaOH in gelatinization provides better control of the pH in the froth flotation and reduces the amount of electrolytes present in the pulp. In order to evaluate the gelatinization degree of different starches and flour were subjected to the addiction of NaOH and temperature variation experiments. Samples of starch (corn, cassava, HIPIX 100, HIPIX 101 and HIPIX 102 commercialized by Ingredion) and flour (cassava and potato) were tested. The starch samples were characterized through Scanning Electronic Microscopy and the amylose content were determined through spectrometry, swelling and solubility tests. The gelatinization was carried out through titration with NaOH, keeping the solution temperature constant at 40 oC. At the end of the tests, the optimal amount of NaOH consumed to gelatinize the starch or flour from different botanical sources was established and a correlation between the content of amylopectin in the starch and the starch/NaOH ratio needed for its gelatinization.

Keywords: froth flotation, gelatinization, sodium hydroxide, starches and flours

Procedia PDF Downloads 334
5351 Bio-Based Polyethylene/Rice Starch Composite Prepared by Twin Screw Extruder

Authors: Waris Piyaphon, Sathaphorn O-Suwankul, Kittima Bootdee, Manit Nithitanakul

Abstract:

Starch from rice was used as a filler in low density polyethylene in preparation of low density polyethylene/rice starch composite. This study aims to prepare LDPE/rice starch composites. Glycerol (GC) was used as a plasticizer in order to increase dispersion and reduce agglomeration of rice starch in low density polyethylene (LDPE) matrix. Low density polyethylene grafted maleic anhydride (LDPE-g-MA) was used as a compatibilizer to increase the compatibility between LDPE and rice starch. The content of rice starch was varied between 10, 20, and 30 %wt. Results indicated that increase of rice starch content reduced tensile strength at break, elongation, and impact strength of composites. LDPE-g-MA showed positive effect on mechanical properties which increased in tensile strength and impact properties as well as compatibility between rice starch and LDPE matrix. Moreover, the addition of LDPE-g-MA significantly improved the impact strength by 50% compared to neat composite. The incorporation of GC enhanced the processability of composite. Introduction of GC affected the viscosity after blending by reducing the viscosity at all shear rate. The presence of plasticizer increased the impact strength but decreased the stiffness of composite. Water absorption of the composite was increased when plasticizer was added.

Keywords: composite material, plastic starch composite, polyethylene composite, PE grafted maleic anhydride

Procedia PDF Downloads 171
5350 Comparison of White Sauce Prepared from Native and Chemically Modified Corn and Pearl Millet Starches

Authors: Marium Shaikh, Tahira M. Ali, Abid Hasnain

Abstract:

Physical and sensory properties of white sauces prepared from native and chemically modified corn and pearl millet starches were compared. Interestingly, no syneresis was observed in hydroxypropylated corn and pearl millet starch containing white sauce even after nine days of cold storage (4 °C), while other modifications also reduced the syneresis significantly in comparison to their native counterparts. White sauce containing succinylated corn starch showed least oil separation due to its greater emulsion stability. Light microscopy was used to visualize the size and shape of fat globules, and it was found that they were most homogenously distributed in succinylated and hydroxypropylated samples. Sensory results revealed that chemical modification of corn and pearl millet starch improved the consistency, thickness and overall acceptability of white sauces. Viscosity profiles showed that pasting parameters of native pearl millet starch are almost similar to native corn starch suggesting pearl millet starch as an alternative of corn starch. Also, white sauce prepared from modified pearl millet starch showed better cold storage stability in terms of various textural attributes like hardness, cohesiveness, chewiness, and springiness.

Keywords: corn starch, pearl millet, hydroxypropylation, succinylation, white sauce

Procedia PDF Downloads 259
5349 Effect of Tapioca Starch on Fresh Properties Concrete

Authors: C. Samita, W. Chalermchai

Abstract:

This project is aimed to be a preliminary study of using Tapioca Starch as a viscosity modifying agent (VMA) in concrete work. Tapioca starch effects on the viscosity of concrete, which could be investigated from the workability of corresponding mortar. Cement only mortars with water to cement ratio (w/c) 0.25 to 0.48, superplasticizer dosage of 1% to 2.5%, starch concentration of 0%, 0.25% and 0.5%, was tested for workability. Mortar mixes that have equivalent workability (flow diameter of 250 mm, and funnel flow time of 5 seconds) for each starch concentration were identified and checked for concrete properties. Concrete were tested for initial workability, workability loss, bleeding, setting times, and compressive strength. The results showed that all concrete mixes provide same initial workability, however the mix with higher starch concentration provides slower loss. Bleeding occurs when concrete has w/c more than 0.45. For setting times, mixing with higher starch concentration provide longer setting times (around 4 hours in this experiment). Compressive strength of starch concretes which always have higher w/c, are lower than that of cement only concrete as in this experiment initial workability were controlled to be same.

