1032 Microstructure and Hot Deformation Behavior of Fe-20Cr-5Al Alloy

Authors: Jung-Ho Moon, Tae Kwon Ha

Abstract:

Abstract—High temperature deformation behavior of cast Fe-20Cr-5Al alloy has been investigated in this study by performing tensile and compression tests at temperatures from 1100 to 1200oC. Rectangular ingots of which the dimensions were 300×300×100 in millimeter were cast using vacuum induction melting. Phase equilibrium was calculated using the FactSage®, thermodynamic software and database. Tensile strength of cast Fe-20Cr-5Al alloy was 4 MPa at 1200oC. With temperature decreased, tensile strength increased rapidly and reached up to 13 MPa at 1100oC. Elongation also increased from 18 to 80% with temperature decreased from 1200oC to 1100oC. Microstructure observation revealed that M23C6 carbide was precipitated along the grain boundary and within the matrix.

Keywords: 20 Cr-5Al ferritic stainless, high temperature deformation, aging treatment, microstructure, mechanical properties

Procedia PDF Downloads 431
1031 Numerical Investigation for Ductile Fracture of an Aluminium Alloy 6061 T-6: Assessment of Critical J-Integral

Authors: R. Bensaada, M. Almansba, M. Ould Ouali, R. Ferhoum, N. E. Hannachi

Abstract:

The aim of this work is to simulate the ductile fracture of SEN specimens in aluminium alloy. The assessment of fracture toughness is performed with the calculation of Jc (the critical value of J-Integral) through the resistance curves. The study is done using finite element code calculation ABAQUSTM including an elastic plastic with damage model of material’s behaviour. The procedure involves specimens of four different thicknesses and four ligament sizes for every thickness. The material of study is an aluminium alloy 6061-T6 for which the necessary parameters to complete the study are given. We found the same results for the same specimen’s thickness and for different ligament sizes when the fracture criterion is evaluated.

Keywords: j-integral, critical-j, damage, fracture toughness

Procedia PDF Downloads 343
1030 Ni-W alloy Coatings: A Promising Electrode Material

Authors: Mr. Liju Elias, A. Chitharanjan Hegde

Abstract:

Ni-W alloy coatings have been developed galvanostatically on copper substrate from tri-sodium citrate bath, using glycerol as the additive. The deposition conditions for production of Ni-W coatings have been optimized for peak performance of their electrocatalytic activity, namely hydrogen evolution reaction (HER) and oxygen evolution reaction (OER). The corrosion behavior of the coatings were tested under working conditions of electrocatalysis (1M KOH). Electrocatalytic behaviours were tested by cyclic voltammetry and chrono-potentiometry techniques. Experimental results demonstrated that Ni-W coatings at low and high current densities (c. d.) showing superior performance for OER and HER respectively. The increased electrocatalytic activity for HER with increase of deposition c. d. was attributed to the phase structure, surface morphology and chemical composition of the coatings, confirmed by XRD, SEM and EDX analysis, respectively. The dependency of hardness and thickness of the coatings on HER and OER were examined, and results were discussed.

Keywords: electrocatalytic behavior, HER, Ni-W alloy, OER

Procedia PDF Downloads 394
1029 Effects of Test Environment on the Sliding Wear Behaviour of Cast Iron, Zinc-Aluminium Alloy and Its Composite

Authors: Mohammad M. Khan, Gajendra Dixit

Abstract:

