93 Engoglaze Development for the Production of Glazed Porcelain Tiles

Authors: Sezgi Isik, Yasin Urersoy, Gizem Ustunel, Ilkyaz Yalcin

Abstract:

Improvement of the digital tile application, lots of process revolutions have occurred in the tile production. In order to create unique and inimitable designs, all the competitors start to try different applications. Both Europian and domestic ceramic producers focus on the deep and realistic surfaces. In this study, the trend of engoglaze, which is becoming widespread in glaze porcelain tile designs to create the most intensive colours, were investigated. The aim of the study is to develop engoglaze formulation that supports digital ink activation. Thermal expansion coefficient values were determined by a dilatometer. Chemical analyses and sintering behaviors of engoglazes were made by X-ray diffraction and heat microscopy analysis. According to these glaze formulation studies, it has been reported that using engoglaze could easily reduce the digital ink consumption of the design. On the other hand, the advantage of the production cost is gained, and deepness of the design is provided.

Keywords: ceramic, engoglaze, digital ink activation, glazed porcelain tile

Procedia PDF Downloads 112
92 A Study on Bonding Strength, Waterproofing and Flexibility of Environment Friendly, and Cost Effective Cementitious Grout Mixture for Tile Joints

Authors: Gowthamraj Vungarala

Abstract:

This paper presents the experimental investigation on the bond strength, waterproofing abilities and flexibility of tile joint when Ordinary Portland Cement (OPC) or White Portland Cement (WPC) CEM II A-LL 42.5N and porcelain powder graded between 200 microns and 75 microns is mixed with vinyl acetate monomer (VAM), hydroxypropyl methyl cellulose ether, ethylene co-polymer rubber powder and Styrene butyl rubber (SBR). Use of porcelain powder which is tough to decompose as a form of industrial refuse which helps environmental safety and waste usage.

Keywords: styrene butane rubber, hydroxypropyl methyl cellulose ether, vinyl acetate monomer, polymer modified cement, polyethylene, porcelain powder

Procedia PDF Downloads 61
91 Historical Studies on Gilt Decorations on Glazed Surfaces

Authors: Sabra Saeidi

Abstract:

This research focuses on the historical techniques associated with the lajevardina and Haft-Rangi production methods in creating tiles, with emphasis on the identification of the techniques of inserting gold sheets on the surface of such historical glazed tiles. In this regard, firstly, the history of the production of enamel, gold plated, and Lajevardina glazed pottery work made during the Khwarizmanshahid and Mongol era (eleventh to the thirteenth century) have been assessed to reach a better understanding of the background and the history associated with historical glazing methods. After the historical overview of the production technique of glazed pottery work and introductions of the civilizations using those techniques, we focused on the niches production methods of enamel and Lajevardina glazing, which are two categories of decorations usually found in tiles. Next, a general classification method for various types of gilt tiles has been introduced, which is applicable to the tile works up to Safavid period (Sixteenth to the seventeenth century). Gilded lajevardina glazed tiles, gilt Haft-Rangi tiles, monolithic glazed gilt tiles, and gilt mosaic tiles are included in the categories.

Keywords: gilt tiles, Islamic art, Iranian art, historical studies, gilding

Procedia PDF Downloads 102
90 The Effect of Artificial Intelligence on Decoration Designs

Authors: Ayed Mouris Gad Elsayed Khalil

Abstract:

This research focuses on historical techniques associated with the Lajevardin and Haft-Rangi production methods in tile production, with particular attention to identifying techniques for applying gold leaf to the surface of these historical glazed tiles. In this context, the history of the production of glazed, gilded and glazed Lajevardin ceramics from the Khwarizmanshahid and Mongol periods (11th to 13th centuries) was first evaluated in order to better understand the context and history of the methods of historical enameling. After a historical overview of glazed ceramic production techniques and the adoption of these techniques by civilizations, we focused on the niche production methods of glazes and Lajevardin glazes, two categories of decoration commonly found on tiles. A general method for classifying the different types of gold tiles was then introduced, applicable to tiles from to the Safavid period (16th-17th centuries). These categories include gold glazed Lajevardina tiles, haft rangi gold tiles, gold glazed monolithic tiles and gold mosaic tiles.

Keywords: ethnicity, multi-cultural, jewelry, craft techniquemycenaean, ceramic, provenance, pigmentAmorium, glass bracelets, image, Byzantine empire

Procedia PDF Downloads 26
89 Use of Residues from Water Treatment and Porcelain Coatings Industry for Producing Eco-Bricks

Authors: Flavio Araujo, Fabiolla Lima, Julio Lima, Paulo Scalize, Antonio Albuquerque, Heitor Reis

Abstract:

One of the great environmental problems in the management of water treatment (WTP) is on the disposal of waste generated during the treatment process. The same occurs with the waste generated during rectification of porcelain tiles. Despite environmental laws in Brazil the residues does not have an ecologically balanced destination. Thus, with the purpose to identify an environmentally sustainable disposal, residues were used to replace part of the soil, for production soil-cement bricks. It was used the residues from WTP and coatings industry Cecrisa (Brazil). Consequently, a greater amount of fine aggregate in the two samples of residues was found. The residue affects the quality of bricks produced, compared to the sample without residues. However, the results of compression and water absorption tests were obtained values that meet the standards, respectively 2.0 MPa and 20% absorption.

