Search results for: degradation study
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 51079

Search results for: degradation study

50959 Rapid Degradation of High-Concentration Methylene Blue in the Combined System of Plasma-Enhanced Photocatalysis Using TiO₂-Carbon

Authors: Teguh Endah Saraswati, Kusumandari Kusumandari, Candra Purnawan, Annisa Dinan Ghaisani, Aufara Mahayum

Abstract:

The present study aims to investigate the degradation of methylene blue (MB) using TiO₂-carbon (TiO₂-C) photocatalyst combined with dielectric discharge (DBD) plasma. The carbon materials used in the photocatalyst were activated carbon and graphite. The thin layer of TiO₂-C photocatalyst was prepared by ball milling method which was then deposited on the plastic sheet. The characteristic of TiO₂-C thin layer was analyzed using X-ray diffraction (XRD), scanning electron microscopy (SEM) with energy dispersive X-ray (EDX) spectroscopy, and UV-Vis diffuse reflectance spectrophotometer. The XRD diffractogram patterns of TiO₂-G thin layer in various weight compositions of 50:1, 50:3, and 50:5 show the 2θ peaks found around 25° and 27° are the main characteristic of TiO₂ and carbon. SEM analysis shows spherical and regular morphology of the photocatalyst. Analysis using UV-Vis diffuse reflectance shows TiO₂-C has narrower band gap energy. The DBD plasma reactor was generated using two electrodes of Cu tape connected with stainless steel mesh and Fe wire separated by a glass dielectric insulator, supplied by a high voltage 5 kV with an air flow rate of 1 L/min. The optimization of the weight composition of TiO₂-C thin layer was studied based on the highest reduction of the MB concentration achieved, examined by UV-Vis spectrophotometer. The changes in pH values and color of MB indicated the success of MB degradation. Moreover, the degradation efficiency of MB was also studied in various higher concentrations of 50, 100, 200, 300 ppm treated for 0, 2, 4, 6, 8, 10 min. The degradation efficiency of MB treated in combination system of photocatalysis and DBD plasma reached more than 99% in 6 min, in which the greater concentration of methylene blue dye, the lower degradation rate of methylene blue dye would be achieved.

Keywords: activated carbon, DBD plasma, graphite, methylene blue, photocatalysis

Procedia PDF Downloads 124
50958 Numerical Simulation of the Effect of 1 Mev Electron Beam on the Performance of a Solar Cell of Type n+/p GaAs

Authors: Waleed Alsaidy, Mourad Mbarki

Abstract:

In this work, it have investigated the effect of electron irradiation on the output characteristics of n+/p GaAs solar cell. The studied solar cell is exposed to an electron beam with kinetic energy of 1 MeV under AM0 illumination. In this work, it have used our own software to calculate the damage caused by these energetic particles. Indeed, these particles produce severe degradation on the performances of the solar cells. The aim of this work is to investigate the effect of electronic irradiation on the J(V) characteristics upon the fluence of particles φ (electron/cm2). Thereafter, we have evaluated the degradation of its performances such as the short circuit current J_sc, the open circuit voltage V_oc the efficiency η with respect to the fluence φ of electrons. it have shown that the variation of these parameters decrease linearly with the logarithm of the fluence φ, and their degradation begins from a threshold value φ_m. To validate our calculation, we have compared our results with other theoretical and experimental results available in the literature and we have found a good agreement between them.

Keywords: solar cells, GaAs, short circuit current, open circuit voltage, fluence, degradation

Procedia PDF Downloads 28
50957 Carbon@NiCoFeS Nanoparticles for Photocatalytic Degradation of Organic Pollutants via Peroxymonosulfate Activation

Authors: Raqiqa Tur Rasool, Ghulam Abbas Ashraf

Abstract:

This study presents the synthesis and application of Carbon@NiCoFeS nanoparticles as a photocatalyst for the degradation of organic pollutants through peroxymonosulfate (PMS) activation. The Carbon@NiCoFeS nanoparticles, synthesized via a hydrothermal method, exhibit a highly crystalline and uniformly distributed nanostructure, as confirmed by XRD, SEM, TEM, and FTIR analyses. The photocatalytic performance was tested using ibuprofen (IBU) as a model pollutant under visible light, demonstrating remarkable efficiency across various conditions, including different concentrations of photocatalyst and PMS and a range of pH values. The enhanced activity is attributed to the synergistic effects of Ni, Co, and Fe, promoting effective electron-hole separation and reactive radical generation, primarily SO4•− and •OH. Quenching experiments highlighted sulfate radicals' predominant role in the degradation process. The Carbon@NiCoFeS photocatalyst also showed excellent reusability and stability over multiple cycles, and its versatility in degrading various organic pollutants underscores its potential for practical wastewater treatment applications. This research offers significant insights into multi-metal sulfide photocatalyst design, showcasing Carbon@NiCoFeS nanoparticles' promising role in environmental remediation via efficient PMS activation.

Keywords: NiCoFeS nanoparticles, photocatalytic degradation, peroxymonosulfate activation, organic pollutant removal, wastewater treatment

Procedia PDF Downloads 48
50956 A Framework for Incorporating Non-Linear Degradation of Conductive Adhesive in Environmental Testing

Authors: Kedar Hardikar, Joe Varghese

Abstract:

Conductive adhesives have found wide-ranging applications in electronics industry ranging from fixing a defective conductor on printed circuit board (PCB) attaching an electronic component in an assembly to protecting electronics components by the formation of “Faraday Cage.” The reliability requirements for the conductive adhesive vary widely depending on the application and expected product lifetime. While the conductive adhesive is required to maintain the structural integrity, the electrical performance of the associated sub-assembly can be affected by the degradation of conductive adhesive. The degradation of the adhesive is dependent upon the highly varied use case. The conventional approach to assess the reliability of the sub-assembly involves subjecting it to the standard environmental test conditions such as high-temperature high humidity, thermal cycling, high-temperature exposure to name a few. In order to enable projection of test data and observed failures to predict field performance, systematic development of an acceleration factor between the test conditions and field conditions is crucial. Common acceleration factor models such as Arrhenius model are based on rate kinetics and typically rely on an assumption of linear degradation in time for a given condition and test duration. The application of interest in this work involves conductive adhesive used in an electronic circuit of a capacitive sensor. The degradation of conductive adhesive in high temperature and humidity environment is quantified by the capacitance values. Under such conditions, the use of established models such as Hallberg-Peck model or Eyring Model to predict time to failure in the field typically relies on linear degradation rate. In this particular case, it is seen that the degradation is nonlinear in time and exhibits a square root t dependence. It is also shown that for the mechanism of interest, the presence of moisture is essential, and the dominant mechanism driving the degradation is the diffusion of moisture. In this work, a framework is developed to incorporate nonlinear degradation of the conductive adhesive for the development of an acceleration factor. This method can be extended to applications where nonlinearity in degradation rate can be adequately characterized in tests. It is shown that depending on the expected product lifetime, the use of conventional linear degradation approach can overestimate or underestimate the field performance. This work provides guidelines for suitability of linear degradation approximation for such varied applications

