423 A Study on the Magnetic and Mechanical Properties of Nd-Fe-B Sintered Magnets According to Sintering Temperature
Authors: J. H. Kim, S. Y. Park, K. M. Lim, S. K. Hyun
Abstract:
The effect of sintering temperature on the magnetic and mechanical properties of Nd-Fe-B sintered magnets has been investigated in this study. The sintering temperature changed from 950°C to 1120°C. While remanence and hardness of the magnets increased with increasing sintering temperature, the coercivity first increased, and then decreased. The optimum magnetic and mechanical properties of the magnets were obtained at the sintering temperature of 1050°C. In order to clarify the reason for the variation on magnetic and mechanical properties of the magnets, we systematically analyzed the microstructure.Keywords: magnetic and mechanical property, microstructure, permanent magnets, sintered Nd-Fe-B magnet
Procedia PDF Downloads 337422 Effect of Zinc Additions on the Microstructure and Mechanical Properties of Mg-3Al Alloy
Authors: Erkan Koç, Mehmet Ünal, Ercan Candan
Abstract:
In this study, the effect of zinc content (0.5-3.0 wt.%) in as-cast Mg-3Al alloy which were fabricated with high-purity raw materials towards the microstructure and mechanical properties was studied. Microstructure results showed that increase in zinc content changed the secondary phase distribution of the alloys. Mechanical test results demonstrate that with the increasing Zn addition the enhancement of the hardness value by 29%, ultimate tensile strength by 16% and yield strength by 15% can be achieved as well as decreasing of elongation by 33%. The improvement in mechanical properties for Mg-Al–Zn alloys with increasing Zn content up to 3% of weight may be ascribed to second phase strengthening.Keywords: magnesium, zinc, mechanical properties, Mg17Al12
Procedia PDF Downloads 422421 Intermetallic Phases in the Fusion Weld of CP Ti to Stainless Steel
Authors: Juzar Vohra, Ravish Malhotra, Tim Pasang, Mana Azizi, Yuan Tao, Masami Mizutani
Abstract:
In this paper, dissimilar welding of titanium to stainless steels is reported. Laser Beam Welding (LBW) and Gas Tungsten Arc Welding (GTAW) were employed to join CPTi to SS304. The welds were examined using scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDS). FeTi, Ti2Cr and Fe2Ti dendrites are formed along with beta phase titanium matrix. The hardness values of these phases are high which makes them brittle and leading to cracking along the weld pool. However, it is believed that cracking, hence, fracturing of this weld joint is largely due to the difference in thermal properties of the two alloys.Keywords: dissimilar metals, fusion welding, intermetallics, brittle
Procedia PDF Downloads 496420 The Effect of Vanadium Addition on the Mechanical Properties and Microstructure of A319 Aluminum Alloy
Authors: Musbah Mahfoud, Ibtisam Mustafa
Abstract:
The present work highlights some of our up-to-date findings on the effect of vanadium addition on the mechanical properties and microstructure of one of the most versatile aluminum-silicon alloys, i.e., A319. In terms of microstructure, it was found that in addition to its ability to refine some of the constituent phases, vanadium also helps in retarding the formation of some of the detrimental intermetallic compounds, such as those involving Al-Fe-Si. Preliminary studies of the effect of vanadium on the mechanical properties of A319 have shown that vanadium additions up to 0.4% cause slight increase in the yield and tensile strength. However, the vanadium addition did not show a significant effect on the hardness of the alloy.Keywords: aluminium, vanadium, intermetallic, microstructure, mechanical properties
Procedia PDF Downloads 633419 Tensile and Fracture Properties of Cast and Forged Composite Synthesized by Addition of in-situ Generated Al3Ti-Al2O3 Particles to Magnesium
Authors: H. M. Nanjundaswamy, S. K. Nath, S. Ray
Abstract:
TiO2 particles have been added in molten aluminium to result in aluminium based cast Al/Al3Ti-Al2O3 composite, which has been added then to molten magnesium to synthesize magnesium based cast Mg-Al/Al3Ti-Al2O3 composite. The nominal compositions in terms of Mg, Al, and TiO2 contents in the magnesium based composites are Mg-9Al-0.6TiO2, Mg-9Al-0.8TiO2, Mg-9Al-1.0TiO2 and Mg-9Al-1.2TiO2 designated respectively as MA6T, MA8T, MA10T and MA12T. The microstructure of the cast magnesium based composite shows grayish rods of intermetallics Al3Ti, inherited from aluminium based composite but these rods, on hot forging, breaks into smaller lengths decreasing the average aspect ratio (length to diameter) from 7.5 to 3.0. There are also cavities in between the broken segments of rods. β-phase in cast microstructure, Mg17Al12, dissolves during heating prior to forging and re-precipitates as relatively finer particles on cooling. The amount of β-phase also decreases on forging as segregation is