1438 Low-Density Polyethylene Film Biodegradation Potential by Fungal Species From Thailand

Authors: Patcharee Pripdeevech, Sarunpron Khruengsai

Abstract:

Thirty fungi were tested for their degradation ability on low-density polyethylene (LDPE) plastic film. Biodegradation of all fungi was screened in mineral salt medium broth containing LDPE film as the sole carbon source for 30 days. Diaporthe italiana, Thyrostroma jaczewskii, Colletotrichum fructicola, and Stagonosporopsis citrulli were able to colonize and cover the surface of LDPE film in media. The degradation test result was compared to those obtained from Aspergillus niger. LDPE films cocultured with D. italiana, T. jaczewskii, C. fructicola, S. citrulli, A. niger, and control showed weight loss of 43.90%, 46.34%, 48.78%, 45.12%, 28.78%, and 10.85%, respectively. The tensile strength of degraded LDPE films cocultured with D. italiana, T. jaczewskii, C. fructicola, S. citrulli, A. niger, and control also reduced significantly by 1.56 MPa, 1.78 MPa, 0.43 MPa, 1.86 MPa, 3.34 MPa, and 9.98 MPa, respectively. Analysis of LDPE films by Fourier transform infrared spectroscopy and scanning electron microscopy confirmed the biodegradation by the presence of morphological changes such as cracks, scions, and holes on the surface of the film. These fungi have the ability to break down and consume the LDPE film, especially C. fructicola. These findings showed the potential of fungi in Thailand that play an important role in LDPE film degradation.

Keywords: plastic biodegradation, LDPE film, fungi, Fourier transform infrared, scanning electron microscopy

Procedia PDF Downloads 96
1437 Influence of Gamma-Radiation Dosimetric Characteristics on the Stability of the Persistent Organic Pollutants

Authors: Tatiana V. Melnikova, Lyudmila P. Polyakova, Alla A. Oudalova

Abstract:

As a result of environmental pollution, the production of agriculture and foodstuffs inevitably contain residual amounts of Persistent Organic Pollutants (POP). The special attention must be given to organic pollutants, including various organochlorinated pesticides (OCP). Among priorities, OCP is DDT (and its metabolite DDE), alfa-HCH, gamma-HCH (lindane). The control of these substances spends proceeding from requirements of sanitary norms and rules. During too time often is lost sight of that the primary product can pass technological processing (in particular irradiation treatment) as a result of which transformation of physicochemical forms of initial polluting substances is possible. The goal of the present work was to study the OCP radiation degradation at a various gamma-radiation dosimetric characteristics. The problems posed for goal achievement: to evaluate the content of the priority of OCPs in food; study the character the degradation of OCP in model solutions (with micro concentrations commensurate with the real content of their agricultural and food products) depending upon dosimetric characteristics of gamma-radiation. Qualitative and quantitative analysis of OCP in food and model solutions by gas chromatograph Varian 3400 (Varian, Inc. (USA)); chromatography-mass spectrometer Varian Saturn 4D (Varian, Inc. (USA)) was carried out. The solutions of DDT, DDE, alpha- and gamma- isomer HCH (0.01, 0.1, 1 ppm) were irradiated on "Issledovatel" (60Co) and "Luch - 1" (60Co) installations at a dose 10 kGy with a variation of dose rate from 0.0083 up to 2.33 kGy/sec. It was established experimentally that OCP residual concentration in individual samples of food products (fish, milk, cereal crops, meat, butter) are evaluated as 10-1-10-4 mg/kg, the value of which depends on the factor-sensations territory and natural migration processes. The results were used in the preparation of model solutions OCP. The dependence of a degradation extent of OCP from a dose rate gamma-irradiation has complex nature. According to our data at a dose 10 kGy, the degradation extent of OCP at first increase passes through a maximum (over the range 0.23 – 0.43 Gy/sec), and then decrease with the magnification of a dose rate. The character of the dependence of a degradation extent of OCP from a dose rate is kept for various OCP, in polar and nonpolar solvents and does not vary at the change of concentration of the initial substance. Also in work conditions of the maximal radiochemical yield of OCP which were observed at having been certain: influence of gamma radiation with a dose 10 kGy, in a range of doses rate 0.23 – 0.43 Gy/sec; concentration initial OCP 1 ppm; use of solvent - 2-propanol after preliminary removal of oxygen. Based on, that at studying model solutions of OCP has been established that the degradation extent of pesticides and qualitative structure of OCP radiolysis products depend on a dose rate, has been decided to continue researches radiochemical transformations OCP into foodstuffs at various of doses rate.

Keywords: degradation extent, dosimetric characteristics, gamma-radiation, organochlorinated pesticides, persistent organic pollutants

Procedia PDF Downloads 223
1436 Stability Indicating RP – HPLC Method Development, Validation and Kinetic Study for Amiloride Hydrochloride and Furosemide in Pharmaceutical Dosage Form

Authors: Jignasha Derasari, Patel Krishna M, Modi Jignasa G.

Abstract:

Chemical stability of pharmaceutical molecules is a matter of great concern as it affects the safety and efficacy of the drug product.Stability testing data provides the basis to understand how the quality of a drug substance and drug product changes with time under the influence of various environmental factors. Besides this, it also helps in selecting proper formulation and package as well as providing proper storage conditions and shelf life, which is essential for regulatory documentation. The ICH guideline states that stress testing is intended to identify the likely degradation products which further help in determination of the intrinsic stability of the molecule and establishing degradation pathways, and to validate the stability indicating procedures. A simple, accurate and precise stability indicating RP- HPLC method was developed and validated for simultaneous estimation of Amiloride Hydrochloride and Furosemide in tablet dosage form. Separation was achieved on an Phenomenexluna ODS C18 (250 mm × 4.6 mm i.d., 5 µm particle size) by using a mobile phase consisting of Ortho phosphoric acid: Acetonitrile (50:50 %v/v) at a flow rate of 1.0 ml/min (pH 3.5 adjusted with 0.1 % TEA in Water) isocratic pump mode, Injection volume 20 µl and wavelength of detection was kept at 283 nm. Retention time for Amiloride Hydrochloride and Furosemide was 1.810 min and 4.269 min respectively. Linearity of the proposed method was obtained in the range of 40-60 µg/ml and 320-480 µg/ml and Correlation coefficient was 0.999 and 0.998 for Amiloride hydrochloride and Furosemide, respectively. Forced degradation study was carried out on combined dosage form with various stress conditions like hydrolysis (acid and base hydrolysis), oxidative and thermal conditions as per ICH guideline Q2 (R1). The RP- HPLC method has shown an adequate separation for Amiloride hydrochloride and Furosemide from its degradation products. Proposed method was validated as per ICH guidelines for specificity, linearity, accuracy; precision and robustness for estimation of Amiloride hydrochloride and Furosemide in commercially available tablet dosage form and results were found to be satisfactory and significant. The developed and validated stability indicating RP-HPLC method can be used successfully for marketed formulations. Forced degradation studies help in generating degradants in much shorter span of time, mostly a few weeks can be used to develop the stability indicating method which can be applied later for the analysis of samples generated from accelerated and long term stability studies. Further, kinetic study was also performed for different forced degradation parameters of the same combination, which help in determining order of reaction.