Keywords: conductive adhesives, nonlinear degradation, physics of failure, acceleration factor model.

Procedia PDF Downloads 135
50955 Control of Airborne Aromatic Hydrocarbons over TiO2-Carbon Nanotube Composites

Authors: Joon Y. Lee, Seung H. Shin, Ho H. Chun, Wan K. Jo

Abstract:

Poly vinyl acetate (PVA)-based titania (TiO2)–carbon nanotube composite nanofibers (PVA-TCCNs) with various PVA-to-solvent ratios and PVA-based TiO2 composite nanofibers (PVA-TN) were synthesized using an electrospinning process, followed by thermal treatment. The photocatalytic activities of these nanofibers in the degradation of airborne monocyclic aromatics under visible-light irradiation were examined. This study focuses on the application of these photocatalysts to the degradation of the target compounds at sub-part-per-million indoor air concentrations. The characteristics of the photocatalysts were examined using scanning electron microscopy, X-ray diffraction, ultraviolet-visible spectroscopy, and Fourier-transform infrared spectroscopy. For all the target compounds, the PVA-TCCNs showed photocatalytic degradation efficiencies superior to those of the reference PVA-TN. Specifically, the average photocatalytic degradation efficiencies for benzene, toluene, ethyl benzene, and o-xylene (BTEX) obtained using the PVA-TCCNs with a PVA-to-solvent ratio of 0.3 (PVA-TCCN-0.3) were 11%, 59%, 89%, and 92%, respectively, whereas those observed using PVA-TNs were 5%, 9%, 28%, and 32%, respectively. PVA-TCCN-0.3 displayed the highest photocatalytic degradation efficiency for BTEX, suggesting the presence of an optimal PVA-to-solvent ratio for the synthesis of PVA-TCCNs. The average photocatalytic efficiencies for BTEX decreased from 11% to 4%, 59% to 18%, 89% to 37%, and 92% to 53%, respectively, when the flow rate was increased from 1.0 to 4.0 L min1. In addition, the average photocatalytic efficiencies for BTEX increased 11% to ~0%, 59% to 3%, 89% to 7%, and 92% to 13% , respectively, when the input concentration increased from 0.1 to 1.0 ppm. The prepared PVA-TCCNs were effective for the purification of airborne aromatics at indoor concentration levels, particularly when the operating conditions were optimized.

Keywords: mixing ratio, nanofiber, polymer, reference photocatalyst

Procedia PDF Downloads 378
50954 Degradation of Mechanical Properties of Offshoring Polymer Composite Pipes in Thermal Environment

Authors: Hamza Benyahia, Mostapha Tarfaoui, Ahmed El-Moumen, Djamel Ouinas

Abstract:

Composite pipes are commonly used in the oil industry, and extreme flow of hot and cold gas fluid can cause degradation of their mechanical performance and properties. Therefore, it is necessary to consider thermomechanical behavior as an important parameter in designing these tubular structures. In this paper, an experimental study is conducted on composite glass/epoxy tubes, with a thickness of 6.2 mm and 86 mm internal diameter made by filament winding of (Փ = ± 55°), to investigate the effects of extreme thermal condition on their mechanical properties b over a temperature range from -40 to 80°C. The climatic chamber is used for the thermal aging and then, combine split disk system is used to perform tensile tests on these composite pies. Thermal aging is carried out for 8hr but each specimen was subjected to various temperature ranges and then, uniaxial tensile test is conducted to evaluate their mechanical performance. Experimental results show degradation in the mechanical properties of composite pipes with an increase in temperature. The rigidity of pipes increases progressively with a decrease in thermal load and results in a radical decrease in their elongation before fracture, thus, decreasing their ductility. However, with an increase in the temperature, there is a decrease in the yield strength and an increase in yield strain, which confirmed an increase in the plasticity of composite pipes.

Keywords: composite pipes, thermal-mechanical properties, filament winding, thermal degradation

Procedia PDF Downloads 147
50953 Improving the Feeding Value of Straws with Pleurotus Ostreatus

Authors: S. Hussain, N. Ahmad, S. Alam, M. Bezabhi, W. H. Hendriks, P. Yu, J. W. Cone

Abstract:

The high content of lignin in cell walls is the major limiting factor in the digestion and utilisation of cereal crop residues by ruminants. The aim of this study was to evaluate the effectiveness of the white rot fungus, Pleurotus ostreatus (P. ostreatus), to degrade lignin and to enhance the rumen degradability of maize stover, rice straw, wheat straw and their mixture in equal proportion on a dry-matter (DM) basis. Four samples of each substrate were incubated aerobically in triplicate with P. ostreatus for 0 (Control), 21, 28 and 35 days under solid-state conditions (temperature, 24 ͦ C; humidity, 70± 5%). The changes in chemical composition, DM and nutrient losses, and rumen fermentation characteristics using in vitro DM digestibility (DMD) and the in vitro gas production (GP) technique were measured. The results showed that incubation with P. ostreatus decreased (P < 0.001) the contents of neutral detergent fibre and lignin with a concomitant increase (P < 0.001) in the contents of ash and crude protein. The losses of nutrients differed (P < 0.001) among the straw types, with rice straw and maize stover showing the largest (P < 0.05) lignin degradation compared to wheat and mixed straws. The DMD and 72-h cumulative GP increased (P < 0.001) consistently with increasing fungal incubation period and for all substrates the highest values of DMD and GP were measured after 35 days of incubation with P. ostreatus. The lignin degradation was strongly associated with hemicellulose degradation (r = 0.71) across the various straws. Results of the present study demonstrated that incubation of low-quality crop residues with P. ostreatus under solid-state conditions upgrades their feeding value by reducing the content of lignin and increasing the content of crude protein and ruminal degradation.

