Search results for: Ni – base superalloy ŽS6K
810 The High Temperature Damage of DV – 2 Turbine Blade Made from Ni – Base Superalloy
Authors: Juraj Belan, Lenka Hurtalová, Eva Tillová, Alan Vaško, Milan Uhríčik
Abstract:
High pressure turbine (HPT) blades of DV – 2 jet engines are made from Ni – based superalloy. This alloy was originally manufactured in the Soviet Union and referred as ŽS6K. For improving alloy’s high temperature resistance are blades coated with Al – Si diffusion layer. A regular operation temperature of HPT blades vary from 705°C to 750°C depending on jet engine regime. An overcrossing working temperature range causes degradation of the protective coating as well as base material which microstructure is formed by the gamma matrix and strengthening phase gamma prime (forming small particles in the microstructure). Diffusion processes inside the material during exposition of the material to high temperatures causes mainly coarsening of the gamma prime particles, thus decreasing its strengthening effect. Degradation of the Al – Si coating caused its thickness growth. All the microstructure changes and coating layer thickness growth results in decreasing of the turbine blade operation lifetime.Keywords: Alitize coating layer, gamma prime phase, high temperature degradation, Ni – base superalloy ŽS6K, turbine blade.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2169809 Recent Advances in Energy Materials for Hot Sections of Modern Gas-Turbine Engines
Authors: Zainul Huda
Abstract:
This presentation reviews recent advances in superalloys and thermal barrier coating (TBC) for application in hot sections of energy-efficient gas-turbine engines. It has been reviewed that in the modern combined-cycle gas turbines (CCGT) applying single-crystal energy materials (SC superalloys) and thermal barrier coatings (TBC), and – in one design – closed-loop steam cooling, thermal efficiency can reach more than 60%. These technological advancements contribute to profitable and clean power generation with reduced emission. Alternatively, the use of advanced superalloys (e.g. GTD-111 superalloy, Allvac 718Plus superalloy) and advanced thermal barrier coatings (TBC) in modern gas-turbines has been shown to yield higher energy-efficiency in power generation.
Keywords: Energy materials, gas turbine engines, superalloy, thermal barrier coating
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2715808 Effect of Pack Aluminising Conditions on βNiAl Coatings
Authors: A. D. Chandio, P. Xiao
Abstract:
In this study, nickel aluminide coatings were deposited onto CMSX-4 single crystal superalloy and pure Ni substrates by using in-situ chemical vapour deposition (CVD) technique. The microstructural evolutions and coating thickness (CT) were studied upon the variation of processing conditions i.e. time and temperature. The results demonstrated (under identical conditions) that coating formed on pure Ni contains no substrate entrapments and have lower CT in comparison to one deposited on the CMSX-4 counterpart. In addition, the interdiffusion zone (IDZ) of Ni substrate is a γ’-Ni3Al in comparison to the CMSX-4 alloy that is βNiAl phase. The higher CT on CMSX-4 superalloy is attributed to presence of γ-Ni/γ’-Ni3Al structure which contains ~ 15 at.% Al before deposition (that is already present in superalloy). Two main deposition parameters (time and temperature) of the coatings were also studied in addition to standard comparison of substrate effects. The coating formation time was found to exhibit profound effect on CT, whilst temperature was found to change coating activities. In addition, the CT showed linear trend from 800 to 1000 °C, thereafter reduction was observed. This was attributed to the change in coating activities.
Keywords: βNiAl, in-situ CVD, CT, CMSX-4, Ni, microstructure.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2396807 Impact Deformation and Fracture Behaviour of Cobalt-Based Haynes 188 Superalloy
Authors: Woei-Shyan Lee, Hao-Chien Kao
Abstract:
The impact deformation and fracture behaviour of cobalt-based Haynes 188 superalloy are investigated by means of a split Hopkinson pressure bar. Impact tests are performed at strain rates ranging from 1×103 s-1 to 5×103 s-1 and temperatures between 25°C and 800°C. The experimental results indicate that the flow response and fracture characteristics of cobalt-based Haynes 188 superalloy are significantly dependent on the strain rate and temperature. The flow stress, work hardening rate and strain rate sensitivity all increase with increasing strain rate or decreasing temperature. It is shown that the impact response of the Haynes 188 specimens is adequately described by the Zerilli-Armstrong fcc model. The fracture analysis results indicate that the Haynes 188 specimens fail predominantly as the result of intensive localised shearing. Furthermore, it is shown that the flow localisation effect leads to the formation of adiabatic shear bands. The fracture surfaces of the deformed Haynes 188 specimens are characterised by dimple- and / or cleavage-like structure with knobby features. The knobby features are thought to be the result of a rise in the local temperature to a value greater than the melting point.