Keywords: amiloride hydrochloride, furosemide, kinetic study, stability indicating RP-HPLC method validation

Procedia PDF Downloads 438
1435 Photo-Fenton Degradation of Organic Compounds by Iron(II)-Embedded Composites

Authors: Marius Sebastian Secula, Andreea Vajda, Benoit Cagnon, Ioan Mamaliga

Abstract:

One of the most important classes of pollutants is represented by dyes. The synthetic character and complex molecular structure make them more stable and difficult to be biodegraded in water. The treatment of wastewaters containing dyes in order to separate/degrade dyes is of major importance. Various techniques have been employed to remove and/or degrade dyes in water. Advanced oxidation processes (AOPs) are known as among the most efficient ones towards dye degradation. The aim of this work is to investigate the efficiency of a cheap Iron-impregnated activated carbon Fenton-like catalyst in order to degrade organic compounds in aqueous solutions. In the presented study an anionic dye, Indigo Carmine, is considered as a model pollutant. Various AOPs are evaluated for the degradation of Indigo Carmine to establish the effect of the prepared catalyst. It was found that the Iron(II)-embedded activated carbon composite enhances significantly the degradation process of Indigo Carmine. Using the wet impregnation procedure, 5 g of L27 AC material were contacted with Fe(II) solutions of FeSO4 precursor at a theoretical iron content in the resulted composite of 1 %. The L27 AC was impregnated for 3h at 45°C, then filtered, washed several times with water and ethanol and dried at 55 °C for 24 h. Thermogravimetric analysis, Fourier transform infrared, X-ray diffraction, and transmission electron microscopy were employed to investigate the structural, textural, and micromorphology of the catalyst. Total iron content in the obtained composites and iron leakage were determined by spectrophotometric method using phenantroline. Photo-catalytic tests were performed using an UV - Consulting Peschl Laboratory Reactor System. UV light irradiation tests were carried out to determine the performance of the prepared Iron-impregnated composite towards the degradation of Indigo Carmine in aqueous solution using different conditions (17 W UV lamps, with and without in-situ generation of O3; different concentrations of H2O2, different initial concentrations of Indigo Carmine, different values of pH, different doses of NH4-OH enhancer). The photocatalytic tests were performed after the adsorption equilibrium has been established. The obtained results emphasize an enhancement of Indigo Carmine degradation in case of the heterogeneous photo-Fenton process conducted with an O3 generating UV lamp in the presence of hydrogen peroxide. The investigated process obeys the pseudo-first order kinetics. The photo-Fenton degradation of IC was tested at different values of initial concentration. The obtained results emphasize an enhancement of Indigo Carmine degradation in case of the heterogeneous photo-Fenton process conducted with an O3 generating UV lamp in the presence of hydrogen peroxide. Acknowledgments: This work was supported by a grant of the Romanian National Authority for Scientific Research and Innovation, CNCS - UEFISCDI, project number PN-II-RU-TE-2014-4-0405.

Keywords: photodegradation, heterogeneous Fenton, anionic dye, carbonaceous composite, screening factorial design

Procedia PDF Downloads 230
1434 Formaldehyde Degradation from Indoor Air by Encapsulated Microbial Cells

Authors: C. C. Castro, T. Senechal, D. Lahem, A. L. Hantson

Abstract:

Formaldehyde is one of the most representative volatile organic compounds present in the indoor air of residential units and workplaces. Increased attention has been given to this toxic compound because of its carcinogenic effect in health. Biological or enzymatic transformation is being explored to degrade this pollutant. Pseudomonas putida is a bacteria able to synthesize formaldehyde dehydrogenase, an enzyme known to use formaldehyde as a substrate and transform it into less toxic compounds. The immobilization of bacterial cells in the surface of different supports through spraying or dip-coating is herein proposed. The determination of the enzymatic activity on the coated surfaces was performed as well as the study of its effect on formaldehyde degradation in an isolated chamber. Results show that the incorporation of microbial cells able to synthesize depolluting enzymes can be an innovative, low-cost, effective and environmentally friendly solution for indoor air depollution.

Keywords: cells encapsulation, formaldehyde, formaldehyde dehydrogenase, indoor air depollution

Procedia PDF Downloads 146
1433 Effect of Carbon Nanotubes on Ultraviolet and Immersion Stability of Diglycidyl Ether of Bisphenol A Epoxy Coating

Authors: Artemova Anastasiia, Shen Zexiang, Savilov Serguei

Abstract:

The marine environment is very aggressive for a number of factors, such as moisture, temperature, winds, ultraviolet radiation, chloride ion concentration, oxygen concentration, pollution, and biofouling, all contributing to marine corrosion. Protective organic coatings provide protection either by a barrier action from the layer, which is limited due to permeability to water and oxygen or from active corrosion inhibition and cathodic protection due to the pigments in the coating. Carbon nanotubes can play not only barrier effect but also passivation effect via adsorbing molecular species of oxygen, hydroxyl, chloride and sulphate anions. Multiwall carbon nanotubes composite provide very important properties such as mechanical strength, non-cytotoxicity, outstanding thermal and electrical conductivity, and very strong absorption of ultraviolet radiation. The samples of stainless steel (316L) coated by epoxy resin with carbon nanotubes-based pigments were exposed to UV irradiation (340nm), and immersion to the sodium chloride solution for 1000h and corrosion behavior in 3.5 wt% sodium chloride (NaCl) solution was investigated. Experimental results showed that corrosion current significantly decreased in the presence of carbon nanotube-based materials, especially nitrogen-doped ones, in the composite coating. Importance of the structure and composition of the pigment materials and its composition was established, and the mechanism of the protection was described. Finally, the effect of nitrogen doping on the corrosion behavior was investigated. The pigment-polymer crosslinking improves the coating performance and the corrosion rate decreases in comparison with pure epoxy coating from 5.7E-05 to 1.4E-05mm/yr for the coating without any degradation; in more than 6 times for the coating after ultraviolet degradation; and more than 16% for the coatings after immersion degradation.