Keywords: viscosity modifying agent(VMA), self-leveling concrete, self-compacting concrete(SCC), low-binder SCC

Procedia PDF Downloads 253
5348 Biodegradability and Thermal Properties of Polycaprolactone/Starch Nanocomposite as a Biopolymer

Authors: Emad A. Jaffar Al-Mulla

Abstract:

In this study, a biopolymer-based nanocomposite was successfully prepared through melt blending technique. Two biodegradable polymers, polycaprolactone and starch, environmental friendly and obtained from renewable, easily available raw materials, have been chosen. Fatty hydrazide, synthesized from palm oil, has been used as a surfactant to modify montmorillonite (natural clay) for preparation of polycaprolactone/starch nanocomposite. X-ray diffraction and transmission electron microscopy were used to characterize nanocomposite formation. Compatibility of the blend was improved by adding 3% weight modified clay. Higher biodegradability and thermal stability of nanocomopeite were also observed compared to those of the polycaprolactone/starch blend. This product will solve the problem of plastic waste, especially disposable packaging, and reduce the dependence on petroleum-based polymers and surfactants.

Keywords: polycaprolactone, starch, biodegradable, nanocomposite

Procedia PDF Downloads 322
5347 Adhesive Based upon Polyvinyl Alcohol And Chemical Modified Oca (Oxalis tuberosa) Starch

Authors: Samantha Borja, Vladimir Valle, Pamela Molina

Abstract:

The development of adhesives from renewable raw materials attracts the attention of the scientific community, due to it promises the reduction of the dependence with materials derived from oil. This work proposes the use of modified 'oca (Oxalis tuberosa)' starch and polyvinyl alcohol (PVA) in the elaboration of adhesives for lignocellulosic substrates. The investigation focused on the formulation of adhesives with 3 different PVA:starch (modified and native) ratios (of 1,0:0,33; 1,0:1,0; 1,0:1,67). The first step to perform it was the chemical modification of starch through acid hydrolysis and a subsequent urea treatment to get carbamate starch. Then, the adhesive obtained was characterized in terms of instantaneous viscosity, Fourier-transform infrared spectroscopy (FTIR) and shear strength. The results showed that viscosity and mechanical tests exhibit data with the same tendency in relation to the native and modified starch concentration. It was observed that the data started to reduce its values to a certain concentration, where the values began to grow. On the other hand, two relevant bands were found in the FTIR spectrogram. The first in 3300 cm⁻¹ of OH group with the same intensity for all the essays and the other one in 2900 cm⁻¹, belonging to the group of alkanes with a different intensity for each adhesive. On the whole, the ratio PVA:starch (1:1) will not favor crosslinking in the adhesive structure and causes the viscosity reduction, whereas, in the others ones, the viscosity is higher. It was also observed that adhesives made with modified starch had better characteristics, but the adhesives with high concentrations of native starch could equal the properties of the adhesives made with low concentrations of modified starch.

Keywords: polyvinyl alcohol, PVA, chemical modification, starch, FTIR, viscosity, shear strength

Procedia PDF Downloads 122
5346 Effect of Modification on the Properties of Blighia sapida (Ackee) Seed Starch

Authors: Olufunmilola A. Abiodun, Adegbola O. Dauda, Ayobami Ojo, Samson A. Oyeyinka

Abstract:

Blighia sapida (Ackee) seed is a neglected and under-utilised crop. The fruit is cultivated for the aril which is used as meat substitute in soup while the seed is discarded. The seed is toxic due to the presence of hypoglycin which causes vomiting and death. The seed is shining black and bigger than the legume seeds. The seed contains high starch content which could serve as a cheap source of starch hereby reducing wastage of the crop during its season. Native starch had limitation in their use; therefore, modification of starch had been reported to improve the functional properties of starches. Therefore, this work determined the effect of modification on the properties of Blighia sapida seed starch. Blighia sapida seed was dehulled manually, milled and the starch extracted using standard method. The starch was subjected to modification using four methods (acid, alkaline, oxidized and acetylated methods). The morphological structure, form factor, granule size, amylose, swelling power, hypoglycin and pasting properties of the starches were determined. The structure of Blighia sapida using light microscope showed that the seed starch demonstrated an oval, round, elliptical, dome-shaped and also irregular shape. The form factors of the starch ranged from 0.32-0.64. Blighia sapida seed starches were smaller in granule sizes ranging from 2-6 µm. Acid modified starch had the highest amylose content (24.83%) and was significantly different ( < 0.05) from other starches. Blighia sapida seed starches showed a progressive increase in swelling power as temperature increased in native, acidified, alkalized, oxidized and acetylated starches but reduced with increasing temperature in pregelatinized starch. Hypoglycin A ranged from 3.89 to 5.74 mg/100 g with pregelatinized starch having the lowest value and alkalized starch having the highest value. Hypoglycin B ranged from 7.17 to 8.47 mg/100 g. Alkali-treated starch had higher peak viscosity (3973 cP) which was not significantly different (p > 0.05) from the native starch. Alkali-treated starch also was significantly different (p > 0.05) from other starches in holding strength value while acetylated starch had higher breakdown viscosity (1161.50 cP). Native starch was significantly different (p > 0.05) from other starches in final and setback viscosities. Properties of Blighia sapida modified starches showed that it could be used as a source of starch in food and other non-food industries and the toxic compound found in the starch was very low when compared to lethal dosage.

Keywords: Blighia sapida seed, modification, starch, hypoglycin

Procedia PDF Downloads 204
5345 Influence of [Emim][OAc] and Water on Gelatinization Process and Interactions with Starch

Authors: Shajaratuldur Ismail, Nurlidia Mansor, Zakaria Man

Abstract:

Thermoplastic starch (TPS) plasticized by 1-ethyl-3-methylimidazolium acetate [Emim][OAc] were obtained through gelatinization process. The gelatinization process occurred in the presence of water and [Emim][OAc] as plasticizer at high temperature (90˚C). The influence of [Emim][OAc] and water on the gelatinization and interactions with starch have been studied over a range of compositions. The homogenous mass was obtained for the samples containing 35, 40 and 43.5 % of water contents which showed that water plays important role in gelatinization process. Detailed IR spectroscopy analysis showed decrease in hydrogen bonding intensity and strong interaction between acetate anion in [Emim][OAc] and starch hydroxyl groups in the presence of [Emim][OAc]. Starch-[Emim][OAc]-water mixture at 10-3-8.7 presented homogenous mass, less hydrogen bonding intensity and strong interaction between acetate anion in [Emim][OAc] and starch hydroxyl groups.

Keywords: starch, ionic liquid, 1-ethyl-3-methylimidazolium acetate, plasticizer, gelatinization, IR spectroscopy

Procedia PDF Downloads 206
5344 Response Surface Methodology Approach to Defining Ultrafiltration of Steepwater from Corn Starch Industry

Authors: Zita I. Šereš, Ljubica P. Dokić, Dragana M. Šoronja Simović, Cecilia Hodur, Zsuzsanna Laszlo, Ivana Nikolić, Nikola Maravić

Abstract:

In this work the concentration of steep-water from corn starch industry is monitored using ultrafiltration membrane. The aim was to examine the conditions of ultrafiltration of steep-water by applying the membrane of 2.5nm. The parameters that vary during the course of ultrafiltration, were the transmembrane pressure, flow rate, while the permeate flux and the dry matter content of permeate and retentive were the dependent parameter constantly monitored during the process. Experiments of ultrafiltration are conducted on the samples of steep-water, which were obtained from the starch wet milling plant Jabuka, Pancevo. The procedure of ultrafiltration on a single-channel 250mm length, with inner diameter of 6.8mm and outer diameter of 10mm membrane were carried on. The membrane is made of a-Al2O3 with TiO2 layer obtained from GEA (Germany). The experiments are carried out at a flow rate ranging from 100 to 200lh-1 and transmembrane pressure of 1-3 bars. During the experiments of steep-water ultrafiltration, the change of permeate flux, dry matter content of permeate and retentive, as well as the absorbance changes of the permeate and retentive were monitored. The experimental results showed that the maximum flux reaches about 40lm-2h-1. For responses obtained after experiments, a polynomial model of the second degree is established to evaluate and quantify the influence of the variables. The quadratic equitation fits with the experimental values, where the coefficient of determination for flux is 0.96. The dry matter content of the retentive is increased for about 6%, while the dry matter content of permeate was reduced for about 35-40%, respectively. During steep-water ultrafiltration in permeate stays 40% less dry matter compared to the feed.

