9036 Multipass Scratch Characterization of TiNbVN Thin Coatings Deposited by Magnetron Sputtering

Authors: Hikmet Cicek

Abstract:

Transition metal nitrides are widely used as protective coatings on machine parts and cutting tools to protect the surfaces from abrasion and corrosion for decades. In this study, the ternary TiNbVN thin coatings were produced with closed field unbalanced magnetron sputtering system and their structural, mechanical and fatigue-like (multi-pass scratch test) properties were investigated. Two different substrates (M2 and H13 steels) were used to explore substrates effects. X-Ray diffractometer, scanning electron microscope, and energy dispersive spectroscopy were used for the structural and chemical analysis of the coatings. Nanohardness tests were proceed for mechanical properties. The fatigue-like properties of the coatings obtained from the multi-scratch test under three different cycle passes. The results showed that TiNbVN films have excellent fatigue resistance and the coatings deposited on M2 steel substrate have higher hardness and better fatigue resistance.

Keywords: physical vapor deposition, fatigue, metal nitride, multipass scratch test

Procedia PDF Downloads 184
9035 Inhibition of Pipelines Corrosion Using Natural Extracts

Authors: Eman Alzahrani, Hala M. Abo-Dief, Ashraf T. Mohamed

Abstract:

The present work is aimed at examining carbon steel oil pipelines corrosion using three natural extracts (Eruca Sativa, Rosell and Mango peels) that are used as inhibitors of different concentrations ranging from 0.05-0.1wt. %. Two sulphur compounds are used as corrosion mediums. Weight loss method was used for measuring the corrosion rate of the carbon steel specimens immersed in technical white oil at 100ºC at various time intervals in absence and presence of the two sulphur compounds. The corroded specimens are examined using the chemical wear test, scratch test and hardness test. The scratch test is carried out using scratch loads from 0.5 Kg to 2.0 Kg. The scratch width is obtained at various scratch load and test conditions. The Brinell hardness test is carried out and investigated for both corroded and inhibited specimens. The results showed that three natural extracts can be used as environmentally friendly corrosion inhibitors.

Keywords: inhibition, natural extract, oil pipelines corrosion, sulphur compounds

Procedia PDF Downloads 479
9034 A Study on Improvement of Straightness of Preform Pulling Process of Hollow Pipe by Finete Element Analysis Method

Authors: Yeon-Jong Jeong, Jun-Hong Park, Hyuk Choi

Abstract:

In this study, we have studied the design of intermediate die in multipass drawing. Research has been continuously studied because of the advantage of better dimensional accuracy, smooth surface and improved mechanical properties in the case of drawing. Among them, multipass drawing, which is a method to realize complicated shape by drawing, was discussed in this study. The most important factor in the multipass drawing is the dimensional accuracy and simplify the process. To accomplish this, a multistage shape drawing was performed using various intermediate die shape designs, and finite element analysis was performed.

Keywords: FEM (Finite Element Method), multipass drawing, intermediate die, hollow pipe

Procedia PDF Downloads 293
9033 Novel Scratch Resistant Self-Healing Automotive Clearcoats Using Hyperbranched Polymers and POSS Nanostructures

Authors: H.Yari, M. Mohseni, Z. Ranjbar

Abstract:

In this work a typical automotive clearcoat is modified with a combination of hyperbranched polymer (HBP) and polyhedral oligomeric silsesquioxane (POSS) nanostructures to simultaneously enhance the scratch resistance and healing ability of the resulting films. Micro-scratch and healing data revealed that these goals were achieved at high loadings of modifiers. Enhanced scratch resistance was attributed to the improved elastic recovery of the clearcoats in presence of modifiers. In addition, improved healing performance due to the partial replacement of covalent cross-links with physical ones resulted from the unique globular highly branched structure of HBP and POSS macromolecules.

Keywords: automotive clearcoat, POSS building blocks scratch resistance, self-healing

Procedia PDF Downloads 362
9032 Studies on Corrosion Resistant Composite Coating for Metallic Surfaces

Authors: Navneetinder Singh, Harprabhjot Singh, Harpreet Singh, Supreet Singh

Abstract:

Many materials are known to mankind that is widely used for synthesis of corrosion resistant hydrophobic coatings. In the current work, novel hydrophobic composite was synthesized by mixing polytetrafluoroethylene (PTFE) and 20 weight% ceria particles followed by sintering. This composite had same hydrophobic behavior as PTFE. Moreover, composite showed better scratch resistance than virgin PTFE. Pits of plasma sprayed Ni₃Al coating were exploited to hold PTFE composite on the substrate as Superni-75 alloy surface through sintering process. Plasma sprayed surface showed good adhesion with the composite coating during scratch test. Potentiodynamic corrosion test showed 100 fold decreases in corrosion rate of coated sample this may be attributed to inert and hydrophobic nature of PTFE and ceria.