Partially lubricated sliding wear behaviour of a zinc-based alloy reinforced with 10wt% SiC particles has been studied as a function of applied load and solid lubricant particle size and has been compared with that of matrix alloy and conventionally used grey cast iron. The wear tests were conducted at the sliding velocities of 2.1m/sec in various partial lubricated conditions using pin on disc machine as per ASTM G-99-05. Base oil (SAE 20W-40) or mixture of the base oil with 5wt% graphite of particle sizes (7-10 µm) and (100 µm) were used for creating lubricated conditions. The matrix alloy revealed primary dendrites of a and eutectoid a + h and Î phases in the Inter dendritic regions. Similar microstructure has been depicted by the composite with an additional presence of the dispersoid SiC particles. In the case of cast iron, flakes of graphite were observed in the matrix; the latter comprised of (majority of) pearlite and (limited quantity of) ferrite. Results show a large improvement in wear resistance of the zinc-based alloy after reinforcement with SiC particles. The cast iron shows intermediate response between the matrix alloy and composite. The solid lubrication improved the wear resistance and friction behaviour of both the reinforced and base alloy. Moreover, minimum wear rate is obtained in oil+ 5wt % graphite (7-10 µm) lubricated environment for the matrix alloy and composite while for cast iron addition of solid lubricant increases the wear rate and minimum wear rate is obtained in case of oil lubricated environment. The cast iron experienced higher frictional heating than the matrix alloy and composite in all the cases especially at higher load condition. As far as friction coefficient is concerned, a mixed trend of behaviour was noted. The wear rate and frictional heating increased with load while friction coefficient was affected in an opposite manner. Test duration influenced the frictional heating and friction coefficient of the samples in a mixed manner.

Keywords: solid lubricant, sliding wear, grey cast iron, zinc based metal matrix composites

Procedia PDF Downloads 292
1028 Multi-Scale Modeling of Ti-6Al-4V Mechanical Behavior: Size, Dispersion and Crystallographic Texture of Grains Effects

Authors: Fatna Benmessaoud, Mohammed Cheikh, Vencent Velay, Vanessa Vidal, Farhad Rezai-Aria, Christine Boher

Abstract:

Ti-6Al-4V titanium alloy is one of the most widely used materials in aeronautical and aerospace industries. Because of its high specific strength, good fatigue, and corrosion resistance, this alloy is very suitable for moderate temperature applications. At room temperature, Ti-6Al-4V mechanical behavior is generally controlled by the behavior of alpha phase (beta phase percent is less than 8%). The plastic strain of this phase notably based on crystallographic slip can be hindered by various obstacles and mechanisms (crystal lattice friction, sessile dislocations, strengthening by solute atoms and grain boundaries…). The grains aspect of alpha phase (its morphology and texture) and the nature of its crystallographic lattice (which is hexagonal compact) give to plastic strain heterogeneous, discontinuous and anisotropic characteristics at the local scale. The aim of this work is to develop a multi-scale model for Ti-6Al-4V mechanical behavior using crystal plasticity approach; this multi-scale model is used then to investigate grains size, dispersion of grains size, crystallographic texture and slip systems activation effects on Ti-6Al-4V mechanical behavior under monotone quasi-static loading. Nine representative elementary volume (REV) are built for taking into account the physical elements (grains size, dispersion and crystallographic) mentioned above, then boundary conditions of tension test are applied. Finally, simulation of the mechanical behavior of Ti-6Al-4V and study of slip systems activation in alpha phase is reported. The results show that the macroscopic mechanical behavior of Ti-6Al-4V is strongly linked to the active slip systems family (prismatic, basal or pyramidal). The crystallographic texture determines which family of slip systems can be activated; therefore it gives to the plastic strain a heterogeneous character thus an anisotropic macroscopic mechanical behavior of Ti-6Al-4V alloy modeled. The grains size influences also on mechanical proprieties of Ti-6Al-4V, especially on the yield stress; by decreasing of the grain size, the yield strength increases. Finally, the grains' distribution which characterizes the morphology aspect (homogeneous or heterogeneous) gives to the deformation fields distribution enough heterogeneity because the crystallographic slip is easier in large grains compared to small grains, which generates a localization of plastic deformation in certain areas and a concentration of stresses in others.

Keywords: multi-scale modeling, Ti-6Al-4V alloy, crystal plasticity, grains size, crystallographic texture

Procedia PDF Downloads 140
1027 Precipitation Kinetics of Al-7%Mg Alloy Studied by DSC and XRD

Authors: M. Fatmi, T. Chihi, M. A. Ghebouli, B. Ghebouli

Abstract:

This work presents the experimental results of the differential scanning calorimetry (DSC), hardness measurements (Hv) and XRD analysis, for order to investigate the kinetics of precipitation phenomena in Al-7%wt. Mg alloy. In the XRD and DSC curves indicates the formation of the intermediate precipitation of β-(Al3Mg2) phase respectively. The activation energies associated with the processes have been determined according to the three models proposed by Kissinger, Ozawa, and Boswell. Consequently, the nucleation mechanism of the precipitates can be explained. These phases are confirmed by XRD analysis.