Keywords: Haynes 188 alloy, impact, strain rate and temperature effect, adiabatic shearing.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2319806 Optimization of a Triangular Fin with Variable Fin Base Thickness
Authors: Hyung Suk Kang
Abstract:
A triangular fin with variable fin base thickness is analyzed and optimized using a two-dimensional analytical method. The influence of fin base height and fin base thickness on the temperature in the fin is listed. For the fixed fin volumes, the maximum heat loss, the corresponding optimum fin effectiveness, fin base height and fin tip length as a function of the fin base thickness, convection characteristic number and dimensionless fin volume are represented. One of the results shows that the optimum heat loss increases whereas the corresponding optimum fin effectiveness decreases with the increase of fin volume.Keywords: A triangular fin, Convection characteristic number, Heat loss, Fin base thickness.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 4112805 Design Method for Knowledge Base Systems in Education Using COKB-ONT
Authors: Nhon Do, Tuyen Trong Tran, Phan Hoai Truong
Abstract:
Nowadays e-Learning is more popular, in Vietnam especially. In e-learning, materials for studying are very important. It is necessary to design the knowledge base systems and expert systems which support for searching, querying, solving of problems. The ontology, which was called Computational Object Knowledge Base Ontology (COB-ONT), is a useful tool for designing knowledge base systems in practice. In this paper, a design method for knowledge base systems in education using COKB-ONT will be presented. We also present the design of a knowledge base system that supports studying knowledge and solving problems in higher mathematics.Keywords: artificial intelligence, knowledge base systems, ontology, educational software.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2023804 Examining of Tool Wear in Cryogenic Machining of Cobalt-Based Haynes 25 Superalloy
Authors: Murat Sarıkaya, Abdulkadir Güllü
Abstract:
Haynes 25 alloy (also known as L-605 alloy) is cobalt based super alloy which has widely applications such as aerospace industry, turbine and furnace parts, power generators and heat exchangers and petroleum refining components due to its excellent characteristics. However, the workability of this alloy is more difficult compared to normal steels or even stainless. In present work, an experimental investigation was performed under cryogenic cooling to determine cutting tool wear patterns and obtain optimal cutting parameters in turning of cobalt based superalloy Haynes 25. In experiments, uncoated carbide tool was used and cutting speed (V) and feed rate (f) were considered as test parameters. Tool wear (VBmax) were measured for process performance indicators. Analysis of variance (ANOVA) was performed to determine the importance of machining parameters.Keywords: Cryogenic machining, difficult-to-cut alloy, tool wear, turning.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2747803 Multiaxial Fatigue Analysis of a High Performance Nickel-Based Superalloy
Authors: P. Selva, B. Lorrain, J. Alexis, A. Seror, A. Longuet, C. Mary, F. Denard
Abstract:
Over the past four decades, the fatigue behavior of nickel-based alloys has been widely studied. However, in recent years, significant advances in the fabrication process leading to grain size reduction have been made in order to improve fatigue properties of aircraft turbine discs. Indeed, a change in particle size affects the initiation mode of fatigue cracks as well as the fatigue life of the material. The present study aims to investigate the fatigue behavior of a newly developed nickel-based superalloy under biaxial-planar loading. Low Cycle Fatigue (LCF) tests are performed at different stress ratios so as to study the influence of the multiaxial stress state on the fatigue life of the material. Full-field displacement and strain measurements as well as crack initiation detection are obtained using Digital Image Correlation (DIC) techniques. The aim of this presentation is first to provide an in-depth description of both the experimental set-up and protocol: the multiaxial testing machine, the specific design of the cruciform specimen and performances of the DIC code are introduced. Second, results for sixteen specimens related to different load ratios are presented. Crack detection, strain amplitude and number of cycles to crack initiation vs. triaxial stress ratio for each loading case are given. Third, from fractographic investigations by scanning electron microscopy it is found that the mechanism of fatigue crack initiation does not depend on the triaxial stress ratio and that most fatigue cracks initiate from subsurface carbides.