Keywords: crop residues, lignin degradation, maize stovers, wheat straws, white rot fungi

Procedia PDF Downloads 63
50952 Environmental Awareness and Community Outreach: A Case Study of Speak Up World Foundation

Authors: Akshita Gaba, Ria P. Dey, Sanya Karotiya, Smrijanee Dash, Soni Gupta

Abstract:

This research paper explores the significance of environmental awareness and community outreach initiatives undertaken by the Speak Up World Foundation; a non-profit organization founded in 2021. The study delves into the historical context of environmental issues, identifies the driving factors contributing to environmental degradation, and outlines tasks undertaken by the foundation to promote environmental consciousness. The paper also highlights the impact of these efforts on the community and emphasizes the need for continued dedication to ensure sustainable coexistence with our environment.

Keywords: environment, social service, organization, degradation, survey

Procedia PDF Downloads 66
50951 Unveiling Electrical Treeing Mechanisms in Epoxy Resin Insulation Degradation

Authors: Chien-Kuo Chang, You-Syuan Wu, Min-Chiu Wu, Bharath-Kumar Boyanapalli

Abstract:

The electrical treeing mechanism in epoxy resin insulation is a critical area of study concerning the degradation of high-voltage electrical equipment. In this study, we conducted pressure-induced degradation experiments on epoxy resin specimens using a needle-plane electrode structure to simulate electrical treeing. The specimens featured two different defect spacings, allowing for detailed observation facilitated by time-lapse photography. Our investigation revealed four distinct stages of insulation degradation: initial dark tree growth, filamentary tree growth, reverse tree growth, and eventual insulation breakdown. The initial dark treeing stage, though shortest in duration, exhibited a thicker main branch and shorter branching, ceasing upon the appearance of filamentary treeing. Filamentary treeing manifested in two forms: dark filamentary treeing during the resin's glassy state, characterized by branching structures, and fuzzy filamentary treeing during the rubbery state, resembling white feathers. The channels formed by filamentary treeing were observed to be as narrow as a few micrometers and continued to grow until the end of the experiment. Additionally, the transition to reverse treeing occurred when filamentary treeing reached the ground electrode, with the earliest manifestation being growth from the ground electrode towards the high-voltage end.

Keywords: epoxy resin insulation, high-voltage equipment, electrical treeing mechanism

Procedia PDF Downloads 77
50950 Kinetics of Phytochemicals and Antioxidant Activity during Thermal Treatment of Cape Gooseberry (Physalis peruviana L)

Authors: Mary-Luz Olivares-Tenorio, Ruud Verkerk, Matthijs Dekker, Martinus A. J. S. van Boekel

Abstract:

Cape gooseberry, the fruit of the plant Physalis peruviana L. has gained interest in research given its contents of promising health-promoting compounds like contents. The presence of carotenoids, ascorbic acid, minerals, polyphenols, vitamins and antioxidants. This project aims to study thermal stability of β-carotene, ascorbic acid, catechin and epicatechin and antioxidant activity in the matrix of the Cape Gooseberry. Fruits were obtained from a Colombian field in Cundinamarca. Ripeness stage was 4 (According to NTC 4580, corresponding to mature stage) at the moment of the experiment. The fruits have been subjected to temperatures of 40, 60, 80, 100 and 120°C for several times. β-Carotene, ascorbic acid, catechin and epicatechin content were assessed with HPLC and antioxidant activity with the DPPH method. β-Carotene was stable upon 100°C, and showed some degradation at 120°C. The same behavior was observed for epicatechin. Catechin increased during treatment at 40°C, at 60°C it remained stable and it showed degradation at 80°C, 100°C and 120°C that could be described by a second order kinetic model. Ascorbic acid was the most heat-sensitive of the analyzed compounds. It showed degradation at all studied temperatures, and could be described by a first order model. The activation energy for ascorbic acid degradation in cape gooseberry was 46.0 kJ/mol and its degradation rate coefficient at 100 °C was 6.53 x 10-3 s-1. The antioxidant activity declined for all studied temperatures. Results from this study showed that cape gooseberry is an important source of different health-promoting compounds and some of them are stable to heat. That makes this fruit a suitable raw material for processed products such as jam, juices and dehydrated fruit, giving the consumer a good intake of these compounds.

Keywords: goldenberry, health-promoting compounds, phytochemical, processing, heat treatment

Procedia PDF Downloads 454
50949 Performance Complexity Measurement of Tightening Equipment Based on Kolmogorov Entropy

Authors: Guoliang Fan, Aiping Li, Xuemei Liu, Liyun Xu

Abstract:

The performance of the tightening equipment will decline with the working process in manufacturing system. The main manifestations are the randomness and discretization degree increasing of the tightening performance. To evaluate the degradation tendency of the tightening performance accurately, a complexity measurement approach based on Kolmogorov entropy is presented. At first, the states of performance index are divided for calibrating the discrete degree. Then the complexity measurement model based on Kolmogorov entropy is built. The model describes the performance degradation tendency of tightening equipment quantitatively. At last, a study case is applied for verifying the efficiency and validity of the approach. The research achievement shows that the presented complexity measurement can effectively evaluate the degradation tendency of the tightening equipment. It can provide theoretical basis for preventive maintenance and life prediction of equipment.