Keywords: discontinuous precipitation, hardening, Al–Mg alloys, mechanical and mechatronics engineering

Procedia PDF Downloads 389
1026 Wet Chemical Synthesis for Fe-Ni Alloy Nanocrystalline Powder

Authors: Neera Singh, Devendra Kumar, Om Parkash

Abstract:

We have synthesized nanocrystalline Fe-Ni alloy powders where Ni varies as 10, 30 and 50 mole% by a wet chemical route (sol-gel auto-combustion) followed by reduction in hydrogen atmosphere. The ratio of citrate to nitrate was maintained at 0.3 where citric acid has worked as a fuel during combustion. The reduction of combusted powders was done at 700°C/1h in hydrogen atmosphere using an atmosphere controlled quartz tube furnace. Phase and microstructure analysis has shown the formation of α-(Fe,Ni) and γ-(Fe,Ni) phases after reduction. An increase in Ni concentration resulted in more γ-(Fe,Ni) formation where complete γ-(Fe,Ni) formation was achieved at 50 mole% Ni concentration. Formation of particles below 50 nm size range was confirmed using Scherrer’s formula and Transmission Electron Microscope. The work is aimed at the effect of Ni concentration on phase, microstructure and magnetic properties of synthesized alloy powders.

Keywords: combustion, microstructure, nanocrystalline, reduction

Procedia PDF Downloads 160
1025 Nanocharacterization of PIII Treated 7075 Aluminum Alloy

Authors: Bruno Bacci Fernandes, Stephan Mändl, Ataíde Ribeiro da Silva Junior, José Osvaldo Rossi, Mário Ueda

Abstract:

Nitrogen implantation in aluminum and its alloys is acquainted for the difficulties in obtaining modified layers deeper than 200 nm. The present work addresses a new method to overcome such a problem; although, the coating with nitrogen and oxygen obtained by plasma immersion ion implantation (PIII) into a 7075 aluminum alloy surface was too shallow. This alloy is commonly used for structural parts in aerospace applications. Such a layer was characterized by secondary ion mass spectroscopy, electron microscopy, and nanoindentation experiments reciprocating wear tests. From the results, one can assume that the wear of this aluminum alloy starts presenting severe abrasive wear followed by an additional adhesive mechanism. PIII produced a slight difference, as shown in all characterizations carried out in this work. The results shown here can be used as the scientific basis for further nitrogen PIII experiments in aluminum alloys which have the goal to produce thicker modified layers or to improve their surface properties.

Keywords: aluminum alloys, plasma immersion ion implantation, tribological properties, hardness, nanofatigue

Procedia PDF Downloads 321
1024 An Experimental Analysis of Squeeze Casting Parameters for 2017 a Wrought Al Alloy

Authors: Mohamed Ben Amar, Najib Souissi, Chedly Bradai

Abstract:

A Taguchi design investigation has been made into the relationship between the ductility and process variables in a squeeze cast 2017A wrought aluminium alloy. The considered process parameters were: squeeze pressure, melt temperature and die preheating temperature. An orthogonal array (OA), main effect, signal-to-noise (S/N) ratio, and the analysis of variance (ANOVA) are employed to analyze the effect of casting parameters. The results have shown that the selected parameters significantly affect the ductility of 2017A wrought Al alloy castings. Optimal squeeze cast process parameters were provided to illustrate the proposed approach and the results were proven to be trustworthy through practical experiments.

