Search results for: Bio-based polyol
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 67

Search results for: Bio-based polyol

67 Biobased Polyurethane Derived from Transesterified Castor Oil: Synthesis and Charecterization

Authors: Sonalee Das, Smita Mohanty, S. K. Nayak

Abstract:

Recent years has witnessed the increasing demand for natural resources and products in polyurethane synthesis because of global warming, sustainable development and oil crisis. For this purpose, different plant oils such as soybean oil, castor oil and linseed oil are extensively used. Moreover, the isocyanate used for the synthesis of polyurethane is derived from petroleum resources. In this present work attempts have been made for the successful synthesis of biobased isocyanate from castor oil with partially biobased isocyanate in presence of catalyst dibutyltin dilaurate (DBTDL). The goal of the present study was to investigate the thermal, mechanical, morphological and chemical properties of the synthesized polyurethane in terms of castor oil modification. The transesterified polyol shows broad and higher hydroxyl value as compared to castor oil which was confirmed by FTIR studies. The FTIR studies also revealed the successful synthesis of bio based polyurethane by showing characteristic peaks at 3300cm-1, 1715cm-1 and 1532cm-1 respectively. The TGA results showed three step degradation mechanism for the synthesized polyurethane from modified and unmodified castor oil. However, the modified polyurethane exhibited higher degradation temperature as compared to unmodified one. The mechanical properties also demonstrated higher tensile strength for modified polyurethane as compared to unmodified one.

Keywords: castor oil, partially biobased Isocyanate, polyurethane synthesis, FTIR

Procedia PDF Downloads 317
66 Newly Developed Epoxy-Polyol and Epoxy- Polyurethane from Renewable Resources

Authors: Akintayo Emmanuel Temitope, Akintayo Cecilia Olufunke, Ziegler Thomas

Abstract:

Bio-polyols are important components in polyurethane industries. The preliminary studies into the synthesis of bio-polyol products (epoxy-polyol and epoxyl-polyurethanes) from Jatropha curcas were investigated. The reactions were followed by both infrared and nuclear magnetic resonance. Physico-chemical characterisation of the samples for iodine value (IV), acid value (AV), saponification value (SV) and hydroxyl value (HV) were carried out. Thermal transitions of the products were studied by heating 5 mg of the sample from 20ºC to 800ºC and then cooling down to -500ºC on a differential scanning calorimeter (DSC). The preparation of epoxylpolyol and polyurethane from Jatropha curcas oil was smooth and efficient. Results of film and solubility properties revealed that coatings of Jatropha curcas epoxy-polyurethanes performed better with increased loading of toluylene 2, 4-diisocyanate (TDI) up to 2 wt% while their solvent resistance decreased beyond a TDI loading of 1.2 wt%. DSC analysis shows the epoxy-polyurethane to be less stable compared to the epoxy-polyol.

Keywords: synthesis, epoxy-polyol, epoxy-polyurethane, jatropha curcas oil

Procedia PDF Downloads 386
65 Synthesis and Use of Bio Polyols in Rigid Polyurethane Foam Production

Authors: A. Esra Pişkin, L. Yusuf Yivlik

Abstract:

Polyurethane consumption in the world increases every year. Polyetherpolyol, which is the main raw material of polyurethane, is produced from petroleum, and bioresources are needed in polyol production due to the damage it causes to the environment and the consumption of too much energy during the production phase. In this present work, bio polyol was synthesized with castor oil and soybean oil, and its use in rigid polyurethane systems was investigated. Transesterification and ring opening methods were applied for polyol synthesis, and the obtained bio polyols were compared with polyols derived petroleum. The goal of the present study was to synthesize biopolyols and to investigate the mechanical, thermal, and chemical properties of the synthesized polyurethane in terms of bio polyols.

Keywords: polyurethane, polyol, biopolyol, vegetable oil, foam, rigid polyurethane foam, ring opening, transesterification

Procedia PDF Downloads 428
64 Measuring Biobased Content of Building Materials Using Carbon-14 Testing

Authors: Haley Gershon

Abstract:

The transition from using fossil fuel-based building material to formulating eco-friendly and biobased building materials plays a key role in sustainable building. The growing demand on a global level for biobased materials in the building and construction industries heightens the importance of carbon-14 testing, an analytical method used to determine the percentage of biobased content that comprises a material’s ingredients. This presentation will focus on the use of carbon-14 analysis within the building materials sector. Carbon-14, also known as radiocarbon, is a weakly radioactive isotope present in all living organisms. Any fossil material older than 50,000 years will not contain any carbon-14 content. The radiocarbon method is thus used to determine the amount of carbon-14 content present in a given sample. Carbon-14 testing is performed according to ASTM D6866, a standard test method developed specifically for biobased content determination of material in solid, liquid, or gaseous form, which requires radiocarbon dating. Samples are combusted and converted into a solid graphite form and then pressed onto a metal disc and mounted onto a wheel of an accelerator mass spectrometer (AMS) machine for the analysis. The AMS instrument is used in order to count the amount of carbon-14 present. By submitting samples for carbon-14 analysis, manufacturers of building materials can confirm the biobased content of ingredients used. Biobased testing through carbon-14 analysis reports results as percent biobased content, indicating the percentage of ingredients coming from biomass sourced carbon versus fossil carbon. The analysis is performed according to standardized methods such as ASTM D6866, ISO 16620, and EN 16640. Products 100% sourced from plants, animals, or microbiological material are therefore 100% biobased, while products sourced only from fossil fuel material are 0% biobased. Any result in between 0% and 100% biobased indicates that there is a mixture of both biomass-derived and fossil fuel-derived sources. Furthermore, biobased testing for building materials allows manufacturers to submit eligible material for certification and eco-label programs such as the United States Department of Agriculture (USDA) BioPreferred Program. This program includes a voluntary labeling initiative for biobased products, in which companies may apply to receive and display the USDA Certified Biobased Product label, stating third-party verification and displaying a product’s percentage of biobased content. The USDA program includes a specific category for Building Materials. In order to qualify for the biobased certification under this product category, examples of product criteria that must be met include minimum 62% biobased content for wall coverings, minimum 25% biobased content for lumber, and a minimum 91% biobased content for floor coverings (non-carpet). As a result, consumers can easily identify plant-based products in the marketplace.