Keywords: water treatment residue, porcelain tile residue, WTP, brick

Procedia PDF Downloads 448
88 Comparison of the Effect of Feldspathic Porcelain and Zirconia on Natural Tooth Wear

Authors: Ammar Neshati, Elham Hamidi Shishavan

Abstract:

Background and Aim: Enamel wear is among the main disadvantages of ceramic restorations. Recently, use of full zirconia crowns without dental porcelain has been suggested. The aim of this study was to compare the effect of feldspathic porcelain and zirconia on the wear of natural teeth. Materials and Methods: In this experimental study, 22 zirconia specimens were fabricated; out of which, 11 specimens were polished and used as zirconia specimens while the remaining 11 were used to fabricate porcelain specimens. A total of 22 natural human teeth were also collected. The natural teeth were photographed by a stereomicroscope in a fixed position and the distance from the cusp tip to a reference point was measured. Next, 11 teeth opposed zirconia and the remaining 11 opposed porcelain specimens in a chewing simulator and subjected to 120,000 masticatory cycles. The teeth were photographed again and the greatest difference between the before and after values was recorded. Results: The mean (± standard deviation) wear rate was 153.8±95.68 and 306.3±127.74, in the zirconia and porcelain groups, respectively; and the two groups had a statistically significant difference in this respect (P=0.007). Conclusion: The mean wear was significantly lower in teeth opposing zirconia than in those opposing feldspathic porcelain.

Keywords: natural tooth wear, feldspathic porcelain, zirconia, effect

Procedia PDF Downloads 381
87 Development of a Porous Porcelain Frape with Thermochromic Visualization

Authors: Jose Gois

Abstract:

The paper presents the development of a porous porcelain frappe with thermochromic visualization for port wines, having as a partner the Institute of Vinhos do Douro and Porto. This ceramic frappe is intended to promote the cooling and maintenance of the temperature of port wines through porous ceramic materials, consisting of a porcelain composite with sawdust addition, so as to contain, on the one hand, the similar cooling properties of the terracotta and, on the other, the resistance of materials such as porcelain. The application of the thermochromic element makes it possible to see if the wine is at optimal service temperatures, allowing users to drink the wine in the ideal conditions and contributing to more efficient maintenance of the service.

Keywords: design, frappe, porcelain, porous, thermochromic

Procedia PDF Downloads 118
86 The Effect of Fe₂O₃ and Sum of Alkalis Elements on Monocotora Tile

Authors: Fatemeh Ansarniya, Fatemeh Mirjalili, Hamid Reza Abedini, Shabnam Salari, M. Horasht

Abstract:

The study of this research is the effect of using Fe₂O₃ and sum of alkalis elements in the floor tile production. At first, raw materials of floor tile with the same formulation of original sample was prepared and sintered for 39 minutes at 1130˚C in roller kiln and finally, physical properties of the sintered bodies based on floor tile standard process was investigated. The results showed that there was the possibility of production of floor tile containing different percentages of Fe₂O₃ and sum of Na₂O+ K₂O. With increasing the Fe₂O₃ and sum of Na₂O+ K₂O elements, the percentages of water absorption and raw, dry and sintered strengths were decreased, but the percentages of shrinkage were increased which caused the decreasing the percentages of expansion.

Keywords: floor tile, physical properties, Na2O+ K2O, Fe2O3

Procedia PDF Downloads 481
85 Wear and Fraction Behavior of Porcelain Coated with Polyurethane/SiO2 Coating Layer

Authors: Ching Yern Chee

Abstract:

Various loading of nano silica is added into polyurethane (PU) and then coated on porcelain substrate. The wear and friction properties of the porcelain substrates coated with polyurethane/nano silica nano composite coatings were investigated using the reciprocating wear testing machine. The friction and wear test of polyurethane/nano silica coated porcelain substrate was studied at different sliding speed and applied load. It was found that the optimum composition of nano silica is 3 wt% which gives the lowest friction coefficient and wear rate in all applied load ranges and sliding speeds. For 3 wt% nano silica filled PU coated porcelain substrate, the increment of sliding speed caused higher wear rates but lower frictions coefficient. Besides, the friction coefficient of nano silica filled PU coated porcelain substrate decreased but the wear rate increased with the applied load.

Keywords: porcelain, nanocomposite coating, morphology, friction, wear behavior

Procedia PDF Downloads 501
84 Strengthening and Toughening of Dental Porcelain by the Inclusion of an Yttria-Stabilized Zirconia Reinforcing Phase

Authors: Buno Henriques, Rafaela Santos, Júlio Matias de Souza, Filipe Silva, Rubens Nascimento, Márcio Fredel

Abstract:

Dental porcelain composites reinforced and toughened by 20 wt.% tetragonal zirconia (3Y-TZP) were processed by hot pressing at 1000°C. Two types of particles were tested: yttria-stabilized zirconia (ZrO2–3%Y2O3) agglomerates and pre-sintered yttria-stabilized zirconia (ZrO2–3%Y2O3) particles. The composites as well as the reinforcing particles were analyzed by the means of optical and Scanning Electron Microscopy (SEM), Energy Dispersion Spectroscopy (EDS) and X-Ray Diffraction (XRD). The mechanical properties were obtained by the transverse rupture strength test, Vickers indentations and fracture toughness. Wear tests were also performed on the composites and monolithic porcelain. The best mechanical and wear results were displayed by the porcelain reinforced with the pre-sintered ZrO2–3%Y2O3 particles.