Keywords: corrosion, coating, carbon nanotubes, degradation

Procedia PDF Downloads 126
1432 Environmental Impact of Trade Sector Growth: Evidence from Tanzania

Authors: Mosses E. Lufuke

Abstract:

This paper attempted to investigate whether there is Granger-causality running from trade to environment as evidenced in the changing climatic condition and land degradation. Using Tanzania as the reference, VAR-Granger-causality test was employed to rationalize the conundrum of causal-effect relationship between trade and environment. The changing climatic condition, as the proxy of both nitrous oxide emissions (in thousand metric tons of CO2 equivalent) and land degradation measured by the size of arable land were tested against trade using both exports and imports variables. The result indicated that neither of the trade variables Granger-cause the variability on gas emissions and arable land size. This suggests the possibility that all trade concerns in relation to environment to have been internalized in domestic policies to offset any likely negative consequence.

Keywords: environment, growth, impact, trade

Procedia PDF Downloads 298
1431 An Optimal Bayesian Maintenance Policy for a Partially Observable System Subject to Two Failure Modes

Authors: Akram Khaleghei Ghosheh Balagh, Viliam Makis, Leila Jafari

Abstract:

In this paper, we present a new maintenance model for a partially observable system subject to two failure modes, namely a catastrophic failure and a failure due to the system degradation. The system is subject to condition monitoring and the degradation process is described by a hidden Markov model. A cost-optimal Bayesian control policy is developed for maintaining the system. The control problem is formulated in the semi-Markov decision process framework. An effective computational algorithm is developed and illustrated by a numerical example.

Keywords: partially observable system, hidden Markov model, competing risks, multivariate Bayesian control

Procedia PDF Downloads 428
1430 Isolation and Identification of Novel Escherichia Marmotae Spp.: Their Enzymatic Biodegradation of Zearalenone and Deep-oxidation of Deoxynivalenol

Authors: Bilal Murtaza, Xiaoyu Li, Liming Dong, Muhammad Kashif Saleemi, Gen Li, Bowen Jin, Lili Wang, Yongping Xu

Abstract:

Fusarium spp. produce numerous mycotoxins, such as zearalenone (ZEN), deoxynivalenol (DON), and its acetylated compounds, 3-acetyl-deoxynivalenol (3-ADON) and 15-acetyl-deoxynivalenol (15-ADON) (15-ADON). In a co-culture system, the soil-derived Escherichia marmotae strain degrades ZEN and DON into 3-keto-DON and DOM-1 via enzymatic deep-oxidation. When pure mycotoxins were subjected to Escherichia marmotae in culture flasks, degradation, and detoxification were also attained. DON and ZEN concentrations, ambient pH, incubation temperatures, bacterium concentrations, and the impact of acid treatment on degradation were all evaluated. The results of the ELISA and high-performance liquid chromatography-electrospray ionization-high resolution mass spectrometry (HPLC-ESI-HRMS) tests demonstrated that the concentration of mycotoxins exposed to Escherichia marmotae was significantly lower than the control. ZEN levels were reduced by 43.9%, while zearalenone sulfate ([M/z 397.1052 C18H21O8S1) was discovered as a derivative of ZEN converted by microbes to a less toxic molecule. Furthermore, Escherichia marmotae appeared to metabolize DON 35.10% into less toxic derivatives (DOM-1 at m/z 281 of [DON - O]+ and 3-keto-DON at m/z 295 of [DON - 2H]+). These results show that Escherichia marmotae can reduce Fusarium mycotoxins production, degrade pure mycotoxins, and convert them to less harmful compounds, opening up new possibilities for study and innovation in mycotoxin detoxification.

Keywords: mycotoxins, zearalenone, deoxynivalenol, bacterial degradation

Procedia PDF Downloads 59
1429 Biodegradation of Carbamazepine and Diclofenac by Bacterial Strain Labrys Portucalensis

Authors: V. S. Bessa, I. S. Moreira, S. Murgolo, C. Piccirillo, G. Mascolo, P. M. L. Castro

Abstract:

The occurrence of pharmaceuticals in the environment has been a topic of increasing concern. Pharmaceuticals are not completely mineralized in the human body and are released on the sewage systems as the pharmaceutical itself and as their “biologically active” metabolites through excretion, as well as by improper elimination and disposal. Conventional wastewater treatment plants (WWTPs) are not designed to remove these emerging pollutants and they are thus released into the environment. The antiepileptic drug carbamazepine (CBZ) and the non-steroidal anti-inflammatory diclofenac (DCF) are two widely used pharmaceuticals, frequently detected in water bodies, including rivers and groundwater, in concentrations ranging from ng L 1 to mg L 1. These two compounds were classified as medium to high-risk pollutants in WWTP effluents and surface waters. Also, CBZ has been suggested as a molecular marker of wastewater contamination in surface water and groundwater and the European Union included DCF in the watch list of substances Directive to be monitored. In the present study, biodegradation of CBZ and DCF by the bacterial strain Labrys portucalensis F11, a strain able to degrade other pharmaceutical compounds, was assessed; tests were performed with F11 as single carbon and energy source, as well as in presence of 5.9mM of sodium acetate. In assays supplemented with 2.0 and 4.0 µM of CBZ, the compound was no longer detected in the bulk medium after 24hr and 5days, respectively. Complete degradation was achieved in 21 days for 11.0 µM and in 23 days for 21.0 µM. For the highest concentration tested (43.0 µM), 95% of degradation was achieved in 30days. Supplementation with acetate increased the degradation rate of CBZ, for all tested concentrations. In the case of DCF, when supplemented as a single carbon source, approximately 70% of DCF (1.7, 3.3, 8.4, 17.5 and 34.0 µM) was degraded in 30days. Complete degradation was achieved in the presence of acetate for all tested concentrations, at higher degradation rates. The detection of intermediates produced during DCF biodegradation was performed by UPLC-QTOF/MS/MS, which allowed the identification of a range of metabolites. Stoichiometric liberation of chorine occurred and no metabolites were detected at the end of the biodegradation assays suggesting a complete mineralization of DCF. Strain Labrys portucalensis F11 proved to be able to degrade these two top priority environmental contaminants and may be potentially useful for biotechnological applications/environment remediation.