removed. In both the cast and forged composite, the Brinell hardness increases rapidly with increasing addition of TiO2 but the hardness is higher in forged composites by about 80 BHN. With addition of higher level of TiO2 in magnesium based cast composite, yield strength decreases progressively but there is marginal increase in yield strength over that of the cast Mg-9 wt. pct. Al, designated as MA alloy. But the ultimate tensile strength (UTS) in the cast composites decreases with the increasing particle content indicating possibly an early initiation of crack in the brittle inter-dendritic region and their easy propagation through the interfaces of the particles. In forged composites, there is a significant improvement in both yield strength and UTS with increasing TiO2 addition and also, over those observed in their cast counterpart, but at higher addition it decreases. It may also be noted that as in forged MA alloy, incomplete recovery of forging strain increases the strength of the matrix in the composites and the ductility decreases both in the forged alloy and the composites. Initiation fracture toughness, JIC, decreases drastically in cast composites compared to that in MA alloy due to the presence of intermetallic Al3Ti and Al2O3 particles in the composite. There is drastic reduction of JIC on forging both in the alloy and the composites, possibly due to incomplete recovery of forging strain in both as well as breaking of Al3Ti rods and the voids between the broken segments of Al3Ti rods in composites. The ratio of tearing modulus to elastic modulus in cast composites show higher ratio, which increases with the increasing TiO2 addition. The ratio decreases comparatively more on forging of cast MA alloy than those in forged composites.Keywords: composite, fracture toughness, forging, tensile properties
Procedia PDF Downloads 250418 Design and Synthesis of Gradient Nanocomposite Materials
Authors: Pu Ying-Chih, Yang Yin-Ju, Hang Jian-Yi, Jang Guang-Way
Abstract:
Organic-Inorganic hybrid materials consisting of graded distributions of inorganic nano particles in organic polymer matrices were successfully prepared by the sol-gel process. Optical and surface properties of the resulting nano composites can be manipulated by changing their compositions and nano particle distribution gradients. Applications of gradient nano composite materials include sealants for LED packaging and screen lenses for smartphones. Optical transparency, prism coupler, TEM, SEM, Energy Dispersive X-ray Spectrometer (EDX), Izod impact strength, conductivity, pencil hardness, and thermogravimetric characterizations of the nano composites were performed and the results will be presented.Keywords: Gradient, Hybrid, Nanocomposite, Organic-Inorganic
Procedia PDF Downloads 506417 Pioneer Synthesis and Characterization of Boron Containing Hard Materials
Authors: Gülşah Çelik Gül, Figen Kurtuluş
Abstract:
The first laboratory synthesis of hard materials such as diamond proceeded to attack of developing materials with high hardness to compete diamond. Boron rich solids are good candidates owing to their short interatomic bond lengths and strong covalent character. Boron containing hard material was synthesized by modified-microwave method under nitrogen atmosphere by using a fuel (glycine or urea), amorphous boron and/or boric acid in appropriate molar ratio. Characterizations were done by x-ray diffraction (XRD), fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy/energy dispersive analyze (SEM/EDS), thermo gravimetric/differantial thermal analysis (TG/DTA).Keywords: boron containing materials, hard materials, microwave synthesis, powder X-ray diffraction
Procedia PDF Downloads 593416 Full Potential Calculation of Structural and Electronic Properties of Perovskite BiAlO3 and BiGaO3
Authors: M. Harmel, H. Khachai
Abstract:
The first principles within the full potential linearized augmented plane wave (FP-LAPW) method were applied to study the structural and electronic properties of cubic perovskite-type compounds BiAlO3 and BiGaO3. The lattice constant, bulk modulus, its pressure derivative, band structure and density of states were obtained. The results show that BiGaO3 should exhibit higher hardness and stiffness than BiAlO3. The Al–O or Ga–O bonds are typically covalent with a strong hybridization as well as Bi–O ones that have a significant ionic character. Both materials are weakly ionic and exhibit wide and indirect band gaps, which are typical of insulators.Keywords: DFT, Ab initio, electronic structure, Perovskite structure, ferroelectrics
Procedia PDF Downloads 397415 Effect of Aging Treatment on Tensile Properties of AZ91D Mg Alloy
Authors: Ju Hyun Won, Seok Hong Min, Tae Kwon Ha
Abstract:
Phase equilibria of AZ91D Mg alloys for nonflammable use, containing Ca and Y, were carried out by using FactSage® and FTLite database, which revealed that solid solution treatment, could be performed at temperatures from 400 to 450 °C. Solid solution treatment of AZ91D Mg alloy without Ca and Y was successfully conducted at 420 °C and supersaturated microstructure with all beta phase resolved into matrix was obtained. In the case of AZ91D Mg alloy with some Ca and Y, however, a little amount of intermetallic particles were observed after solid solution treatment. After solid solution treatment, each alloy was annealed at temperatures of 180 and 200 °C for time intervals from 1 min to 48 hrs and hardness of each condition was measured by micro-Vickers method. Peak aging conditions were deduced as at the temperature of 200 °C for 10 hrs.Keywords: Mg alloy, AZ91D, nonflammable alloy, phase equilibrium, peak aging
Procedia PDF Downloads 431414 Effect of Farsi gum (Amygdalus Scoparia Spach) in Combination with Sodium Caseinate on Textural, Stability, Sensory Characteristics and Rheological Properties of Whipped Cream
Authors: Samaneh Mashayekhi
Abstract:
Cream (whipped cream) is one of the dairy products that can be used in desserts, pastries, cakes, and ice creams. In this product, some parameters such as taste and flavor, quality stability, whipping ability, and stability of foam after whipping are very important. The objective of this study is applicable of Farsi gum and sodium caseinate in 3 biopolymer ratios (1:1, 1:2, and 2:1) and 0.15, 0.30, and 0.45 %wt. concentrations in whipped cream formulation. Sample without hydrocolloids was considered as a control. Before whipping, viscosity of all creams was increased continuously with increasing shear rate. In addition, the viscosity was increased with the increasing hydrocolloids addition (in constant shear rate). Microscopic observations showed that polydispersity of systems before whipping. Overrun of F, FC11, and FC21 samples were increased (with increasing total hydrocollid concentration 0.15 to 0.30 % wt.); then decreased this parameter with increasing to 0.45 % wt. concentration. However, mean comparison of FC12 samples overrun showed that this value was increased with increasing total hydrocolloids concentration. 0.45FC21 sample had significantly (P<0.05) highest overrun (118.44±9.11). Synersis of whipped cream samples are reduced with hydrocolloid addition. B sample had significantly (P<0.05) highest serum separation (16.66±0.80%), and 0.45FC12 had a low one (5.94±0.19%) in compered with others synersis. Mean comparison of hardness and adhesiveness of whipped cream revealed that Farsi gum addition alone and in combination with sodium caseinate increased the previous textural characteristics. Results exhibited that 0.4FG12 had significantly (P<0.05) highest hardness (267.00±18.38 g).Mean comparison of droplet size of cream sample before whipping displaced that hydrocolloid addition had no significant effect (P>0.05), and mean droplet size of the samples ranged between 1.93-2.16 µm. Generally, the mean droplet size of whipped cream increased after whipping with increasing hydrocolloid concentration (0.15-0.45 % wt.). Color parameter analysis showed that Farsi gum addition alone and in combination with sodium caseinate had no significant effect (P>0.05) on these parameters (Lightness, Redness, and Yellowness). Based on sensory evaluation results, appearance, color, flavor, and taste of whipped creams not influenced by hydrocolloids addition; but 0.45FC12 sample had higher value. Based on the above results, Farsi gum had suggested to potential application in a whipped cream formulation; however, further research need to foundingof their functionality.Keywords: whipped cream, farsi gum, sodium caseinate, overrun, droplet size, texture analysis, sensory evaluation
Procedia PDF Downloads 98413 A Generalization of the Secret Sharing Scheme Codes Over Certain Ring
Authors: Ibrahim Özbek, Erdoğan Mehmet Özkan
Abstract:
In this study, we generalize (k,n) threshold secret sharing scheme on the study Ozbek and Siap to the codes over the ring Fq+ αFq. In this way, it is mentioned that the method obtained in that article can also be used on codes over rings, and new advantages to be obtained. The method of securely sharing the key in cryptography, which Shamir first systematized and Massey carried over to codes, became usable for all error-correcting codes. The firewall of this scheme is based on the hardness of the syndrome decoding problem. Also, an open study area is left for those working for other rings and code classes. All codes that correct errors with this method have been the working area of this method.Keywords: secret sharing scheme, linear codes, algebra, finite rings
Procedia PDF Downloads 76412 The Relation Between Protein-Protein and Polysaccharide-Protein Interaction on Aroma Release from Brined Cheese Model
Authors: Mehrnaz Aminifar
Abstract:
The relation between textural parameters and casein network on release of aromatic compounds was investigated over 90-days of ripening. Low DE maltodextrin and WPI were used to modify the textural properties of low fat brined cheese. Hardness, brittleness and compaction of casein network were affected by addition of maltodextrin and WPI. Textural properties and aroma release from cheese texture were affected by interaction of WPI protein-cheese protein and maltodexterin-cheese protein.Keywords: aroma release, brined cheese, maltodexterin, WPI
Procedia PDF Downloads 355411 Some Fundamental Physical Properties of BiGaO₃ Cubic Perovskite
Authors: B. Gueridi, T. Chihi, M. Fatmi, A. Faci
Abstract:
Some fundamental physical properties of BiGaO₃ were investigated under pressure and temperature effect using generalized gradient approximation and local density approximation approaches. The effect of orientation on Debye temperature and sound waves velocities were estimated from elastic constants. The value of the bulk modulus of BiGaO₃ is a sign of its high hardness because it is linked to an isotropic deformation. BiGaO₃ is a semiconductor and ductile material with covalent bonding (Ga–O), and the Bi-O bonding is ionic. The optical transitions were observed when electrons pass from the top of the valence band (O-2p) to the bottom of the conduction band (Ga-4p or Bi-6p). The thermodynamic parameters are determined in temperature and pressure ranging from 0 to 1800 K and 0 to 50 GPa.Keywords: BiGaO₃ perovskite, optical absorption, first principle, band structure
Procedia PDF Downloads 133410 Quality of Donut Supplemented with Hom Nin Rice Flour
Authors: Supatchalee Sirichokworrakit, Pannin Intasen, Chansuda Angkawut
Abstract:
Hom Nin rice (Oryza Sativa L.) was processed into flour and used to substitute wheat flour in donuts. The donuts were prepared with 0, 20, 40, 60, and 80% Hom Nin rice flour (HNF). The donuts were subjected to proximate, texture, color and sensory evaluations. The results of the study revealed that the ash, moisture, crude fiber contents increased while crude fat and protein contents decreased as the level of HNF increased. The hardness and chewiness of donut increased as the HNF increased but the cohesiveness, springiness, and specific volume decreased. Color of donut (L*, a*, and b* values) decreased with the addition of HNF. Overall acceptability for the 20-40% HNF additions did not differ significantly from the score of the 100% wheat flour.Keywords: Hom Nin rice, donut, texture evaluation, sensory evaluation
Procedia PDF Downloads 295409 Transparency Phenomenon in Kuew Teow
Authors: Muhammad Heikal Ismail, Law Chung Lim, Hii Ching Lik
Abstract:
In maintaining food quality and shelf life, drying is employed in food industry as the most reliable perseverance technique. In this way, heat pump drying and hot air drying of fresh rice noodles was deduced to freeze drying in achieving quality attributes of oil content Scanning Electron Microscope (SEM) images, texture, and colour. Soxthlet analysis shows freeze dried noodles contain more than 10 times oil content, distinct pores of SEM images, higher hardness by more than three times, and wider colour changes by average more than two times to both methods to explain the less transparency physical outlook of freeze dried samples.Keywords: freeze drying, heat pump drying, noodles, Soxthlet
Procedia PDF Downloads 486408 Effect of Y Addition on the Microstructure and Mechanical Properties of Sn-Zn Eutectic Alloy
Authors: Jung-Ho Moon, Tae Kwon Ha
Abstract:
The effect of Yttrium addition on the microstructure and mechanical properties of Sn-Zn eutectic alloy, which has been attracting intensive focus as a Pb-free solder material, was investigated in this study. Phase equilibrium has been calculated by using FactSage® to evaluate the composition and fraction of equilibrium intermetallic compounds and construct a phase diagram. In the case of Sn-8.8 Zn eutectic alloy, the as-cast microstructure was typical lamellar. With addition of 0.25 wt. %Y, a large amount of pro-eutectic phases have been observed and various YZnx intermetallic compounds were expected to successively form during cooling. Hardness of Sn-8.8 Zn alloy was not affected by Y-addition and both alloys could be rolled by 90% at room temperature.Keywords: Sn-Zn eutectic alloy, yttrium, FactSage®, microstructure, mechanical properties
Procedia PDF Downloads 470407 Benzimidazole as Corrosion Inhibitor for Heat Treated 6061 Al-SiCp Composite in Acetic Acid
Authors: Melby Chacko, Jagannath Nayak
Abstract:
6061 Al-SiCp composite was solutionized at 350 °C for 30 minutes and water quenched. It was then underaged at 140 °C (T6 treatment). The aging behaviour of the composite was studied using Rockwell B hardness measurement. Corrosion behaviour of the underaged sample was studied in different concentrations of acetic acid and at different temperatures. Benzimidazole at different concentrations was used for the inhibition studies. Inhibition efficiency of benzimidazole was calculated for different experimental conditions. Thermodynamic parameters were found out which suggested benzimidazole is an efficient inhibitor and it adsorbed onto the surface of composite by mixed adsorption where chemisorption is predominant.Keywords: 6061 Al-SiCp composite, T6 treatment, corrosion inhibition, chemisorption