Keywords: carbon-14 testing, biobased, biobased content, radiocarbon dating, accelerator mass spectrometry, AMS, materials

Procedia PDF Downloads 130
63 Preparation of Nano-Scaled linbo3 by Polyol Method

Authors: Gabriella Dravecz, László Péter, Zsolt Kis

Abstract:

Abstract— The growth of optical LiNbO3 single crystal and its physical and chemical properties are well known on the macroscopic scale. Nowadays the rare-earth doped single crystals became important for coherent quantum optical experiments: electromagnetically induced transparency, slow down of light pulses, coherent quantum memory. The expansion of applications is increasingly requiring the production of nano scaled LiNbO3 particles. For example, rare-earth doped nanoscaled particles of lithium niobate can be act like single photon source which can be the bases of a coding system of the quantum computer providing complete inaccessibility to strangers. The polyol method is a chemical synthesis where oxide formation occurs instead of hydroxide because of the high temperature. Moreover the polyol medium limits the growth and agglomeration of the grains producing particles with the diameter of 30-200 nm. In this work nano scaled LiNbO3 was prepared by the polyol method. The starting materials (niobium oxalate and LiOH) were diluted in H2O2. Then it was suspended in ethylene glycol and heated up to about the boiling point of the mixture with intensive stirring. After the thermal equilibrium was reached, the mixture was kept in this temperature for 4 hours. The suspension was cooled overnight. The mixture was centrifuged and the particles were filtered. Dynamic Light Scattering (DLS) measurement was carried out and the size of the particles were found to be 80-100 nms. This was confirmed by Scanning Electron Microscope (SEM) investigations. The element analysis of SEM showed large amount of Nb in the sample. The production of LiNbO3 nano particles were succesful by the polyol method. The agglomeration of the particles were avoided and the size of 80-100nm could be reached.

Keywords: lithium-niobate, nanoparticles, polyol, SEM

Procedia PDF Downloads 102
62 Biobased Facade: Illuminated Natural Fibre Polymer with Cardboard Core

Authors: Ralf Gliniorz, Carolin Petzoldt, Andreas Ehrlich, Sandra Gelbrich, Lothar Kroll

Abstract:

The building envelope is integral part of buildings, and renewable resources have a key role in energy consumption. So our aim was the development and implementation of a free forming facade system, consisting of fibre-reinforced polymer, which is built up of commercial biobased resin systems and natural fibre reinforcement. The field of application is aimed in modern architecture, like the office block 'Fachagentur Nachwachsende Rohstoffe e.V.' with its oak wood recyclate facade. The build-up of our elements is a classically sandwich-structured composite: face sheets as fibre-reinforced composite using polymer matrix, here a biobased epoxy, and natural fibres. The biobased core consists of stuck cardboard structure (BC-flute). Each element is manufactured from two shells in a counterpart, via hand lay-up laminate. These natural fibre skins and cardboard core have adhered 'wet-on-wet'. As a result, you get the effect of translucent face sheets with matrix illumination. Each created pixel can be controlled in RGB-colours and form together a screen at buildings. A 10 x 5 m² area 'NFP-BIO' with 25 elements is planned as a reference object in Chemnitz. The resolution is about 100 x 50 pixels. Specials are also the efficient technology of production and the possibility to extensively 3D-formed elements for buildings, replacing customary facade systems, which can give out information or advertising.

Keywords: biobased facade, cardboard core, natural fibre skins, sandwich element

Procedia PDF Downloads 178
61 Optimization of Batch to Up-Scaling of Soy-Based Prepolymer Polyurethane

Authors: Flora Elvistia Firdaus

Abstract:

The chemical structure of soybean oils have to be chemically modified through its tryglyceride to attain resemblance properties with petrochemicals. Sulfur acid catalyst in peracetic acid co-reagent has good performance on modified soybean oil strucutures through its unsaturated fatty acid moiety to the desired hydroxyl functional groups. A series of screening reactions have indicated that the ratio of acetic/peroxide acid 1:7.25 (mol/mol) with temperature of 600°C for soy-epoxide synthesis are prevailed for up-scaling of bodied soybean into 10 and 20 folds from initials. A two-step process was conducted for the preparation of soy-polyol in designated temperatures.

Keywords: soybean, polyol, up-scaling, polyurethane

Procedia PDF Downloads 326
60 The Interactive Effect of Sodium Chloride and Diatomaceous Earth (DE) on Bacillus aquimaris

Authors: Bassam O AlJohny

Abstract:

The growth of Bacillus aquimaris was inhibited from 6 - 20 % of NaCl but it showed some tolerance when Diatomaceous earth (DE) added from 2 - 12% NaCl. Concerning the effect of NaCl on polyol production, we can conclude that, the test bacterium showed some tolerance to NaCl by producing glycerol up to 8 % of NaCl. Then decreased sharply. The addition of DE decrease the amount of polyol and glycerol remarkably and this due to the productive effect of DE to the bacterial cells. The SEM figures represented the presence of electron dense bodies due to the accumulation of small particles of DE as protective molecules.