Keywords: Taguchi method, squeeze casting, process parameters, ductility, microstructure

Procedia PDF Downloads 378
1023 Using the Micro Computed Tomography to Study the Corrosion Behavior of Magnesium Alloy at Different pH Values

Authors: Chia-Jung Chang, Sheng-Che Chen, Ming-Long Yeh, Chih-Wei Wang, Chih-Han Chang

Abstract:

Introduction and Motivation: In recent years, magnesium alloy is used to be a kind of medical biodegradable materials. Magnesium is an essential element in the body and is efficiently excreted by the kidneys. Furthermore, the mechanical properties of magnesium alloy is closest to human bone. However, in some cases magnesium alloy corrodes so quickly that it would release hydrogen on surface of implant. The other product is hydroxide ion, it can significantly increase the local pH value. The above situations may have adverse effects on local cell functions. On the other hand, nowadays magnesium alloy corrode too fast to maintain the function of implant until the healing of tissue. Therefore, much recent research about magnesium alloy has focused on controlling the corrosion rate. The in vitro corrosion behavior of magnesium alloys is affected by many factors, and pH value is one of factors. In this study, we will study on the influence of pH value on the corrosion behavior of magnesium alloy by the Micro-CT (micro computed tomography) and other instruments.Material and methods: In the first step, we make some guiding plates for specimens of magnesium alloy AZ91 by Rapid Prototyping. The guiding plates are able to be a standard for the degradation of specimen, so that we can use it to make sure the position of specimens in the CT image. We can also simplify the conditions of degradation by the guiding plates.In the next step, we prepare the solution with different pH value. And then we put the specimens into the solution to start the corrosion test. The CT image, surface photographs and weigh are measured on every twelve hours. Results: In the primary results of the test, we make sure that CT image can be a way to quantify the corrosion behavior of magnesium alloy. Moreover we can observe the phenomenon that corrosion always start from some erosion point. It’s possibly based on some defect like dislocations and the voids with high strain energy in the materials. We will deal with the raw data into Mass Loss (ML) and corrosion rate by CT image, surface photographs and weigh in the near future. Having a simple prediction, the pH value and degradation rate will be negatively correlated. And we want to find out the equation of the pH value and corrosion rate. We also have a simple test to simulate the change of the pH value in the local region. In this test the pH value will rise to 10 in a short time. Conclusion: As a biodegradable implant for the area with stagnating body fluid flow in the human body, magnesium alloy can cause the increase of local pH values and release the hydrogen. Those may damage the human cell. The purpose of this study is finding out the equation of the pH value and corrosion rate. After that we will try to find the ways to overcome the limitations of medical magnesium alloy.

Keywords: magnesium alloy, biodegradable materials, corrosion, micro-CT

Procedia PDF Downloads 437
1022 Barriers to Marital Expectation among Individuals with Hearing Impairment in Oyo State

Authors: Adebomi M. Oyewumi, Sunday Amaize

Abstract:

The study was designed to examine the barriers to marital expectations among unmarried persons with hearing impairment in Oyo State, Nigeria. Descriptive survey research design was adopted. Purposive sampling technique was used to select one hundred participants made up forty-four (44) males and fifty-six (56) females, all with varying degrees of hearing impairment. Eight research questions were raised and answered. The instrument used was Marital Expectations Scale with reliability coefficient of 0.86. Data was analyzed using descriptive statistics tools of frequency count and simple percentage as well as inferential statistics tools of T-TEST and ANOVA. The findings revealed that there was a significant relationship existing among the main identified barriers (environmental barrier, communication barrier, hearing loss, unemployment and poor sexuality education) to the marital expectations of unmarried persons with hearing impairment. The joint contribution of the independent variables (identified barriers) to the dependent variable (marital expectations) was significant, F = 5.842, P < 0.05, accounting for about 89% of the variance. The relative contribution of the identified barriers to marital expectations of unmarried persons with hearing impairment is as follows: environmental barrier (β = 0.808, t = 5.176, P < 0.05), communication barrier (β = 0.533, t = 3.305, P < 0.05), hearing loss (β = 0.550, t = 2.233, P < 0.05), unemployment (β = 0.431, t = 2.102, P < 0.05), poor sexuality education (β = 0.361, t = 1.985, P < 0.05). Environmental barrier proved to be the most potent contributor to the poor marital expectations among unmarried persons with hearing impairment. Therefore, it is recommended that society dismantles the nagging environmental barrier through positive identification with individuals suffering from hearing impairment. In this connection, members of society should change their negative attitudes and do away with all the wrong notions about the marital ability of individuals with hearing impairment.