Keywords: Cruciform specimen, multiaxial fatigue, Nickelbased superalloy.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2179802 Study of Base-Isolation Building System
Authors: G. W. Ni, Y. M. Zhang, D. L. Jiang, J. N. Chen, B. Liu
Abstract:
In order to improve the effect of isolation structure, the principles and behaviours of the base-isolation system are studied, and the types and characteristics of the base-isolation are also discussed. Compared to the traditional aseismatic structures, the base isolation structures decrease the seismic response obviously: the total structural aseismatic value decreases to 1/4-1/32 and the seismic shear stress in the upper structure decreases to 1/14-1/23. In the huge seism, the structure can have an obvious aseismatic effect.Keywords: Base-isolation, earthquake wave, dynamic response.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2337801 Process Optimisation for Internal Cylindrical Rough Turning of Nickel Alloy 625 Weld Overlay
Authors: Lydia Chan, Islam Shyha, Dale Dreyer, John Hamilton, Phil Hackney
Abstract:
Nickel-based superalloys are generally known to be difficult to cut due to their strength, low thermal conductivity, and high work hardening tendency. Superalloy such as alloy 625 is often used in the oil and gas industry as a surfacing material to provide wear and corrosion resistance to components. The material is typically applied onto a metallic substrate through weld overlay cladding, an arc welding technique. Cladded surfaces are always rugged and carry a tough skin; this creates further difficulties to the machining process. The present work utilised design of experiment to optimise the internal cylindrical rough turning for weld overlay surfaces. An L27 orthogonal array was used to assess effects of the four selected key process variables: cutting insert, depth of cut, feed rate, and cutting speed. The optimal cutting conditions were determined based on productivity and the level of tool wear.Keywords: Cylindrical turning, nickel superalloy, turning of overlay, weld overlay.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 912800 Investigation of Gas Tungsten Arc Welding Parameters on Residual Stress of Heat Affected Zone in Inconel X750 Super Alloy Welding Using Finite Element Method
Authors: Kimia Khoshdel Vajari, Saber Saffar
Abstract:
Reducing the residual stresses caused by welding is desirable for the industry. The effect of welding sequence, as well as the effect of yield stress on the number of residual stresses generated in Inconel X750 superalloy sheets and beams, have been investigated. The finite element model used in this research is a three-dimensional thermal and mechanical model, and the type of analysis is indirect coupling. This analysis is done in two stages. First, thermal analysis is performed, and then the thermal changes of the first analysis are used as the applied load in the second analysis. ABAQUS has been used for modeling, and the Dflux subroutine has been used in the Fortran programming environment to move the arc and the molten pool. The results of this study show that the amount of tensile residual stress in symmetric, discontinuous, and symmetric-discontinuous welds is reduced to a maximum of 27%, 54%, and 37% compared to direct welding, respectively. The results also show that the amount of residual stresses created by welding increases linearly with increasing yield stress with a slope of 40%.
