Search results for: iron doped zeolite
1618 Synthesis of Iron Oxide Doped Zeolite: An Antimicrobial Nanomaterial for Drinking Water Purification Applications
Authors: Muhammad Zeeshan, Rabia Nazir, Lubna Tahir
Abstract:
Low cost filter based on iron doped zeolite (Fe-Z) and pottery clay was developed for an effective and efficient treatment of the drinking water contaminated with microbes. Fe-Z was characterized using powder XRD, SEM and EDX and shown to have average particle size of 49 nm with spongy appearance. The simulated samples of water self-contaminated with six microbes (S. typhi, B. subtilus, E. coli, S. aures, K. pneumoniae, and P. aeruginosa) after treatment with Fe-Z indicated effective removal of all the microbes in less than 30 min. Equally good results were obtained when actual drinking water samples, totally unfit for human consumption, were treated with Fe-Z.Keywords: iron doped zeolite, biological and chemical treatment, drinking water
Procedia PDF Downloads 4481617 Zeolite Supported Iron-Sensitized TIO₂ for Tetracycline Photocatalytic Degradation under Visible Light: A Comparison between Doping and Ion Exchange
Authors: Ghadeer Jalloul, Nour Hijazi, Cassia Boyadjian, Hussein Awala, Mohammad N. Ahmad, Ahmad Albadarin
Abstract:
In this study, we applied Fe-sensitized TiO₂ supported over embryonic Beta zeolite (BEA) zeolite for the photocatalytic degradation of Tetracycline (TC) antibiotic under visible light. Four different samples having 20, 40, 60, and 100% w/w as a ratio of TiO₂/BEA were prepared. The immobilization of solgel TiO₂ (33 m²/g) over BEA (390 m²/g) increased its surface area to (227 m²/g) and enhanced its adsorption capacity from 8% to 19%. To expand the activity of TiO₂ photocatalyst towards the visible light region (λ>380 nm), we explored two different metal sensitization techniques with Iron ions (Fe³⁺). In the ion-exchange method, the substitutional cations in the zeolite in TiO₂/BEA were exchanged with (Fe³⁺) in an aqueous solution of FeCl₃. In the doping technique, solgel TiO₂ was doped with (Fe³⁺) from FeCl₃ precursor during its synthesis and before its immobilization over BEA. (Fe-TiO₂/BEA) catalysts were characterized using SEM, XRD, BET, UV-VIS DRS, and FTIR. After testing the performance of the various ion-exchanged catalysts under blue and white lights, only (Fe-TiO₂/BEA 60%) showed better activity as compared to pure TiO₂ under white light with 100 ppm initial catalyst concentration and 20 ppm TC concentration. As compared to ion-exchanged (Fe-TiO₂/BEA), doped (Fe-TiO₂/BEA) resulted in higher photocatalytic efficiencies under blue and white lights. The 3%-Fe-doped TiO₂/BEA removed 92% of TC compared to 54% by TiO₂ under white light. The catalysts were also tested under real solar irradiations. This improvement in the photocatalytic performance of TiO₂ was due to its higher adsorption capacity due to BEA support combined with the presence of Iron ions that enhance the visible light absorption and minimize the recombination effect by the charge carriers. Keywords: Tetracycline, photocatalytic degradation, immobilized TiO₂, zeolite, iron-doped TiO₂, ion-exchange
Procedia PDF Downloads 1061616 Advanced Humidity Sensors Using Cobalt and Iron-Doped ZnO-rGO Composites
Authors: Wallia Majeed
Abstract:
Humidity sensors based on doped ZnO-rGO composites have shown promise due to their sensitivity to humidity changes. Here, it report on the hydrothermal synthesis of ZnO-rGO and doped ZnO-rGO nanocomposites, incorporating cobalt and iron dopants at 2% concentration. X-ray diffraction confirmed successful doping, while scanning electron microscopy revealed the composite's layered structure with embedded ZnO rods. To evaluate their performance, humidity sensors were fabricated by depositing aluminum electrodes on silicon substrates coated with the composites. The Fe-doped ZnO-rGO sensor exhibited rapid response (27 s) and recovery times (24 s) across a wide humidity range (11% to 97% RH), surpassing ZnO-rGO and Co-doped ZnO-rGO variants in sensitivity (2.2k at 100 Hz). These findings highlight Fe-doped ZnO-rGO composites as ideal candidates for humidity sensing applications, offering enhanced performance crucial for environmental monitoring and industrial processes.Keywords: humidity sensors, nanocomposites, hydrothermal synthesis, sensitivity
Procedia PDF Downloads 351615 Design and Synthesis of Copper Doped Zeolite Composite for Antimicrobial Activity and Heavy Metal Removal from Waste Water
Authors: Feleke Terefe Fanta
Abstract:
The existence of heavy metals and microbial contaminants in aquatic system of Akaki river basin, a sub city of Addis Ababa, has become a public concern as human population increases and land development continues. This is because effluents from chemical and pharmaceutical industries are directly discharged onto surrounding land, irrigation fields and surface water bodies. In the present study, we synthesised zeolites and copper- zeolite composite based adsorbent through cost effective and simple approach to mitigate the problem. The study presents determination of heavy metal content and microbial contamination level of waste water sample collected from Akaki river using zeolites and copper- doped zeolites as adsorbents. The synthesis of copper- zeolite X composite was carried out by ion exchange method of copper ions into zeolites frameworks. The optimum amount of copper ions loaded into the zeolites frameworks were studied using the pore size determination concept via iodine test. The copper- loaded zeolites were characterized by X-ray diffraction (XRD). The XRD analysis showed clear difference in phase purity of zeolite before and after copper ion exchange. The concentration of Cd, Cr, and Pb were determined in waste water sample using atomic absorption spectrophotometry. The mean concentrations of Cd, Cr, and Pb in untreated sample were 0.795, 0.654 and 0.7025 mg/L respectively. The concentration of Cd, Cr, and Pb decreased to 0.005, 0.052 and BDL mg/L for sample treated with bare zeolite X while a further decrease in concentration of Cd, Cr, and Pb (0.005, BDL and BDL) mg/L respectively was observed for the sample treated with copper- zeolite composite. The antimicrobial activity was investigated by exposing the total coliform to the Zeolite X and Copper-modified Zeolite X. Zeolite X and Copper-modified Zeolite X showed complete elimination of microbilas after 90 and 50 minutes contact time respectively. This demonstrates effectiveness of copper- zeolite composite as efficient disinfectant. To understand the mode of heavy metals removal and antimicrobial activity of the copper-loaded zeolites; the adsorbent dose, contact time, temperature was studied. Overall, the results obtained in this study showed high antimicrobial disinfection and heavy metal removal efficiencies of the synthesized adsorbent.Keywords: waste water, copper doped zeolite x, adsorption heavy metal, disinfection
Procedia PDF Downloads 811614 Ultrathin Tin-Silicalite 1 Zeolite Membrane in Ester Solvent Recovery
Authors: Kun Liang Ang, Eng Toon Saw, Wei He, Xuecheng Dong, Seeram Ramakrishna
Abstract:
Ester solvents are widely used in pharmaceutical, printing and flavor industry due to their good miscibility, low toxicity, and high volatility. Through pervaporation, these ester solvents can be recovered from industrial wastewater. While metal-doped silicalite 1 zeolite membranes are commonly used in organic solvent recovery in the pervaporation process, these ceramic membranes suffer from low membrane permeation flux, mainly due to the high thickness of the metal-doped zeolite membrane. Herein, a simple method of fabricating an ultrathin tin-silicalite 1 membrane supported on alumina tube is reported. This ultrathin membrane is able to achieve high permeation flux and separation factor for an ester in a diluted aqueous solution. Nanosized tin-Silicalite 1 seeds which are smaller than 500nm has been formed through hydrothermal synthesis. The sn-Silicalite 1 seeds were then seeded onto alumina tube through dip coating, and the tin-Silicalite 1 membrane was then formed by hydrothermal synthesis in an autoclave through secondary growth method. Multiple membrane synthesis factors such as seed size, ceramic substrate surface pore size selection, and secondary growth conditions were studied for their effects on zeolite membrane growth. The microstructure, morphology and the membrane thickness of tin-Silicalite 1 zeolite membrane were examined. The membrane separation performance and stability will also be reported.Keywords: ceramic membrane, pervaporation, solvent recovery, Sn-MFI zeolite
Procedia PDF Downloads 1891613 Enhancement of CO2 Capture by Using Cu-Nano-Zeolite Synthesized
Authors: Pham-Thi Huong, Byeong-Kyu Lee, Chi-Hyeon Lee, Jitae Kim
Abstract:
In this study synthesized Cu-nano-zeolite was evaluated for its potential use in CO2 capture. The specific surface area of Cu-nano zeolite was measured as 869.32 m2/g with a pore size of 3.86 nm. The adsorption capacity of CO2 by Cu-nano zeolite was decreased with increasing temperature. The identified adsorption capacity of CO2 by Cu-nano zeolite was 7.16 mmol/g at a temperature of 20 oC and at pressure of 1 atm. The adoption selectivity of CO2 over N2 strongly depend on the temperature and the highest selectivity by Cu-nano zeolite was 50.71 at 20 oC. From analysis of regeneration characteristics of CO2 loaded adsorbent, the percentage removal of CO2 was maintained at more than 78.2 % even after 10 cycles of adsorption-desorption. Based on these result, the Cu-nano zeolite can be used as an effective and economical adsorbent for CO2 capture.Keywords: CO2 capture, selectivity, Cu-nano zeolite, regeneration.