Keywords: complexity measurement, Kolmogorov entropy, manufacturing system, performance evaluation, tightening equipment

Procedia PDF Downloads 260
50948 Study on the Heavy Oil Degradation Performance and Kinetics of Immobilized Bacteria on Modified Zeolite

Authors: Xiao L Dai, Wen X Wei, Shuo Wang, Jia B Li, Yan Wei

Abstract:

Heavy oil pollution generated from both natural and anthropogenic sources could cause significant damages to the ecological environment, due to the toxicity of some of its constituents. Nowadays, microbial remediation is becoming a promising technology to treat oil pollution owing to its low cost and prevention of secondary pollution; microorganisms are key players in the process. Compared to the free microorganisms, immobilized microorganisms possess several advantages, including high metabolic activity rates, strong resistance to toxic chemicals and natural competition with the indigenous microorganisms, and effective resistance to washing away (in open water system). Many immobilized microorganisms have been successfully used for bioremediation of heavy oil pollution. Considering the broad choices, low cost, simple process, large specific surface area and less impact on microbial activity, modified zeolite were selected as a bio-carrier for bacteria immobilization. Three strains of heavy oil-degrading bacteria Bacillus sp. DL-13, Brevibacillus sp. DL-1 and Acinetobacter sp. DL-34 were immobilized on the modified zeolite under mild conditions, and the bacterial load (bacteria /modified zeolite) was 1.12 mg/g, 1.11 mg/g, and 1.13 mg/g, respectively. SEM results showed that the bacteria mainly adsorbed on the surface or punctured in the void of modified zeolite. The heavy oil degradation efficiency of immobilized bacteria was 62.96%, higher than that of the free bacteria (59.83%). The heavy oil degradation process of immobilized bacteria accords with the first-order reaction equation, and the reaction rate constant is 0.1483 d⁻¹, which was significantly higher than the free bacteria (0.1123 d⁻¹), suggesting that the immobilized bacteria can rapidly start up the heavy oil degradation and has a high activity of heavy oil degradation. The results suggested that immobilized bacteria are promising technology for bioremediation of oil pollution.

Keywords: heavy oil pollution, microbial remediation, modified zeolite, immobilized bacteria

Procedia PDF Downloads 150
50947 Characterization of Gamma Irradiated PVDF and PVDF/Graphene Oxide Composites by Spectroscopic Techniques

Authors: Juliana V. Pereira, Adriana S. M. Batista, Jefferson P. Nascimento, Clascídia A. Furtado, Luiz O. Faria

Abstract:

The combination of the properties of graphene oxide (OG) and PVDF homopolymer makes their combined composite materials as multifunctional systems with great potential. Knowledge of the molecular structure is essential for better use. In this work, the degradation of PVDF polymer exposed to gamma irradiation in oxygen atmosphere in high dose rate has been studied and compared to degradation of PVDF/OG composites. The samples were irradiated with a Co-60 source at constant dose rate, with doses ranging from 100 kGy to 1,000 kGy. In FTIR data shown that the formation of oxidation products was at the both samples with formation of carbonyl and hydroxyl groups amongst the most prevalent products in the pure PVDF samples. In the other hand, the composites samples exhibit less presence of degradation products with predominant formation of carbonyl groups, these results also seen in the UV-Vis analysis. The results show that the samples of composites may have greater resistance to the irradiation process, since they have less degradation products than pure PVDF samples seen by spectroscopic techniques.

Keywords: gamma irradiation, PVDF, PVDF/OG composites, spectroscopic techniques

Procedia PDF Downloads 572
50946 Challenges of Peri-Urban Agriculture in Cities of Developing Countries: A Case Study of Nairobi City Peri-Urban Area

Authors: Aggrey Daniel Maina Thuo

Abstract:

Rapid urban population growth means an increasing demand for urban land, particularly for housing, and also for various other urban uses. This land is not available within cities but in peri-urban areas. The expansion of the cities into the peri-urban areas is creating direct and indirect impacts with those living there facing new challenges and opportunities in meeting their life needs and accommodating the by-products of urbanization. Although urbanization of these areas provides opportunities for employment, better housing, education, knowledge and technology transfer, and ready markets for the agricultural products, increase in population places enormous stress on natural resources and existing social services and infrastructure, therefore causing environmental degradation. This environmental degradation is affecting agriculture for those still holding onto their farms for agricultural purposes. This paper, using a multiple theoretical framework and qualitative research approach, attempts to describe the positive and adverse effects of urbanization on peri-urban agriculture, using the Town Council of Karuri within Nairobi peri-urban areas as a case study.

Keywords: peri-urban agriculture, urbanization, land use, environmental degradation, planning

Procedia PDF Downloads 361
50945 Environmental Degradation and Globalization with Special Reference to Developing Economics

Authors: Indira Sinha

Abstract:

According to the Oxford Advanced Learner's English Dictionary of Current English, environment is the complex of physical, chemical and biotic factors that act upon an organism or an ecological community and ultimately determines its form and survival. It is defined as conditions and circumstances which are affecting people's lives. The meaning of environmental degradation is the degradation of the environment through depletion of resources such as air, water and soil and the destruction of ecosystems and extinction of wildlife. Globalization is a significant feature of recent world history. The aim of this phenomenon is to integrate societies, economies and cultures through a common link of trading policies, technology and communication. Undoubtedly it has opened up the world economy at a very high speed but at the same time it has an adverse impact on the environment. The purpose of the present study is to investigate the impact of globalization on the environmental conditions. An overview of what the forces of globalization have in store for the environment with constructing large number of industries and destroying large forests lands will be given in this paper. The forces of globalization have created many serious environmental problems like high temperature, extinction of many species of plant and animal and outlet of poisonous chemicals from industries. The revelation of this study is that in case of developing economics these problems are more critical. In developing countries like India many factories are built with less environmental regulations, while developed economies maintain positive environmental practices. The present study is a micro level study which aims to employ a combination of theoretical, descriptive, empirical and analytical approach in addition to the time tested case method.

Keywords: globalization, trade policies, environmental degradation, developing economies, large industries

Procedia PDF Downloads 240
50944 Photocatalytic Activity of Pure and Doped CeO2 Nanoparticles

Authors: Mohamed Khedr, Ahmed Farghali, Waleed El Rouby, Abdelrhman Hamdeldeen

Abstract:

Pure CeO2, Sm and Gd doped CeO2 were successfully prepared via hydrothermal method. The effect of hydrothermal temperature, reaction time and precursors were investigated. The prepared nanoparticles were characterized using X-ray diffraction (XRD), FT-Raman Spectroscopy, transmission electron microscope (TEM) and field emission scanning electron microscope (FESEM). The prepared pure and doped CeO2 nanoparticles were used as photo-catalyst for the degradation of Methylene blue (MB) dye under UV light irradiation. The results showed that Gd doped CeO2 nano-particles have the best catalytic degradation effect for MB under UV irradiation. The degradation pathways of MB were followed using liquid chromatography (LC/MS) and it was found that Gd doped CeO2 was able to oxidize MB dye with a complete mineralization of carbon, nitrogen and sulfur heteroatoms into CO2, NH4+, NO3- and SO42-.