Keywords: ultrafiltration, steep-water, starch industry, ceramic membrane

Procedia PDF Downloads 253
5343 Effect of Dehydration Methods of the Proximate Composition, Mineral Content and Functional Properties of Starch Flour Extracted from Maize

Authors: Olakunle M. Makanjuola, Adebola Ajayi

Abstract:

Effect of the dehydrated method on proximate, functional and mineral properties of corn starch was evaluated. The study was carried and to determine the proximate, functional and mineral properties of corn starch produced using three different drying methods namely (sun) (oven) and (cabinet) drying methods. The corn starch was obtained by cleaning, steeping, milling, sieving, dewatering and drying corn starch was evaluated for proximate composition, functional properties, and mineral properties to determine the nutritional properties, moisture, crude protein, crude fat, ash, and carbohydrate were in the range of 9.35 to 12.16, 6.5 to 10.78 1.08 to 2.5, 1.08 to 2.5, 4.0 to 5.2, 69.58 to 75.8% respectively. Bulk density range between 0.610g/dm3 to 0.718 g/dm3, water, and oil absorption capacities range between 116.5 to 117.25 and 113.8 to 117.25 ml/g respectively. Swelling powder had value varying from 1.401 to 1.544g/g respectively. The results indicate that the cabinet method had the best result item of the quality attribute.

Keywords: starch flour, maize, dehydration, cabinet dryer

Procedia PDF Downloads 210
5342 Concentration of Waste Waters by Enzyme-Assisted Low-Temperature Evaporation

Authors: Ahokas Mikko, Taskila Sanna, Varrio Kalle, Tanskanen Juha

Abstract:

The present research aimed at the development of an energy efficient process for the concentration of starchy waste waters. The selected principle is mechanical vapor recompression evaporation (MVR) which leads to concentrated solid material and evaporated water phase. Evaporation removes water until a certain viscosity limit is reached. Materials with high viscosity cannot be concentrated using standard evaporators due to limitations of pumps and other constraints, such as wetting. Control of viscosity is thus essential for efficient evaporation. This applies especially to fluids in which due starch or other compounds the viscosity tends to increase via removal of water. In the present research, the effect of enzymes on evaporation of highly viscous starch industry waste waters was investigated. Wastewater samples were received from starch industry at pH of 4.8. Response surface methodology (RSM) was applied for the investigation of factor effects on the behaviour of concentrate during evaporation. The RSM was prepared using quadratic face-centered central composite design (CCF). The evaporation performance was evaluated by monitoring the viscosity of fluid during processing. Based on viscosity curves, the addition of glucoamylase reduced the viscosity during evaporation. This assumption was confirmed by CCF, suggesting that the use of starch decomposing glucoamylase allowed evaporation of the starchy wastewater to a relatively high total solid concentration without a detrimental increase in the viscosity. The results suggest that use of enzymes for reduction of viscosity during the evaporation allows more effective concentration of the wastewater and thereby recovery of potable water.

Keywords: viscous, wastewater, treatment, evaporation, concentration

Procedia PDF Downloads 217
5341 Mimosa Tannin – Starch - Sugar Based Wood Adhesive

Authors: Salise Oktay, Nilgün Kizilcan, Başak Bengü

Abstract:

At present, formaldehyde based adhesives such as urea formaldehyde (UF), melamine formaldehyde (MF), melamine – urea formaldehyde (MUF), etc. are mostly used in wood based panel industry because of their high reactivity, chemical versatility, and economic competitiveness. However, formaldehyde based wood adhesives are produced from non- renewable resources. Hence, there has been a growing interest in the development of environment friendly, economically competitive, bio-based wood adhesives in order to meet wood based panel industry requirements. In this study, as formaldehyde free adhesive, Mimosa tannin, starch, sugar based wood adhesivewas synthesized. Citric acid and tartaric acid were used as hardener for the resin system. Solid content, viscosity, and gel time analyzes of the prepared adhesive were performed in order to evaluate the adhesive processability. FTIR characterization technique was used to elucidate the chemical structures of the cured adhesivesamples. In order to evaluate the performance of the prepared bio-based resin formulation, particleboards were produced in a laboratory scale, and mechanical, physical properties of the boards were investigated. Besides, the formaldehyde contents of the boards were determined by using the perforator method. The obtained results revealed that the developed bio-based wood adhesive formulation can be a good potential candidate to use wood based panel industry with some developments.