Keywords: Bacillus aquimaris, Diatomaceous earth (DE), osmoticstress, sodium chloride

Procedia PDF Downloads 260
59 In situ Polymerization and Properties of Biobased Polyurethane/Epoxy Interpenetrating Network Nanocomposites

Authors: Aiswarea Mathew, Smita Mohanty, Jr., S. K. Nayak

Abstract:

Polyurethane networks based on castor oil (CO) as a renewable resource polyol were synthesized. Polyurethane/epoxy resin interpenetrating network nanocomposites containing modified montmorillonite organoclay (C30B-PU/EP nanocomposites) were prepared by an in situ intercalation method. The conventional spectroscopic characterization of the synthesized samples using FT-IR confirms the existence of the proposed castor oil based PU structure and also showed that strong interactions existed between C30B and EP/PU matrix. The dispersion degree of C30B in EP/PU matrix was characterized by X-Ray diffraction (XRD) method. Scanning electronic microscopy analysis showed that the interpenetrating process of PU and EP increases the exfoliation degree of C30B, and it improves the compatibility and the phase structure of polyurethane/epoxy resin interpenetrating polymer networks (PU/EP IPNs). The thermal stability improves compared to the polyurethane when the PU/EP IPN is formed. Mechanical properties including the Young’s modulus and tensile strength reflected marked improvement with addition of C30B.

Keywords: castor oil, epoxy, montmorillonite, polyurethane

Procedia PDF Downloads 368
58 Choosing the Right Lignin for Phenolic Adhesive Application

Authors: Somayyeh Kalami, Mojgan Nejad

Abstract:

Based on the source (softwood, hardwood or annual crop) and isolation method (kraft, organosolv, sulfite or pre-enzymatic treatment), there are significant variations in lignin structure and properties. The first step in using lignin as biobased feedstock is to make sure that specific lignin is suitable for intended application. Complete characterization of lignin and measuring its chemical, physical and thermal properties can help to predict its suitability. To replace 100% phenol portion of phenolic adhesive, lignin should have high reactivity toward formaldehyde. Theoretically, lignins with closer backbone structure to phenol should be better candidate for this application. In this study, a number of different lignins were characterized and used to formulate phenolic adhesive. One of the main findings was that lignin sample with higher percentage of hydroxyl-phenyl units was better candidate than lignin with more syringyl units. This could be explained by the fact that hydroxyl-phenyl lignin units have two available ortho positions for reaction with formaldehyde while in syringyl units all ortho and para positions are occupied, and there is no available site in lignin structure to react with formaldehyde.

Keywords: lignin, phenolic adhesive, biobased, sustainable

Procedia PDF Downloads 185
57 New Platform of Biobased Aromatic Building Blocks for Polymers

Authors: Sylvain Caillol, Maxence Fache, Bernard Boutevin

Abstract:

Recent years have witnessed an increasing demand on renewable resource-derived polymers owing to increasing environmental concern and restricted availability of petrochemical resources. Thus, a great deal of attention was paid to renewable resources-derived polymers and to thermosetting materials especially, since they are crosslinked polymers and thus cannot be recycled. Also, most of thermosetting materials contain aromatic monomers, able to confer high mechanical and thermal properties to the network. Therefore, the access to biobased, non-harmful, and available aromatic monomers is one of the main challenges of the years to come. Starting from phenols available in large volumes from renewable resources, our team designed platforms of chemicals usable for the synthesis of various polymers. One of these phenols, vanillin, which is readily available from lignin, was more specifically studied. Various aromatic building blocks bearing polymerizable functions were synthesized: epoxy, amine, acid, carbonate, alcohol etc. These vanillin-based monomers can potentially lead to numerous polymers. The example of epoxy thermosets was taken, as there is also the problematic of bisphenol A substitution for these polymers. Materials were prepared from the biobased epoxy monomers obtained from vanillin. Their thermo-mechanical properties were investigated and the effect of the monomer structure was discussed. The properties of the materials prepared were found to be comparable to the current industrial reference, indicating a potential replacement of petrosourced, bisphenol A-based epoxy thermosets by biosourced, vanillin-based ones. The tunability of the final properties was achieved through the choice of monomer and through a well-controlled oligomerization reaction of these monomers. This follows the same strategy than the one currently used in industry, which supports the potential of these vanillin-derived epoxy thermosets as substitutes of their petro-based counterparts.

Keywords: lignin, vanillin, epoxy, amine, carbonate

Procedia PDF Downloads 200
56 Synthesis of Cardanol Oil Building Blocks for Polymer Synthesis

Authors: Sylvain Caillol

Abstract:

Uncertainty in terms of price and availability of petroleum, in addition to global political and institutional tendencies toward the principles of sustainable development, urge chemical industry to a sustainable chemistry and particularly the use of renewable resources in order to synthesize biobased chemicals and products. We propose a platform approach for the synthesis of various building blocks from cardanol in one or two-steps syntheses. Cardanol, which is a natural phenol, is issued from Cashew Nutshell Liquid (CNSL), a non-edible renewable resource, co-produced from cashew industry in large commercial volumes. Cardanol is particularly interesting to replace fossil aromatic groups in polymers and materials. Our team studied various routes for the synthesis of cardanol-derived biobased building blocks used after that in polymer syntheses. For example, we used phenolation to dimerize/oligomerize cardanol to propose increase functionality of cardanol. Thio-ene was used to synthesize new reactive amines. Epoxidation and (meth)acrylation were also used to insert oxirane or (meth)acrylate groups in order to synthesize polymers and materials.