Keywords: Residual stress, X750 superalloy, finite element, welding, thermal analysis.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 147799 Cooperative Scheme Using Adjacent Base Stations in Wireless Communication
Authors: Young-Min Ko, Seung-Jun Yu, Chang-Bin Ha, Hyoung-Kyu Song
Abstract:
In a wireless communication system, the failure of base station can result in a communication disruption in the cell. This paper proposes a way to deal with the failure of base station in a wireless communication system based on OFDM. Cooperative communication of the adjacent base stations can be a solution of the problem. High performance is obtained by the configuration of transmission signals which is applied CDD scheme in the cooperative communication. The Cooperative scheme can be a e ective solution in case of the particular situation.Keywords: Base station, CDD, OFDM, Diversity gain, MIMO.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1884798 Effect of Base Coarse Layer on Load-Settlement Characteristics of Sandy Subgrade Using Plate Load Test
Authors: A. Nazeri, R. Ziaie Moayed, H. Ghiasinejad
Abstract:
The present research has been performed to investigate the effect of base course application on load-settlement characteristics of sandy subgrade using plate load test. The main parameter investigated in this study was the subgrade reaction coefficient. The model tests were conducted in a 1.35 m long, 1 m wide, and 1 m deep steel test box of Imam Khomeini International University (IKIU Calibration Chamber). The base courses used in this research were in three different thicknesses of 15 cm, 20 cm, and 30 cm. The test results indicated that in the case of using base course over loose sandy subgrade, the values of subgrade reaction coefficient can be increased from 7 to 132 , 224 , and 396 in presence of 15 cm, 20 cm, and 30 cm base course, respectively.
Keywords: Base course, calibration chamber, plate load test, loose sand, subgrade reaction coefficient.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1158797 Numerical Study of Base Drag Reduction Using Locked Vortex Flow Management Technique for Lower Subsonic Regime
Authors: Kailas S. Jagtap, Karthik Sundarraj, Nirmal Kumar, S. Rajnarasimha, Prakash S. Kulkarni
Abstract:
The issue of turbulence base streams and the drag related to it have been of important attention for rockets, missiles, and aircraft. Different techniques are used for base drag reduction. This paper presents the numerical study of numerous drag reduction technique. The base drag or afterbody drag of bluff bodies can be reduced easily using locked vortex drag reduction technique. For bluff bodies having a cylindrical shape, the base drag is much larger compared to streamlined bodies. For such bodies using splitter plates, the vortex can be trapped between the base and the plate, which results in smooth flow. Splitter plate with round and curved corner shapes has influence in drag reduction. In this paper, the comparison is done between single splitter plate as different positions and with the bluff body. Base drag for the speed of 30m/s can be reduced about 20% to 30% by using single splitter plate as compared to the bluff body.
Keywords: Base drag, bluff body, splitter plate, vortex flow, ANSYS, Fluent.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 900796 Compatibility of Integrated Satellite Systems with Another Satellite System Operating in Adjacent Beam
Authors: Hyemi Gam, Dae-Sub Oh, Bon-Jun Ku
Abstract:
This paper addresses the analysis of the interference between complementary ground component (CGC) base station and mobile earth station (MES). In the frequency sharing scenario between CGC base station and MES, the interference from the adjacent beams must be considered. In this paper, we estimated the interference to MES of an integrated satellite system and the result is presented as the carrier to interference ratio(C/I) with respect to the number of CGC base station in the adjacent beam and the ratio of satellite beam center radius to the total beam radius (R1/R). By using these results, we can determine the minimum separation distance between the CGC base stations of adjacent beam and MES for compatibility. This result can be applied to the CGC base station of an integrated satellite system for the effective frequency sharing.
Keywords: Integrated satellite system, interference, frequency reuse pattern, CGC base station, MES, frequency sharing.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1772795 A New Version of Annotation Method with a XML-based Knowledge Base
Authors: Mohammad Yasrebi, Somayeh Khosravi
Abstract:
Machine-understandable data when strongly interlinked constitutes the basis for the SemanticWeb. Annotating web documents is one of the major techniques for creating metadata on the Web. Annotating websitexs defines the containing data in a form which is suitable for interpretation by machines. In this paper, we present a better and improved approach than previous [1] to annotate the texts of the websites depends on the knowledge base.Keywords: Knowledge base, ontology, semantic annotation, XML.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1546794 Inverse Dynamics of the Mould Base of Blow Molding Machines
Authors: Vigen Arakelian
Abstract:
This paper deals with the study of devices for displacement of the mould base of blow-molding machines. The displacement of the mould in the studied case is carried out by a linear actuator, which ensures the descent of the mould base and by extension springs, which return the letter in the initial position. The aim of this paper is to study the inverse dynamics of the device for displacement of the mould base of blow-molding machines and to determine its optimum parameters for higher rate of production. In the other words, it is necessary to solve the inverse dynamic problem to find the equation of motion linking applied forces with displacements. This makes it possible to determine the stiffness coefficient of the spring to turn the mold base back to the initial position for a given time. The obtained results are illustrated by a numerical example. It is shown that applying a spring with stiffness returns the mould base of the blow molding machine into the initial position in 0.1 sec.Keywords: Design, blow-molding machines, dynamics.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 671793 Verification of the Simultaneous Local Extraction Method of Base and Thermal Resistance of Bipolar Transistors
Authors: Robert Setekera, Luuk Tiemeijer, Ramses van der Toorn
Abstract:
In this paper an extensive verification of the extraction method (published earlier) that consistently accounts for self-heating and Early effect to accurately extract both base and thermal resistance of bipolar junction transistors is presented. The method verification is demonstrated on advanced RF SiGe HBTs were the extracted results for the thermal resistance are compared with those from another published method that ignores the effect of Early effect on internal base-emitter voltage and the extracted results of the base resistance are compared with those determined from noise measurements. A self-consistency of our method in the extracted base resistance and thermal resistance using compact model simulation results is also carried out in order to study the level of accuracy of the method.