Keywords: bio-based wood adhesives, mimosa tannin, corn starch, sugar, polycarboxyclic acid

Procedia PDF Downloads 205
5340 Starch-Based Systems for the Nano-Delivery of Quercetin

Authors: Fernando G. Torres, Omar P. Troncoso

Abstract:

Quercetin is a naturally occurring polyphenol found in many vegetables, such as onion, with antioxidant properties. It is a dietary component with a documented role in reducing different human cancers. However, its low bioavailability, poor water solubility, and chemical instability limit its applications. Different nano-delivery systems such as nanoparticles, micelles, and nanohydrogels have been studied in order to improve the bioavailability of quercetin. Nanoparticles based on natural polymers such as starch have the advantage of being biocompatible, biodegradable, and non-toxic. In this study, quercetin was loaded into starch nanoparticles using a nanoprecipitation method. Different routes, using sodium tripolyphosphate and Tween® 80 as tensioactive agents, were tested in order to obtain an optimized starch-based nano-delivery system. The characterization of the nanoparticles loaded with quercetin was assessed by Fourier Transform Infrared Spectroscopy, Dynamic Light Scattering, Zeta potential, and Differential scanning calorimetry. UV-vis spectrophotometry was used to evaluate the loading efficiency and capacity of the samples. The results showed that starch-based systems could be successfully used for the nano-delivery of quercetin.

Keywords: starch nanoparticles, nanoprecipitation, quercetin, biomedical applications

Procedia PDF Downloads 103
5339 Preparation and Properties of Chloroacetated Natural Rubber Rubber Foam Using Corn Starch as Curing Agent

Authors: Ploenpit Boochathum, Pitchayanad Kaolim, Phimjutha Srisangkaew

Abstract:

In general, rubber foam is produced based on the sulfur curing system. However, the remaining sulfur in the rubber product waste is burned to sulfur dioxide gas causing the environment pollution. To avoid using sulfur as curing agent in the rubber foam products, this research work proposes non-sulfur curing system by using corn starch as a curing agent. The ether crosslinks were proposed to be produced via the functional bonding between hydroxyl groups of the starch molecules and chloroacetate groups added on the natural rubber molecules. The chloroacetated natural rubber (CNR) latex was prepared via the epoxidation reaction of the concentrated natural rubber latex, subsequently, epoxy rings were attacked by chloroacetic acid to produce hydroxyl groups and chloroacetate groups on the rubber molecules. Foaming agent namely NaHCO3 was selected to add in the CNR latex due to the low decomposition temperature at about 50°C. The appropriate curing temperature was assigned to be 90°C that is above gelatinization temperature; 60-70°C, of starch. The effect of weight ratio of starch, i.e., 0 phr, 3 phr and 5 phr, on the physical properties of CNR rubber foam was investigated. It was found that density reduced from 0.81 g/cm3 for 0 phr to 0.75 g/cm3 for 3 phr and 0.79 g/cm3 for 5 phr. The ability to return to its original thickness after prolonged compressive stresses of CNR rubber foam cured with starch loading of 5 phr was found to be considerably better than that of CNR rubber foam cured with starch 3 phr and CNR rubber foam without addition of starch according to the compression set that was determined to decrease from 66.67% to 40% and 26.67% with the increase loading of starch. The mechanical properties including tensile strength and modulus of CNR rubber foams cured using starch were determined to increase except that the elongation at break was found to decrease. In addition, all mechanical properties of CNR rubber foams cured with the starch 3 phr and 5 phr were found to be slightly different and drastically higher than those of CNR rubber foam without the addition of starch. This research work indicates that starch can be applicable as a curing agent for CNR rubber. This is confirmed by the increase of the elastic modulus (G') of CNR rubber foams that was cured with the starch over the CNR rubber foam without curing agent. This type of rubber foam is believed to be one of the biodegradable and environment-friendly product that can be cured at low temperature of 90°C.