Keywords: biodegradation, carbamazepine, diclofenac, pharmaceuticals

Procedia PDF Downloads 241
1428 Photocatalytic Degradation of Aqueous Organic Pollutant under UV Light Irradiation

Authors: D. Tassalit, N. Chekir, O. Benhabiles, N. A. Laoufi, F. Bentahar

Abstract:

In the setting of the waters purification, some molecules appear recalcitrant to the traditional treatments. The exploitation of the properties of some catalysts permits to amplify the oxidization performances with ultraviolet radiance and to remove this pollution by a non biological way. This study was conducted to investigate the effect of a photocatalysis oxidation system for organic pollutants treatment using a new reactor design and ZnO/TiO2 as a catalyst under UV light. Oxidative degradation of tylosin by hydroxyl radicals (OH°) was studied in aqueous medium using suspended forms of ZnO and TiO2. The results improve that the treatment was affected by many factors such as flow-rate of solution, initial pollutant concentration and catalyst concentration. The rate equation for the tylosin degradation followed first order kinetics and the rate-constants were determined. The reaction rate fitted well with Langmuir–Hinshelwood model and the removed ratio of tylosin was 97 % in less than 60 minutes. To determine the optimum catalyst loading, a series of experiments were carried out by varying the amount of catalyst from 0.05 to 0.5 g/L. The results demonstrate that the rate of photodegradation is optimum with catalyst loading of 0.1 g/L, reaction flow rate of 3.79 mL/s and solution natural pH. The rate was found to increase with the decrease in tylosin concentration from 30 to 5 mg/L. Therefore, this simple photoreactor design for the removal of organic pollutants has the potential to be used in wastewater treatment.

Keywords: advanced oxidation, photocatalysis, TiO2, ZnO, UV light, pharmaceuticals pollutants, Spiramycin, tylosin, wastewater treatment

Procedia PDF Downloads 398
1427 The Concentration of Formaldehyde in Rainwater and Typhoon Rainwater at Sakai City, Japan

Authors: Chinh Nguyen Nhu Bao, Hien To Thi, Norimichi Takenaka

Abstract:

Formaldehyde (HCHO) concentrations in rainwater including in tropical storms in Sakai City, Osaka, Japan have been measured continuously during rain event by developed chemiluminescence method. The level of formaldehyde was ranged from 15 µg/L to 500 µg/L. The high concentration of HCHO in rainwater is related to the wind direction from the south and west sides of Sakai City where manufactures related to chemicals, oil-refinery, and steel. The in-situ irradiated experiment on rainwater sample was conducted to prove the aqueous phase photo-production of HCHO and the degradation of HCHO. In the daytime, the aqueous phase photolysis is the source of HCHO in rainwater (4.52 ± 5.74 µg/L/h for UV light source in-situ condition, 2.84-8.96 µg/L/h under sunlight). However, in the night time, the degradation is the function of microorganism.

Keywords: chemiluminescence, formaldehyde, rainwater, typhoon

Procedia PDF Downloads 137
1426 An Assessment of the Factors Affecting Green Building Technology (GBT) Adoption

Authors: Nuruddeen Usman, Usman Mohammed Gidado

Abstract:

A construction and post construction activity in buildings contributes to environmental degradation, because of the generation of solid waste during construction to the production of carbon dioxide by the occupants during utilization. These problems were caused as a result of lack of adopting green building technology during and after construction. However, this study aims at conceptualizing the factors that are affecting the adoption of green building technology with a view to suggest better ways for its successful adoption in the construction industry through developing a green building technology model. Thus, the research findings show that: Economic, social, cultural, and technological progresses are the factors affecting Green Building Technology Adoption. Therefore, identifying these factors and developing the model might help in the successful adoption of green building technology.

Keywords: green building technology, construction, post construction, degradation

Procedia PDF Downloads 621
1425 Degradation of the Mechanical Properties of the Polypropylene Talc Nanocomposite in Chemical Environment

Authors: Ahmed Ouadah Bouakkaz, Mohamed Elmeguenni, Bel Abbes Bachir Bouiadjra, Mohamed Belhouari, Abdulmohsen Albedah

Abstract:

In this study, the effect of the chemical environment on the mechanical properties of the polypropylene-talc composite was analyzed. The talc proportion was varied in order to highlight the combined effects of time of immersion in the chemical environment 'benzene' and talc concentration on the mechanical properties of the composite. Tensile test was carried out to evaluate the mechanical properties of PP-talc composite and to analyze the effect of the immersion time on the variation of these properties. The obtained results show that increasing the time of immersion has a very negative effect on the mechanical strength of the PP-talc composite, but this effect can be significantly reduced by the augmentation of the talc proportion.

Keywords: polypropylene (PP), talc, nanocomposite, degradation

Procedia PDF Downloads 347
1424 Synthesis of Novel Nanostructure Copper(II) Metal-Organic Complex for Photocatalytic Degradation of Remdesivir Antiviral COVID-19 from Aqueous Solution: Adsorption Kinetic and Thermodynamic Studies

Authors: Sam Bahreini, Payam Hayati

Abstract:

Metal-organic coordination [Cu(L)₄(SCN)₂] was synthesized applying ultrasonic irradiation, and its photocatalytic performance for the degradation of Remdesivir (RS) under sunlight irradiation was systematically explored for the first time in this study. The physicochemical properties of the synthesized photocatalyst were investigated using Fourier-transform infrared (FT-IR), field emission scanning electron microscopy (FE-SEM), powder x-ray diffraction (PXRD), energy-dispersive x-ray (EDX), thermal gravimetric analysis (TGA), diffuse reflectance spectroscopy (DRS) techniques. Systematic examinations were carried out by changing irradiation time, temperature, solution pH value, contact time, RS concentration, and catalyst dosage. The photodegradation kinetic profiles were modeled in pseudo-first order, pseudo-second-order, and intraparticle diffusion models reflected that photodegradation onto [Cu(L)₄(SCN)₂] catalyst follows pseudo-first order kinetic model. The fabricated [Cu(L)₄(SCN)₂] nanostructure bandgap was determined as 2.60 eV utilizing the Kubelka-Munk formula from the diffuse reflectance spectroscopy method. Decreasing chemical oxygen demand (COD) (from 70.5 mgL-1 to 36.4 mgL-1) under optimal conditions well confirmed mineralizing of the RS drug. The values of ΔH° and ΔS° was negative, implying the process of adsorption is spontaneous and more favorable in lower temperatures.