Keywords: polytetrafluoroethylene, PTFE, ceria, coating, corrosion

Procedia PDF Downloads 338
9031 Mechanical Response Investigation of Wafer Probing Test with Vertical Cobra Probe via the Experiment and Transient Dynamic Simulation

Authors: De-Shin Liu, Po-Chun Wen, Zhen-Wei Zhuang, Hsueh-Chih Liu, Pei-Chen Huang

Abstract:

Wafer probing tests play an important role in semiconductor manufacturing procedures in accordance with the yield and reliability requirement of the wafer after the backend-of-the-line process. Accordingly, the stable physical and electrical contact between the probe and the tested wafer during wafer probing is regarded as an essential issue in identifying the known good die. The probe card can be integrated with multiple probe needles, which are classified as vertical, cantilever and micro-electro-mechanical systems type probe selections. Among all potential probe types, the vertical probe has several advantages as compared with other probe types, including maintainability, high probe density and feasibility for high-speed wafer testing. In the present study, the mechanical response of the wafer probing test with the vertical cobra probe on 720 μm thick silicon (Si) substrate with a 1.4 μm thick aluminum (Al) pad is investigated by the experiment and transient dynamic simulation approach. Because the deformation mechanism of the vertical cobra probe is determined by both bending and buckling mechanisms, the stable correlation between contact forces and overdrive (OD) length must be carefully verified. Moreover, the decent OD length with corresponding contact force contributed to piercing the native oxide layer of the Al pad and preventing the probing test-induced damage on the interconnect system. Accordingly, the scratch depth of the Al pad under various OD lengths is estimated by the atomic force microscope (AFM) and simulation work. In the wafer probing test configuration, the contact phenomenon between the probe needle and the tested object introduced large deformation and twisting of mesh gridding, causing the subsequent numerical divergence issue. For this reason, the arbitrary Lagrangian-Eulerian method is utilized in the present simulation work to conquer the aforementioned issue. The analytic results revealed a slight difference when the OD is considered as 40 μm, and the simulated is almost identical to the measured scratch depths of the Al pad under higher OD lengths up to 70 μm. This phenomenon can be attributed to the unstable contact of the probe at low OD length with the scratch depth below 30% of Al pad thickness, and the contact status will be being stable when the scratch depth over 30% of pad thickness. The splash of the Al pad is observed by the AFM, and the splashed Al debris accumulates on a specific side; this phenomenon is successfully simulated in the transient dynamic simulation. Thus, the preferred testing OD lengths are found as 45 μm to 70 μm, and the corresponding scratch depths on the Al pad are represented as 31.4% and 47.1% of Al pad thickness, respectively. The investigation approach demonstrated in this study contributed to analyzing the mechanical response of wafer probing test configuration under large strain conditions and assessed the geometric designs and material selections of probe needles to meet the requirement of high resolution and high-speed wafer-level probing test for thinned wafer application.

Keywords: wafer probing test, vertical probe, probe mark, mechanical response, FEA simulation

Procedia PDF Downloads 27
9030 Solving a Micromouse Maze Using an Ant-Inspired Algorithm

Authors: Rolando Barradas, Salviano Soares, António Valente, José Alberto Lencastre, Paulo Oliveira

Abstract:

This article reviews the Ant Colony Optimization, a nature-inspired algorithm, and its implementation in the Scratch/m-Block programming environment. The Ant Colony Optimization is a part of Swarm Intelligence-based algorithms and is a subset of biological-inspired algorithms. Starting with a problem in which one has a maze and needs to find its path to the center and return to the starting position. This is similar to an ant looking for a path to a food source and returning to its nest. Starting with the implementation of a simple wall follower simulator, the proposed solution uses a dynamic graphical interface that allows young students to observe the ants’ movement while the algorithm optimizes the routes to the maze’s center. Things like interface usability, Data structures, and the conversion of algorithmic language to Scratch syntax were some of the details addressed during this implementation. This gives young students an easier way to understand the computational concepts of sequences, loops, parallelism, data, events, and conditionals, as they are used through all the implemented algorithms. Future work includes the simulation results with real contest mazes and two different pheromone update methods and the comparison with the optimized results of the winners of each one of the editions of the contest. It will also include the creation of a Digital Twin relating the virtual simulator with a real micromouse in a full-size maze. The first test results show that the algorithm found the same optimized solutions that were found by the winners of each one of the editions of the Micromouse contest making this a good solution for maze pathfinding.

Keywords: nature inspired algorithms, scratch, micromouse, problem-solving, computational thinking

Procedia PDF Downloads 96
9029 Austempered Compacted Graphite Irons: Influence of Austempering Temperature on Microstructure and Microscratch Behavior

Authors: Rohollah Ghasemi, Arvin Ghorbani

Abstract:

This study investigates the effect of austempering temperature on microstructure and scratch behavior of the austempered heat-treated compacted graphite irons. The as-cast was used as base material for heat treatment practices. The samples were extracted from as-cast ferritic CGI pieces and were heat treated under austenitising temperature of 900°C for 60 minutes which followed by quenching in salt-bath at different austempering temperatures of 275°C, 325°C and 375°C. For all heat treatments, an austempering holding time of 30 minutes was selected for this study. Light optical microscope (LOM) and scanning electron microscope (SEM) and electron back scattered diffraction (EBSD) analysis confirmed the ausferritic matrix formed in all heat-treated samples. Microscratches were performed under the load of 200, 600 and 1000 mN using a sphero-conical diamond indenter with a tip radius of 50 μm and induced cone angle 90° at a speed of 10 μm/s at room temperature ~25°C. An instrumented nanoindentation machine was used for performing nanoindentation hardness measurement and microscratch testing. Hardness measurements and scratch resistance showed a significant increase in Brinell, Vickers, and nanoindentation hardness values as well as microscratch resistance of the heat-treated samples compared to the as-cast ferritic sample. The increase in hardness and improvement in microscratch resistance are associated with the formation of the ausferrite matrix consisted of carbon-saturated retained austenite and acicular ferrite in austempered matrix. The maximum hardness was observed for samples austempered at 275°C which resulted in the formation of very fine acicular ferrite. In addition, nanohardness values showed a quite significant variation in the matrix due to the presence of acicular ferrite and carbon-saturated retained austenite. It was also observed that the increase of austempering temperature resulted in increase of volume of the carbon-saturated retained austenite and decrease of hardness values.