Keywords: dental restoration, zirconia, porcelain, composites, strengthening, toughening, wear

Procedia PDF Downloads 412
83 A Comparison between Shear Bond Strength of VMK Master Porcelain with Three Base-Metal Alloys (Ni-Cr-T3, Verabond, Super Cast) and One Noble Alloy (X-33) in Metal-Ceramic Restorations

Authors: Ammar Neshati, Elham Hamidi Shishavan

Abstract:

Statement of Problem: The increase in the use of metal-ceramic restorations and a high prevalence of porcelain chipping entails introducing an alloy which is more compatible with porcelain and which causes a stronger bond between the two. This study is to compare shear bond strength of three base-metal alloys and one noble alloy with the common VMK Master Porcelain. Materials and Method: Three different groups of base-metal alloys (Ni-cr-T3, Super Cast, Verabond) and one group of noble alloy (x-33) were selected. The number of alloys in each group was 15. All the groups went through the casting process and change from wax pattern into metal disks. Then, VMK Master Porcelain was fired on each group. All the specimens were put in the UTM and a shear force was loaded until a fracture occurred. The fracture force was then recorded by the machine. The data was subjected to SPSS Version 16 and One-Way ANOVA was run to compare shear strength between the groups. Furthermore, the groups were compared two by two through running Tukey test. Results: The findings of this study revealed that shear bond strength of Ni-Cr-T3 alloy was higher than the three other alloys (94 Mpa or 330 N). Super Cast alloy had the second greatest shear bond strength (80. 87 Mpa or 283.87 N). Both Verabond (69.66 Mpa or 245 N) and x-33 alloys (66.53 Mpa or 234 N) took the third place. Conclusion: Ni-Cr-T3 with VMK Master Porcelain has the greatest shear bond strength. Therefore, the use of this low-cost alloy is recommended in metal-ceramic restorations.

Keywords: shear bond, base-metal alloy, noble alloy, porcelain

Procedia PDF Downloads 462
82 The Textual Criticism on the Age of ‘Wan Li’ Shipwreck Porcelain and Its Comparison with ‘Whitte Leeuw’ and Hatcher Shipwreck Porcelain

Authors: Yang Liu, Dongliang Lyu

Abstract:

After the Wan li shipwreck was discovered 60 miles off the east coast of Tan jong Jara in Malaysia, numerous marvelous ceramic shards have been salvaged from the seabed. Remarkable pieces of Jing dezhen blue-and-white porcelain recovered from the site represent the essential part of the fascinating research. The porcelain cargo of Wan li shipwreck is significant to the studies on exported porcelains and Jing dezhen porcelain manufacture industry of Late-Ming dynasty. Using the ceramic shards categorization and the study of the Chinese and Western historical documents as a research strategy, the paper wants to shed new light on the Wan li shipwreck wares classification with Jingdezhen kiln ceramic as its main focus. The article is also discussing Jing dezhen blue-and-white porcelains from the perspective of domestic versus export markets and further proceeding to the systematization and analyses of Wan li shipwreck porcelain which bears witness to the forms, styles, and types of decoration that were being traded in this period. The porcelain data from two other shipwrecked projects -White Leeuw and Hatcher- were chosen as comparative case studies and Wan li shipwreck Jing dezhen blue-and-white porcelain is being reinterpreted in the context of art history and archeology of the region. The marine archaeologist Sten Sjostrand named the ship ‘Wanli shipwreck’ because its porcelain cargoes are typical of those made during the reign of Emperor Wan li of Ming dynasty. Though some scholars question the appropriateness of the name, the final verdict of the history is still to be made. Based on previous historical argumentation, the article uses a comparative approach to review the Wan li shipwreck blue-and-white porcelains on the grounds of the porcelains unearthed from the tomb or abandoned in the towns and carrying the time-specific reign mark. All these materials provide a very strong evidence which suggests that the porcelain recovered from Wan li ship can be dated to as early as the second year of Tianqi era (1622) and early Chongzhen reign. Lastly, some blue-and-white porcelain intended for the domestic market and some bowls of blue-and-white porcelain from Jing dezhen kilns recovered from the Wan li shipwreck all carry at the bottom the specific residue from the firing process. The author makes the corresponding analysis for these two interesting phenomena.

Keywords: blue-and-white porcelain, Ming dynasty, Jing dezhen kiln, Wan li shipwreck

Procedia PDF Downloads 155
81 Manufacturing Commercial Bricks with Construction and Demolition Wastes

Authors: Mustafa Kara, Yasemin Kilic, Bahattin Murat Demir, Ümit Ustaoglu, Cavit Unal

Abstract:

This paper reports utilization of different kind of construction and demolition wastes (C&D) in the production of bricks at industrial scale. Plastered brick waste and tile wastes were collected from ISTAÇ Co. Compost and Recovery Plant, Istanbul, Turkey. Plastered brick waste and tile waste are mixed with brick clay in the proportion of 0-30% and fired at 900ºC. The physical and mechanical properties of the produced bricks were determined and evaluated according to IKIZLER Brick Company Production values, Brick Industry Association (BIA) and Turkish Standards (TS). The resulted showed that plastered brick waste and tile waste can be used to produce good quality brick for various engineering applications in construction and building. The replacement of brick clay by plastered brick waste and tile waste at the levels of 30% has good effects on the compressive strength of the bricks.