Keywords: Photocatalytic degradation, COVID-19, density functional theory (DFT), molecular electrostatic potential (MEP)

Procedia PDF Downloads 136
1423 Degradation of Acetaminophen with Fe3O4 and Fe2+ as Activator of Peroxymonosulfate

Authors: Chaoqun Tan, Naiyun Gao, Xiaoyan Xin

Abstract:

Perxymonosulfate (PMS)-based oxidation processes, as an alternative of hydrogen peroxide-based oxidation processes, are more and more popular because of reactive radical species (SO4-•, OH•) produced in systems. Magnetic nano-scaled particles Fe3O4 and ferrous anion (Fe2+) were studied for the activation of PMS for degradation of acetaminophen (APAP) in water. The Fe3O4 MNPs were found to effectively catalyze PMS for APAP and the reactions well followed a pseudo-first-order kinetics pattern (R2 > 0.95), while the degradation of APAP in PMS-Fe2+ system proceeds through two stages: a fast stage and a much slower stage. Within 5 min, approximately 7% and 18% of 10 ppm APAP was accomplished by 0.2 mM PMS in Fe3O4 (0.8g/L) and Fe2+ (0.1mM) activation process. However, as reaction proceed to 120 min, approximately 75% and 35% of APAP was removed in Fe3O4 activation process and Fe2+ activation process, respectively. Within 120 min, the mineralization of APAP was about 7.5% and 5.0% (initial APAP of 10 ppm and [PMS]0 of 0.2 mM) in Fe3O4-PMS and Fe2+-PMS system, while the mineralization could be greatly increased to about 31% and 40% as [PMS]0 increased to 2.0 mM in in Fe3O4-PMS and Fe2+-PMS system, respectively. At last, the production of reactive radical species were validated directly from Electron Paramagnetic Resonance (ESR) tests with 0.1 M 5,5-dimethyl-1-pyrrolidine N-oxide (DMPO). Plausible mechanisms on the radical generation from Fe3O4 and Fe2+ activation of PMS are proposed on the results of radial identification tests. The results demonstrated that Fe3O4 MNPs activated PMS and Fe2+ anion activated PMS systems are promising technologies for water pollution caused by contaminants such as pharmaceutical. Fe3O4-PMS system is more suitable for slowly remediation, while Fe2+-PMS system is more suitable for fast remediation.

Keywords: acetaminophen, peroxymonosulfate, radicals, Fe3O4

Procedia PDF Downloads 222
1422 Robust Diagnosis Efficiency by Bond-Graph Approach

Authors: Benazzouz Djamel, Termeche Adel, Touati Youcef, Alem Said, Ouziala Mahdi

Abstract:

This paper presents an approach which detect and isolate efficiently a fault in a system. This approach avoids false alarms, non-detections and delays in detecting faults. A study case have been proposed to show the importance of taking into consideration the uncertainties in the decision-making procedure and their effect on the degradation diagnostic performance and advantage of using Bond Graph (BG) for such degradation. The use of BG in the Linear Fractional Transformation (LFT) form allows generating robust Analytical Redundancy Relations (ARR’s), where the uncertain part of ARR’s is used to generate the residuals adaptive thresholds. The study case concerns an electromechanical system composed of a motor, a reducer and an external load. The aim of this application is to show the effectiveness of the BG-LFT approach to robust fault detection.

Keywords: bond graph, LFT, uncertainties, detection and faults isolation, ARR

Procedia PDF Downloads 278
1421 Tribological Behaviour of the Degradation Process of Additive Manufactured Stainless Steel 316L

Authors: Yunhan Zhang, Xiaopeng Li, Zhongxiao Peng

Abstract:

Additive manufacturing (AM) possesses several key characteristics, including high design freedom, energy-efficient manufacturing process, reduced material waste, high resolution of finished products, and excellent performance of finished products. These advantages have garnered widespread attention and fueled rapid development in recent decades. AM has significantly broadened the spectrum of available materials in the manufacturing industry and is gradually replacing some traditionally manufactured parts. Similar to components produced via traditional methods, products manufactured through AM are susceptible to degradation caused by wear during their service life. Given the prevalence of 316L stainless steel (SS) parts and the limited research on the tribological behavior of 316L SS samples or products fabricated using AM technology, this study aims to investigate the degradation process and wear mechanisms of 316L SS disks fabricated using AM technology. The wear mechanisms and tribological performance of these AM-manufactured samples are compared with commercial 316L SS samples made using conventional methods. Additionally, methods to enhance the tribological performance of additive-manufactured SS samples are explored. Four disk samples with a diameter of 75 mm and a thickness of 10 mm are prepared. Two of them (Group A) are prepared from a purchased SS bar using a milling method. The other two disks (Group B), with the same dimensions, are made of Gas Atomized 316L Stainless Steel (size range: 15-45 µm) purchased from Carpenter Additive and produced using Laser Powder Bed Fusion (LPBF). Pin-on-disk tests are conducted on these disks, which have similar surface roughness and hardness levels. Multiple tests are carried out under various operating conditions, including varying loads and/or speeds, and the friction coefficients are measured during these tests. In addition, the evolution of the surface degradation processes is monitored by creating moulds of the wear tracks and quantitatively analyzing the surface morphologies of the mould images. This analysis involves quantifying the depth and width of the wear tracks and analyzing the wear debris generated during the wear processes. The wear mechanisms and wear performance of these two groups of SS samples are compared. The effects of load and speed on the friction coefficient and wear rate are investigated. The ultimate goal is to gain a better understanding of the surface degradation of additive-manufactured SS samples. This knowledge is crucial for enhancing their anti-wear performance and extending their service life.

Keywords: degradation process, additive manufacturing, stainless steel, surface features

Procedia PDF Downloads 40
1420 Influence of Hydrolytic Degradation on Properties of Moisture Membranes Used in Fire-Protective Clothing

Authors: Rachid El Aidani, Phuong Nguyen-Tri, Toan Vu-Khanh

Abstract:

This study intends to show the influence of the hydrolytic degradation on the properties of the e-PTFE/NOMEX® membranes used in fire-protective clothing. The modification of water vapour permeability, morphology and chemical structure was examined by MOCON Permatran, electron microscopy scanning (SEM), and ATR-FTIR, respectively. A decrease in permeability to water vapour of the aged samples was observed following closure of transpiration pores. Analysis of fiber morphology indicates the appearance of defects at the fibers surface with the presence of micro cavities as well as the of fibrils. ATR-FTIR analysis reveals the presence of a new absorption band attributed to carboxylic acid terminal groups generated during the amide bond hydrolysis.