Keywords: austempered CGI, austempering, scratch testing, scratch plastic deformation, scratch hardness

Procedia PDF Downloads 111
9028 Performance Comparison of Deep Convolutional Neural Networks for Binary Classification of Fine-Grained Leaf Images

Authors: Kamal KC, Zhendong Yin, Dasen Li, Zhilu Wu

Abstract:

Intra-plant disease classification based on leaf images is a challenging computer vision task due to similarities in texture, color, and shape of leaves with a slight variation of leaf spot; and external environmental changes such as lighting and background noises. Deep convolutional neural network (DCNN) has proven to be an effective tool for binary classification. In this paper, two methods for binary classification of diseased plant leaves using DCNN are presented; model created from scratch and transfer learning. Our main contribution is a thorough evaluation of 4 networks created from scratch and transfer learning of 5 pre-trained models. Training and testing of these models were performed on a plant leaf images dataset belonging to 16 distinct classes, containing a total of 22,265 images from 8 different plants, consisting of a pair of healthy and diseased leaves. We introduce a deep CNN model, Optimized MobileNet. This model with depthwise separable CNN as a building block attained an average test accuracy of 99.77%. We also present a fine-tuning method by introducing the concept of a convolutional block, which is a collection of different deep neural layers. Fine-tuned models proved to be efficient in terms of accuracy and computational cost. Fine-tuned MobileNet achieved an average test accuracy of 99.89% on 8 pairs of [healthy, diseased] leaf ImageSet.

Keywords: deep convolution neural network, depthwise separable convolution, fine-grained classification, MobileNet, plant disease, transfer learning

Procedia PDF Downloads 157
9027 Hand Motion Tracking as a Human Computer Interation for People with Cerebral Palsy

Authors: Ana Teixeira, Joao Orvalho

Abstract:

This paper describes experiments using Scratch games, to check the feasibility of employing cerebral palsy users gestures as an alternative of interaction with a computer carried out by students of Master Human Computer Interaction (HCI) of IPC Coimbra. The main focus of this work is to study the usability of a Web Camera as a motion tracking device to achieve a virtual human-computer interaction used by individuals with CP. An approach for Human-computer Interaction (HCI) is present, where individuals with cerebral palsy react and interact with a scratch game through the use of a webcam as an external interaction device. Motion tracking interaction is an emerging technology that is becoming more useful, effective and affordable. However, it raises new questions from the HCI viewpoint, for example, which environments are most suitable for interaction by users with disabilities. In our case, we put emphasis on the accessibility and usability aspects of such interaction devices to meet the special needs of people with disabilities, and specifically people with CP. Despite the fact that our work has just started, preliminary results show that, in general, computer vision interaction systems are very useful; in some cases, these systems are the only way by which some people can interact with a computer. The purpose of the experiments was to verify two hypothesis: 1) people with cerebral palsy can interact with a computer using their natural gestures, 2) scratch games can be a research tool in experiments with disabled young people. A game in Scratch with three levels is created to be played through the use of a webcam. This device permits the detection of certain key points of the user’s body, which allows to assume the head, arms and specially the hands as the most important aspects of recognition. Tests with 5 individuals of different age and gender were made throughout 3 days through periods of 30 minutes with each participant. For a more extensive and reliable statistical analysis, the number of both participants and repetitions in further investigations should be increased. However, already at this stage of research, it is possible to draw some conclusions. First, and the most important, is that simple scratch games on the computer can be a research tool that allows investigating the interaction with computer performed by young persons with CP using intentional gestures. Measurements performed with the assistance of games are attractive for young disabled users. The second important conclusion is that they are able to play scratch games using their gestures. Therefore, the proposed interaction method is promising for them as a human-computer interface. In the future, we plan to include the development of multimodal interfaces that combine various computer vision devices with other input devices improvements in the existing systems to accommodate more the special needs of individuals, in addition, to perform experiments on a larger number of participants.

Keywords: motion tracking, cerebral palsy, rehabilitation, HCI

Procedia PDF Downloads 213
9026 Nano Effects of Nitrogen Ion Implantation on TiN Hard Coatings Deposited by Physical Vapour Deposition and Ion Beam Assisted Deposition

Authors: Branko Skoric, Aleksandar Miletic, Pal Terek, Lazar Kovacevic, Milan Kukuruzovic

Abstract:

In this paper, we present the results of a study of TiN thin films which are deposited by a Physical Vapour Deposition (PVD) and Ion Beam Assisted Deposition (IBAD). In the present investigation the subsequent ion implantation was provided with N5+ ions. The ion implantation was applied to enhance the mechanical properties of surface. The thin film deposition process exerts a number of effects such as crystallographic orientation, morphology, topography, densification of the films. A variety of analytic techniques were used for characterization, such as scratch test, calo test, Scanning electron microscopy (SEM), Atomic Force Microscope (AFM), X-ray diffraction (XRD) and Energy Dispersive X-ray analysis (EDAX).