Keywords: commercial brick, construction and demolition waste, manufacturing, recycling

Procedia PDF Downloads 321
80 Horn Snail (Telescopium Telescopium) Shells Waste as an Alternative for Ceramic Tile Manufacturing

Authors: Patricia N. Baguio, Angel Amy M. Bunag, Paul Bryan E. Ornopia, John Paul C. Suel

Abstract:

This research investigates the viability and efficiency of employing ceramic tile additives derived from horn snail shell material, specifically calcium carbonate (CaCO₃). The study aims to evaluate the mechanical properties of ceramic tiles with Calcium Carbonate with varying amounts of CaCO₃, focusing on breaking and flexural strength. The research employs a comprehensive methodology, including material collection, slurry forming, shaping, drying, firing, and statistical analysis using paired sample T-tests. The result indicates a positive correlation between calcium carbonate (CaCO₃) application and ceramic tile strength, revealing increased breaking strength from 29.41 N (non-calcium Carbonate) to 46.02 N (70g CaCO3) and a substantial enhancement to 82.61 N with 150g CaCO₃. Comparative analyses show higher breaking and flexural strength in tiles with Calcium Carbonate with 150g CaCO₃ analysis (p = 0.011), indicating its feasibility for ceramic tile manufacturing, while 70g CaCO₃ shows no significant difference from non-calcium Carbonate tiles (p = 0.135). The addition of horn snail shells shows potential for improving ceramic tile quality and contributes positively to waste management in standard tile production processes.

Keywords: Horn snail shell, calcium carbonate, breaking strength, flexural strength

Procedia PDF Downloads 30
79 Horn Snail (Telescopium telescopium) Shells Waste as an Alternative for Ceramic Tile Manufacturing

Authors: Patricia N. Baguio, Angel Amy M. Buñag, Paul Bryan E. Ornopia, John Paul C. Suel

Abstract:

This research investigates the viability and efficiency of employing ceramic tile additives derived from horn snail shell material, specifically calcium carbonate (CaCO₃). The study aims to evaluate the mechanical properties of ceramic tiles with calcium carbonate with varying amounts of CaCO₃, focusing on breaking and flexural strength. The research employs a comprehensive methodology, including material collection, slurry forming, shaping, drying, firing, and statistical analysis using paired sample T-tests. The result indicates a positive correlation between calcium carbonate (CaCO₃) application and ceramic tile strength, revealing increased breaking strength from 29.41 N (non-calcium carbonate) to 46.02 N (70g CaCO₃) and a substantial enhancement to 82.61 N with 150g CaCO₃. Comparative analyses show higher breaking and flexural strength in tiles calcium carbonate with 150g CaCO₃ analysis (p = 0.011), indicating its feasibility for ceramic tile manufacturing, while 70g CaCO₃ shows no significant difference from non-calcium carbonate tiles (p = 0.135). The addition of horn snail shells shows potential for improving ceramic tile quality and contributes positively to waste management in standard tile production processes.

Keywords: horn snail shell, calcium carbonate, breaking strength, flexural strength

Procedia PDF Downloads 31
78 Study of Pottery And Glazed Canopic Vessels

Authors: Abdelrahman Mohamed

Abstract:

The ancient Egyptians used canopic vessels in embalming operations in order to preserve the guts of the mummified corpse. Canopic vessels were made of many materials, including pottery and glazed pottery. In this research, we study a pottery canopic vessel and a glazed pottery vessel. An analysis to find out the compounds and elements of the materials from which the container is made and the colors, and also to make some analysis for the organic materials present inside it, such as the Fourier Transform Infrared Spectroscopy analysis and the Gas chromatograph mass spectrometers analysis of the organic residue. Through the study and analysis, it was proved that some of the materials present in the pot were coniferous oil and animal fats. In the other pot, the analysis showed the presence of some plant resins (mastic) inside rolls of linen. Restoration operations were carried out, such as mechanical cleaning, strengthening, and completing the reinforcement of the pots.

Keywords: canopic jar, embalming, FTIR, GCMS, linen.

Procedia PDF Downloads 49
77 Optical and Surface Characteristics of Direct Composite, Polished and Glazed Ceramic Materials After Exposure to Tooth Brush Abrasion and Staining Solution

Authors: Maryam Firouzmandi, Moosa Miri

Abstract:

Aim and background: esthetic and structural reconstruction of anterior teeth may require the application of different restoration material. In this regard combination of direct composite veneer and ceramic crown is a common treatment option. Despite the initial matching, their long term harmony in term of optical and surface characteristics is a matter of concern. The purpose of this study is to evaluate and compare optical and surface characteristic of direct composite polished and glazed ceramic materials after exposure to tooth brush abrasion and staining solution. Materials and Methods: ten 2 mm thick disk shape specimens were prepared from IPS empress direct composite and twenty specimens from IPS e.max CAD blocks. Composite specimens and ten ceramic specimens were polished by using D&Z composite and ceramic polishing kit. The other ten specimens of ceramic were glazed with glazing liquid. Baseline measurement of roughness, CIElab coordinate, and luminance were recorded. Then the specimens underwent thermocycling, tooth brushing, and coffee staining. Afterword, the final measurements were recorded. Color coordinate were used to calculate ΔE76, ΔE00, translucency parameter, and contrast ratio. Data were analyzed by One-way ANOVA and post hoc LSD test. Results: baseline and final roughness of the study group were not different. At baseline, the order of roughness for the study group were as follows: composite < glazed ceramic < polished ceramic, but after aging, no difference. Between ceramic groups was not detected. The comparison of baseline and final luminance was similar to roughness but in reverse order. Unlike differential roughness which was comparable between the groups, changes in luminance of the glazed ceramic group was higher than other groups. ΔE76 and ΔE00 in the composite group were 18.35 and 12.84, in the glazed ceramic group were 1.3 and 0.79, and in polished ceramic were 1.26 and 0.85. These values for the composite group were significantly different from ceramic groups. Translucency of composite at baseline was significantly higher than final, but there was no significant difference between these values in ceramic groups. Composite was more translucency than ceramic at baseline and final measurement. Conclusion: Glazed ceramic surface was smoother than polished ceramic. Aging did not change the roughness. Optical properties (color and translucency) of the composite were influenced by aging. Luminance of composite, glazed ceramic, and polished ceramic decreased after aging, but the reduction in glazed ceramic was more pronounced.