Procedia PDF Downloads 3201612 Design and Synthesis of Copper-Zeolite Composite for Antimicrobial Activity and Heavy Metal Removal From Waste Water
Authors: Feleke Terefe Fanta
Abstract:
Background: The existence of heavy metals and coliform bacteria contaminants in aquatic system of Akaki river basin, a sub city of Addis Ababa, Ethiopia has become a public concern as human population increases and land development continues. Hence, it is the right time to design treatment technologies that can handle multiple pollutants. Results: In this study, we prepared a synthetic zeolites and copper doped zeolite composite adsorbents as cost effective and simple approach to simultaneously remove heavy metals and total coliforms from wastewater of Akaki river. The synthesized copper–zeolite X composite was obtained by ion exchange method of copper ions into zeolites frameworks. Iodine test, XRD, FTIR and autosorb IQ automated gas sorption analyzer were used to characterize the adsorbents. The mean concentrations of Cd, Cr, and Pb in untreated sample were 0.795, 0.654 and 0.7025 mg/L respectively. These concentrations decreased to Cd (0.005 mg/L), Cr (0.052 mg/L) and Pb (bellow detection limit, BDL) for sample treated with bare zeolite X while a further decrease in concentration of Cd (0.005 mg/L), Cr (BDL) and Pb (BDL) was observed for the sample treated with copper–zeolite composite. Zeolite X and copper-modified zeolite X showed complete elimination of total coliforms after 90 and 50 min contact time respectively. Conclusion: The results obtained in this study showed high antimicrobial disinfection and heavy metal removal efficiencies of the synthesized adsorbents. Furthermore, these sorbents are efficient in significantly reducing physical parameters such as electrical conductivity, turbidity, BOD and COD.Keywords: WASTE WATER, COPPER DOPED ZEOITE X, ADSORPITION, HEAVY METAL, DISINFECTION, AKAKI RIVER
Procedia PDF Downloads 691611 Characterization of Iron Doped Titanium Dioxide Nanoparticles and Its Photocatalytic Degradation Ability for Congo Red Dye
Authors: Vishakha Parihar
Abstract:
This study reports the preparation of iron metal-doped nanoparticles of Titanium dioxide by the sol-gel process and the photocatalytic degradation of dye. Nano-particles were characterized by SEM, EDX, and UV-Vis spectroscopy. The detailed study confirmed that nanoparticles have grown in high density and have good optical properties. The photocatalytic batch experiment was performed in an aqueous solution where congo red dye was used as a dye pollutant under the irradiation of ultraviolet rays created by using a mercury lamp source. Total degradation efficiency achieved was approximately 85% to 93% in the duration of 100-120 minutes of irradiation under an ultraviolet light source. The decolorization ability of this process was measured by absorbance at a maximum wavelength of 498nm. The results indicated that the iron-doped Titanium dioxide nanoparticles showed an excellent photocatalytic response to the degradation of dye under the ultraviolet light source within a very short period of time.Keywords: titanium dioxide, nano-particles iron dope, photocatalytic degradation, Congo red dye, sol-gel process
Procedia PDF Downloads 1831610 Isotherm Study of Modified Zeolite in Sorption of Naphthalene from Water Sample
Authors: Homayon Ahmad Panahi, Amir Hesam Hassani, Akram Torki, Elham Moniri
Abstract:
A new sorbent was synthesized through chemical modification of clinoptilolite zeolite using 2-naphtol, and characterized with fourier transform infrared spectroscopy and elemental analysis methods and applied for the removal and elimination of trace naphthalene from water samples. The optimum pH value for sorption of the naphthalene by modified zeolite was in acidic pH. The sorption capacity of modified zeolite was 142 mg. g−1. Isotherm models, Langmuir, Frendlich and Temkin were employed to analyze the adsorption capacity of modified zeolite, which revealed that naphthalene adsorption by this zeolite follows Langmuir model.Keywords: zeolite, clinoptilolite, modification, naphthalene
Procedia PDF Downloads 4891609 Recovery of Cd (II) and Pb (II) under the Effect of Temperature with the Synthetic Zeolite NaA
Authors: Karima Menad, Ahmed Feddag
Abstract:
In this study, large crystals of the zeolite NaA were synthesized by hydrothermal way. By following this zeolite was used to recover two heavy metals that are allowing the most dangerous toxic, lead and cadmium. The synthesized zeolite was analyzed by XRD and SEM aims to verify its purity and its good morphology; after it was undergoing ion exchange operations by aqueous solution with lead and cadmium in two salts Pb(CH3COOH)2 and CdCl2 at different concentrations. The exchange was carried out under the effect of two temperatures (25 °C and 60 °C). The contents of Pb++, Cd++ and Na+ were analyzed by atomic absorption and the results are given in the form of exchange rates. At the end the samples are analyzed by XRD exchanged to confirm their conservation of their zeolite framework. It is found that the exchange rate increases with the increase of initial concentration and the best results are found for the temperature of 60 °C.Keywords: exchange rate, ion exchange, LTA zeolite, zeolite NaA
Procedia PDF Downloads 4141608 Possibilities of Utilization Zeolite in Concrete
Authors: M. Sedlmajer, J. Zach, J. Hroudova, P. Rovnaníkova
Abstract:
There are several possibilities of reducing the required amount of cement in concrete production. Natural zeolite is one of the raw materials which can partly substitute Portland cement. The effort to reduce the amount of Portland cement used in concrete production is brings both economical as well as ecological benefits. The paper presents the properties of concrete containing natural zeolite as an active admixture in the concrete which partly substitutes Portland cement. The properties discussed here bring information about the basic mechanical properties and frost resistance of concrete containing zeolite. The properties of concretes with the admixture of zeolite are compared with a reference concrete with no content of zeolite. The properties of the individual concretes are observed for 360 days.Keywords: concrete, zeolite, compressive strength, modulus of elasticity, durability
Procedia PDF Downloads 3681607 Synchrotron X-Ray Based Investigation of Fe Environment in Porous Anode of Shewanella oneidensis Microbial Fuel Cell
Authors: Sunil Dehipawala, Gayathrie Amarasuriya, N. Gadura, G. Tremberger Jr, D.Lieberman, Harry Gafney, Todd Holden, T. Cheung
Abstract:
The iron environment in Fe-doped Vycor Anode was investigated with EXAFS using Brookhaven Synchrotron Light Source. The iron-reducing Shewanella oneidensis culture was grown in a microbial fuel cell under anaerobic respiration. The Fe bond length was found to decrease and correlate with the amount of biofilm growth on the Fe-doped Vycor Anode. The data suggests that Fe-doped Vycor Anode would be a good substrate to study the Shewanella oneidensis nanowire structure using EXAFS.Keywords: EXAFS, fourier transform, Shewanella oneidensis, microbial fuel cell
Procedia PDF Downloads 4011606 Removal of P-Nitrophenol in Wastewater by Using Fe-Nano Zeolite Synthesized
Authors: Pham-Thi Huong, Byeong-Kyu Lee, Chi-Hyeon Lee, JiTae Kim
Abstract:
This study analyzed the removal of p-nitrophenol from wastewater using Fe-nano zeolite synthesized. The basic physical-chemical properties of Fe-nano zeolite was determined by X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy. We focus on finding out the optimum conditions in adsorption and desorption processes for removal of p-nitrophenol by using Fe-nano zeolite in wastewater. The optimum pH for p-nitrophenol removal in wastewater was 5.0. Adsorption isotherms were better fitted with the Langmuir isotherm than with the Freundlich with 165.58 mg/g adsorption capacity of p-nitrophenol. These findings support potential of Fe-nano zeolite as an effective adsorbent for p-nitrophenol removal from wastewater.Keywords: Fe-nano zeolite, adsorption, wastewater, regeneration
Procedia PDF Downloads 3111605 Recovery of Heavy Metals by Ion Exchange on the Zeolite Materials
Abstract:
Zeolites are a family of mineral compounds. With special properties that have led to several important industrial applications. Ion exchange has enabled the first industrial application in the field of water treatment. The exchange by aqueous pathway is the method most used in the case of such microporous materials and this technique will be used in this work. The objective of this work is to find performance materials for the recovery of heavy metals such as cadmium. The study is to compare the properties of different ion exchange zeolite Na-X, Na-A, their physical mixture and the composite A (LTA) / X (FAU). After the synthesis of various zeolites X and A, it was designed a model Core-Shell to form a composite zeolite A on zeolite X. Finally, ion exchange studies were performed on these zeolite materials. The cation is exclusively tested for cadmium, a toxic element and is harmful to health and the environment.Keywords: zeolite A, zeolite X, ion exchange, water treatment
Procedia PDF Downloads 4311604 Porous Carbon Nanoparticels Co-Doped with Nitrogen and Iron as an Efficient Catalyst for Oxygen Reduction Reaction
Authors: Bita Bayatsarmadi, Shi-Zhang Qiao
Abstract:
Oxygen reduction reaction (ORR) performance of iron and nitrogen co-doped porous carbon nanoparticles (Fe-NPC) with various physical and (electro) chemical properties have been investigated. Fe-NPC nanoparticles are synthesized via a facile soft-templating procedure by using Iron (III) chloride hexa-hydrate as iron precursor and aminophenol-formaldehyde resin as both carbon and nitrogen precursor. Fe-NPC nanoparticles shows high surface area (443.83 m2g-1), high pore volume (0.52 m3g-1), narrow mesopore size distribution (ca. 3.8 nm), high conductivity (IG/ID=1.04), high kinetic limiting current (11.71 mAcm-2) and more positive onset potential (-0.106 V) compared to metal-free NPC nanoparticles (-0.295V) which make it high efficient ORR metal-free catalysts in alkaline solution. This study may pave the way of feasibly designing iron and nitrogen containing carbon materials (Fe-N-C) for highly efficient oxygen reduction electro-catalysis.Keywords: electro-catalyst, mesopore structure, oxygen reduction reaction, soft-template
Procedia PDF Downloads 3791603 Determination and Preconcentration of Chromium Ion in Environmental Samples by Clinoptilolite Zeolite
Authors: Elham Moniri, Homayon Ahmad Panahi, Mitra Hoseini
Abstract:
In this research, clinoptilolite zeolite was prepared. The zeolite was characterized by fourier transform infra-red spectroscopy. Then the effects of various parameters on Cr(III) sorption such as pH, contact time were studied. The optimum pH value for sorption of Cr(III) was 6 respectively. The sorption capacity of zeolite for Cr(III) were 7.9 mg g−1. A recovery of 89% was obtained for the metal ions with 0.5 M nitric acid as the eluting agent. The effects of interfering ions on Cr(III) sorption was also investigated. The profile of Cr(III) uptake on this sorbent reflects a good accessibility of the chelating sites in the clinoptilolite zeolite. The developed method was utilized for the determination of Cr(III) in environmental water samples by flame atomic absorption spectrometry with satisfactory results.Keywords: clinoptilolite zeolite, chromium, environmental sample, determination