Keywords: CeO2, doped CeO2, photocatalysis, methylene blue

Procedia PDF Downloads 328
50943 Floristic Diversity, Carbon Stocks and Degradation Factors in Two Sacred Forests in the West Cameroon Region

Authors: Maffo Maffo Nicole Liliane, Mounmeni Kpoumie Hubert, Mbaire Matindje Karl Marx, Zapfack Louis

Abstract:

Sacred forests play a valuable role in conserving local biodiversity and provide numerous ecosystem services in Cameroon. The study was carried out in the sacred forests of Bandrefam and Batoufam (western Cameroon). The aim was to estimate the diversity of woody species, carbon stocks and degradation factors in these sacred forests. The floristic inventory was carried out in plots measuring 25m × 25m for trees with diameters greater than 10 cm and 5m × 5m for trees with diameters less than 10 cm. Carbon stocks were estimated using the non-destructive method and the allometric equations. Data on degradation factors were collected using semi-structured surveys in the Bandrefam and Batoufam neighborhoods. The floristic inventory identified 65 species divided into 57 genera and 30 families in the Bandrefam Sacred Forest and 45 species divided into 42 genera and 27 families in the Batoufam Sacres Forest. The families common to both sacred forests are as follows: Phyllanthaceae, Fabaceae, Moraceae, Lamiaceae, Malvaceae, Rubiaceae, Meliaceae, Anacardiaceae, and Sapindaceae. Three genera are present in both sites. These are: Albizia, Macaranga, Trichillia. In addition, there are 27 species in common between the two sites. The total carbon stock is 469.26 tC/ha at Batoufam and 291.41 tC/ha at Bandrefam. The economic value varies between 15 823 877.05 fcfa at Batoufam and 9 825 530.528 fcfa at Bandrefam. The study shows that despite the sacred nature of these forests, they are subject to degradation factors such as bushfires (35.42 %), the creation of plantations (23.96 %), illegal timber exploitation (21.88 %), young people's lack of interest in the notion of conservation (9.38 %), climate change (7.29 %) and growing urbanization (2.08 %). These factors threaten biodiversity and reduce carbon storage in these forests.

Keywords: sacred forests, degradation factors, carbon stocks, semi-structured surveys

Procedia PDF Downloads 49
50942 Durability of Wood Shavel Composites with Environmental Friendly Based Binder

Authors: Jul Endawati

Abstract:

The composite element of 20 mm in thickness were manufactured using high volume fly ash, silica fume as alternative hydraulic binders and Portland cement Type II. Pine wood shavel as by product of local small wood working industries were used as the composite filler. The elements were given in situ wet and dry treatment for 9 months. Visually there is no fiber degradation as a result of the interaction of the environment. The assessment were done to the elements bending strength and dimensional properties. Increase in MoR after 180 days of exposure shown that mechanically this degradation is not seen yet. The increment of MoR (213%) compare to that of 28 days might be affected by the formation of calcium hydroxide (CH) or ettringite in the transition zone. The use of pozzolan showed also a delay or minimize degradation of composites while improving the pore structure, and minimize the mineralization of the fiber bond with the cement matrix. The water absorption is 4,22% at 180 days, 7,94% at 120 days and 12,38% at 28 days, in line with the 68% decrease in Thickness Swelling (TS). This unoccured degradation could also be affected by the presence of silica fume in the binder matrix. After 270 days of exposure under tropical condition, the flexural strength started to decrease.

Keywords: durability, fly ash, natural fibre, silica fume

Procedia PDF Downloads 262
50941 Effect of the pH on the Degradation Kinetics of Biodegradable Mg-0.8Ca Orthopedic Implants

Authors: A. Mohamed, A. El-Aziz

Abstract:

The pH of the body plays a great role in the degradation kinetics of biodegradable Mg-Ca orthopedic implants. At the location of fracture, the pH of the body becomes no longer neutral which draws the attention towards studying a range of different pH values of the body fluid. In this study, the pH of Hank’s balanced salt solution (HBSS) was modified by phosphate buffers into an aggressive acidic pH 1.8, a slightly acidic pH 5.3 and an alkaline pH 8.1. The biodegradation of Mg-0.8Ca implant was tested in those three different media using immersion test and electrochemical polarization means. It was proposed that the degradation rate has increased with decreasing the pH of HBSS. The immersion test revealed weight gain for all the samples followed by weight loss as the immersion time increased. The highest weight gain was pronounced for the acidic pH 1.8 and the least weight gain was observed for the alkaline pH 8.1. This was in agreement with the electrochemical polarization test results where the degradation rate was found to be high (7.29 ± 2.2 mm/year) in the aggressive acidic solution of pH 1.8 and relatively minimum (0.31 ± 0.06 mm/year) in the alkaline medium of pH 8.1. Furthermore, it was confirmed that the pH of HBSS has reached a steady state of an alkaline pH (~pH 11) at the end of the two-month immersion period regardless of the initial pH of the solution. Finally, the corrosion products formed on the samples’ surface were investigated by SEM, EDX and XRD analyses that revealed the formation of magnesium and calcium phosphates with different morphologies according to the pH.

Keywords: biodegradable, electrochemical polarization means, orthopedics, immersion test, simulated body fluid

Procedia PDF Downloads 124
50940 Moisture Absorption Analysis of LLDPE-NR Nanocomposite for HV Insulation

Authors: M. S. Kamarulzaman, N. A. Muhamad, N. A. M. Jamail, M. A. M. Piah, N. F. Kasri

Abstract:

Insulation for high voltage application that has been service for a very long time is subjected to several types of degradation. The degradation can lead to premature breakdown and definitely will spent highly cost to replace the cable. Thus, there are many research on nano composite material get serious attention attention due to their abilities to enhance electrical performance by addition of nano filler. In this paper, water absorption of Low Linear Density Polyethyelene (LLDPE) with different amount of nano filler added is studied. This study is necessary to be conducted since most of electrical apparatus such as cable insulation are dominant used especially in high voltage application. The cable insulation are continuously exposed in uncontrolled environment may suffer degradation process. Three type of nano fillers, was used in this study are: Silicon dioxide (SiO2), Titanium dioxide (TiO2) and Monmorillonite (MMT). The percentage absorption of water was measured by weighted using high precision scales for absorption process up to 92 days. Experimental result demonstrate that SiO2 absorb less water than other filler while, the MMT has hydrophilic properties which it absorbs more water compare to another sample.