Keywords: ceramic, tooth-brush abrasion, staining solution, composite resin

Procedia PDF Downloads 152
76 Traditional Ceramics Value in the Middle East

Authors: Abdelmessih Malak Sadek Labib

Abstract:

The Stability in harsh environments thanks to excellent electrical, mechanical and thermal properties is what ceramics are all about selected materials for many applications despite advent of new materials such as plastics and composites. However, ceramic materials have disadvantages, including brittleness. Fragility is often attributed to pottery strong covalent and ionic bonds in the ceramic body. There is still much to learn about brittle cracks in a attention to detail, hence the fragility of the ceramic and its catastrophic failure of a frequently studied topic, particularly in charging applications. One of the most commonly used ceramics for load-bearing applications such as veneers is porcelain. Porcelain is a type of traditional pottery. Traditional pottery consists mainly of three basic ingredients: clay, which gives plasticity; silica which maintains the shape and stability of the ceramic body over temperature high temperature; and feldspar affecting glazing. In traditional pottery, the inversion of quartz during cooling the process can create microcracks that act as a stress concentration centers. Consequently, subcritical crack growth is caused due to quartz inversion origins unpredictable catastrophic failure of the work of ceramic bodies when reloading. In the case of porcelain, however, this is what the mullite hypothesis says the strength of porcelain can be significantly increased with felt Interlocking of mullite needles in the ceramic body.in this way realistic assessment of the role of quartz and mullite Porcelain with a strength of is needed to grow stronger and smaller fragile porcelain. Currently,the lack of reports on Young's moduli in the literature leads to erroneous conclusions in this regard mechanical behavior of porcelain. Therefore, the current project uses the Young's modulus approach for the investigation the role of quartz and mullite on the mechanical strength of various porcelains, in addition to reducing particle size, flexural strength fractographic forces and techniques.

Keywords: materials, technical, ceramics, properties, thermal, stability, advantages

Procedia PDF Downloads 58
75 Durability Study of Binary Blended High Performance Concrete

Authors: Vatsal Patel, Niraj Shah

Abstract:

This paper presents the results of a laboratory study on the properties of binary blended High Performance cementitious systems containing blends of ordinary Portland cement (OPC), Porcelain Powder or Marble Powder blend proportions of 100:00, 95:05, 90:10, 85:15, 80:20 for OPC: Porcelain Powder/Marble Powder. Studies on the Engineering Properties of the cementitious concrete, namely compressive strength, flexural strength, sorptivity, rapid chloride penetration test and accelerated corrosion test have been performed and those of OPC concrete. The results show that the inclusion of Porcelain powder or Marble Powder as binary blended cement alters to a great degree the properties of the binder as well as the resulting concrete. In addition, the results show that the Porcelain powder with 85:15 proportions and Marble powder with 90:10 proportions as binary systems to produce high-performance concrete could potentially be used in the concrete construction industry particular in lowering down the volume of OPC used and lowering emission of CO2 produces during manufacturing of cement.

Keywords: accelerated corrosion, binary blended cementitious system, rapid chloride penetration, sorptivity

Procedia PDF Downloads 369
74 Utilization of Waste Crushed Tile as Coarse Aggregate in Concrete

Authors: Harkaranjit Singh, Arun Kumar

Abstract:

Depletion of natural resources is a common phenomenon in developing countries like India due to rapid urbanization and industrialization involving construction of infrastructure and other amenities. In view of this, people have started searching for suitable other viable alternative materials for concrete so that the existing natural resources could be preserved to the possible extent for the future generation. In this process, different industrial waste materials such as fly ash, blast furnace slag, quarry dust, tile waste, bricks, broken glass waste, waste aggregate from demolition of structures, ceramic insulator waste, etc. have been tried as a viable substitute material to the conventional materials in concrete and has also been succeeded. This paper describes the studies conducted on strength characteristics of concrete made with utilizing of crushed tiles as a coarse aggregate. The waste crushed tiles can be used as coarse aggregates with the replacement ratio of 0, 50, 75 and 100% were used. Mechanical and physical tests were conducted on specimens. It was found that, the concrete made of waste ceramic tile aggregate produced more strength in compression, and flexure.

Keywords: compressive strength, flexural strength, waste crushed tile, concrete

Procedia PDF Downloads 377
73 Porcelain Paste Processing by Robocasting 3D: Parameters Tuning

Authors: A. S. V. Carvalho, J. Luis, L. S. O. Pires, J. M. Oliveira

Abstract:

Additive manufacturing technologies (AM) experienced a remarkable growth in the latest years due to the development and diffusion of a wide range of three-dimensional (3D) printing techniques. Nowadays we can find techniques available for non-industrial users, like fused filament fabrication, but techniques like 3D printing, polyjet, selective laser sintering and stereolithography are mainly spread in the industry. Robocasting (R3D) shows a great potential due to its ability to shape materials with a wide range of viscosity. Industrial porcelain compositions showing different rheological behaviour can be prepared and used as candidate materials to be processed by R3D. The use of this AM technique in industry is very residual. In this work, a specific porcelain composition with suitable rheological properties will be processed by R3D, and a systematic study of the printing parameters tuning will be shown. The porcelain composition was formulated based on an industrial spray dried porcelain powder. The powder particle size and morphology was analysed. The powders were mixed with water and an organic binder on a ball mill at 200 rpm/min for 24 hours. The batch viscosity was adjusted by the addition of an acid solution and mixed again. The paste density, viscosity, zeta potential, particle size distribution and pH were determined. In a R3D system, different speed and pressure settings were studied to access their impact on the fabrication of porcelain models. These models were dried at 80 °C, during 24 hours and sintered in air at 1350 °C for 2 hours. The stability of the models, its walls and surface quality were studied and their physical properties were accessed. The microstructure and layer adhesion were observed by SEM. The studied processing parameters have a high impact on the models quality. Moreover, they have a high impact on the stacking of the filaments. The adequate tuning of the parameters has a huge influence on the final properties of the porcelain models. This work contributes to a better assimilation of AM technologies in ceramic industry. Acknowledgments: The RoboCer3D project – project of additive rapid manufacturing through 3D printing ceramic material (POCI-01-0247-FEDER-003350) financed by Compete 2020, PT 2020, European Regional Development Fund – FEDER through the International and Competitive Operational Program (POCI) under the PT2020 partnership agreement.