Procedia PDF Downloads 399406 Effect of Waste Dumping on Groundwater Quality at Guntun Layi Funtua, Katsina State
Authors: Isiya Aminu Dabai, Adebola Kayode, Adeosun Kayode Daniel
Abstract:
Rural water supply relies mainly on groundwater exploitation, because it is more accessible, reliable, cheaper to develop and maintain, also with good quality compared to the surface water. Despite these advantages, groundwater has come under pollution threats like waste dumps, mineral exploitation, industrialization etc. This study investigates the effects of an open dumping to the surrounding groundwater. Ten hand dug well water samples were collected from the surroundings and tested. The average result shows that temperature, colour and turbidity to be 8.50 c, 6.1 TCU and 3.1 NTU respectively and pH, conductivity, total dissolved solids, chloride content and hardness to be 7.2, 4.78, 1.8, 5.7, and 3.4 respectively while in the bacteriological test well no. 1, 2, 3, and 5 shows the presence of coliforms and E. Coli bacteria.Keywords: groundwater, pollution, waste, dump site, unsafe, quality
Procedia PDF Downloads 683405 Effect of Aging Condition on Semisolid Cast 2024 Aluminum Alloy
Authors: S. Wisutmethangoon, S. Pannaray, T. Plookphol, J. Wannasin
Abstract:
2024 Aluminium alloy was squeezed cast by the Gas Induced Semi Solid (GISS) process. Effect of artificial aging on microstructure and mechanical properties of this alloy was studied in the present work. The solutionized specimens were aged hardened at temperatures of 175°C, 200°C, and 225°C under various time durations. The highest hardness of about 77.7 HRE was attained from specimen aged at the temperature of 175 °C for 36 h. Upon investigation the microstructure by using Transmission Electron Microscopy (TEM), the phase was mainly attributed to the strengthening effect in the aged alloy. The apparent activation energy for precipitation hardening of the alloy was calculated as 133,805 J/mol.Keywords: 2024 aluminium alloy, gas induced semi solid, T6 heat treatment, aged hardening, transmission electron microscopy
Procedia PDF Downloads 312404 Physiochemical Analysis of Ground Water in Zaria, Kaduna state, Nigeria
Authors: E. D. Paul, F. G. Okibe, C. E. Gimba, S. Yakubu
Abstract:
Some physicochemical characteristics and heavy metal concentrations of water samples collected from ten boreholes in Samaru, Zaria, Kaduna state, Nigeria were analysed in order to assess the drinking water quality. Physicochemical parameters were determined using classical methods while the heavy metals were determined using Atomic Absorption Spectrometry. Results of the analysis obtained were as follows: Temperature 29 – 310C, pH 5.74 – 6.19, Electrical conductivity 3.21 – 7.54 µs, DO 0.51 – 1.00 mg/L, BOD 0.0001 – 0.006 mg/L, COD 160 – 260 mg/L, TDS 2.08 – 4.55 mg/L, Total Hardness 97.44 – 401.36 mg/L CaCO3, and Chloride 0.97 – 59.12 mg/L. Concentrations of heavy metals were in the range; Zinc 0.000 – 0.7568 mg/L, Lead 0.000 – 0.070 mg/L and Cadmium 0.000 – 0.009 mg/L. The implications of these findings are discussed.Keywords: ground water, water quality, heavy metals, Atomic Absorption Spectrometry (AAS)
Procedia PDF Downloads 535403 Mechanical and Material Characterization on the High Nitrogen Supersaturated Tool Steels for Die-Technology
Authors: Tatsuhiko Aizawa, Hiroshi Morita
Abstract:
The tool steels such as SKD11 and SKH51 have been utilized as punch and die substrates for cold stamping, forging, and fine blanking processes. The heat-treated SKD11 punches with the hardness of 700 HV wrought well in the stamping of SPCC, normal steel plates, and non-ferrous alloy such as a brass sheet. However, they suffered from severe damage in the fine blanking process of smaller holes than 1.5 mm in diameter. Under the high aspect ratio of punch length to diameter, an elastoplastic bucking of slender punches occurred on the production line. The heat-treated punches had a risk of chipping at their edges. To be free from those damages, the blanking punch must have sufficient rigidity and strength at the same time. In the present paper, the small-hole blanking punch with a dual toughness structure was proposed to provide a solution to this engineering issue in production. The low-temperature plasma nitriding process was utilized to form the nitrogen supersaturated thick layer into the original SKD11 punch. Through the plasma nitriding at 673 K for 14.4 ks, the nitrogen supersaturated layer, with the thickness of 50 μm and without nitride precipitates, was formed as a high nitrogen steel (HNS) layer surrounding