Keywords: nano composite, nano filler, water absorption, hydrophilic properties

Procedia PDF Downloads 357
50939 Degradation Kinetics of Cardiovascular Implants Employing Full Blood and Extra-Corporeal Circulation Principles: Mimicking the Human Circulation In vitro

Authors: Sara R. Knigge, Sugat R. Tuladhar, Hans-Klaus HöFfler, Tobias Schilling, Tim Kaufeld, Axel Haverich

Abstract:

Tissue engineered (TE) heart valves based on degradable electrospun fiber scaffold represent a promising approach to overcome the known limitations of mechanical or biological prostheses. But the mechanical stress in the high-pressure system of the human circulation is a severe challenge for the delicate materials. Hence, the prediction of the scaffolds` in vivo degradation kinetics must be as accurate as possible to prevent fatal events in future animal or even clinical trials. Therefore, this study investigates whether long-term testing in full blood provides more meaningful results regarding the degradation behavior than conventional tests in simulated body fluids (SBF) or Phosphate Buffered Saline (PBS). Fiber mats were produced from a polycaprolactone (PCL)/tetrafluoroethylene solution by electrospinning. The morphology of the fiber mats was characterized via scanning electron microscopy (SEM). A maximum physiological degradation environment utilizing a test set-up with porcine full blood was established. The set-up consists of a reaction vessel, an oxygenator unit, and a roller pump. The blood parameters (pO2, pCO2, temperature, and pH) were monitored with an online test system. All tests were also carried out in the test circuit with SBF and PBS to compare conventional degradation media with the novel full blood setting. The polymer's degradation is quantified by SEM picture analysis, differential scanning calorimetry (DSC), and Raman spectroscopy. Tensile and cyclic loading tests were performed to evaluate the mechanical integrity of the scaffold. Preliminary results indicate that PCL degraded slower in full blood than in SBF and PBS. The uptake of water is more pronounced in the full blood group. Also, PCL preserved its mechanical integrity longer when degraded in full blood. Protein absorption increased during the degradation process. Red blood cells, platelets, and their aggregates adhered on the PCL. Presumably, the degradation led to a more hydrophilic polymeric surface which promoted the protein adsorption and the blood cell adhesion. Testing degradable implants in full blood allows for developing more reliable scaffold materials in the future. Material tests in small and large animal trials thereby can be focused on testing candidates that have proven to function well in an in-vivo-like setting.

Keywords: Electrospun scaffold, full blood degradation test, long-term polymer degradation, tissue engineered aortic heart valve

Procedia PDF Downloads 152
50938 Eco-Degradation and Phytodiversity of Pulicat Lagoon, Eastcoast of Southern India

Authors: Khasim Munir Bhasha Shaik

Abstract:

Pulicat Lake is the second largest brackish water lagoon after Chilika Lake of Orissa along the east coast of India. Estuaries and lagoons have brackish water which shows high biological productivity than fresh or sea water. Hence, it has a wide range of aquatic, terrestrial flora. The World Wide Fund for Nature declared it as a protected area. The present study aims to explore the flora of the lagoon along with the various threats for its eco-degradation which helps to plan necessary conservation methods.

Keywords: phytodiversity, pulicat lake, threats, conservation

Procedia PDF Downloads 288
50937 Relationship between Structure of Some Nitroaromatic Pollutants and Their Degradation Kinetic Parameters in UV-VIS/TIO2 System

Authors: I. Nitoi, P. Oancea, M. Raileanu, M. Crisan, L. Constantin, I. Cristea

Abstract:

Hazardous organic compounds like nitroaromatics are frequently found in chemical and petroleum industries discharged effluents. Due to their bio-refractory character and high chemical stability cannot be efficiently removed by classical biological or physical-chemical treatment processes. In the past decades, semiconductor photocatalysis has been frequently applied for the advanced degradation of toxic pollutants. Among various semiconductors titania was a widely studied photocatalyst, due to its chemical inertness, low cost, photostability and nontoxicity. In order to improve optical absorption and photocatalytic activity of TiO2 many attempts have been made, one feasible approach consists of doping oxide semiconductor with metal. The degradation of dinitrobenzene (DNB) and dinitrotoluene (DNT) from aqueous solution under UVA-VIS irradiation using heavy metal (0.5% Fe, 1%Co, 1%Ni ) doped titania was investigated. The photodegradation experiments were carried out using a Heraeus laboratory scale UV-VIS reactor equipped with a medium-pressure mercury lamp which emits in the range: 320-500 nm. Solutions with (0.34-3.14) x 10-4 M pollutant content were photo-oxidized in the following working conditions: pH = 5-9; photocatalyst dose = 200 mg/L; irradiation time = 30 – 240 minutes. Prior to irradiation, the photocatalyst powder was added to the samples, and solutions were bubbled with air (50 L/hour), in the dark, for 30 min. Dopant type, pH, structure and initial pollutant concentration influence on the degradation efficiency were evaluated in order to set up the optimal working conditions which assure substrate advanced degradation. The kinetics of nitroaromatics degradation and organic nitrogen mineralization was assessed and pseudo-first order rate constants were calculated. Fe doped photocatalyst with lowest metal content (0.5 wt.%) showed a considerable better behaviour in respect to pollutant degradation than Co and Ni (1wt.%) doped titania catalysts. For the same working conditions, degradation efficiency was higher for DNT than DNB in accordance with their calculated adsobance constants (Kad), taking into account that degradation process occurs on catalyst surface following a Langmuir-Hinshalwood model. The presence of methyl group in the structure of DNT allows its degradation by oxidative and reductive pathways, while DNB is converted only by reductive route, which also explain the highest DNT degradation efficiency. For highest pollutant concentration tested (3 x 10-4 M), optimum working conditions (0.5 wt.% Fe doped –TiO2 loading of 200 mg/L, pH=7 and 240 min. irradiation time) assures advanced nitroaromatics degradation (ηDNB=89%, ηDNT=94%) and organic nitrogen mineralization (ηDNB=44%, ηDNT=47%).