Keywords: additive manufacturing, porcelain, robocasting, R3D

Procedia PDF Downloads 140
72 The Traditional Ceramics Value in the Middle East

Authors: Abdelmessih Malak Sadek Labib

Abstract:

Ceramic materials are known for their stability in harsh environments and excellent electrical, mechanical, and thermal properties. They have been widely used in various applications despite the emergence of new materials such as plastics and composites. However, ceramics are often brittle, which can lead to catastrophic failure. The fragility of ceramics and the mechanisms behind their failure have been a topic of extensive research, particularly in load-bearing applications like veneers. Porcelain, a type of traditional pottery, is commonly used in such applications. Traditional pottery consists of clay, silica, and feldspar, and the presence of quartz in the ceramic body can lead to microcracks and stress concentrations. The mullite hypothesis suggests that the strength of porcelain can be improved by increasing the interlocking of mullite needles in the ceramic body. However, there is a lack of reports on Young's moduli in the literature, leading to erroneous conclusions about the mechanical behavior of porcelain. This project aims to investigate the role of quartz and mullite on the mechanical strength of various porcelains while considering factors such as particle size, flexural strength, and fractographic forces. Research Aim: The aim of this research project is to assess the role of quartz and mullite in enhancing the mechanical strength of different porcelains. The project will also explore the effect of reducing particle size on the properties of porcelain, as well as investigate flexural strength and fractographic techniques. Methodology: The methodology for this project involves using scientific expressions and a mix of modern English to ensure the understanding of all attendees. It will include the measurement of Young's modulus and the evaluation of the mechanical behavior of porcelains through various experimental techniques. Findings: The findings of this study will provide a realistic assessment of the role of quartz and mullite in strengthening and reducing the fragility of porcelain. The research will also contribute to a better understanding of the mechanical behavior of ceramics, specifically in load-bearing applications. Theoretical Importance: The theoretical importance of this research lies in its contribution to the understanding of the factors influencing the mechanical strength and fragility of ceramics, particularly porcelain. By investigating the interplay between quartz, mullite, and other variables, this study will enhance our knowledge of the properties and behavior of traditional ceramics. Data Collection and Analysis Procedures: Data for this research will be collected through experiments involving the measurement of Young's modulus and other mechanical properties of porcelains. The effects of quartz, mullite, particle size, flexural strength, and fractographic forces will be examined and analyzed using appropriate statistical techniques and fractographic analysis. Questions Addressed: This research project aims to address the following questions: (1) How does the presence of quartz and mullite affect the mechanical strength of porcelain? (2) What is the impact of reducing particle size on the properties of porcelain? (3) How do flexural strength and fractographic forces influence the behavior of porcelains? Conclusion: In conclusion, this research project aims to enhance the understanding of the role of quartz and mullite in strengthening and reducing the fragility of porcelain. By investigating the mechanical properties of porcelains and considering factors such as particle size, flexural strength, and fractographic forces, this study will contribute to the knowledge of traditional ceramics and their potential applications. The findings will have practical implications for the use of ceramics in various fields.

Keywords: stability, harsh environments, electrical, techniques, mechanical disadvantages, materials

Procedia PDF Downloads 41
71 Correlation Mapping for Measuring Platelet Adhesion

Authors: Eunseop Yeom

Abstract:

Platelets can be activated by the surrounding blood flows where a blood vessel is narrowed as a result of atherosclerosis. Numerous studies have been conducted to identify the relation between platelets activation and thrombus formation. To measure platelet adhesion, this study proposes an image analysis technique. Blood samples are delivered in the microfluidic channel, and then platelets are activated by a stenotic micro-channel with 90% severity. By applying proposed correlation mapping, which visualizes decorrelation of the streaming blood flow, the area of adhered platelets (APlatelet) was estimated without labeling platelets. In order to evaluate the performance of correlation mapping on the detection of platelet adhesion, the effect of tile size was investigated by calculating 2D correlation coefficients with binary images obtained by manual labeling and the correlation mapping method with different sizes of the square tile ranging from 3 to 50 pixels. The maximum 2D correlation coefficient is observed with the optimum tile size of 5×5 pixels. As the area of the platelet adhesion increases, the platelets plug the channel and there is only a small amount of blood flows. This image analysis could provide new insights for better understanding of the interactions between platelet aggregation and blood flows in various physiological conditions.