Keywords: cardanol, cashew nutshell liquid, epoxy, vinyl ester, latex, emulsion

Procedia PDF Downloads 142
55 NENU2PHAR: PHA-Based Materials from Micro-Algae for High-Volume Consumer Products

Authors: Enrique Moliner, Alba Lafarga, Isaac Herraiz, Evelina Castellana, Mihaela Mirea

Abstract:

NENU2PHAR (GA 887474) is an EU-funded project aimed at the development of polyhydroxyalkanoates (PHAs) from micro-algae. These biobased and biodegradable polymers are being tested and validated in different high-volume market applications including food packaging, cosmetic packaging, 3D printing filaments, agro-textiles and medical devices, counting on the support of key players like Danone, BEL Group, Sofradim or IFG. At the moment the project has achieved to produce PHAs from micro-algae with a cumulated yield around 17%, i.e. 1 kg PHAs produced from 5.8 kg micro-algae biomass, which in turn capture 11 kg CO₂ for growing up. These algae-based plastics can therefore offer the same environmental benefits than current bio-based plastics (reduction of greenhouse gas emissions and fossil resource depletion), using a 3rd generation biomass feedstock that avoids the competition with food and the environmental impacts of agricultural practices. The project is also dealing with other sustainability aspects like the ecodesign and life cycle assessment of the plastic products targeted, considering not only the use of the biobased plastics but also many other ecodesign strategies. This paper will present the main progresses and results achieved to date in the project.

Keywords: NENU2PHAR, Polyhydroxyalkanoates, micro-algae, biopolymer, ecodesign, life cycle assessment

Procedia PDF Downloads 47
54 Role of NaCl and Temperature in Glycerol Mediated Rapid Growth of Silver Nanostructures

Authors: L. R. Shobin, S. Manivannan

Abstract:

One dimensional silver nanowires and nanoparticles gained more interest in developing transparent conducting films, catalysis, biological and chemical sensors. Silver nanostructures can be synthesized by varying reaction conditions such as the precursor concentration, molar ratio of the surfactant, injection speed of silver ions, etc. in the polyol process. However, the reaction proceeds for greater than 2 hours for the formation of silver nanowires. The introduction of etchant in the medium promotes the growth of silver nanowires from silver nanoparticles along the [100] direction. Rapid growth of silver nanowires is accomplished using the Cl- ions from NaCl and polyvinyl pyrrolidone (PVP) as surfactant. The role of Cl- ion was investigated in the growth of the nanostructured silver. Silver nanoparticles (<100 nm) were harvested from glycerol medium in the absence of Cl- ions. Trace amount of Cl- ions (2.5 mM -NaCl) produced the edge joined nanowires of length upto 2 μm and width ranging from 40 to 65 nm. Formation and rapid growth (within 25 minutes) of long, uniform silver nanowires (upto 5 μm) with good yield were realized in the presence of 5 mM NaCl at 200ºC. The growth of nanostructures was monitored by UV-vis-NIR spectroscopy. Scanning and transmission electron microscopes reveal the morphology of the silver nano harvests. The role of temperature in the reduction of silver ions, growth mechanism for nanoparticles, edge joined and straight nanowires will be discussed.

Keywords: silver nanowires, glycerol mediated polyol process, scanning electron microscopy, UV-Vis- NIR spectroscopy, transmission electron microscopy

Procedia PDF Downloads 272
53 Syntheses in Polyol Medium of Inorganic Oxides with Various Smart Optical Properties

Authors: Shian Guan, Marie Bourdin, Isabelle Trenque, Younes Messaddeq, Thierry Cardinal, Nicolas Penin, Issam Mjejri, Aline Rougier, Etienne Duguet, Stephane Mornet, Manuel Gaudon

Abstract:

At the interface of the studies performed by 3 Ph.D. students: Shian Guan (2017-2020), Marie Bourdin (2016-2019) and Isabelle Trenque (2012-2015), a single synthesis route: polyol-mediated process, was used with success for the preparation of different inorganic oxides. Both of these inorganic oxides were elaborated for their potential application as smart optical compounds. This synthesis route has allowed us to develop nanoparticles of zinc oxide, vanadium oxide or tungsten oxide. This route is with easy implementation, inexpensive and with large-scale production potentialities and leads to materials of high purity. The obtaining by this route of nanometric particles, however perfectly crystalline, has notably led to the possibility of doping these matrix materials with high doping ion concentrations (high solubility limits). Thus, Al3+ or Ga3+ doped-ZnO powder, with high doping rate in comparison with the literature, exhibits remarkable infrared absorption properties thanks to their high free carrier density. Note also that due to the narrow particle size distribution of the as-prepared nanometric doped-ZnO powder, the original correlation between crystallite size and unit-cell parameters have been established. Also, depending on the annealing atmosphere use to treat vanadium precursors, VO2, V2O3 or V2O5 oxides with thermochromic or electrochromic properties can be obtained without any impurity, despite the versatility of the oxidation state of vanadium. This is of more particular interest on vanadium dioxide, a relatively difficult-to-prepare oxide, whose first-order metal-insulator phase transition is widely explored in the literature for its thermochromic behavior (in smart windows with optimal thermal insulation). Finally, the reducing nature of the polyol solvents ensures the production of oxygen-deficient tungsten oxide, thus conferring to the nano-powders exotic colorimetric properties, as well as optimized photochromic and electrochromic behaviors.

Keywords: inorganic oxides, electrochromic, photochromic, thermochromic

Procedia PDF Downloads 188
52 Can We Meet the New Challenges of NonIsocyanates Polyurethanes (NIPU) towards NIPU Foams?

Authors: Adrien Cornille, Marine Blain, Bernard Boutevin, Sylvain Caillol

Abstract:

Generally, linear polyurethanes (PUs) are obtained by the reaction between an oligomeric diol, a short diol as chain extender and a diisocyanate. However the use of diisocyanate should be avoided since they are generally very harmful for human health. Therefore the synthesis of NIPUs (non isocyanate PUs) from step growth polymerization of dicyclocarbonates and diamines should be favoured. This method is particularly interesting since no hazardous isocyanates are used. Thus, this reaction, extensively studied by Endo et al. is currently gaining a lot of attention as a substitution route for the synthesis of NIPUs, both from industrial and academic community. However, the reactivity of reaction between amine and cyclic carbonate is a major scientific issue, since cyclic carbonates are poorly reactive. Thus, our team developed several synthetic ways for the synthesis of various di-cyclic carbonates based on C5-, C6- and dithio- cyclic carbonates, from different biobased raw materials (glycerin isosorbide, vegetable oils…). These monomers were used to synthesize NIPUs with various mechanical and thermal properties for various applications. We studied the reactivity of reaction with various catalysts and find optimized conditions for room temperature reaction. We also studied the radical copolymerization of cyclic carbonate monomers in styrene-acrylate copolymers for coating applications. We also succeeded in the elaboration of biobased NIPU flexible foams. To the best of our knowledge, there is no report in literature on the preparation of non-isocyanate polyurethane foams.