Keywords: environmental barrier, hearing impairment, marriage, marital expectations

Procedia PDF Downloads 346
1021 Atom Probe Study of Early Stage of Precipitation on Binary Al-Li, Al-Cu Alloys and Ternary Al-Li-Cu Alloys

Authors: Muna Khushaim

Abstract:

Aluminum-based alloys play a key role in modern engineering, especially in the aerospace industry. Introduction of solute atoms such as Li and Cu is the main approach to improve the strength in age-hardenable Al alloys via the precipitation hardening phenomenon. Knowledge of the decomposition process of the microstructure during the precipitation reaction is particularly important for future technical developments. The objective of this study is to investigate the nano-scale chemical composition in the Al-Cu, Al-Li and Al-Li-Cu during the early stage of the precipitation sequence and to describe whether this compositional difference correlates with variations in the observed precipitation kinetics. Comparing the random binomial frequency distribution and the experimental frequency distribution of concentrations in atom probe tomography data was used to investigate the early stage of decomposition in the different binary and ternary alloys which were experienced different heat treatments. The results show that an Al-1.7 at.% Cu alloy requires a long ageing time of approximately 8 h at 160 °C to allow the diffusion of Cu atoms into Al matrix. For the Al-8.2 at.% Li alloy, a combination of both the natural ageing condition (48 h at room temperature) and a short artificial ageing condition (5 min at 160 °C) induces increasing on the number density of the Li clusters and hence increase number of precipitated δ' particles. Applying this combination of natural ageing and short artificial ageing conditions onto the ternary Al-4 at.% Li-1.7 at.% Cu alloy induces the formation of a Cu-rich phase. Increasing the Li content in the ternary alloy up to 8 at.% and increasing the ageing time to 30 min resulted in the precipitation processes ending with δ' particles. Thus, the results contribute to the understanding of Al-alloy design.

Keywords: aluminum alloy, atom probe tomography, early stage, decomposition

Procedia PDF Downloads 326
1020 Depressive Trends in Children and Adolescents Suffering from Beta-Thalassemia

Authors: Sanober Khanum, Barerah Siddiqui, Asim Qidwai

Abstract:

Objective: To determine the risk factors and frequency of depressive trends in children and adolescents suffering from Beta-Thalassemia. Background: Thalassemia is a chronic disease affecting 10,000 people in 60 countries. Many studies show that prolonged medical conditions cause depression. Due to the invasive procedures and suffering, Beta-Thalassemia cause great psychological distress to both children and their caregivers. The study shows 14-24% prevalence of psychiatric problems in Thalassemic patients. Method: Sample consisted of 195 registered patients of A.M.T.F (Female=95 and Male=100). Based on age range the sample was divided into two groups, Group A = children (4-9 years) and Group B = adolescent (10-16 years). A detailed interview with a self-made screening measure was administered on parents to find out the level of depression in patients. Statistics: Chi-square and t-test was applied in order to analyze the data. Results show high prevalence of depression, depression n= 131(66.83%), no depression n=65(33.16%). Analyses reflect that age influences the level of depression Adolescent (71.05%) and Children (64.16%). The analysis also shows a difference in level of depression between both genders. (t=2.975, p < .05). Conclusion: There is a high possibility of developing depressive trend in children affected with Beta Thalassemia; especially females. Therefore, there is a dire need for psychological screening and appropriate treatment in order to improve physical; as well as mental health.