Procedia PDF Downloads 4441602 Synthesis and Characterization of Zeolite/Fe3O4 Nanocomposite Material and Investigation of Its Catalytic Reaction
Authors: Mojgan Zendehdel, Safura Molla Mohammad Zamani
Abstract:
In this paper, Fe3O4/NaY zeolite nanocomposite with different molar ratio were successfully synthesized and characterized using FT-IR, XRD, TGA, SEM and VSM techniques. The SEM graphs showed that much of Fe3O4 was successfully coated by the NaY zeolite layer. Also, the results show that the magnetism of the products is stable with added zeolite. The catalytic effect of nanocomposite investigated for esterification reaction under solvent-free conditions. Hence, the effect of the catalyst amount, reaction time, reaction temperature and reusability of catalyst were considered and nanocomposite that created from zeolite and 16.6 percent of Fe3O4 showed the highest yield. The catalyst can be easily separated from reaction with the magnet and it can also be used for several times.Keywords: zeolite, magnetic, nanocompsite, esterification
Procedia PDF Downloads 4611601 Preparation of Protective Coating Film on Metal Alloy
Authors: Rana Th. A. Al-rubaye
Abstract:
A novel chromium-free protective coating films based on a zeolite coating was growing onto a FeCrAlloy metal using in –situ hydrothermal method. The zeolite film was obtained using in-situ crystallization process that is capable of coating large surfaces with complex shape and in confined spaces has been developed. The zeolite coating offers an advantage of a high mechanical stability and thermal stability. The physico-chemical properties were investigated using X-ray diffraction (XRD), Electron microscopy (SEM), Energy Dispersive X–ray analysis (EDX) and Thermogravimetric Analysis (TGA). The transition from oxide-on-alloy wires to hydrothermally synthesised uniformly zeolite coated surfaces was followed using SEM and XRD. In addition, the robustness of the prepared coating was confirmed by subjecting these to thermal cycling (ambient to 550°C).Keywords: fecralloy, zsm-5 zeolite, zeolite coatings, hydrothermal method
Procedia PDF Downloads 3951600 Natural Mexican Zeolite Modified with Iron to Remove Arsenic Ions from Water Sources
Authors: Maritza Estela Garay-Rodriguez, Mirella Gutierrez-Arzaluz, Miguel Torres-Rodriguez, Violeta Mugica-Alvarez
Abstract:
Arsenic is an element present in the earth's crust and is dispersed in the environment through natural processes and some anthropogenic activities. Naturally released into the environment through the weathering and erosion of sulphides mineral, some activities such as mining, the use of pesticides or wood preservatives potentially increase the concentration of arsenic in air, water, and soil. The natural arsenic release of a geological material is a threat to the world's drinking water sources. In aqueous phase is found in inorganic form, as arsenate and arsenite mainly, the contamination of groundwater by salts of this element originates what is known as endemic regional hydroarsenicism. The International Agency for Research on Cancer (IARC) categorizes the inorganic As within group I, as a substance with proven carcinogenic action for humans. It has been found the presence of As in groundwater in several countries such as Argentina, Mexico, Bangladesh, Canada and the United States. Regarding the concentration of arsenic in drinking water according to the World Health Organization (WHO) and the Environmental Protection Agency (EPA) establish maximum concentrations of 10 μg L⁻¹. In Mexico, in some states as Hidalgo, Morelos and Michoacán concentrations of arsenic have been found in bodies of water around 1000 μg L⁻¹, a concentration that is well above what is allowed by Mexican regulations with the NOM-127- SSA1-1994 that establishes a limit of 25 μg L⁻¹. Given this problem in Mexico, this research proposes the use of a natural Mexican zeolite (clinoptilolite type) native to the district of Etla in the central valley region of Oaxaca, as an adsorbent for the removal of arsenic. The zeolite was subjected to a conditioning with iron oxide by the precipitation-impregnation method with 0.5 M iron nitrate solution, in order to increase the natural adsorption capacity of this material. The removal of arsenic was carried out in a column with a fixed bed of conditioned zeolite, since it combines the advantages of a conventional filter with those of a natural adsorbent medium, providing a continuous treatment, of low cost and relatively easy to operate, for its implementation in marginalized areas. The zeolite was characterized by XRD, SEM/EDS, and FTIR before and after the arsenic adsorption tests, the results showed that the modification methods used are adequate to prepare adsorbent materials since it does not modify its structure, the results showed that with a particle size of 1.18 mm, an initial concentration of As (V) ions of 1 ppm, a pH of 7 and at room temperature, a removal of 98.7% was obtained with an adsorption capacity of 260 μg As g⁻¹ zeolite. The results obtained indicated that the conditioned zeolite is favorable for the elimination of arsenate in water containing up to 1000 μg As L⁻¹ and could be suitable for removing arsenate from pits of water.Keywords: adsorption, arsenic, iron conditioning, natural zeolite