Keywords: foam, nonisocyanate polyurethane, cyclic carbonate, blowing agent, scanning electron microscopy

Procedia PDF Downloads 202
51 Syntheses of Biobased Hybrid Poly(epoxy-hydroxyurethane) Polymers

Authors: Adrien Cornille, Sylvain Caillol, Bernard Boutevon

Abstract:

The development of polyurethanes began in 1937 at I. G. Farbenindustrie where Bayer with coworkers discovered the addition polymerization reaction between diisocyanates and diols. Since their discovery, the demand in PU has continued to increase and it will attain in 2016 a production of 18 million tons. However, isocyanates compounds are harmful to human and environment. Methylene diphenyl 4,4’-diisocyanate (MDI) and toluene diisocyanate (TDI), the most widely used isocyanates in PU industry, are classified as CMR (Carcinogen, Mutagen, and Reprotoxic). In order to design isocyanate-free materials, an interesting alternative is the use of Polyhydroxyurethanes (PHUs) by reaction between cyclic carbonate and polyfunctional amines. The main problem concerning PHUs synthesis relates to the low reactivity of carbonate/amine reaction. To solve this issue, many studies in the literature have been conducted to design PHU from more reactive cyclic-carbonates, bearing electro-withdrawing substituent or by using six-membered, seven-membered or thio-cyclic carbonate. The main drawback of all these systems remains the low molar masses obtained for the synthesized PHUs, which hinders their use for material applications. Therefore, we developed another strategy to afford new hybrid PHU with high conversion. This very innovative two-step approach consists in the first step in the synthesis of aminotelechelic PHU oligomers with different chain length from bis-cyclic carbonate with different excess of primary amine functions. In the second step, these aminotelechelic PHU oligomers were used in formulation with biobased epoxy monomers (from cashew nut shell liquid and tannins) to synthesize hybrid polyepoxyurethane polymers. These materials were then characterized by thermal and mechanical analyses.

Keywords: polyurethane, polyhydroxyurethane, aminotelechelic NIPU oligomers, carbonates, epoxy, amine, epoxyurethane polymers, hybrid polymers

Procedia PDF Downloads 182
50 Preparation and Properties of Gelatin-Bamboo Fibres Foams for Packaging Applications

Authors: Luo Guidong, Song Hang, Jim Song, Virginia Martin Torrejon

Abstract:

Due to their excellent properties, polymer packaging foams have become increasingly essential in our current lifestyles. They are cost-effective and lightweight, with excellent mechanical and thermal insulation properties. However, they constitute a major environmental and health concern due to litter generation, ocean pollution, and microplastic contamination of the food chain. In recent years, considerable efforts have been made to develop more sustainable alternatives to conventional polymer packaging foams. As a result, biobased and compostable foams are increasingly becoming commercially available, such as starch-based loose-fill or PLA trays. However, there is still a need for bulk manufacturing of bio-foams planks for packaging applications as a viable alternative to their fossil fuel counterparts (i.e., polystyrene, polyethylene, and polyurethane). Gelatin is a promising biopolymer for packaging applications due to its biodegradability, availability, and biocompatibility, but its mechanical properties are poor compared to conventional plastics. However, as widely reported for other biopolymers, such as starch, the mechanical properties of gelatin-based bioplastics can be enhanced by formulation optimization, such as the incorporation of fibres from different crops, such as bamboo. This research aimed to produce gelatin-bamboo fibre foams by mechanical foaming and to study the effect of fibre content on the foams' properties and structure. As a result, foams with virtually no shrinkage, low density (<40 kg/m³), low thermal conductivity (<0.044 W/m•K), and mechanical properties comparable to conventional plastics were produced. Further work should focus on developing formulations suitable for the packaging of water-sensitive products and processing optimization, especially the reduction of the drying time.

Keywords: biobased and compostable foam, sustainable packaging, natural polymer hydrogel, cold chain packaging

Procedia PDF Downloads 71
49 Using Sugar Mill Waste for Biobased Epoxy Composites

Authors: Ulku Soydal, Mustafa Esen Marti, Gulnare Ahmetli

Abstract:

In this study, precipitated calcium carbonate lime waste (LW) from sugar beet process was recycled as the raw material for the preparation of composite materials. Epoxidized soybean oil (ESO) was used as a co-matrix in 50 wt% with DGEBA type epoxy resin (ER). XRD was used for characterization of composites. Effects of ESO and LW filler amounts on mechanical properties of neat ER were investigated. Modification of ER with ESO remarkably enhanced plasticity of ER.