Keywords: hydrolytic ageing, moisture membrane, water vapor permeability, morphology

Procedia PDF Downloads 281
1419 Biodegradation Ability of Polycyclic Aromatic Hydrocarbon (PAHs) Degrading Bacillus cereus Strain JMG-01 Isolated from PAHs Contaminated Soil

Authors: Momita Das, Sofia Banu, Jibon Kotoky

Abstract:

Environmental contamination of natural resources with persistent organic pollutants is of great world-wide apprehension. Polycyclic aromatic hydrocarbons (PAHs) are among the organic pollutants, released due to various anthropogenic activities. Due to their toxic, carcinogenic and mutagenic properties, PAHs are of environmental and human concern. Presently, bioremediation has evolved as the most promising biotechnology for cleanup of such contaminants because of its economical and less cost effectiveness. In the present study, distribution of 16 USEPA priority PAHs was determined in the soil samples collected from fifteen different sites of Guwahati City, the Gateway of the North East Region of India. The total concentrations of 16 PAHs (Σ16 PAHs) ranged from 42.7-742.3 µg/g. Higher concentration of total PAHs was found more in the Industrial areas compared to all the sites (742.3 µg/g and 628 µg/g). It is noted that among all the PAHs, Naphthalene, Acenaphthylene, Anthracene, Fluoranthene, Chrysene and Benzo(a)Pyrene were the most available and contain the higher concentration of all the PAHs. Since microbial activity has been deemed the most influential and significant cause of PAH removal; further, twenty-three bacteria were isolated from the most contaminated sites using the enrichment process. These strains were acclimatized to utilize naphthalene and anthracene, each at 100 µg/g concentration as sole carbon source. Among them, one Gram-positive strain (JMG-01) was selected, and biodegradation ability and initial catabolic genes of PAHs degradation were investigated. Based on 16S rDNA analysis, the isolate was identified as Bacillus cereus strain JMG-01. Topographic images obtained using Scanning Electron Microscope (SEM) and Atomic Force Microscope (AFM) at scheduled time intervals of 7, 14 and 21 days, determined the variation in cell morphology during the period of degradation. AFM and SEM micrograph of biomass showed high filamentous growth leading to aggregation of cells in the form of biofilm with reference to the incubation period. The percentage degradation analysis using gas chromatography and mass analyses (GC-MS) suggested that more than 95% of the PAHs degraded when the concentration was at 500 µg/g. Naphthalene, naphthalene-2-methy, benzaldehyde-4-propyl, 1, 2, benzene di-carboxylic acid and benzene acetic acid were the major metabolites produced after degradation. Moreover, PCR experiments with specific primers for catabolic genes, ndo B and Cat A suggested that JMG-01 possess genes for PAHs degradation. Thus, the study concludes that Bacillus cereus strain JMG-01 has efficient biodegrading ability and can trigger the clean-up of PAHs contaminated soil.

Keywords: AFM, Bacillus cereus strain JMG-01, degradation, polycyclic aromatic hydrocarbon, SEM

Procedia PDF Downloads 237
1418 Polyethylene Terephthalate Plastic Degradation by Fungus Rasamsonia Emersonii

Authors: Naveen Kumar

Abstract:

Microplastics, tiny plastic particles less than 5 mm in size formed by the disposal and breakdown of industrial and consumer products, have become a primary environmental concern due to their ubiquitous presence and application in the environment and their potential to cause harm to the ecosystem, wildlife and human health. In this, we study the ability of the fungus Rasamsonia emersonii IMI 393752 to degrade the rigid microplastics of Coke bottles. Microplastics were extracted from Coke bottles and incubated with Rasamsonia emersonii in Sabouraud dextrose agar media. Microplastics were pre-sterilized without altering the chemistry of microplastic. Preliminary analysis was performed by observing radial growth assessment of microplastic-containing media enriched with fungi vs. control. The assay confirmed no impedance or change in the fungi's growth pattern and rate by introducing microplastics. The degradation of the microplastics was monitored over time using microscopy and FTIR, and biodegradation/deterioration on the plastic surface was observed. Furthermore, the liquid assay was performed. HPLC and GCMS will be conducted to check the biodegradation and presence of enzyme release by fungi to counteract the presence of microplastics. These findings have important implications for managing plastic waste, as they suggest that fungi such as Rasamsonia emersonii can potentially degrade microplastics safely and effectively. However, further research to optimise the conditions for microplastic degradation by Rasamsonia emersonii and to develop strategies for scaling up the process for industrial applications will be beneficial.

Keywords: bioremediation, mycoremediation, plastic degradtion, polyethylene terephthalate

Procedia PDF Downloads 52
1417 Analytical Study on Threats to Wetland Ecosystems and Their Solutions in the Framework of the Ramsar Convention

Authors: Ehsan Daryadel, Farhad Talaie

Abstract:

Wetlands are one of the most important ecosystems on Earth. Nevertheless, various challenges threaten these ecosystems and disrupt their ecological character. Among these, the effects of human-based threats are more devastating. Following mass degradation of wetlands during 1970s, the Ramsar Convention on Wetlands (Ramsar, Iran, 1971) was concluded to conserve wetlands of international importance and prevent destruction and degradation of such ecosystems through wise use of wetlands as a mean to achieve sustainable development in all over the world. Therefore, in this paper, efforts have been made to analyze threats to wetlands and then investigate solutions in the framework of the Ramsar Convention. Finally, in order to operate these mechanisms, this study concludes that all states should in turn make their best effort to improve and restore global wetlands through preservation of environmental standards and close contribution and also through taking joint measures with other states effectively.