the original SKD11 punch. In this two-zone structured SKD11 punch, the surface hardness increased from 700 HV for the heat-treated SKD11 to 1400 HV. This outer high nitrogen SKD11 (HN-SKD11) layer had a homogeneous nitrogen solute depth profile with a nitrogen solute content plateau of 4 mass% till the border between the outer HN-SKD11 layer and the original SKD11 matrix. When stamping the brass sheet with the thickness of 1 mm by using this dually toughened SKD11 punch, the punch life was extended from 500 K shots to 10000 K shots to attain a much more stable production line to yield the brass American snaps. Furthermore, with the aid of the masking technique, the punch side surface layer with the thickness of 50 μm was modified by this high nitrogen super-saturation process to have a stripe structure where the un-nitrided SKD11 and the HN-SKD11 layers were alternatively aligned from the punch head to the punch bottom. This flexible structuring promoted the mechanical integrity of total rigidity and toughness as a punch with an extremely small diameter.Keywords: high nitrogen supersaturation, semi-dry cold stamping, solid solution hardening, tool steel dies, low temperature nitriding, dual toughness structure, extremely small diameter punch
Procedia PDF Downloads 89402 Optimization of Human Hair Concentration for a Natural Rubber Based Composite
Authors: Richu J. Babu, Sony Mathew, Sharon Rony Jacob, Soney C. George, Jibin C. Jacob
Abstract:
Human hair is a non-biodegradable waste available in plenty throughout the world but is rarely explored for applications in engineering fields. Tensile strength of human hair ranges from 170 to 220 MPa. This property of human hair can be made use in the field of making bio-composites[1]. The composite is prepared by commixing the human hair and natural rubber in a two roll mill along with additives followed by vulcanization. Here the concentration of the human hair is varied by fine-tuning the fiber length as 20 mm and sundry tests like tensile, abrasion, tear and hardness were conducted. While incrementing the fiber length up to a certain range the mechanical properties shows superior amendments.Keywords: human hair, natural rubber, composite, vulcanization, fiber loading
Procedia PDF Downloads 384401 Effect of Accelerated Aging on Antibacterial and Mechanical Properties of SEBS Compounds
Authors: Douglas N. Simoes, Michele Pittol, Vanda F. Ribeiro, Daiane Tomacheski, Ruth M. C. Santana
Abstract:
Thermoplastic elastomers (TPE) compounds are used in a wide range of applications, like home appliances, automotive components, medical devices, footwear, and others. These materials are susceptible to microbial attack, causing a crack in polymer chains compounds based on SEBS copolymers, poly (styrene-b-(ethylene-co-butylene)-b-styrene, are a class of TPE, largely used in domestic appliances like refrigerator seals (gaskets), bath mats and sink squeegee. Moisture present in some areas (such as shower area and sink) in addition to organic matter provides favorable conditions for microbial survival and proliferation, contributing to the spread of diseases besides the reduction of product life cycle due the biodegradation process. Zinc oxide (ZnO) has been studied as an alternative antibacterial additive due its biocidal effect. It is important to know the influence of these additives in the properties of the compounds, both at the beginning and during the life cycle. In that sense, the aim of this study was to evaluate the effect of accelerated aging in oven on antibacterial and mechanical properties of ZnO loaded SEBS based TPE compounds. Two different comercial zinc oxide, named as WR and Pe were used in proportion of 1%. A compound with no antimicrobial additive (standard) was also tested. The compounds were prepared using a co-rotating double screw extruder (L/D ratio of 40/1 and 16 mm screw diameter). The extrusion parameters were kept constant for all materials, screw rotation rate was set at 226 rpm, with a temperature profile from 150 to 190 ºC. Test specimens were prepared using the injection molding machine at 190 ºC. The Standard Test Method for Rubber Property—Effect of Liquids was applied in order to simulate the exposition of TPE samples to detergent ingredients during service. For this purpose, ZnO loaded TPE samples were immersed in a 3.0% w/v detergent (neutral) and accelerated aging in oven at 70°C for 7 days. Compounds were characterized by changes in mechanical (hardness and tension properties) and mass. The Japan Industrial Standard (JIS) Z 2801:2010 was applied to evaluate antibacterial properties against Staphylococcus aureus (S. aureus) and Escherichia coli (E. coli). The microbiological tests showed a reduction up to 42% in E. coli and up to 49% in S. aureus population in non-aged samples. There were observed variations in elongation and hardness values with the addition of zinc The changes in tensile at rupture and mass were not significant between non-aged and aged samples.Keywords: antimicrobial, domestic appliance, sebs, zinc oxide