Keywords: epoxy resin, biocomposite, lime waste, properties

Procedia PDF Downloads 284
48 An Enzyme Technology - Metnin™ - Enables the Full Replacement of Fossil-Based Polymers by Lignin in Polymeric Composites

Authors: Joana Antunes, Thomas Levée, Barbara Radovani, Anu Suonpää, Paulina Saloranta, Liji Sobhana, Petri Ihalainen

Abstract:

Lignin is an important component in the exploitation of lignocellulosic biomass. It has been shown that within the next years, the yield of added-value lignin-based chemicals and materials will generate renewable alternatives to oil-based products (e.g. polymeric composites, resins and adhesives) and enhance the economic feasibility of biorefineries. In this paper, a novel technology for lignin valorisation (METNIN™) is presented. METNIN™ is based on the oxidative action of an alkaliphilic enzyme in aqueous alkaline conditions (pH 10-11) at mild temperature (40-50 °C) combined with a cascading membrane operation, yielding a collection of lignin fractions (from oligomeric down to mixture of tri-, di- and monomeric units) with distinct molecular weight distribution, low polydispersity and favourable physicochemical properties. The alkaline process conditions ensure the high processibility of crude lignin in an aqueous environment and the efficiency of the enzyme, yielding better compatibility of lignin towards targeted applications. The application of a selected lignin fraction produced by METNIN™ as a suitable lignopolyol to completely replace a commercial polyol in polyurethane rigid foam formulations is presented as a prototype. Liquid lignopolyols with a high lignin content were prepared by oxypropylation and their full utilization in the polyurethane rigid foam formulation was successfully demonstrated. Moreover, selected technical specifications of different foam demonstrators were determined, including closed cell count, water uptake and compression characteristics. These specifications are within industrial standards for rigid foam applications. The lignin loading in the lignopolyol was a major factor determining the properties of the foam. In addition to polyurethane foam demonstrators, other examples of lignin-based products related to resins and sizing applications will be presented.

Keywords: enzyme, lignin valorisation, polyol, polyurethane foam

Procedia PDF Downloads 122
47 Influence Study of the Molar Ratio between Solvent and Initiator on the Reaction Rate of Polyether Polyols Synthesis

Authors: María José Carrero, Ana M. Borreguero, Juan F. Rodríguez, María M. Velencoso, Ángel Serrano, María Jesús Ramos

Abstract:

Flame-retardants are incorporated in different materials in order to reduce the risk of fire, either by providing increased resistance to ignition, or by acting to slow down combustion and thereby delay the spread of flames. In this work, polyether polyols with fire retardant properties were synthesized due to their wide application in the polyurethanes formulation. The combustion of polyurethanes is primarily dependent on the thermal properties of the polymer, the presence of impurities and formulation residue in the polymer as well as the supply of oxygen. There are many types of flame retardants, most of them are phosphorous compounds of different nature and functionality. The addition of these compounds is the most common method for the incorporation of flame retardant properties. The employment of glycerol phosphate sodium salt as initiator for the polyol synthesis allows obtaining polyols with phosphate groups in their structure. However, some of the critical points of the use of glycerol phosphate salt are: the lower reactivity of the salt and the necessity of a solvent (dimethyl sulfoxide, DMSO). Thus, the main aim in the present work was to determine the amount of the solvent needed to get a good solubility of the initiator salt. Although the anionic polymerization mechanism of polyether formation is well known, it seems convenient to clarify the role that DMSO plays at the starting point of the polymerization process. Regarding the fact that the catalyst deprotonizes the hydroxyl groups of the initiator and as a result of this, two water molecules and glycerol phosphate alkoxide are formed. This alkoxide, together with DMSO, has to form a homogeneous mixture where the initiator (solid) and the propylene oxide (PO) are soluble enough to mutually interact. The addition rate of PO increased when the solvent/initiator ratios studied were increased, observing that it also made the initiation step shorter. Furthermore, the molecular weight of the polyol decreased when higher solvent/initiator ratios were used, what revealed that more amount of salt was activated, initiating more chains of lower length but allowing to react more phosphate molecules and to increase the percentage of phosphorous in the final polyol. However, the final phosphorous content was lower than the theoretical one because only a percentage of salt was activated. On the other hand, glycerol phosphate disodium salt was still partially insoluble in DMSO studied proportions, thus, the recovery and reuse of this part of the salt for the synthesis of new flame retardant polyols was evaluated. In the recovered salt case, the rate of addition of PO remained the same than in the commercial salt but a shorter induction period was observed, this is because the recovered salt presents a higher amount of deprotonated hydroxyl groups. Besides, according to molecular weight, polydispersity index, FT-IR spectrum and thermal stability, there were no differences between both synthesized polyols. Thus, it is possible to use the recovered glycerol phosphate disodium salt in the same way that the commercial one.

Keywords: DMSO, fire retardants, glycerol phosphate disodium salt, recovered initiator, solvent

Procedia PDF Downloads 247
46 Biobased Sustainable Films from the Algerian Opuntia Ficus-Indica Cladodes Powder: Effect of Plasticizer Content

Authors: Nadia Chougui, Nawal Makhloufi, Farouk Rezgui, Elias Benramdane, Carmen S. R. Freire, Carla Vilela, Armando J. D. Silvestre

Abstract:

Native to Mexico, Opuntia ficus-indica was introduced in southern Spain, and thereafter, it was spread throughout the Mediterranean Basin by the Spanish conquerors in the 16th and 17th centuries. O. ficus-indica is a tropical and subtropical plant able to grow in arid and semi-arid regions, such as the Mediterranean and Central America regions. The culture of Opuntia covers about 200,000 ha in North Africa. This tree is used against soil erosion and desertification for fruit production and is encouraged to promote the livestock sector. It has recently received ever-increasing attention from researchers worldwide for the multivalent pharmaceutical and cosmetical potential of its different compartments (fruits, seeds, cladodes). The present study investigated the elaboration by casting method and characterization of new biodegradable films composed of cladodes powder (CP) of the plant raw material mentioned above, and a marine seaweed derivative, namely agar (A). The effect of glycerol concentration on the properties of the films was evaluated at four different contents (30, 40, 50 and 60 wt.%). The films present UV-blocking properties, thermal stability as well as moderate mechanical performance and water vapor transmission rate (WVTR). The results point to an increase in thickness, elongation at break, moisture content, water solubility, and WVTR with increasing glycerol content. On the contrary, Young’s modulus, tensile strength and contact angle decreased as glycerol concentration increased. The best combination is obtained for the film with 30% glycerol, based on an intermediate compromise between physical, mechanical, thermal and barrier properties. All these outcomes express the potentiality of the powder obtained from grinding the OFI cladodes as raw material to produce low-cost films for the development of sustainable packaging materials.