Keywords: Avalanche, Base resistance, Bipolar transistor, Compact modeling, Early voltage, Thermal resistance, Self-heating, parameter extraction.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2034792 Evaluation of the Inhibitive Effect of Novel Quinoline Schiff Base on Corrosion of Mild Steel in HCl Solution
Authors: Smita Jauhari, Bhupendra Mistry
Abstract:
Schiff base (E)-2-methyl-N-(tetrazolo[1,5-a]quinolin-4-ylmethylene)aniline (QMA) was synthesized, and its inhibitive effect for mild steel in 1N HCl solution was investigated by weight loss measurement and electrochemical tests. From the weight loss measurements and electrochemical tests, it was observed that the inhibition efficiency increases with the increase in the Schiff base concentration and reaches a maximum at the optimum concentration. This is further confirmed by the decrease in corrosion rate. It is found that the system follows Langmuir adsorption isotherm.
Keywords: Schiff base, acid corrosion, electrochemical impedance spectroscopy, polarization.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1867791 The Effect of Slow Variation of Base Flow Profile on the Stability of Slightly Curved Mixing Layers
Authors: Irina Eglite, Andrei A. Kolyshkin
Abstract:
The effect of small non-parallelism of the base flow on the stability of slightly curved mixing layers is analyzed in the present paper. Assuming that the instability wavelength is much smaller than the length scale of the variation of the base flow we derive an amplitude evolution equation using the method of multiple scales. The proposed asymptotic model provides connection between parallel flow approximations and takes into account slow longitudinal variation of the base flow.Keywords: shallow water, parallel flow assumption, weaklynonlinear analysis, method of multiple scales
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1460790 Developing an Online Library for Faster Retrieval of Mold Base and Standard Parts of Injection Molding
Authors: Alan C. Lin, Ricky N. Joevan
Abstract:
This paper focuses on developing a system to transfer mold base plates and standard parts faster during the stage of injection mold design. This system not only provides a way to compare the file version, but also it utilizes Siemens NX 10 to isolate the updated information into a single executable file (.dll), and then, the file can be transferred without the need of transferring the whole file. By this way, the system can help the user to download only necessary mold base plates and standard parts, and those parts downloaded are only the updated portions.Keywords: CAD, injection molding, mold base, data retrieval.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1153789 Formulation and Evaluation of Vaginal Suppositories Containing Lactobacillus
Authors: Sanae Kaewnopparat, Nattha Kaewnopparat
Abstract:
The objective of this study was to develop vaginal suppository containing lactobacillus. Four kinds of vaginal suppositories containing Lactobacillus paracasei HL32 were formulated: 1) a conventional suppository with Witepsol H-15 as a base, 2) a conventional suppository with mixed polyethylene glycols (PEGs) as a base, 3) a hollow-type suppository with Witepsol H-15 as a base and 4) a hollow-type suppository with mixed PEGs as a base. The release studies demonstrated that the hollow-type suppository with mixed PEGs as the base gave the highest release of L. paracasei HL32 and was microbiological stable after storage at 2- 8°C over the period of 3 months.Keywords: Lactobacillus paracasei HL32, vaginal suppository, release study, hollow-type, viability.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 3519788 Seismic Response Reduction of Structures using Smart Base Isolation System