Keywords: coating, super hard, ion implantation, nanohardness

Procedia PDF Downloads 308
9025 Automating Test Activities: Test Cases Creation, Test Execution, and Test Reporting with Multiple Test Automation Tools

Authors: Loke Mun Sei

Abstract:

Software testing has become a mandatory process in assuring the software product quality. Hence, test management is needed in order to manage the test activities conducted in the software test life cycle. This paper discusses on the challenges faced in the software test life cycle, and how the test processes and test activities, mainly on test cases creation, test execution, and test reporting is being managed and automated using several test automation tools, i.e. Jira, Robot Framework, and Jenkins.

Keywords: test automation tools, test case, test execution, test reporting

Procedia PDF Downloads 548
9024 Design of an Instrumentation Setup and Data Acquisition System for a GAS Turbine Engine Using Suitable DAQ Software

Authors: Syed Nauman Bin Asghar Bukhari, Mohtashim Mansoor, Mohammad Nouman

Abstract:

Engine test-Bed system is a fundamental tool to measure dynamic parameters, economic performance, and reliability of an aircraft Engine, and its automation and accuracy directly influences the precision of acquired and analysed data. In this paper, we present the design of digital Data Acquisition (DAQ) system for a vintage aircraft engine test bed that lacks the capability of displaying all the analyzed parameters at one convenient location (one panel-one screen). Recording such measurements in the vintage test bed is not only time consuming but also prone to human errors. Digitizing such measurement system requires a Data Acquisition (DAQ) system capable of recording these parameters and displaying them on one screen-one panel monitor. The challenge in designing upgrade to the vintage systems arises with a need to build and integrate digital measurement system from scratch with a minimal budget and modifications to the existing vintage system. The proposed design not only displays all the key performance / maintenance parameters of the gas turbine engines for operator as well as quality inspector on separate screens but also records the data for further processing / archiving.

Keywords: Gas turbine engine, engine test cell, data acquisition, instrumentation

Procedia PDF Downloads 100
9023 High-Frequency Induction Heat Sintering of Al/SiC/GNS Nanocomposites and Their Tribological Properties

Authors: Mohammad Islam, Iftikhar Ahmad, Hany S. Abdo, Yasir Khalid

Abstract:

High-frequency induction heat sintering (HFIHS) is a fast, efficient powder consolidation technique. In this work, aluminum (Al) powder was mixed with silicon carbide (SiC) and/or graphene nanosheets (GNS) in different proportions and compacted using HFIHS process to produce dense nanocomposites. The nanostructures dispersion was assessed via electron microscopy using both SEM and TEM. Tribological behavior of the nanocomposites was investigated at different loads to determine wear rate and coefficient of friction. The scratch profiles were examined under the microscope to correlate wear properties with the microstructure. While the addition of SiC nanoparticles enhances microhardness values, GNS incorporation promotes dry lubricity with strikingly different wear scratch morphologies. Such Al/SiC/GNS material compositions can be explored for use in automotive brake pad and thermal management applications.

Keywords: aluminum nanocomposites, silicon carbide, graphene nanosheets, tribology

Procedia PDF Downloads 279
9022 Turning Parameters Affect Time up and Go Test Performance in Pre-Frail Community-Dwelling Elderly

Authors: Kuei-Yu Chien, Hsiu-Yu Chiu, Chia-Nan Chen, Shu-Chen Chen

Abstract:

Background: Frailty is associated with decreased physical performances that affect mobility of the elderly. Time up and go test (TUG) was the common method to evaluate mobility in the community. The purpose of this study was to compare the parameters in different stages of Time up and go test (TUG) and physical performance between pre-frail elderly (PFE) and non-frail elderly (NFE). We also investigated the relationship between TUG parameters and physical performance. Methods: Ninety-two community-dwelling older adults were as participants in this study. Based on Canadian Study of Health and Aging Clinical Frailty Scale, 22 older adults were classified as PFE (71.77 ± 6.05 yrs.) and 70 were classified as NFE (71.2 ± 5.02 yrs.). We performed body composition and physical performance, including balance, muscular strength/endurance, mobility, cardiorespiratory endurance, and flexibility. Results: Pre-frail elderly took significantly longer time than NFE in TUG test (p=.004). Pre-frail elderly had lower turning average angular velocity (p = .017), turning peak angular velocity (p = .041) and turning-stand to sit peak angular velocity (p = .037) than NFE. The turning related parameters related to open-eye stand on right foot, 30-second chair stand test, back scratch, and 2-min step tests. Conclusions: Turning average angular velocity, turning peak angular velocity and turning-stand to sit peak angular velocity mainly affected the TUG performance. We suggested that static/dynamic balance, agility, flexibility, and muscle strengthening of lower limbs exercise were important to PFE.