Keywords: Opuntia ficus-indica cladodes powder, agar, biobased films, effect of plasticizer, sustainable packaging

Procedia PDF Downloads 38
45 Study of Phase Separation Behavior in Flexible Polyurethane Foam

Authors: El Hatka Hicham, Hafidi Youssef, Saghiri Khalid, Ittobane Najim

Abstract:

Flexible polyurethane foam (FPUF) is a low-density cellular material generally used as a cushioning material in many applications such as furniture, bedding, packaging, etc. It is commercially produced during a continuous process, where a reactive mixture of foam chemicals is poured onto a moving conveyor. FPUFs are produced by the catalytic balancing of two reactions involved, the blowing reaction (isocyanate-water) and the gelation reaction (isocyanate-polyol). The microstructure of FPUF is generally composed of soft phases (polyol phases) and rigid domains that separate into two domains of different sizes: the rigid polyurea microdomains and the macrodomains (larger aggregates). The morphological features of FPUF are strongly influenced by the phase separation morphology that plays a key role in determining the global FPUF properties. This phase-separated morphology results from a thermodynamic incompatibility between soft segments derived from aliphatic polyether and hard segments derived from the commonly used aromatic isocyanate. In order to improve the properties of FPUF against the different stresses faced by this material during its use, we report in this work a study of the phase separation phenomenon in FPUF that has been examined using SAXS WAXS and FTIR. Indeed, we have studied with these techniques the effect of water, isocyanates, and alkaline chlorides on the phase separation behavior. SAXS was used to study the morphology of the microphase separated, WAXS to examine the nature of the hard segment packing, and FTIR to investigate the hydrogen bonding characteristics of the materials studied. The prepared foams were shown to have different levels of urea phase connectivity; the increase in water content in the FPUF formulation leads to an increase in the amount of urea formed and consequently the increase of the size of urea aggregates formed. Alkali chlorides (NaCl, KCl, and LiCl) incorporated into FPUF formulations show that is the ability to prevent hydrogen bond formation and subsequently alter the rigid domains. FPUFs prepared by different isocyanate structures showed that urea aggregates are difficult to be formed in foams prepared by asymmetric diisocyanate, while are more easily formed in foams prepared by symmetric and aliphatic diisocyanate.

Keywords: flexible polyurethane foam, hard segments, phase separation, soft segments

Procedia PDF Downloads 113
44 Nano Composite of Clay and Modified Ketonic Resin as Fire Retardant Polyol for Polyurethane

Authors: D. Önen, N. Kızılcan, B. Yıldız, A. Akar

Abstract:

In situ modified cyclohexanone-formaldehyde resins were prepared by addition of alendronic acid during resin preparation. Clay nanocomposites in ketonic resins were achieved by adding clay into the flask at the beginning of the resin preparation. The prepared resins were used for the synthesis of fire resistant polyurethanes foam. Both phosphorous containing modifier compound alendronic acid and nanoclay increases fire resistance of the cyclohexanone-formaldehyde resin thus polyurethane produced from these resins. The effect of the concentrations of alendronic acid and clay on the fire resistance and physical properties of polyurethanes was studied.

Keywords: alendronic acid, clay, ketonic resin, polyurethane

Procedia PDF Downloads 364
43 Eco-Friendly Natural Filler Based Epoxy Composites

Authors: Suheyla Kocaman, Gulnare Ahmetli

Abstract:

In this study, acrylated soybean oil (AESO) was used as modifying agent for DGEBF-type epoxy resin (ER). AESO was used as a co-matrix in 50 wt % with ER. Composites with eco-friendly natural fillers-banana bark and seashell were prepared. MNA was used as a hardener. Effect of banana peel (BP) and seashell (SSh) fillers on mechanical properties, such as tensile strength, elongation at break, and hardness of M-ERs were investigated. The structure epoxy resins (M-ERs) cured with MNA and sebacic acid (SAc) hardeners were characterized by Fourier transform infrared spectroscopy (FTIR). Tensile test results show that Young’s (elastic) modulus, tensile strength and hardness of SSh particles reinforced with M-ERs were higher than the M-ERs reinforced with banana bark.

Keywords: biobased composite, epoxy resin, mechanical properties, natural fillers

Procedia PDF Downloads 203
42 Development of Plantar Insoles Reinforcement Using Biocomposites

Authors: A. C. Vidal, D. R. Mulinari, C. F. Bandeira, S. R. Montoro

Abstract:

Due to the great effort suffered by foot during movement, is of great importance to count on a shoe that has a proper structure and excellent support tread to prevent the immediate and long-term consequences in all parts of the body. In this sense, new reinforcements of insoles with high impact absorption were developed in this work, from a polyurethane (PU) biocomposite derived from castor oil reinforced or not with palm fibers. These insoles have been obtained from the mixture with polyol prepolymer (diisocyanate) and subsequently were evaluated morphologically, mechanically and by thermal analysis. The results revealed that the biocomposites showed lower flexural strength, higher impact strength and open interconnected pores in their microstructure, but with smaller cells and degradation temperature slightly higher compared to the marketed material, showing interesting properties for a possible application as reinforcement of insoles.

Keywords: composite, polyurethane insole, palm fibers, plantar insoles reinforcement

Procedia PDF Downloads 387
41 Synthesis and Physico-Chemical Analysis of Jatropha curcas Seed Oil for ISO VG32 and VG46 Applications

Authors: M. Nuhu, M. S. Amina, A. H. Aminu, A. J. Abbas, N. Salahudeen, A. Z. Yusuf

Abstract:

Transesterification of jatropha methyl ester (JME) with the common polyol, trimethylolpropane (TMP) produced the TMP based ester which exhibits improved temperature properties. This paper discusses the physic-chemical properties of jatropha bio-lubricant base oil applicable for ISO VG32 and VG46 requirement. The catalyst employed for the JME was CaO synthesized in National Research Institute for Chemical Technology (NARICT) that gives 100% conversion. The molar ratio of JME to TMP was 3.5:1 and the catalyst (NaOCH3) loading were found to be 0.8% of the weight of the total reactants. The final fractionated jatropha bio-lubricant base was found to contain 11.95% monoesters, 43.89% diesters and 44.16% triesters (desired product). In addition, it was found that the bio-lubricant base oil produced is comparable to the ISO VG46 commercial standards for light and industrial gears applications and other plant based bio-lubricant.