Authors: H.S. Kim
Abstract:
In this study, control performance of a smart base isolation system consisting of a friction pendulum system (FPS) and a magnetorheological (MR) damper has been investigated. A fuzzy logic controller (FLC) is used to modulate the MR damper so as to minimize structural acceleration while maintaining acceptable base displacement levels. To this end, a multi-objective optimization scheme is used to optimize parameters of membership functions and find appropriate fuzzy rules. To demonstrate effectiveness of the proposed multi-objective genetic algorithm for FLC, a numerical study of a smart base isolation system is conducted using several historical earthquakes. It is shown that the proposed method can find optimal fuzzy rules and that the optimized FLC outperforms not only a passive control strategy but also a human-designed FLC and a conventional semi-active control algorithm.Keywords: Fuzzy logic controller, genetic algorithm, MR damper, smart base isolation system
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2178787 Multivalued Knowledge-Base based on Multivalued Datalog
Authors: Agnes Achs
Abstract:
The basic aim of our study is to give a possible model for handling uncertain information. This model is worked out in the framework of DATALOG. The concept of multivalued knowledgebase will be defined as a quadruple of any background knowledge; a deduction mechanism; a connecting algorithm, and a function set of the program, which help us to determine the uncertainty levels of the results. At first the concept of fuzzy Datalog will be summarized, then its extensions for intuitionistic- and interval-valued fuzzy logic is given and the concept of bipolar fuzzy Datalog is introduced. Based on these extensions the concept of multivalued knowledge-base will be defined. This knowledge-base can be a possible background of a future agent-model.
Keywords: Fuzzy-, intuitionistic-, bipolar datalog, multivalued knowledge-base
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1139786 Dynamic Response of Fixed-base Core-tube and Base-isolated Frame Structure Subjected to Strong Earthquake Motions
Authors: Z.D. Yang, E.S.S. Lam
Abstract:
Considering the merits and limitations of energy dissipation system, seismic isolation system and suspension system, a new earthquake resistant system is proposed and is demonstrated numerically through a frame-core structure. Base isolators and story isolators are installed in the proposed system. The former “isolates" the frame from the foundation and the latter “separates" the frame from the center core. Equations of motion are formulated to study the response of the proposed structural system to strong earthquake motion. As compared with the fixed-base building system, the proposed structural system shows substantial reduction on structural response.
Keywords: Base Isolator, Core-tube, Isolated frame, Seismic Mitigation, Story Isolator
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2003785 Mitigation of Radiation Levels for Base Transceiver Stations based on ITU-T Recommendation K.70
Abstract:
This essay presents applicative methods to reduce human exposure levels in the area around base transceiver stations in a environment with multiple sources based on ITU-T recommendation K.70. An example is presented to understand the mitigation techniques and their results and also to learn how they can be applied, especially in developing countries where there is not much research on non-ionizing radiations.