Keywords: mobility, aglity, active ageing, functional fitness

Procedia PDF Downloads 155
9021 Characterization of a Pure Diamond-Like Carbon Film Deposited by Nanosecond Pulsed Laser Deposition

Authors: Camilla G. Goncalves, Benedito Christ, Walter Miyakawa, Antonio J. Abdalla

Abstract:

This work aims to investigate the properties and microstructure of diamond-like carbon film deposited by pulsed laser deposition by ablation of a graphite target in a vacuum chamber on a steel substrate. The equipment was mounted to provide one laser beam. The target of high purity graphite and the steel substrate were polished. The mechanical and tribological properties of the film were characterized using Raman spectroscopy, nanoindentation test, scratch test, roughness profile, tribometer, optical microscopy and SEM images. It was concluded that the pulsed laser deposition (PLD) technique associated with the low-pressure chamber and a graphite target provides a good fraction of sp3 bonding, that the process variable as surface polishing and laser parameter have great influence in tribological properties and in adherence tests performance. The optical microscopy images are efficient to identify the metallurgical bond.

Keywords: characterization, DLC, mechanical properties, pulsed laser deposition

Procedia PDF Downloads 130
9020 Assessment of Hamstring, Lower Back and Upper Body Flexibility in War Disabled Individuals in Sri Lanka North and East Region

Authors: Esther Liyanage, Indrajith Liyanage, A. A. J. Rajaratne

Abstract:

During the 30 year civil war in Sri Lanka, a large number of individuals were injured and disabled. These disabilities have reduced their daily physical activities which may cause reduction in flexibility of upper limb, shoulder girdle, lower back and lower limb. Muscle flexibility is important for a healthy lifestyle. The main objective of the study was to assess the upper limb, shoulder girdle and lower back, hamstring flexibility of the intact lower limb in disabled individuals in the North and Eastern parts of Sri Lanka. Back saver sits and reach test and shoulder scratch test described in FITNESS GRAM was used in the study. A total of 125 disabled soldiers with lower limb disabilities were recruited for the study. Flexibility of the lower back and hamstring muscles of uninjured lower limb was measured using back saver sit and reach test described by Wells and Dillon (1952). Upper limb and shoulder girdle flexibility was assessed using shoulder stretch test. Score 0-3 was given according to the ability to reach Superior medial angle of the opposite scapula, top of the head or the mouth. The results indicate that 31 (24.8%) disabled soldiers have lower limb flexibility less than 8, 2 (1.6 % ) have flexibility of 8, 2 (1.6 %) have flexibility of 8.5, 11 ( 8.8% ) have flexibility of 9, 14 (11.2 %) have flexibility of 9.5, 23 (18.4 %) have flexibility of 10, 17 (13.6 %) have 10.5 flexibility, 13 (10.4%) have 11 flexibility, 2 (1.6%) have 11.5 flexibility, 10 (8 %) have flexibility of 12 and 3 (2.34 %) have flexibility of 12.5. Six disabled soldiers (4.8%) have upper limb flexibility of 2 and remaining 95.2% have normal upper limb flexibility (score 3). A reduction in the flexibility of muscles in lower body and lower limbs was seen in 25% disabled soldiers which could be due to reduction in their daily physical activities.

Keywords: disability, flexibility, rehabilitation, quality of life

Procedia PDF Downloads 443
9019 Controlling the Degradation Rate of Biodegradable Mg Implant Using Magnetron-Sputtered (Zr-Nb) Thin Films

Authors: Somayeh Azizi, Mohammad Hossein Ehsani, Amir Zareidoost

Abstract:

In this research, a technique has been developed to reduce the corrosion rate of magnesium (Mg) metal by creating Zr-Nb thin film coatings. In this regard, thin-film coatings of niobium (Nb) zirconium (Zr) double alloy are applied on pure Mg specimens under different processes conditions, such as the change of the substrate temperature, substrate bias, and coating thickness using the magnetron sputtering method. Then, deposited coatings are analyzed in terms of surface features via field-emission scanning electron microscopy (FE-SEM), thin-layer X-ray diffraction (GI-XRD), energy-dispersive X-ray spectroscopy (EDS), atomic force microscopy (AFM), and corrosion tests. Also, nano-scratch tests were carried out to investigate the adhesion of the thin film. The results showed that the (Zr-Nb) thin films could control the degradation rate of Mg in the simulated body fluid (SBF). The nano-scratch studies depicted that the (Zr-Nb) thin films have a proper adhesion with the Mg substrate. Therefore, this technique could be used to enhance the corrosion resistance of bare Mg and could result in improving the performance of the biodegradable Mg implant for orthopedic applications.

Keywords: (Zr-Nb) thin film, magnetron sputtering, biodegradable Mg, degradation rate

Procedia PDF Downloads 89
9018 Investigation of Electrochemical, Morphological, Rheological and Mechanical Properties of Nano-Layered Graphene/Zinc Nanoparticles Incorporated Cold Galvanizing Compound at Reduced Pigment Volume Concentration

Authors: Muhammad Abid

Abstract:

The ultimate goal of this research was to produce a cold galvanizing compound (CGC) at reduced pigment volume concentration (PVC) to protect metallic structures from corrosion. The influence of the partial replacement of Zn dust by nano-layered graphene (NGr) and Zn metal nanoparticles on the electrochemical, morphological, rheological, and mechanical properties of CGC was investigated. EIS was used to explore the electrochemical nature of coatings. The EIS results revealed that the partial replacement of Zn by NGr and Zn nanoparticles enhanced the cathodic protection at reduced PVC (4:1) by improving the electrical contact between the Zn particles and the metal substrate. The Tafel scan was conducted to support the cathodic behaviour of the coatings. The sample formulated solely with Zn at PVC 4:1 was found to be dominated in physical barrier characteristics over cathodic protection. By increasing the concentration of NGr in the formulation, the corrosion potential shifted towards a more negative side. The coating with 1.5% NGr showed the highest galvanic action at reduced PVC. FE-SEM confirmed the interconnected network of conducting particles. The coating without NGr and Zn nanoparticles at PVC 4:1 showed significant gaps between the Zn dust particles. The novelty was evidenced when micrographs showed the consistent distribution of NGr and Zn nanoparticles all over the surface, which acted as a bridge between spherical Zn particles and provided cathodic protection at a reduced PVC. The layered structure of graphene also improved the physical shielding effect of the coatings, which limited the diffusion of electrolytes and corrosion products (oxides/hydroxides) into the coatings, which was reflected by the salt spray test. The rheological properties of coatings showed good liquid/fluid properties. All the coatings showed excellent adhesion but had different strength values. A real-time scratch resistance assessment showed all the coatings had good scratch resistance.

Keywords: protective coatings, anti-corrosion, galvanization, graphene, nanomaterials, polymers

Procedia PDF Downloads 62
9017 Hot Cracking Susceptibility Evaluation of the Advanced UNS S31035 Austenitic Stainless Steel by Varestraint Weldability Testing

Authors: Mikael M. Johansson, Peter Stenvall, Leif Karlsson, Joel Andersson

Abstract:

Sandvik Sanicro 25, UNS S31035, is an advanced high temperature austenitic stainless steel that potentially can be used in super-heaters and reheaters in the next generation of advanced ultra-super critical power plants. The material possesses both high creep strength and good corrosion resistance at temperatures up to 700°C. Its high temperature properties are positioned between other commercially available high temperature austenitic stainless steels and nickel-based alloys. It is, however, well known that an austenitic solidification mode combined with a fully austenitic microstructure exacerbate susceptibility towards hot cracking. The problem increases even more for thick walled material in multipass welding and could compromise the integrity of the welded component. Varestraint weldability testing is commonly used to evaluate susceptibility towards hot cracking of materials. In this paper, Varestraint test results are evaluated for base material of both UNS S31035 steel and are compared to those of the well-known and well-characterized UNS S31008 grade. The more creep resistant alloy, UNS S31035, is metallurgically more complicated than the UNS S31008 grade and has additions of several alloying elements to improve its high temperature properties. It benefits from both solid solution hardening as well as precipitation hardening. This investigation therefore attempts, based on the Varestraint weldability test, to understand if there are any differences in cracking mechanisms between these two grades due to the additional alloying elements used in UNS S31035. Results from Varestraint testing and crack type investigations will be presented and discussed in some detail. It is shown that hot cracking susceptibility of the UNS S31035 steel is only slightly higher than that of UNS S31008 despite the more complicated metallurgy. Weldability of the two alloys is therefore judged to be comparable making the newer alloy well suited also for critical applications.

Keywords: austenitic stainless steel, hot cracking susceptibility, UNS S31035, UNS S31008, varestraint weldability testing

Procedia PDF Downloads 106
9016 Development and Characterization of Bio-Tribological, Nano- Multilayer Coatings for Medical Tools Application

Authors: L. Major, J. M. Lackner, M. Dyner, B. Major

Abstract:

Development of new generation bio- tribological, multilayer coatings, opens an avenue for fabrication of future high- tech functional surfaces. In the presented work, nano- composite, Cr/CrN+[Cr/ a-C:H implanted by metallic nanocrystals] multilayer coatings have been developed for surface protection of medical tools. Thin films were fabricated by a hybrid Pulsed Laser Deposition technique. Complex microstructure analysis of nano- multilayer coatings, subjected to mechanical and biological tests, were performed by means of transmission electron microscopy (TEM). Microstructure characterization revealed the layered arrangement of Cr23C6 nanoparticles in multilayer structure. Influence of deposition conditions on bio- tribological properties of the coatings were studied. The bio-tests were used as a screening tool for the analyzed nano- multilayer coatings before they could be deposited on medical tools. Bio- medical tests were done using fibroblasts. The mechanical properties of the coatings were investigated by means of a ball-on-disc mechanical test. The microhardness was done using Berkovich indenter. The scratch adhesion test was done using Rockwell indenter. From the bio- tribological point of view, the optimal properties had the C106_1 material.

Keywords: bio- tribological coatings, cell- material interaction, hybrid PLD, tribology

Procedia PDF Downloads 348
9015 Synthesis and Characterization of Renewable Resource Based Green Epoxy Coating

Authors: Sukanya Pradhan, Smita Mohanty, S. K Nayak

Abstract:

Plant oils are a great renewable source for being a reliable starting material to access new products with a wide spectrum of structural and functional variations. Even though petroleum products might also render the same, but it would also impose a high risk factor of environmental and health hazard. Since epoxidized vegetable oils are easily available, eco-compatible, non-toxic and renewable, hence these have drawn much of the attentions in the polymer industrial sector especially for the development of eco-friendly coating materials. In this study a waterborne epoxy coating was prepared from epoxidized soyabean oil by using triethanolamine. Because of its hydrophobic nature, it was a tough and tedius task to make it hydrophilic. The hydrophobic biobased epoxy was modified into waterborne epoxy by the help of a plant based anhydride as curing agent. Physico-mechanical, chemical resistance tests and thermal analysis of the green coating material were carried out which showed good physic-mechanical, chemical resistance properties as well as environment friendly. The complete characterization of the final material was done in terms of scratch hardness, gloss test, impact resistance, adhesion and bend test.