Keywords: chloroacetated natural rubber, corn starch, non-sulfur curing system, rubber foam

Procedia PDF Downloads 274
5338 Interfacial Adhesion and Properties Improvement of Polyethylene/Thermoplastic Starch Blend Compatibilized by Stearic Acid-Grafted-Starch

Authors: Nattaporn Khanoonkon, Rangrong Yoksan, Amod A. Ogale

Abstract:

Polyethylene (PE) is one of the most petroleum-based thermoplastic materials used in many applications including packaging due to its cheap, light-weight, chemically inert and capable to be converted into various shapes and sizes of products. Although PE is a commercially potential material, its non-biodegradability caused environmental problems. At present, bio-based polymers become more interesting owing to its bio-degradability, non-toxicity, and renewability as well as being eco-friendly. Thermoplastic starch (TPS) is a bio-based and biodegradable plastic produced from the plasticization of starch under applying heat and shear force. In many researches, TPS was blended with petroleum-based polymers including PE in order to reduce the cost and the use of those polymers. However, the phase separation between hydrophobic PE and hydrophilic TPS limited the amount of TPS incorporated. The immiscibility of two different polarity polymers can be diminished by adding compatibilizer. PE-based compatibilizers, e.g. polyethylene-grafted-maleic anhydride, polyethylene-co-vinyl alcohol, etc. have been applied for the PE/TPS blend system in order to improve their miscibility. Until now, there is no report about the utilization of starch-based compatibilizer for PE/TPS blend system. The aims of the present research were therefore to synthesize a new starch-based compatibilizer, i.e. stearic acid-grafted starch (SA-g-starch) and to study the effect of SA-g-starch on chemical interaction, morphological properties, tensile properties and water vapor as well as oxygen barrier properties of the PE/TPS blend films. PE/TPS blends without and with incorporating SA-g-starch with a content of 1, 3 and 5 part(s) per hundred parts of starch (phr) were prepared using a twin screw extruder and then blown into films using a film blowing machine. Incorporating 1 phr and 3 phr of SA-g-starch could improve miscibility of the two polymers as confirmed from the reduction of TPS phase size and the good dispersion of TPS phase in PE matrix. In addition, the blend containing SA-g-starch with contents of 1 phr and 3 phr exhibited higher tensile strength and extensibility, as well as lower water vapor and oxygen permeabilities than the naked blend. The above results suggested that SA-g-starch could be potentially applied as a compatibilizer for the PE/TPS blend system.

Keywords: blend, compatibilizer, polyethylene, thermoplastic starch

Procedia PDF Downloads 408
5337 Synthesis and Characterisation of Starch-PVP as Encapsulation Material for Drug Delivery System

Authors: Nungki Rositaningsih, Emil Budianto

Abstract:

Starch has been widely used as an encapsulation material for drug delivery system. However, starch hydrogel is very easily degraded during metabolism in human stomach. Modification of this material is needed to improve the encapsulation process in drug delivery system, especially for gastrointestinal drug. In this research, three modified starch-based hydrogels are synthesized i.e. Crosslinked starch hydrogel, Semi- and Full- Interpenetrating Polymer Network (IPN) starch hydrogel using Poly(N-Vinyl-Pyrrolidone). Non-modified starch hydrogel was also synthesized as a control. All of those samples were compared as biomaterials, floating drug delivery, and their ability in loading drug test. Biomaterial characterizations were swelling test, stereomicroscopy observation, Differential Scanning Calorimetry (DSC), and Fourier Transform Infrared Spectroscopy (FTIR). Buoyancy test and stereomicroscopy scanning were done for floating drug delivery characterizations. Lastly, amoxicillin was used as test drug, and characterized with UV-Vis spectroscopy for loading drug observation. Preliminary observation showed that Full-IPN has the most dense and elastic texture, followed by Semi-IPN, Crosslinked, and Non-modified in the last position. Semi-IPN and Crosslinked starch hydrogel have the most ideal properties and will not be degraded easily during metabolism. Therefore, both hydrogels could be considered as promising candidates for encapsulation material. Further analysis and issues will be discussed in the paper.