Procedia PDF Downloads 247400 Ni-W alloy Coatings: A Promising Electrode Material
Authors: Mr. Liju Elias, A. Chitharanjan Hegde
Abstract:
Ni-W alloy coatings have been developed galvanostatically on copper substrate from tri-sodium citrate bath, using glycerol as the additive. The deposition conditions for production of Ni-W coatings have been optimized for peak performance of their electrocatalytic activity, namely hydrogen evolution reaction (HER) and oxygen evolution reaction (OER). The corrosion behavior of the coatings were tested under working conditions of electrocatalysis (1M KOH). Electrocatalytic behaviours were tested by cyclic voltammetry and chrono-potentiometry techniques. Experimental results demonstrated that Ni-W coatings at low and high current densities (c. d.) showing superior performance for OER and HER respectively. The increased electrocatalytic activity for HER with increase of deposition c. d. was attributed to the phase structure, surface morphology and chemical composition of the coatings, confirmed by XRD, SEM and EDX analysis, respectively. The dependency of hardness and thickness of the coatings on HER and OER were examined, and results were discussed.Keywords: electrocatalytic behavior, HER, Ni-W alloy, OER
Procedia PDF Downloads 417399 Development of Sound Tactile Interface by Use of Human Sensation of Stiffness
Authors: K. Doi, T. Nishimura, M. Umeda
Abstract:
There are very few sound interfaces that both healthy people and hearing handicapped people can use to play together. In this study, we developed a sound tactile interface that makes use of the human sensation of stiffness. The interface comprises eight elastic objects having varying degrees of stiffness. Each elastic object is shaped like a column. When people with and without hearing disabilities press each elastic object, different sounds are produced depending on the stiffness of the elastic object. The types of sounds used were “Do Re Mi sounds.” The interface has a major advantage in that people with or without hearing disabilities can play with it. We found that users were able to recognize the hardness sensation and relate it to the corresponding Do Re Mi sounds.Keywords: tactile sense, sound interface, stiffness perception, elastic object
Procedia PDF Downloads 285398 Mathematical Analysis of Matrix and Filler Formulation in Composite Materials
Authors: Olusegun A. Afolabi, Ndivhuwo Ndou
Abstract:
Composite material is an important area that has gained global visibility in many research fields in recent years. Composite material is the combination of separate materials with different properties to form a single material having different properties from the parent materials. Material composition and combination is an important aspect of composite material. The focus of this study is to provide insight into an easy way of calculating the compositions and formulations of constituent materials that make up any composite material. The compositions of the matrix and filler used for fabricating composite materials are taken into consideration. From the composite fabricated, data can be collected and analyzed based on the test and characterizations such as tensile, flexural, compression, impact, hardness, etc. Also, the densities of the matrix and the filler with regard to their constituent materials are discussed.Keywords: composite material, density, filler, matrix, percentage weight, volume fraction
Procedia PDF Downloads 68397 Groundwater Quality Assessment in the Vicinity of Tannery Industries in Warangal, India
Authors: Mohammed Fathima Shahanaaz, Shaik Fayazuddin, M. Uday Kiran
Abstract:
Groundwater quality is deteriorating day by day in different parts of the world due to various reasons, toxic chemicals are being discharged without proper treatment into inland water bodies and land which in turn add pollutants to the groundwater. In this kind of situation, the rural communities which do not have municipal drinking water have to rely on groundwater though it is polluted for various uses. Tannery industry is one of the major industry which provides economy and employment to India. Since most of the developed countries stopped using chemicals which are toxic, the tanning industry which uses chromium as its major element are being shifted towards developing countries. Most of the tanning industries in India can be found in clusters concentrated mainly in states of Tamilnadu, West Bengal, Uttar Pradesh and limited places of Punjab. Limited work is present in the case of tanneries of Warangal. There exists 18 group of tanneries in Desaipet, Enamamula region of Warangal, out of which 4 are involved in dry process and are low responsible for groundwater pollution. These units of tanneries are discharging their effluents