Keywords: epoxidized soybean oil, waterborne, curing agent, green coating

Procedia PDF Downloads 520
9014 Analysis of the Result for the Accelerated Life Cycle Test of the Motor for Washing Machine by Using Acceleration Factor

Authors: Youn-Sung Kim, Jin-Ho Jo, Mi-Sung Kim, Jae-Kun Lee

Abstract:

Accelerated life cycle test is applied to various products or components in order to reduce the time of life cycle test in industry. It must be considered for many test conditions according to the product characteristics for the test and the selection of acceleration parameter is especially very important. We have carried out the general life cycle test and the accelerated life cycle test by applying the acceleration factor (AF) considering the characteristics of brushless DC (BLDC) motor for washing machine. The final purpose of this study is to verify the validity by analyzing the results of the general life cycle test and the accelerated life cycle test. It will make it possible to reduce the life test time through the reasonable accelerated life cycle test.

Keywords: accelerated life cycle test, reliability test, motor for washing machine, brushless dc motor test

Procedia PDF Downloads 585
9013 Equipment Design for Lunar Lander Landing-Impact Test

Authors: Xiaohuan Li, Wangmin Yi, Xinghui Wu

Abstract:

In order to verify the performance of lunar lander structure, landing-impact test is urgently needed. Moreover, the test equipment is necessary for the test. The functions and the key points of the equipment is presented to satisfy the requirements of the test,and the design scheme is proposed. The composition, the major function and the critical parts’ design of the equipment are introduced. By the load test of releasing device and single-beam hoist, and the compatibility test of landing-impact testing system, the rationality and reliability of the equipment is proved.

Keywords: landing-impact test, lunar lander, releasing device, test equipment

Procedia PDF Downloads 594
9012 Effect of Micaceous Iron Oxide and Nanocrystalline Al on the Electrochemical Behavior of Aliphatic Amine Cured Epoxy Coating

Authors: Asiful H. Seikh, Jabair A. Mohammed, Ubair A. Samad, Mohammad A. Alam, Saeed M. Al-Zahrani, El-Sayed M. Sherif

Abstract:

Three coating formulations were fabricated by incorporating different percentages of MIO (micaceous iron oxide ) (1, 2, and wt%) with ball-milled nanocrystalline Al (2 wt%) particles, which was optimized earlier. These coatings were characterized by means of different methods, namely, SEM, TGA, pendulum hardness, scratch test, and nano-indentation. The EIS measurements were carried out to report the effect of adding MIO powder in fabricated coatings on their corrosion behavior in 3.5 wt% NaCl solutions. In order to report the effect of immersion time on the corrosion and degradation of the prepared coatings, the EIS data were also acquired after various exposure periods of time, i.e., 1 h, 7 d, 14 d, 21 d, and 30 d in the test chloride solution. It has been found that the obtained EIS data for the fabricated coatings proved that the presence of 2% MIO provided the highest corrosion resistance amongst all coatings and that effect was recorded after all immersion periods of time. But, the MIO-incorporated coatings have less corrosion resistance than Al based epoxy coatings. It was also shown that with prolonged immersion, the resistance to corrosion declined after 7d, then with a longer period of immersion, i.e. 14 d, 21 d, and 30 d increases the resistance to corrosion by forming oxide products on the coatings surface. The results obtained from both mechanical and electrochemical testing confirmed that the fabricated coating with 2 wt% Al exhibited better hardness and higher resistance to corrosion as compared to coatings with 1 wt% Al and 3 wt% Al.

Keywords: epoxy coatings, nanomaterials, corrosion resistance, EIS, nanoindentation

Procedia PDF Downloads 28
9011 In situ High Temperature Characterization of Diamond-Like Carbon Films

Authors: M. Rouhani, F. C. N. Hong, Y. R. Jeng

Abstract:

The tribological performance of DLC films is limited by graphitization at elevated temperatures. Despite of numerous studies on the thermal stability of DLC films, a comprehensive in-situ characterization at elevated temperature is still lacking. In this study, DLC films were deposited using filtered cathodic arc vacuum method. Thermal stability of the films was characterized in-situally using a synchronized technique integrating Raman spectroscopy and depth-sensing measurements. Tests were performed in a high temperature chamber coupled with feedback control to make it possible to study the temperature effects in the range of 21 – 450 ̊C. Co-located SPM and Raman microscopy maps at different temperature over a specific area on the surface of the film were prepared. The results show that the thermal stability of the DLC films depends on their sp3 content. Films with lower sp3 content endure graphitization during the temperature-course used in this study. The graphitization is accompanied with significant changes in surface roughness and Raman spectrum of the film. Surface roughness of the films start to change even before graphitization transformation could be detected using Raman spectroscopy. Depth-sensing tests (nanoindentation, nano-scratch and wear) endorse the surface roughness change seen before graphitization occurrence. This in-situ study showed that the surface of the films is more sensitive to temperature rise compared to the bulk. We presume the changes observed in films hardness, surface roughness and scratch resistance with temperature rise, before graphitization occurrence, is due to surface relaxation.