Keywords: biomaterial, drug delivery system, interpenetrating polymer network, poly(N-vinyl-pyrrolidone), starch hydrogel

Procedia PDF Downloads 223
5336 Melaleuca alternifolia Fibre Composites: Effect of Different Type of Fibre on Mechanical and Physical Properties

Authors: Sahari Japar, Rodney Jammy, M. A. Maleque

Abstract:

The fabrication of melaleuca alternifolia fibre reinforced thermoplastic starch composites was successfully done. This paper aims to show the effect of melaleuca alternifolia fibres on mechanical and physical properties of composites by using starch as a matrix. The fibres were extracted from three different part i.e. tea tree trunk (TTT), tea tree bunch (TTB) and tea tree leaf (TTL) and combined with tapioca starch by casting method. All composites showed superior mechanical properties in comparison to TS. The addition of 5% (v/v) fibres as a filler to TS led to the improvement in young’s modulus by 350% for TTB/TS, 282% for TTT/TS and 220% for TTL/TS. The tensile strength also increased to 34.39% for TTL/TS, 82.80% for TTB/TS and 203.18% for TTT/TS respectively. The trend can be correlated to the amount of cellulose in the fibres. For physical properties, it can be seen that, with the addition of fibres, the water absorption and swelling of composites decreased. The addition of melaleuca alternifolia fibre improved mechanical and physical properties of thermoplastic starch composites.

Keywords: melaleuca alternifolia, fibre, starch, mechanical, physical

Procedia PDF Downloads 364
5335 Reactive Blending of Thermoplastic Starch, Ethylene-1-Butene Rubber, and Chitosan

Authors: Kittisak Jantanasakulwong, Toshiaki Ougizawa

Abstract:

Thermoplastic starch (TPS) was prepared by melt-blending of cassava starch with glycerol (70/30 wt%/wt%) at 130 ◦C for 10 min. Chitosan (CTS) was used as a compatibilizer. TPS/CTS blend was melt-blended with maleic anhydride grafted ethylene-1-butene rubber (EB-MAH) in the composition of 80/20 respectively. Addition of CTS in TPS/EB-MAH blend decreased particles size of EB-MAH rubber to 1µm in TPS matrix. Mechanical properties, solubility, swelling property, morphology, and water contact angle of TPS/EB-MAH blend were improved by CTS incorporation. FTIR confirmed a reaction had occurred between amino groups (-NH2) of CTS and the MAH groups of EB-MAH. This reaction and the enhanced miscibility between TPS and CTS improved morphology and properties of the TPS/EB-MAH/CTS blend.

Keywords: thermoplastic starch, rubber, reactive blending, chitosan

Procedia PDF Downloads 174
5334 Extraction, Synthesis, Characterization and Antioxidant Properties of Oxidized Starch from an Abundant Source in Nigeria

Authors: Okafor E. Ijeoma, Isimi C. Yetunde, Okoh E. Judith, Kunle O. Olobayo, Emeje O. Martins

Abstract:

Starch has gained interest as a renewable and environmentally compatible polymer due to the increase in its use. However, starch by itself could not be satisfactorily applied in industrial processes due to some inherent disadvantages such as its hydrophilic character, poor mechanical properties, its inability to withstand processing conditions such as extreme temperatures, diverse pH, high shear rate, freeze-thaw variation and dimensional stability. The range of physical properties of parent starch can be enlarged by chemical modification which invariably enhances their use in a number of applications found in industrial processes and food manufacture. In this study, Manihot esculentus starch was subjected to modification by oxidation. Fourier Transmittance Infra- Red (FTIR) and Raman spectroscopies were used to confirm the synthesis while Scanning Electron Microscopy (SEM) and X- Ray Diffraction (XRD) were used to characterize the new polymer. DPPH (2, 2-diphenyl-1-picryl-hydrazyl-hydrate) free radical assay was used to determine the antioxidant property of the oxidized starch. Our results show that the modification had no significant effect on the foaming capacity as well as on the emulsion capacity. Scanning electron microscopy revealed that oxidation did not alter the predominantly circular-shaped starch granules, while the X-ray pattern of both starch, native and modified were similar. FTIR results revealed a new band at 3007 and 3283cm-1. Differential scanning calorimetry returned two new endothermic peaks in the oxidized starch with an improved gelation capacity and increased enthalpy of gelatinization. The IC50 of oxidized starch was notably higher than that of the reference standard, ascorbic acid.

Keywords: antioxidant activity, DPPH, M. esculentus, oxidation, starch

Procedia PDF Downloads 265