Keywords: Ramsar Convention, threats, wetland wcosystems, wise use

Procedia PDF Downloads 366
1416 Simultaneous Determination of Methotrexate and Aspirin Using Fourier Transform Convolution Emission Data under Non-Parametric Linear Regression Method

Authors: Marwa A. A. Ragab, Hadir M. Maher, Eman I. El-Kimary

Abstract:

Co-administration of methotrexate (MTX) and aspirin (ASP) can cause a pharmacokinetic interaction and a subsequent increase in blood MTX concentrations which may increase the risk of MTX toxicity. Therefore, it is important to develop a sensitive, selective, accurate and precise method for their simultaneous determination in urine. A new hybrid chemometric method has been applied to the emission response data of the two drugs. Spectrofluorimetric method for determination of MTX through measurement of its acid-degradation product, 4-amino-4-deoxy-10-methylpteroic acid (4-AMP), was developed. Moreover, the acid-catalyzed degradation reaction enables the spectrofluorimetric determination of ASP through the formation of its active metabolite salicylic acid (SA). The proposed chemometric method deals with convolution of emission data using 8-points sin xi polynomials (discrete Fourier functions) after the derivative treatment of these emission data. The first and second derivative curves (D1 & D2) were obtained first then convolution of these curves was done to obtain first and second derivative under Fourier functions curves (D1/FF) and (D2/FF). This new application was used for the resolution of the overlapped emission bands of the degradation products of both drugs to allow their simultaneous indirect determination in human urine. Not only this chemometric approach was applied to the emission data but also the obtained data were subjected to non-parametric linear regression analysis (Theil’s method). The proposed method was fully validated according to the ICH guidelines and it yielded linearity ranges as follows: 0.05-0.75 and 0.5-2.5 µg mL-1 for MTX and ASP respectively. It was found that the non-parametric method was superior over the parametric one in the simultaneous determination of MTX and ASP after the chemometric treatment of the emission spectra of their degradation products. The work combines the advantages of derivative and convolution using discrete Fourier function together with the reliability and efficacy of the non-parametric analysis of data. The achieved sensitivity along with the low values of LOD (0.01 and 0.06 µg mL-1) and LOQ (0.04 and 0.2 µg mL-1) for MTX and ASP respectively, by the second derivative under Fourier functions (D2/FF) were promising and guarantee its application for monitoring the two drugs in patients’ urine samples.

Keywords: chemometrics, emission curves, derivative, convolution, Fourier transform, human urine, non-parametric regression, Theil’s method

Procedia PDF Downloads 402
1415 Antioxidant Juice Prevents UV- Induced Skin Damage in Rats

Authors: S. P. Gomes, D. C. Goncalves, E. Ribeiro, M. C. L. Seelaender

Abstract:

Skin is susceptible to photo damage induced by exposure to sunlight, or ultraviolet (UV) radiation, which induces breakdown of extracellular matrix, DNA degradation, skin cell lesion and apoptosis, and development of cancer. Phytonutrients demonstrate protective effects against UV damage. The purpose of this study was evaluating the effect of an antioxidant juice (AJ) contaning Brazilian natural products upon skin damage. The juice was produced by Metabolics®. Male Wistar rats were divided in 4 groups: Animals receiving the antioxidant juice (AJ): orange, carrot, honey, tomato extract, avocado, ginger and camu-camu (Brazilian fruit, a major source of vitamin C) ad libitum for 21 days; or water (C), subdivided in groups exposed or not to UV radiation for 2 non consecutive days, during five hours each day, after 15 days of juice supplementation. On the 22nd day, rats were killed by decapitation and epithelium samples from the dorsal skin removed, fixed in bouin and embedded in paraffin. The sections were stained with hematoxylin and eosin or mallory and picrosirius red. Isolated DNA was submitted to electrophoresis (1.8% agarose gel, 0.5% ethidium bromide). UV radiation significantly induced sunburn of superficial epithelial cells of C, AJ treatment reduced this effect. Collagen changes were observed in UV groups, yet AJ treatment prevented collagen degradation. UV radiation induced significant DNA degradation, in C, which was prevented by AJ treatment. The antioxidant juice consumed chronically protected against acute skin damage.

Keywords: nutraceuticals, antioxidants, photoprotection, uv radiation

Procedia PDF Downloads 595
1414 Fatigue Test and Stress-Life Analysis of Nanocomposite-Based Bone Fixation Device

Authors: Jisoo Kim, Min Su Lee, Sunmook Lee

Abstract:

Durability assessment of nanocomposite-based bone fixation device was performed by flexural fatigue tests, for which the changes in the life cycles of nanocomposite samples synthesized by blending bioabsorbable polymer (PLGA) and ceramic nanoparticles (β-TCP) with different ratios were monitored. The nanocomposite samples were kept in a constant temperature/humidity chamber at 37°C/50%RH for varied incubation periods for the degradation of nanocomposite samples under the temperature/humidity stress. It was found that the life cycles were increasing as the incubation time in the chamber were increasing in the initial stage irrespective of sample compositions, which was due to the annealing effect of the polymer. However, the life cycle was getting shorter as the incubation time increased afterward, which was due to the overall degradation of nanocomposites. It was found that the life cycle of the nanocomposite sample with high ceramic content was shorter than the one with low ceramic content, which was attributed to the increased brittleness of the composite with high ceramic content. The changes in chemical properties were also monitored by FT-IR, which indicated that the degradation of the biodegradable polymer could be confirmed by the increased intensities of carboxyl groups and hydroxyl groups since the hydrolysis of ester bonds connecting two successive monomers yielded carboxyl end groups and hydroxyl groups.

Keywords: bioabsorbable polymer, bone fixation device, ceramic nanoparticles, durability assessment, fatigue test

Procedia PDF Downloads 370
1413 Optimal Portfolio of Multi-service Provision based on Stochastic Model Predictive Control

Authors: Yifu Ding, Vijay Avinash, Malcolm McCulloch

Abstract:

As the proliferation of decentralized energy systems, the UK power system allows small-scale entities such as microgrids (MGs) to tender multiple energy services including energy arbitrage and frequency responses (FRs). However, its operation requires the balance between the uncertain renewable generations and loads in real-time and has to fulfill their provision requirements of contract services continuously during the time window agreed, otherwise it will be penalized for the under-delivered provision. To hedge against risks due to uncertainties and maximize the economic benefits, we propose a stochastic model predictive control (SMPC) framework to optimize its operation for the multi-service provision. Distinguished from previous works, we include a detailed economic-degradation model of the lithium-ion battery to quantify the costs of different service provisions, as well as accurately describe the changing dynamics of the battery. Considering a branch of load and generation scenarios and the battery aging, we formulate a risk-averse cost function using conditional value at risk (CVaR). It aims to achieve the maximum expected net revenue and avoids severe losses. The framework will be performed on a case study of a PV-battery grid-tied microgrid in the UK with real-life data. To highlight its performance, the framework will be compared with the case without the degradation model and the deterministic formulation.