Keywords: DLC film, nanoindentation, Raman spectroscopy, thermal stability

Procedia PDF Downloads 170
9010 A Survey on the Status of Test Automation

Authors: Andrei Contan, Richard Torkar

Abstract:

Aim: The process of test automation and its practices in industry have to be better understood, both for the industry itself and for the research community. Method: We conducted a quantitative industry survey by asking IT professionals to answer questions related to the area of test automation. Results: Test automation needs and practices vary greatly between organizations at different stages of the software development life cycle. Conclusions: Most of the findings are general test automation challenges and are specific to small- to medium-sized companies, developing software applications in the web, desktop or mobile domain.

Keywords: survey, testing, test automation, status of test automation

Procedia PDF Downloads 620
9009 The Creation of Calcium Phosphate Coating on Nitinol Substrate

Authors: Kirill M. Dubovikov, Ekaterina S. Marchenko, Gulsharat A. Baigonakova

Abstract:

NiTi alloys are widely used as implants in medicine due to their unique properties such as superelasticity, shape memory effect and biocompatibility. However, despite these properties, one of the major problems is the release of nickel after prolonged use in the human body under dynamic stress. This occurs due to oxidation and cracking of NiTi implants, which provokes nickel segregation from the matrix to the surface and release into living tissues. As we know, nickel is a toxic element and can cause cancer, allergies, etc. One of the most popular ways to solve this problem is to create a corrosion resistant coating on NiTi. There are many coatings of this type, but not all of them have good biocompatibility, which is very important for medical implants. Coatings based on calcium phosphate phases have excellent biocompatibility because Ca and P are the main constituents of the mineral part of human bone. This fact suggests that a Ca-P coating on NiTi can enhance osteogenesis and accelerate the healing process. Therefore, the aim of this study is to investigate the structure of Ca-P coating on NiTi substrate. Plasma assisted radio frequency (RF) sputtering was used to obtain this film. This method was chosen because it allows the crystallinity and morphology of the Ca-P coating to be controlled by the sputtering parameters. It allows us to obtain three different NiTi samples with Ca-P coating. XRD, AFM, SEM and EDS were used to study the composition, structure and morphology of the coating phase. Scratch tests were carried out to evaluate the adhesion of the coating to the substrate. Wettability tests were used to investigate the hydrophilicity of the different coatings and to suggest which of them had better biocompatibility. XRD showed that the coatings of all samples were hydroxyapatite, but the matrix was represented by TiNi intermetallic compounds such as B2, Ti2Ni and Ni3Ti. The SEM shows that the densest and defect-free coating has only one sample after three hours of sputtering. Wettability tests show that the sample with the densest coating has the lowest contact angle of 40.2° and the largest free surface area of 57.17 mJ/m2, which is mostly disperse. A scratch test was carried out to investigate the adhesion of the coating to the surface and it was shown that all coatings were removed by a cohesive mechanism. However, at a load of 30N, the indenter reached the substrate in two out of three samples, except for the sample with the densest coating. It was concluded that the most promising sputtering mode was the third, which consisted of three hours of deposition. This mode produced a defect-free Ca-P coating with good wettability and adhesion.

Keywords: biocompatibility, calcium phosphate coating, NiTi alloy, radio frequency sputtering.

Procedia PDF Downloads 44
9008 Evaluation of the Efficacy of Titanium Alloy Dental Implants Coated by Bio-ceramic Apatite Wollastonite (Aw) and Hydroxyapatite (Ha) by Pulsed Laser Deposition

Authors: Betsy S. Thomas, Manjeet Marpara, K. M. Bhat

Abstract:

Introduction: After the initial enthusiasm and interest in hydroxyapatite products subsided due to dissolution of the coating and failure at the coating interface, this was a unique attempt to create a next generation of dental implant. Materials and Methods: The adhesion property of AW and HA coatings at various temperature by pulsed laser deposition was assessed on titanium plates. Moreover, AW/HA coated implants implanted in the femur of the rabbits was evaluated at various intervals. Results: Decohesion load was more for AW in scratch test and more bone formation around AW coated implants on histological evaluation. Discussion: AW coating by pulsed laser deposition was more adherent to the titanium surface and led to faster bone formation than HA. Conclusion: This experiment opined that AW coated by pulsed laser deposition seems to be a promising method in achieving bioactive coatings on titanium implants.

Keywords: surface coating, dental implants, osseo integration, biotechnology

Procedia PDF Downloads 337
9007 Prioritization of Mutation Test Generation with Centrality Measure

Authors: Supachai Supmak, Yachai Limpiyakorn

Abstract:

Mutation testing can be applied for the quality assessment of test cases. Prioritization of mutation test generation has been a critical element of the industry practice that would contribute to the evaluation of test cases. The industry generally delivers the product under the condition of time to the market and thus, inevitably sacrifices software testing tasks, even though many test cases are required for software verification. This paper presents an approach of applying a social network centrality measure, PageRank, to prioritize mutation test generation. The source code with the highest values of PageRank will be focused first when developing their test cases as these modules are vulnerable to defects or anomalies which may cause the consequent defects in many other associated modules. Moreover, the approach would help identify the reducible test cases in the test suite, still maintaining the same criteria as the original number of test cases.

Keywords: software testing, mutation test, network centrality measure, test case prioritization

Procedia PDF Downloads 75