Keywords: Electromagnetic fields (EMF), human exposure limits, intentional radiator, cumulative exposure ratio, base transceiver station (BTS), radiation levels.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2675784 Effect of Cooling Rate on base Metals Recovery from Copper Matte Smelting Slags
Authors: N. Tshiongo , R K.K. Mbaya , K Maweja, L.C. Tshabalala
Abstract:
Slag sample from copper smelting operation in a water jacket furnace from DRC plant was used. The study intends to determine the effect of cooling in the extraction of base metals. The cooling methods investigated were water quenching, air cooling and furnace cooling. The latter cooling ways were compared to the original as received slag. It was observed that, the cooling rate of the slag affected the leaching of base metals as it changed the phase distribution in the slag and the base metals distribution within the phases. It was also found that fast cooling of slag prevented crystallization and produced an amorphous phase that encloses the base metals. The amorphous slags from the slag dumps were more leachable in acidic medium (HNO3) which leached 46%Cu, 95% Co, 85% Zn, 92% Pb and 79% Fe with no selectivity at pH0, than in basic medium (NH4OH). The leachability was vice versa for the modified slags by quenching in water which leached 89%Cu with a high selectivity as metal extractions are less than 1% for Co, Zn, Pb and Fe at ambient temperature and pH12. For the crystallized slags, leaching of base metals increased with the increase of temperature from ambient temperature to 60°C and decreased at the higher temperature of 80°C due to the evaporation of the ammonia solution used for basic leaching, the total amounts of base metals that were leached in slow cooled slags were very low compared to the quenched slag samples.Keywords: copper slag, leaching, amorphous, cooling rate
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 3741783 Behaviour of Base-Isolated Structures with High Initial Isolator Stiffness
Authors: Ajay Sharma, R.S. Jangid
Abstract:
Analytical seismic response of multi-story building supported on base isolation system is investigated under real earthquake motion. The superstructure is idealized as a shear type flexible building with lateral degree-of-freedom at each floor. The force-deformation behaviour of the isolation system is modelled by the bi-linear behaviour which can be effectively used to model all isolation systems in practice. The governing equations of motion of the isolated structural system are derived. The response of the system is obtained numerically by step-by-method under three real recorded earthquake motions and pulse motions associated in the near-fault earthquake motion. The variation of the top floor acceleration, interstory drift, base shear and bearing displacement of the isolated building is studied under different initial stiffness of the bi-linear isolation system. It was observed that the high initial stiffness of the isolation system excites higher modes in base-isolated structure and generate floor accelerations and story drift. Such behaviour of the base-isolated building especially supported on sliding type of isolation systems can be detrimental to sensitive equipment installed in the building. On the other hand, the bearing displacement and base shear found to reduce marginally with the increase of the initial stiffness of the initial stiffness of the isolation system. Further, the above behaviour of the base-isolated building was observed for different parameters of the bearing (i.e. post-yield stiffness and characteristic strength) and earthquake motions (i.e. real time history as well as pulse type motion).Keywords: base isolation, base shear, bi-linear, earthquake, floor accelerations, inter-story drift, multi-story building, pulsemotion, stiffness ratio.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2290782 Vector Space of the Extended Base-triplets over the Galois Field of five DNA Bases Alphabet
Authors: Robersy Sánchez, Ricardo Grau
Abstract:
A plausible architecture of an ancient genetic code is derived from an extended base triplet vector space over the Galois field of the extended base alphabet {D, G, A, U, C}, where the letter D represent one or more hypothetical bases with unspecific pairing. We hypothesized that the high degeneration of a primeval genetic code with five bases and the gradual origin and improvements of a primitive DNA repair system could make possible the transition from the ancient to the modern genetic code. Our results suggest that the Watson-Crick base pairing and the non-specific base pairing of the hypothetical ancestral base D used to define the sum and product operations are enough features to determine the coding constraints of the primeval and the modern genetic code, as well as the transition from the former to the later. Geometrical and algebraic properties of this vector space reveal that the present codon assignment of the standard genetic code could be induced from a primeval codon assignment. Besides, the Fourier spectrum of the extended DNA genome sequences derived from the multiple sequence alignment suggests that the called period-3 property of the present coding DNA sequences could also exist in the ancient coding DNA sequences.
Keywords: Genetic code vector space, primeval genetic code, power spectrum.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2348781 A New Floating Point Implementation of Base 2 Logarithm
Authors: Ahmed M. Mansour, Ali M. El-Sawy, Ahmed T Sayed
Abstract:
Logarithms reduce products to sums and powers to products; they play an important role in signal processing, communication and information theory. They are primarily used for hardware calculations, handling multiplications, divisions, powers, and roots effectively. There are three commonly used bases for logarithms; the logarithm with base-10 is called the common logarithm, the natural logarithm with base-e and the binary logarithm with base-2. This paper demonstrates different methods of calculation for log2 showing the complexity of each and finds out the most accurate and efficient besides giving insights to their hardware design. We present a new method called Floor Shift for fast calculation of log2, and then we combine this algorithm with Taylor series to improve the accuracy of the output, we illustrate that by using two examples. We finally compare the algorithms and conclude with our remarks.
Keywords: Logarithms, log2, floor, iterative, CORDIC, Taylor series.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 3800