Keywords: model predictive control (MPC), battery degradation, frequency response, microgrids

Procedia PDF Downloads 100
1412 Dehalogenation of Aromatic Compounds in Wastewater by Bacterial Cultures

Authors: Anne Elain, Magali Le Fellic

Abstract:

Halogenated Aromatic Compounds (HAC) are major organic pollutants that are detected in several environmental compartments as a result of their widespread use as solvents, pesticides and other industrial chemicals. The degradation of HAC simultaneously at low temperature and under saline conditions would be useful for remediation of polluted sites. Hence, microbial processes based on the metabolic activities of anaerobic bacteria are especially attractive from an economic and environmental point of view. Metabolites are generally less toxic, less likely to bioaccumulate and more susceptible for further degradation. Studies on biological reductive dehalogenation have largely been restricted to chlorinated compounds while relatively few have focussed on other HAC i.e., fluorinated, brominated or iodinated compounds. The objectives of the present work were to investigate the biodegradation of a mixture of triiodoaromatic molecules in industrial wastewater by an enriched bacterial consortium. Biodegradation of the mixture was studied during batch experiments in an anaerobic reactor. The degree of mineralization and recovery of halogen were monitored by HPLC-UV, TOC analysis and potentiometric titration. Providing ethanol as an electron donor was found to stimulate anaerobic reductive dehalogenation of HAC with a deiodination rate up to 12.4 mg.L-1 per day. Sodium chloride even at high concentration (10 mM) was found to have no influence on the degradation rates nor on the microbial viability. An analysis of the 16S rDNA (MicroSeq®) revealed that at least 6 bacteria were predominant in the enrichment, including Pseudomonas aeruginosa, Pseudomonas monteilii, Kocuria rhizophila, Ochrobacterium anthropi, Ralstonia pickettii and Rhizobium rhizogenes.

Keywords: halogenated aromatics, anaerobic biodegradation, deiodination, bacterial consortium

Procedia PDF Downloads 151
1411 Modelling the Impacts of Geophysical Parameters on Deforestation and Forest Degradation in Pre and Post Ban Logging Periods in Hindu Kush Himalayas

Authors: Alam Zeb, Glen W. Armstrong, Muhammad Qasim

Abstract:

Loss of forest cover is one of the most important land cover changes and has been of great concern to policy makers. This study quantified forest cover changes over pre logging ban (1973-1993) and post logging ban (1993-2015) to examine the role of geophysical factors and spatial attributes of land in the two periods. We show that despite a complete ban on green felling, forest cover decreased by 28% and mostly converted to rangeland. Nevertheless, the logging ban was completely effective in controlling agriculture expansion. The binary logistic regression revealed that the south facing aspects at low elevation witnessed more deforestation in the pre-ban period compared to post-ban. Opposite to deforestation, forest degradation was more prominent on the northern aspects at higher elevation during the policy period. Agriculture expansion was widespread in the low elevation flat areas with gentle slope, while during the policy period agriculture contraction in the form of regeneration was observed on the low elevation areas of north facing slopes. All proximity variables, except distance to administrative boundary, showed a similar trend across the two periods and were important explanatory variables in understanding forest and agriculture expansion. The changes in determinants of forest and agriculture expansion and contraction over the two periods might be attributed to the influence of policy and a general decrease in resource availability.

Keywords: forest conservation , wood harvesting ban, logistic regression, deforestation, forest degradation, agriculture expansion, Chitral, Pakistan

Procedia PDF Downloads 201
1410 Bioremediation of Phenanthrene by Monocultures and Mixed Culture Bacteria Isolated from Contaminated Soil

Authors: A. Fazilah, I. Darah, I. Noraznawati

Abstract:

Three different bacteria capable of degrading phenanthrene were isolated from hydrocarbon contaminated site. In this study, the phenanthrene-degrading activity by defined monoculture was determined and mixed culture was identified as Acinetobacter sp. P3d, Bacillus sp. P4a and Pseudomonas sp. P6. All bacteria were able to grow in a minimal salt medium saturated with phenanthrene as the sole source of carbon and energy. Phenanthrene degradation efficiencies by different combinations (consortia) of these bacteria were investigated and their phenanthrene degradation was evaluated by gas chromatography. Among the monocultures, Pseudomonas sp. P6 exhibited 58.71% activity compared to Acinetobacter sp. P3d and Bacillus sp. P4a which were 56.97% and 53.05%, respectively after 28 days of cultivation. All consortia showed high phenanthrene elimination which were 95.64, 79.37, 87.19, 79.21% for Consortia A, B, C and D, respectively. The results indicate that all of the bacteria isolated may effectively degrade target chemical and have a promising application in bioremediation of hydrocarbon contaminated soil purposes.

Keywords: phenanthrene, consortia, acinetobacter sp. P3d, bacillus sp. P4a, pseudomonas sp. P6

Procedia PDF Downloads 263
1409 Simulative Study of the Influence of Degraded Twin-Tube Shock Absorbers on the Lateral Forces of Vehicle Axles

Authors: Tobias Schramm, Günther Prokop

Abstract:

Degraded vehicle shock absorbers represent a risk for road safety. The exact effect of degraded vehicle dampers on road safety is still the subject of research. This work is intended to contribute to estimating the effect of degraded twin-tube dampers of passenger cars on road safety. An axle model was built using a damper model to simulate different degradation levels. To parameterize the model, a realistic parameter space was estimated based on test rig measurements and database analyses, which is intended to represent the vehicle field in Germany. Within the parameter space, simulations of the axle model were carried out, which calculated the transmittable lateral forces of the various axle configurations as a function of vehicle speed, road surface, damper conditions and axle parameters. A degraded damper has the greatest effect on the transmittable lateral forces at high speeds and in poor road conditions. If a vehicle is traveling at a speed of 100 kph on a Class D road, a degraded damper reduces the transmissible lateral forces of an axle by 20 % on average. For individual parameter configurations, this value can rise to 50 %. The axle parameters that most influence the effect of a degraded damper are the vertical stiffness of the tire, the unsprung mass and the stabilizer stiffness of the axle.

Keywords: vehicle dynamics, vehicle simulation, vehicle component degradation, shock absorber model, shock absorber degradation

Procedia PDF Downloads 75