Keywords: biodegradability, methyl ester, pour point, transesterification, viscosity index

Procedia PDF Downloads 629
40 Comparison of Non-destructive Devices to Quantify the Moisture Content of Bio-Based Insulation Materials on Construction Sites

Authors: Léa Caban, Lucile Soudani, Julien Berger, Armelle Nouviaire, Emilio Bastidas-Arteaga

Abstract:

Improvement of the thermal performance of buildings is a high concern for the construction industry. With the increase in environmental issues, new types of construction materials are being developed. These include bio-based insulation materials. They capture carbon dioxide, can be produced locally, and have good thermal performance. However, their behavior with respect to moisture transfer is still facing some issues. With a high porosity, the mass transfer is more important in those materials than in mineral insulation ones. Therefore, they can be more sensitive to moisture disorders such as mold growth, condensation risks or decrease of the wall energy efficiency. For this reason, the initial moisture content on the construction site is a piece of crucial knowledge. Measuring moisture content in a laboratory is a mastered task. Diverse methods exist but the easiest and the reference one is gravimetric. A material is weighed dry and wet, and its moisture content is mathematically deduced. Non-destructive methods (NDT) are promising tools to determine in an easy and fast way the moisture content in a laboratory or on construction sites. However, the quality and reliability of the measures are influenced by several factors. Classical NDT portable devices usable on-site measure the capacity or the resistivity of materials. Water’s electrical properties are very different from those of construction materials, which is why the water content can be deduced from these measurements. However, most moisture meters are made to measure wooden materials, and some of them can be adapted for construction materials with calibration curves. Anyway, these devices are almost never calibrated for insulation materials. The main objective of this study is to determine the reliability of moisture meters in the measurement of biobased insulation materials. The determination of which one of the capacitive or resistive methods is the most accurate and which device gives the best result is made. Several biobased insulation materials are tested. Recycled cotton, two types of wood fibers of different densities (53 and 158 kg/m3) and a mix of linen, cotton, and hemp. It seems important to assess the behavior of a mineral material, so glass wool is also measured. An experimental campaign is performed in a laboratory. A gravimetric measurement of the materials is carried out for every level of moisture content. These levels are set using a climatic chamber and by setting the relative humidity level for a constant temperature. The mass-based moisture contents measured are considered as references values, and the results given by moisture meters are compared to them. A complete analysis of the uncertainty measurement is also done. These results are used to analyze the reliability of moisture meters depending on the materials and their water content. This makes it possible to determine whether the moisture meters are reliable, and which one is the most accurate. It will then be used for future measurements on construction sites to assess the initial hygrothermal state of insulation materials, on both new-build and renovation projects.

Keywords: capacitance method, electrical resistance method, insulation materials, moisture transfer, non-destructive testing

Procedia PDF Downloads 63
39 Production of Polyurethane Foams from Bark Wastes

Authors: Luísa P. Cruz-Lopes, Liliana Rodrigues, Idalina Domingos, José Ferreira, Luís Teixeira de Lemos, Bruno Esteves

Abstract:

Currently, the polyurethanes industry is dependent on fossil resources to obtain their basic raw materials (polyols and isocyanate), as these are obtained from petroleum products. The aim of this work was to use biopolyols from liquefied Pseudotsuga (Pseudotsuga menziesii) and Turkey oak (Quercus cerris) barks for the production of polyurethane foams and optimize the process. Liquefaction was done with glycerol catalyzed by KOH. Foams were produced following different formulations and using biopolyols from both barks. Subsequently, the foams were characterized according to their mechanical properties and the reaction of the foam formation was monitored by FTIR-ATR. The results show that it is possible to produce polyurethane foams using bio-based polyols and the liquefaction conditions are very important because they influence the characteristics of biopolyols and, consequently the characteristics of the foams. However, the process has to be further optimized so that it can obtain better quality foams.

Keywords: Bio-based polyol, mechanical tests, polyurethane foam, Pseudotsuga bark, renewable resources, Turkey oak bark

Procedia PDF Downloads 301
38 Effect of Catalyst on Castor Oil Based Polyurethane with Different Hard/Soft Segment Ratio

Authors: Swarnalata Sahoo, Smita Mohanty, S. K. Nayak

Abstract:

Environmentally friendly Polyurethane(PU) synthesis from Castor oil(CO) has been studied extensively. Probably due to high proportion of fatty hydroxy acids and unsaturated bond, CO showed better performance than other oil, can be easily utilized as commercial applications. In this work, cured PU polymers having different –NCO/OH ratio with and without catalyst were synthesized by using partially biobased Isocyanate with castor oil (CO). Curing time has been studied by observing at the time of reaction, which can be confirmed by AT-FTIR. DSC has been studied to monitor the reaction between CO & Isocyanates using non Isothermal process. Curing kinetics have also been studied to investigate the catalytic effect of the NCO / OH ratio of Polyurethane. Adhesion properties were evaluated from Lapshear test. Tg of the PU polymer was evaluated by DSC which can be compared by DMA. Surface Properties were studied by contact angle measurement. Improvement of the interfacial adhesion between the nonpolar surface of Aluminum substrate and the polar adhesive has been studied by modifying surface.

Keywords: polyurethane, partially bio-based isocyanate, castor oil, catalyst

Procedia PDF Downloads 421