Keywords: platelet activation, correlation coefficient, image analysis, shear rate

Procedia PDF Downloads 310
70 Analyses of Uniaxial and Biaxial Flexure Tests Used in Ceramic Materials

Authors: Barry Hojjatie

Abstract:

Uniaxial (e.g., three-point bending) and biaxial flexure tests are used frequently for determining the strength of ceramics. It is generally believed that the biaxial test has an advantage as compared to uniaxial test because it produces a state of pure tension on the lower surface of the specimen and the maximum tensile stress, which is usually responsible for crack initiation and failure is unaffected by the edge condition. However, inconsistent strength values have been reported for the same material and testing conditions. The objective of this study was to analyze the strength of dental porcelain materials using the two different test methods and evaluate the main contributions to variability in biaxial testing and to analyze the relative influence of variables such as specimen geometric conditions and loading conditions on calculated strength of porcelain subjected to biaxial testing. Porcelain disks (16 mm dia x 2 mm thick) were subjected to biaxial flexure (pin-on-three-ball), and flexure strength values were calculated. A 3-D finite element model was developed to simulate various biaxial flexure test conditions. Stresses were analyzed for ceramic thickness in the range of 1.0-3.0 mm. For a 2-mm-thick disk subjected to a point load of 200 N, the maximum tensile stress at the lower surface was 180 MPa. This stress decreased to 95, 77, 68, and 59 MPa for the radius of the load values of 0.15, 0.3, 0.6, and 1.0 mm, respectively. Tensile stresses which developed at the top surface near the site of loading were small for the radius of the load ≥ 0.6 mm.

Keywords: ceramis, biaxial, flexure test, uniaxial

Procedia PDF Downloads 122
69 Roof Material Detection Based on Object-Based Approach Using WorldView-2 Satellite Imagery

Authors: Ebrahim Taherzadeh, Helmi Z. M. Shafri, Kaveh Shahi

Abstract:

One of the most important tasks in urban area remote sensing is detection of impervious surface (IS), such as building roof and roads. However, detection of IS in heterogeneous areas still remains as one of the most challenging works. In this study, detection of concrete roof using an object-oriented approach was proposed. A new rule-based classification was developed to detect concrete roof tile. The proposed rule-based classification was applied to WorldView-2 image. Results showed that the proposed rule has good potential to predict concrete roof material from WorldView-2 images with 85% accuracy.

Keywords: object-based, roof material, concrete tile, WorldView-2

Procedia PDF Downloads 398
68 A Review on the Usage of Ceramic Wastes in Concrete Production

Authors: O. Zimbili, W. Salim, M. Ndambuki

Abstract:

Construction and Demolition (C&D) wastes contribute the highest percentage of wastes worldwide (75%). Furthermore, ceramic materials contribute the highest percentage of wastes within the C&D wastes (54%). The current option for disposal of ceramic wastes is landfill. This is due to unavailability of standards, avoidance of risk, lack of knowledge and experience in using ceramic wastes in construction. The ability of ceramic wastes to act as a pozzolanic material in the production of cement has been effectively explored. The results proved that temperatures used in the manufacturing of these tiles (about 900 ⁰C) are sufficient to activate pozzolanic properties of clay. They also showed that, after optimization (11-14% substitution), the cement blend performs better, with no morphological differences between the cement blended with ceramic waste, and that blended with other pozzolanic materials. Sanitary ware and electrical insulator porcelain wastes are some wastes investigated for usage as aggregates in concrete production. When optimized, both produced good results, better than when natural aggregates are used. However, the research on ceramic wastes as partial substitute for fine aggregates or cement has not been overly exploited as the other areas. This review has been concluded with focus on investigating whether ceramic wall tile wastes used as partial substitute for cement and fine aggregates could prove to be beneficial since the two materials are the most high-priced during concrete production.

Keywords: blended, morphological, pozzolanic, waste

Procedia PDF Downloads 337
67 The Non-Existence of Perfect 2-Error Correcting Lee Codes of Word Length 7 over Z

Authors: Catarina Cruz, Ana Breda

Abstract:

Tiling problems have been capturing the attention of many mathematicians due to their real-life applications. In this study, we deal with tilings of Zⁿ by Lee spheres, where n is a positive integer number, being these tilings related with error correcting codes on the transmission of information over a noisy channel. We focus our attention on the question ‘for what values of n and r does the n-dimensional Lee sphere of radius r tile Zⁿ?’. It seems that the n-dimensional Lee sphere of radius r does not tile Zⁿ for n ≥ 3 and r ≥ 2. Here, we prove that is not possible to tile Z⁷ with Lee spheres of radius 2 presenting a proof based on a combinatorial method and faithful to the geometric idea of the problem. The non-existence of such tilings has been studied by several authors being considered the most difficult cases those in which the radius of the Lee spheres is equal to 2. The relation between these tilings and error correcting codes is established considering the center of a Lee sphere as a codeword and the other elements of the sphere as words which are decoded by the central codeword. When the Lee spheres of radius r centered at elements of a set M ⊂ Zⁿ tile Zⁿ, M is a perfect r-error correcting Lee code of word length n over Z, denoted by PL(n, r). Our strategy to prove the non-existence of PL(7, 2) codes are based on the assumption of the existence of such code M. Without loss of generality, we suppose that O ∈ M, where O = (0, ..., 0). In this sense and taking into account that we are dealing with Lee spheres of radius 2, O covers all words which are distant two or fewer units from it. By the definition of PL(7, 2) code, each word which is distant three units from O must be covered by a unique codeword of M. These words have to be covered by codewords which dist five units from O. We prove the non-existence of PL(7, 2) codes showing that it is not possible to cover all the referred words without superposition of Lee spheres whose centers are distant five units from O, contradicting the definition of PL(7, 2) code. We achieve this contradiction by combining the cardinality of particular subsets of codewords which are distant five units from O. There exists an extensive literature on codes in the Lee metric. Here, we present a new approach to prove the non-existence of PL(7, 2) codes.