after treatment into Sai Cheruvu. Though the treatment effluents are being discharged, the Sai Cheruvu is turned in to Pink colour, with higher levels of BOD, COD, chromium, chlorides, total hardness, TDS and sulphates. An attempt was made to analyse the groundwater samples around this polluted Sai Cheruvu region since literature shows that a single tannery can pollute groundwater to a radius of 7-8 kms from the point of disposal. Sample are collected from 6 different locations around Sai Cheruvu. Analysis was performed for determining various constituents in groundwater such as pH, EC, TDS, TH, Ca+2, Mg+2, HCO3-, Na+, K+, Cl-, SO42-, NO3-, F and Cr+6. The analysis of these constitutes gave values greater than permissible limits. Even chromium is also present in groundwater samples which is exceeding permissible limits People in Paidepally and Sardharpeta villages already stopped the usage of groundwater. They are buying bottle water for drinking purpose. Though they are not using groundwater for drinking purpose complaints are made about using this water for washing also. So treatment process should be adopted for groundwater which should be simple and efficient. In this study rice husk silica (RHS) is used to treat pollutants in groundwater with varying dosages of RHS and contact time. Rice husk is treated, dried and place in a muffle furnace for 6 hours at 650°C. Reduction is observed in total hardness, chlorides and chromium levels are observed after the application RHS. Pollutants reached permissible limits for 27.5mg/l and 50 mg/l of dosage for a contact time of 130 min at constant pH and temperature.Keywords: chromium, groundwater, rice husk silica, tanning industries
Procedia PDF Downloads 202396 Characterization of Thixoformed AlSi12 Alloy with the Addition of Trace Amounts of Silver
Authors: Nursen Saklakoglu, Adnan Turker
Abstract:
The main objective of this study is to reveal the effect of the Thixoforming process on the microstructure and mechanical properties of the AlSi12 alloy with trace amounts of silver. It is concluded that Thixoforming has an important effect on the morphology of intermetallics and Si formation, as well as globular α-Al morphology. The intermetallics have been fractured during thixoforming. It is believed that the fine distribution of the intermetallics is one mechanism for the improved mechanical properties of Thixoformed alloys. The discrete Si particles have been observed during both isothermal heating to the semi-solid range and Thixoforming, also have an important effect on mechanical properties. The Thixoforming process has a greater effect on hardness than the addition of Ag does.Keywords: AlSi alloys, intermetallic phases, mechanical properties trace element, silver, thixoforming
Procedia PDF Downloads 326395 Characterization of Sintered Fe-Cr-Mn Powder Mixtures Containing Intermetallics
Authors: A. Yonetken, A. Erol, M. Cakmakkaya
Abstract:
Intermetallic materials are among advanced technology materials that have outstanding mechanical and physical properties for high temperature applications. Especially creep resistance, low density and high hardness properties stand out in such intermetallics. The microstructure, mechanical properties of %88Ni-%10Cr and %2Mn powders were investigated using specimens produced by tube furnace sintering at 900-1300°C temperature. A composite consisting of ternary additions, a metallic phase, Fe ,Cr and Mn have been prepared under Ar shroud and then tube furnace sintered. XRD, SEM (Scanning Electron Microscope), were investigated to characterize the properties of the specimens. Experimental results carried out for composition %88Ni-%10Cr and %2Mn at 1300°C suggest that the best properties as 138,80HV and 6,269/cm3 density were obtained at 1300°C.Keywords: composite, high temperature, intermetallic, sintering
Procedia PDF Downloads 409394 A Study on Behaviour of Normal Strength Concrete and High Strength Concrete Subjected to Elevated Temperatures
Authors: Butchi Kameswara Rao Chittem, Rooban Kumar
Abstract:
Cement concrete is a complex mixture of different materials. Concrete is believed to have a good fire resistance. Behaviour of concrete depends on its mix proportions and its constituent materials when it is subjected to elevated temperatures. Loss in compressive strength, loss in weight or mass, change in colour and spall of concrete are reported in literature as effects of elevated temperature on concrete. In this paper results are reported on the behaviour of normal strength concrete and high strength concrete subjected to temperatures 200°C, 400°C, 600°C, and 800°C and different cooling regimes viz. air cooling, water quenching. Rebound hammer test was also conducted to study the changes in surface hardness of concrete specimens subjected to elevated temperatures.Keywords: normal strength concrete, high-strength concrete, temperature, NDT
Procedia PDF Downloads 441