Keywords: hazardous organic compounds, irradiation, nitroaromatics, photocatalysis

Procedia PDF Downloads 317
50936 Radiation Annealing of Radiation Embrittlement of the Reactor Pressure Vessel

Authors: E. A. Krasikov

Abstract:

Influence of neutron irradiation on RPV steel degradation are examined with reference to the possible reasons of the substantial experimental data scatter and furthermore – nonstandard (non-monotonous) and oscillatory embrittlement behavior. In our glance, this phenomenon may be explained by presence of the wavelike component in the embrittlement kinetics. We suppose that the main factor affecting steel anomalous embrittlement is fast neutron intensity (dose rate or flux), flux effect manifestation depends on state-of-the-art fluence level. At low fluencies, radiation degradation has to exceed normative value, then approaches to normative meaning and finally became sub normative. Data on radiation damage change including through the ex-service RPVs taking into account chemical factor, fast neutron fluence and neutron flux were obtained and analyzed. In our opinion, controversy in the estimation on neutron flux on radiation degradation impact may be explained by presence of the wavelike component in the embrittlement kinetics. Therefore, flux effect manifestation depends on fluence level. At low fluencies, radiation degradation has to exceed normative value, then approaches to normative meaning and finally became sub normative. Moreover as a hypothesis we suppose that at some stages of irradiation damaged metal have to be partially restored by irradiation i.e. neutron bombardment. Nascent during irradiation structure undergo occurring once or periodically transformation in a direction both degradation and recovery of the initial properties. According to our hypothesis, at some stage(s) of metal structure degradation neutron bombardment became recovering factor. As a result, oscillation arises that in turn leads to enhanced data scatter.

Keywords: annealing, embrittlement, radiation, RPV steel

Procedia PDF Downloads 342
50935 Nonlinear Estimation Model for Rail Track Deterioration

Authors: M. Karimpour, L. Hitihamillage, N. Elkhoury, S. Moridpour, R. Hesami

Abstract:

Rail transport authorities around the world have been facing a significant challenge when predicting rail infrastructure maintenance work for a long period of time. Generally, maintenance monitoring and prediction is conducted manually. With the restrictions in economy, the rail transport authorities are in pursuit of improved modern methods, which can provide precise prediction of rail maintenance time and location. The expectation from such a method is to develop models to minimize the human error that is strongly related to manual prediction. Such models will help them in understanding how the track degradation occurs overtime under the change in different conditions (e.g. rail load, rail type, rail profile). They need a well-structured technique to identify the precise time that rail tracks fail in order to minimize the maintenance cost/time and secure the vehicles. The rail track characteristics that have been collected over the years will be used in developing rail track degradation prediction models. Since these data have been collected in large volumes and the data collection is done both electronically and manually, it is possible to have some errors. Sometimes these errors make it impossible to use them in prediction model development. This is one of the major drawbacks in rail track degradation prediction. An accurate model can play a key role in the estimation of the long-term behavior of rail tracks. Accurate models increase the track safety and decrease the cost of maintenance in long term. In this research, a short review of rail track degradation prediction models has been discussed before estimating rail track degradation for the curve sections of Melbourne tram track system using Adaptive Network-based Fuzzy Inference System (ANFIS) model.

Keywords: ANFIS, MGT, prediction modeling, rail track degradation

Procedia PDF Downloads 337
50934 Phenol Removal from Water in the Presence of Nano-TiO₂ and a Natural Activated Carbon: Intensive and Extensive Processes

Authors: Hanane Belayachi, Fadila Nemchi, Amel Belayachi, Sarra Bourahla, Mostefa Belhakem

Abstract:

In this work, two photocatalytic processes for the degradation of phenol in water are presented. The first one is extensive (EP), which is carried out in a treatment chain of two steps, allowing the adsorption of the pollutant by a naturally activated carbon from the grapes. This operation is followed by a photocatalytic degradation of the residual phenol in the presence of TiO₂. The second process is intensive (IP) and is realized in one step in the presence of a hybrid photocatalytic nanomaterial prepared from naturally activated carbon and TiO₂. The evaluation of the two processes, EP and IP, is based on the analytical monitoring of the initial and final parameters of the water to be treated, i.e., the phenol concentration by liquid phase chromatography (HPLC) and total organic carbon (TOC). For both processes, the sampling was carried out every 10 min for 120 min of treatment time to measure the phenol concentrations. The elimination and degradation rates in the case of the intensive process are better than the extensive process. In both processes, the catechol molecule was detected as an under product of degradation. In the IP case, this intermediate phenol was totally eliminated, and only traces of catechol persisted in the water.

Keywords: photocatalysis, hybrid, activated carbon, phenol

Procedia PDF Downloads 58
50933 Self-Assembled ZnFeAl Layered Double Hydroxides as Highly Efficient Fenton-Like Catalysts

Authors: Marius Sebastian Secula, Mihaela Darie, Gabriela Carja

Abstract:

Ibuprofen is a non-steroidal anti-inflammatory drug (NSAIDs) and is among the most frequently detected pharmaceuticals in environmental samples and among the most widespread drug in the world. Its concentration in the environment is reported to be between 10 and 160 ng L-1. In order to improve the abatement efficiency of this compound for water source prevention and reclamation, the development of innovative technologies is mandatory. AOPs (advanced oxidation processes) are known as highly efficient towards the oxidation of organic pollutants. Among the promising combined treatments, photo-Fenton processes using layered double hydroxides (LDHs) attracted significant consideration especially due to their composition flexibility, high surface area and tailored redox features. This work presents the self-supported Fe, Mn or Ti on ZnFeAl LDHs obtained by co-precipitation followed by reconstruction method as novel efficient photo-catalysts for Fenton-like catalysis. Fe, Mn or Ti/ZnFeAl LDHs nano-hybrids were tested for the degradation of a model pharmaceutical agent, the anti-inflammatory agent ibuprofen, by photocatalysis and photo-Fenton catalysis, respectively, by means of a lab-scale system consisting of a batch reactor equipped with an UV lamp (17 W). The present study presents comparatively the degradation of Ibuprofen in aqueous solution UV light irradiation using four different types of LDHs. The newly prepared Ti/ZnFeAl 4:1 catalyst results in the best degradation performance. After 60 minutes of light irradiation, the Ibuprofen removal efficiency reaches 95%. The slowest degradation of Ibuprofen solution occurs in case of Fe/ZnFeAl 4:1 LDH, (67% removal efficiency after 60 minutes of process). Evolution of Ibuprofen degradation during the photo Fenton process is also studied using Ti/ZnFeAl 2:1 and 4:1 LDHs in the presence and absence of H2O2. It is found that after 60 min the use of Ti/ZnFeAl 4:1 LDH in presence of 100 mg/L H2O2 leads to the fastest degradation of Ibuprofen molecule. After 120 min, both catalysts Ti/ZnFeAl 4:1 and 2:1 result in the same value of removal efficiency (98%). In the absence of H2O2, Ibuprofen degradation reaches only 73% removal efficiency after 120 min of degradation process. Acknowledgements: This work was supported by a grant of the Romanian National Authority for Scientific Research and Innovation, CNCS - UEFISCDI, project number PN-II-RU-TE-2014-4-0405.

Keywords: layered double hydroxide, advanced oxidation process, micropollutant, heterogeneous Fenton

Procedia PDF Downloads 230
50932 Biodegradable Polymeric Composites of Polylactide and Epoxidized Natural Rubber

Authors: Masek A., Diakowska K., Zaborski M.

Abstract:

Polymeric materials have found their use almost in every branch of industry worldwide. Most of them constitute so-called “petropolymers" obtained from crude oil. However literature information sounds a warning that its global sources are running out. Thus, it seems that one should search for polymeric materials from renewable raw materials belonging to the group of green polymers. Therefore on account of environmental protection and the issue of sustainable technologies, nowadays greater and greater achievements have been observed in the field of green technology using engineering sciences to develop composite materials. The main aim of this study was to research what is the influence of biofillers on the properties. We used biofillers like : cellulose with different length of fiber, cellulose UFC100, silica and montmorillonite. In our research, we reported on biodegradable composites exhibitingspecificity properties by melt blending of polylactide (PLA), one of the commercially available biodegradable material, and epoxidized natural rubber (ENR) containing 50 mol.%epoxy group. Blending hydrophilic natural polymers and aliphatic polyesters is of significant interest, since it could lead to the development of a new range of biodegradable polymeric materials. We research the degradation of composites on the basis epoxidized natural rubber and poly(lactide). The addition of biofillers caused far-reaching degradation processes. The greatest resistance to biodegradation showed a montmorillonite-based mixtures, the smallest inflated cellulose fibers of varying length.The final aim in the present study is to use ENR and poly(lactide) to design composite from renewable resources with controlled degradation.

Keywords: renewable resources, biopolymer, degradation, polylactide

Procedia PDF Downloads 376
50931 PVMODREL© Development Based on Reliability Evaluation of a PV Module Using Accelerated Degradation Testing

Authors: Abderafi Charki, David Bigaud

Abstract:

The aim of this oral speach is to present the PVMODREL© (PhotoVoltaic MODule RELiability) new software developed in the University of Angers. This new tool permits us to evaluate the lifetime and reliability of a PV module whatever its geographical location and environmental conditions. The electrical power output of a PV module decreases with time mainly as a result of the effects of corrosion, encapsulation discoloration, and solder bond failure. The failure of a PV module is defined as the point where the electrical power degradation reaches a given threshold value. Accelerated life tests (ALTs) are commonly used to assess the reliability of a PV module. However, ALTs provide limited data on the failure of a module and these tests are expensive to carry out. One possible solution is to conduct accelerated degradation tests. The Wiener process in conjunction with the accelerated failure time model makes it possible to carry out numerous simulations and thus to determine the failure time distribution based on the aforementioned threshold value. By this means, the failure time distribution and the lifetime (mean and uncertainty) can be evaluated. An example using the damp heat test is shown to demonstrate the usefulness PVMODREL.

Keywords: lifetime, reliability, PV Module, accelerated life testing, accelerated degradation testing

Procedia PDF Downloads 575
50930 Environmental Degradation and Biodiversity Loss in Bangladesh

Authors: Mohammad Atiqur Rahman

Abstract:

The study aimed at inventorying the threatened biodiversity of Bangladesh and assessing the rate of loss of biodiversity caused due to environmental degradation for conservation management. The impact assessment of environmental depletion and rate of biodiversity loss determination have been made by a long term field investigation, examination of preserved herbarium specimens and survey of relevant floristic literature following the IUCN’s threatened criteria of assessing Red List Plants under the Flora Bangladesh Project. Biodiversity of Bangladesh, as evaluated, has been affected to a large extent during the last four and half decades due to spontaneous environmental degradation caused by frequent occurrence of cyclonic storms and tidal bores since 1970 and flooding, draught, unilateral diversion of trans-boundary waters by operating Farakka Barrage since 1975, indiscriminate destruction and over exploitation of natural resources, unplanned development and industrialization, overpopulation etc. Depletion of world’s largest mangrove biodiversity in Sundarbans, coastal and island biodiversity in southern part, agro-biodiversity and agro-fisheries all over the country, Haor and wetland biodiversity of plain lands, terrestrial and forest biodiversity in central and eastern hilly part of Bangladesh, as assessed, have greatly been occurred at a higher rate due to environmental degradation which in turn affect directly or indirectly the economy, food security and environmental health of the country. Complete inventory of 30 plant families resulted in the recognition of 45.18% species of Bangladesh as threatened environmentally and 13.23% species as possibly extinct from the flora since these have neither been reported or could be traced in the field for more than 100 years. The rate of extinction is determined to be 2.65% per 20 years. Hence the study indicates that the loss of biodiversity and environmental degradation in Bangladesh occurring at an alarming rate. The study focuses on the issues of environment, the extent of loss of different plant biodiversities in Bangladesh, prioritizing and implementing national conservation strategies for sustainable management of the environment.

Keywords: Bangladesh, biodiversity, conservation, environmental management

Procedia PDF Downloads 252