Procedia PDF Downloads 1721599 Phenol Degradation via Photocatalytic Oxidation Using Fe Doped TiO₂
Authors: Sherif Ismail
Abstract:
Degradation of phenol-contaminated wastewater using Photocatalytic oxidation process was investigated in batch experiments using Fe doped TiO₂. Moreover, the effect of oxygen aeration on the performance of photocatalytic oxidation process by iron (Fe⁺²) doped titanium dioxide (TiO₂) was assessed. Photocatalytic oxidation using Fe doped TiO₂ effectively reduce the phenol concentration in wastewater with optimum condition of light intensity, pH, catalyst-dosing and initial concentration of phenol were 50 W/m2, 5.3, 600 mg/l and 10 mg/l respectively. The results obtained that removal efficiency of phenol was 88% after 180 min in case of N₂ addition. However, aeration by oxygen resulted in a 99% removal efficiency in 120 min. The results of photo-catalysis oxidation experiments fitted the pseudo-first-order kinetic equation with high correlation. Costs estimation of 30 m3/d full-scale photo-catalysis oxidation plant was assessed.Keywords: phenol degradation, Fe-doped TiO2, AOPs, cost analysis
Procedia PDF Downloads 1631598 Improvement in Ni (II) Adsorption Capacity by Using Fe-Nano Zeolite
Authors: Pham-Thi Huong, Byeong-Kyu Lee, Jitae Kim, Chi-Hyeon Lee
Abstract:
Fe-nano zeolite adsorbent was used for removal of Ni (II) ions from aqueous solution. The adsorbent was characterized by Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM) and the surface area Brunauer–Emmett–Teller (BET) using for analysis of functional groups, morphology and surface area. Bath adsorption experiments were analyzed on the effect of pH, time, adsorbent doses and initial Ni (II) concentration. The optimum pH for Ni (II) removal using Fe-nano zeolite was found at 5.0 and 90 min of reaction time. The maximum adsorption capacity of Ni (II) was 231.68 mg/g based on the Langmuir isotherm. The kinetics data for the adsorption process was fitted with the pseudo-second-order model. The desorption of Ni (II) from Ni-loaded Fe-nano zeolite was analyzed and even after 10 cycles 72 % desorption was achieved. These finding supported that Fe-nano zeolite with high adsorption capacity, high reuse ability would be utilized for Ni (II) removal from water.Keywords: Fe-nano zeolite, adsorption, Ni (II) removal, regeneration
Procedia PDF Downloads 2321597 Production of 100 Kg/Day Zeolite a Using Locally Fabricated Crystallizer from Nigeria Ahoko Kaolin
Authors: M. S. Haruna, A. R. Agava, N. J. Sani, A. S. Kovo
Abstract:
The recent effort for cheaper raw material for the production of Zeolite A that is economically beneficial necessitated the reason for this work. The studies explore the use of locally fabricated crystallizer for the production of zeolite A using Nigeria Ahoko Kaolin as the main raw material. To achieve this intention, a systematic chemical engineering approach for the design of processes was adopted. Firstly a unique simplified flowsheet was developed, and then material and energy balance was conducted and finally followed by a detail design of the crystallizer. The summary of the result of the design showed that the optimum design parameters of 0.45 m and 1.125 were obtained for the diameter and height, respectively. The fabricated crystallizer was successfully tested for the production of Zeolite A, which is the expectation of this work.Keywords: Zeolite A, design, crystallizer, Ahoko, Kaolin
Procedia PDF Downloads 891596 Biodiesel Production from Animal Fat Using Trans-Esterification Process with Zeolite as a Solid Catalyst to Improve the Efficiency of Production
Authors: Dinda A. Utami, Muhammad N. Alfarizi
Abstract:
The purpose of this study was to determine the ability of zeolite catalyst for the trans- esterification reaction in biodiesel production from animal fat. The ability of the zeolite as a catalyst is determined by the structure and composition of the zeolite. An important factor that determines the properties of zeolites in catalysis includes adsorption capability to the compound of the reactants. Zeolites with a pore size of specific properties selectively adsorbing molecules. A molecule can be adsorbed by either the zeolite cavities if the size and shape of the molecule in accordance with the size and shape of the cavity in the zeolite. At this time, it is common to use homogeneous catalysts for biodiesel. We know these catalysts have some disadvantages in its use. Such as the difficulty of separation of the product with the catalyst, the generation of waste that is harmful to the environment due to residual catalysts can’t be reused, and the difficulty of handling and storage. But nowadays, solid catalyst developed technically to improve the efficiency of biodiesel production. In this case of study, we used trans-esterification process wherein the triglyceride is reacted with an alcohol with zeolite as a solid catalyst and it will produce biodiesel and glycerol as a byproduct. Development of solid catalyst seems to be the perfect solution to address the problems associated with homogeneous catalysts.Keywords: biodiesel, animal fat, trans esterification, zeolite catalyst
Procedia PDF Downloads 2601595 Dissolution of Zeolite as a Sorbent in Flue Gas Desulphurization Process Using a pH Stat Apparatus
Authors: Hilary Rutto, John Kabuba
Abstract:
Sulphur dioxide is a harmful gaseous product that needs to be minimized in the atmosphere. This research work investigates the use of zeolite as a possible additive that can improve the sulphur dioxide capture in wet flue gas desulphurisation dissolution process. This work determines the effect of temperature, solid to liquid ratio, acid concentration and stirring speed on the leaching of zeolite using a pH stat apparatus. The atomic absorption spectrometer was used to measure the calcium ions from the solution. It was found that the dissolution rate of zeolite decreased with increase in solid to liquid ratio and increases with increase in temperature, stirring speed and acid concentration. The activation energy for the dissolution rate of zeolite in hydrochloric acid was found to be 9.29kJ/mol. and therefore the product layer diffusion was the rate limiting step.Keywords: calcium ion, pH stat apparatus, wet flue gas desulphurization, zeolite
Procedia PDF Downloads 2841594 Adsorptive Desulfurization of Using Cu(I) – Y Zeolite via π-Complexation
Authors: Moshe Mello, Hilary Rutto, Tumisang Seodigeng, Itumeleng Kohitlhetse
Abstract:
The accelerating requirement to reach 0% sulfur content in liquid fuels demand researchers to seek efficient alternative technologies to challenge the predicament. In this current study, the adsorption capabilities of modified Cu(I)-Y zeolite were tested for the removal of organosulfur compounds (OSC) present in tire pyrolytic oil (TPO). The π-complexation-based adsorbent was obtained by ion exchanging Y-zeolite with Cu+ cation using liquid phase ion exchange (LPIE). Preparation of the adsorbent involved firstly ion exchange between Na-Y zeolite with a Cu(NO₃)₂ aqueous solution of 0.5M for 48 hours followed by reduction of Cu²⁺ to Cu+. Fixed-bed breakthrough studies for TPO in comparison with model diesel comprising of sulfur compounds such as thiophene, benzothiophenes (BT), and dibenzothiophenes (DBT) showed that modified Cu(I)-Y zeolite is an effective adsorbent for removal of OSC in liquid fuels. The effect of operating conditions such as adsorbent dosage and reaction time were studied to optimize the adsorptive desulfurization process. For model diesel fuel, the selectivity for adsorption of sulfur compounds followed the order DBT> BT> Thiophene. The Cu(I)-Y zeolite is fully regeneratable and this is achieved by a simple procedure of blowing the adsorbent with air at 350 °C, followed by reactivation at 450 °C in a rich helium surrounding.Keywords: adsorption, desulfurization, TPO, zeolite
Procedia PDF Downloads 1141593 Iron Doped Biomaterial Calcium Borate: Synthesis and Characterization
Authors: G. Çelik Gül, F. Kurtuluş
Abstract:
Colemanite is the most common borate mineral, and the main source of the boron required by plants, human, and earth. Transition metals exhibit optical and physical properties such as; non-linear optical character, structural diversity, thermal stability, long cycle life and luminescent radiation. The doping of colemanite with a transition metal, bring it very interesting and attractive properties which make them applicable in industry. Iron doped calcium borate was synthesized by conventional solid state method at 1200 °C for 12 h with a systematic pathway. X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy/energy dispersive analyze (SEM/EDS) were used to characterize structural and morphological properties. Also, thermal properties were recorded by thermogravimetric-differential thermal analysis (TG/DTA).Keywords: colemanite, conventional synthesis, powder x-ray diffraction, borates
Procedia PDF Downloads 3321592 Thermal Decomposition Behaviors of Hexafluoroethane (C2F6) Using Zeolite/Calcium Oxide Mixtures
Authors: Kazunori Takai, Weng Kaiwei, Sadao Araki, Hideki Yamamoto
Abstract:
HFC and PFC gases have been commonly and widely used as refrigerant of air conditioner and as etching agent of semiconductor manufacturing process, because of their higher heat of vaporization and chemical stability. On the other hand, HFCs and PFCs gases have the high global warming effect on the earth. Therefore, we have to be decomposed these gases emitted from chemical apparatus like as refrigerator. Until now, disposal of these gases were carried out by using combustion method like as Rotary kiln treatment mainly. However, this treatment needs extremely high temperature over 1000 °C. In the recent year, in order to reduce the energy consumption, a hydrolytic decomposition method using catalyst and plasma decomposition treatment have been attracted much attention as a new disposal treatment. However, the decomposition of fluorine-containing gases under the wet condition is not able to avoid the generation of hydrofluoric acid. Hydrofluoric acid is corrosive gas and it deteriorates catalysts in the decomposition process. Moreover, an additional process for the neutralization of hydrofluoric acid is also indispensable. In this study, the decomposition of C2F6 using zeolite and zeolite/CaO mixture as reactant was evaluated in the dry condition at 923 K. The effect of the chemical structure of zeolite on the decomposition reaction was confirmed by using H-Y, H-Beta, H-MOR and H-ZSM-5. The formation of CaF2 in zeolite/CaO mixtures after the decomposition reaction was confirmed by XRD measurements. The decomposition of C2F6 using zeolite as reactant showed the closely similar behaviors regardless the type of zeolite (MOR, Y, ZSM-5, Beta type). There was no difference of XRD patterns of each zeolite before and after reaction. On the other hand, the difference in the C2F6 decomposition for each zeolite/CaO mixtures was observed. These results suggested that the rate-determining process for the C2F6 decomposition on zeolite alone is the removal of fluorine from reactive site. In other words, the C2F6 decomposition for the zeolite/CaO improved compared with that for the zeolite alone by the removal of the fluorite from reactive site. HMOR/CaO showed 100% of the decomposition for 3.5 h and significantly improved from zeolite alone. On the other hand, Y type zeolite showed no improvement, that is, the almost same value of Y type zeolite alone. The descending order of C2F6 decomposition was MOR, ZSM-5, beta and Y type zeolite. This order is similar to the acid strength characterized by NH3-TPD. Hence, it is considered that the C-F bond cleavage is closely related to the acid strength.Keywords: hexafluoroethane, zeolite, calcium oxide, decomposition