Keywords: Golomb-Welch conjecture, Lee metric, perfect Lee codes, tilings

Procedia PDF Downloads 131
66 Characterization of Leakage Current on the Surface of Porcelain Insulator under Contaminated Conditions

Authors: Hocine Terrab , Abdelhafid Bayadi, Adel Kara, Ayman El-Hag

Abstract:

Insulator flashover under polluted conditions has been a serious threat on the reliability of power systems. It is known that the flashover process is mainly affected by the environmental conditions such as; the pollution level and humidity. Those are the essential parameters influencing the wetting process. This paper presents an investigation of the characteristics of leakage current (LC) developed on the surface of porcelain insulator at contaminated conditions under AC voltage. The study is done in an artificial fog chamber and the LC is characterized for different stages; dry, wetted and presence of discharge activities. Time-frequency and spectral analysis are adopted to calculate the evolution of LC characteristics with various stages prior to flashover occurrence. The preliminary results could be used in analysing the LC to develop more effective diagnosis of early signs of dry band arcing as an indication for insulation washing.

Keywords: flashover, harmonic components, leakage current, phase angle, statistical analysis

Procedia PDF Downloads 402
65 Evaluation of Complications Observed in Porcelain Fused to Metal Crowns Placed at a Teaching Institution

Authors: Shizrah Jamal, Robia Ghafoor, Farhan Raza

Abstract:

Porcelain fused to metal crown is the most versatile variety of crown that is commonly placed worldwide. Various complications have been reported in the PFM crowns with use over the period of time. These include chipping of the porcelain, recurrent caries, loss of retention, open contacts, and tooth fracture. The objective of the present study was to determine the frequency of these complications in crowns cemented over a period of five years in a tertiary care hospital and also to report the survival of these crowns. A retrospective study was conducted in Dental clinics, Aga Khan University Hospital in which 150 PFM crowns cemented over a period of five years were evaluated. Patient demographics, oral hygiene habits, para-functional habits, crown insertion and follow-up dates were recorded in a specially designed proforma. All PFM crowns fulfilling the inclusion criteria were assessed both clinically and radiographically for the presence of any complication. SPSS version 22.0 was used for statistical analysis. Frequency distribution and proportion of complications were determined. Chi-square test was used to determine the association of complications of PFM crowns with multiple variables including tooth wear, opposing dentition and betel nut chewing. Kaplan- meier survival analysis was used to determine the survival of PFM crowns over the period of five years. Level of significance was kept at 0.05. A total of 107 patients, with a mean age of 43.51 + 12.4 years, having 150 PFM crowns were evaluated. The most common complication observed was open proximal contacts (8.7%) followed by porcelain chipping (6%), decementation (5.3%), and abutment fracture (1.3%). Chi square test showed that there was no statistically significant association of PFM crown complication with tooth wear, betel nut and opposing dentition (p-value <0.05). The overall success and survival rates of PFM crowns turned out to be 78.7 and 84.7% respectively. Within the limitations of the study, it can be concluded that PFM crowns are an effective treatment modality with high success and survival rates. Since it was a single centered study; the results should be generalized with caution.

Keywords: chipping, complication, crown, survival rate

Procedia PDF Downloads 169
64 Effect of Particle Size Variations on the Tribological Properties of Porcelain Waste Added Epoxy Composites

Authors: B. Yaman, G. Acikbas, N. Calis Acikbas

Abstract:

Epoxy based materials have advantages in tribological applications due to their unique properties such as light weight, self-lubrication capacity and wear resistance. On the other hand, their usage is often limited by their low load bearing capacity and low thermal conductivity values. In this study, it is aimed to improve tribological and also mechanical properties of epoxy by reinforcing with ceramic based porcelain waste. It is well-known that the reuse or recycling of waste materials leads to reduction in production costs, ease of manufacturing, saving energy, etc. From this perspective, epoxy and epoxy matrix composites containing 60wt% porcelain waste with different particle size in the range of below 90µm and 150-250µm were fabricated, and the effect of filler particle size on the mechanical and tribological properties was investigated. The microstructural characterization was carried out by scanning electron microscopy (SEM), and phase analysis was determined by X-ray diffraction (XRD). The Archimedes principle was used to measure the density and porosity of the samples. The hardness values were measured using Shore-D hardness, and bending tests were performed. Microstructural investigations indicated that porcelain particles were homogeneously distributed and no agglomerations were encountered in the epoxy resin. Mechanical test results showed that the hardness and bending strength were increased with increasing particle size related to low porosity content and well embedding to the matrix. Tribological behavior of these composites was evaluated in terms of friction, wear rates and wear mechanisms by ball-on-disk contact with dry and rotational sliding at room temperature against WC ball with a diameter of 3mm. Wear tests were carried out at room temperature (23–25°C) with a humidity of 40 ± 5% under dry-sliding conditions. The contact radius of cycles was set to 5 mm at linear speed of 30 cm/s for the geometry used in this study. In all the experiments, 3N of constant test load was applied at a frequency of 8 Hz and prolonged to 400m wear distance. The friction coefficient of samples was recorded online by the variation in the tangential force. The steady-state CoFs were changed in between 0,29-0,32. The dimensions of the wear tracks (depth and width) were measured as two-dimensional profiles by a stylus profilometer. The wear volumes were calculated by integrating these 2D surface areas over the diameter. Specific wear rates were computed by dividing the wear volume by the applied load and sliding distance. According to the experimental results, the use of porcelain waste in the fabrication of epoxy resin composites can be suggested to be potential materials due to allowing improved mechanical and tribological properties and also providing reduction in production cost.

Keywords: epoxy composites, mechanical properties, porcelain waste, tribological properties

Procedia PDF Downloads 177