Procedia PDF Downloads 4811591 Structural and Magnetic Properties of Undoped and Ni Doped CdZnS
Authors: Sabit Horoz, Ahmet Ekicibil, Omer Sahin, M. Akyol
Abstract:
In this study, CdZnS and Ni-doped CdZnS quantum dots(QDs) were prepared by the wet-chemical method at room temperature using mercaptoethanol as a capping agent. The structural and magnetic properties of the CdZnS and CdZnS doped with different concentrations of Ni QDs were examined by XRD and magnetic susceptibility measurements, respectively. The average particles size of cubic QDs obtained by full-width half maxima (FWHM) analysis, increases with increasing doping concentrations. The investigation of the magnetic properties showed that the Ni-doped samples exhibit signs of ferromagnetism, on the other hand, un-doped CdZnS is diamagnetic.Keywords: un-doped and Ni doped CdZnS Quantum Dots (QDs), co-precipitation method, structural and optical properties of QDs, diluted magnetic semiconductor materials (DMSMs)
Procedia PDF Downloads 2981590 Reuse of Municipal Solid Waste Incinerator Fly Ash for the Synthesis of Zeolite: Effects of Different Operation Conditions
Authors: Jyh-Cherng Chen, Yi-Jie Lin
Abstract:
This study tries to reuse the fly ash of municipal solid waste incinerator (MSWI) for the synthesis of zeolites. The fly ashes were treated with NaOH alkali fusion at different temperatures for 40 mins and then synthesized the zeolites with hydrothermal method at 105oC for different operation times. The effects of different operation conditions and the optimum synthesis parameters were explored. The specific surface area, surface morphology, species identification, adsorption capacity, and the reuse potentials of the synthesized zeolites were analyzed and evaluated. Experimental results showed that the optimum operation conditions for the synthesis of zeolite from the mixed fly ash were Si/Al=20, alkali/ash=1.5, alkali fusion reaction with NaOH at 800oC for 40 mins, hydrolysis with L/S=200 at 105oC for 24 hr, and hydrothermal synthesis at 105oC for 48 hr. The largest specific surface area of synthesized zeolite could be increased to 943.05m2/g. The influence of different operation parameters on the synthesis of zeolite from mixed fly ash followed the sequence of Si/Al > hydrolysis L/S> hydrothermal time > alkali fusion temperature > alkali/ash ratio. The XRD patterns of synthesized zeolites were identified to be similar with the ZSM-23 zeolite. The adsorption capacities of synthesized zeolite for pollutants were increased as rising the specific surface area of synthesized zeolite. In summary, MSWI fly ash can be treated and reused to synthesize the zeolite with high specific surface area by the alkali fusion and hydrothermal method. The zeolite can be reuse for the adsorption of various pollutants. They have great potential for development.Keywords: alkali fusion, hydrothermal, fly ash, zeolite
Procedia PDF Downloads 1741589 Generation of Catalytic Films of Zeolite Y and ZSM-5 on FeCrAlloy Metal
Authors: Rana Th. A. Al-Rubaye, Arthur A. Garforth
Abstract:
This work details the generation of thin films of structured zeolite catalysts (ZSM–5 and Y) onto the surface of a metal substrate (FeCrAlloy) using in-situ hydrothermal synthesis. In addition, the zeolite Y is post-synthetically modified by acidified ammonium ion exchange to generate US-Y. Finally the catalytic activity of the structured ZSM-5 catalyst films (Si/Al = 11, thickness 146 µm) and structured US–Y catalyst film (Si/Al = 8, thickness 23µm) were compared with the pelleted powder form of ZSM–5 and USY catalysts of similar Si/Al ratios. The structured catalyst films have been characterised using a range of techniques, including X-ray diffraction (XRD), Electron microscopy (SEM), Energy Dispersive X–ray analysis (EDX) and Thermogravimetric Analysis (TGA). The transition from oxide-on-alloy wires to hydrothermally synthesised uniformly zeolite coated surfaces was followed using SEM and XRD. In addition, the robustness of the prepared coating was confirmed by subjecting these to thermal cycling (ambient to 550°C). The cracking of n–heptane over the pellets and structured catalysts for both ZSM–5 and Y zeolite showed very similar product selectivities for similar amounts of catalyst with an apparent activation energy of around 60 kJ mol-1. This paper demonstrates that structured catalysts can be manufactured with excellent zeolite adherence and when suitably activated/modified give comparable cracking results to the pelleted powder forms. These structured catalysts will improve temperature distribution in highly exothermic and endothermic catalysed processes.Keywords: FeCrAlloy, structured catalyst, zeolite Y, zeolite ZSM-5
Procedia PDF Downloads 380