Keywords: childhood depression, chronic illness, psychopathology, Thalassemia

Procedia PDF Downloads 305
1019 Study of Corrosion Behavior of Experimental Alloys with Different Levels of Cr and High Levels of Mo Compared to Aisi 444

Authors: Ana P. R. N. Barroso, Maurício N. Kleinberg, Frederico R. Silva, Rodrigo F. Guimarães, Marcelo M. V. Parente, Walney S. Araújo

Abstract:

The fight against accelerated wear of the equipment used in the oil and gas sector is a challenge for minimizing maintenance costs. Corrosion being one of the main agents of equipment deterioration, we seek alternative materials that exhibit improved corrosion resistance at low cost of production. This study aims to evaluate the corrosion behavior of experimental alloys containing 15% and 17% of chromium (Cr) and 5% of molybdenum (Mo) in comparison with an AISI 444 commercial alloy. Microstructural analyzes were performed on samples of the alloys before and after the electrochemical tests. Two samples of each solubilized alloy were also taken for analysis of the corrosion behavior by testing potentiodynamic polarization (PP) and Electrochemical Impedance Spectroscopy (EIS) with immersion time of 24 hours in electrolytic solution with acidic character. The graphics obtained through electrochemical tests of PP and EIS indicated that among the experimental alloys, the alloy with higher chromium content (17%) had a higher corrosion resistance, confirming the beneficial effect of adding chromium. When comparing the experimental alloys with the AISI 444 commercial alloy, it is observed that the AISI 444 commercial alloy showed superior corrosion resistance to that of the experimental alloys for both assays, PP and EIS. The microstructural analyzes performed after the PP and EIS tests confirmed the results previously described. These results suggest that the addition of these levels of molybdenum did not favor the electrochemical behavior of experimental ferritic alloys for the electrolytic medium studied.

Keywords: corrosion, molybdenum, electrochemical tests, experimental alloys

Procedia PDF Downloads 551
1018 Double Beta Decay Experiments in Novi Sad

Authors: Nataša Todorović, Jovana Nikolov

Abstract:

Despite the great interest in β⁻β⁻ decay, β⁺β⁺ decays are rarely investigated due to the low probability of detecting these processes with available low-level equipment. If β⁺β⁺, β⁺EC, or ECEC decay occurs in a thin sample of a material, the positrons will be stopped and annihilated inside the material, leading to the emission of two or four coincidence gamma photons energy of 511 keV. The paper presents the results of measurements of double beta decay of ⁶⁴Zn, ⁵⁰Cr, and ⁵⁴Fe isotopes. In the first experiment, 511-keV gamma rays originating from the annihilation of positrons in natural zinc were measured by a coincidence technique to obtain a non-zero value for the (0ν+2ν) half-life. In the second experiment, the result of measuring double beta decay of ⁵⁰Cr is presented, which suggests a result other than zero at 95% CL and gives the lowest limit for the half-life of this process. In the third experiment, neutrino-less ECEC decay of ⁵⁴Fe was examined. Under the decay theory, gamma rays are emitted whose energy does not coincide with the energies of gamma rays emitted by nuclei from known discrete excited states. Iron shield of an internal volume of 1 m³ and thickness of 25 cm served as a source for measuring the (0ν+2ν) process in ⁵⁴Fe, whose yield in natural iron is 5.4%. We obtain the lower limit for the half-life for ⁵⁴Fe: T(0ν, K, K)>4.4x10²⁰ yr, T(0ν, K, L)>4.1x10²⁰ yr, and T(0ν, L, L)>5.0x10²⁰ yr. For ⁵⁰Cr limit for the half-life is T(0ν+2ν)>1.3(6)x10¹⁸ yr, and for ⁶⁴Zn T(0ν+2ν, ECβ+)=1.1(0.9)x10⁹ years.

Keywords: neutrinoless double beta decay, half-life, ⁶⁴Zn, ⁵⁰Cr, and, ⁵⁴Fe

Procedia PDF Downloads 89
1017 Investigation of Nd-Al-Fe Added Nd-Fe-B Alloy Produced by Arc Melting

Authors: Gülten Sadullahoğlu, Baki Altuncevahir

Abstract:

The scope of this study, to investigate the magnetic properties and microstructure of Nd₂Fe₁₄B₁ by alloying with Nd₃₃.₄Fe₆₂.₆Al₄, and heat treating it at different temperatures. The stoichiometric Nd₂Fe₁₄B hard magnetic alloy and Nd₃₃.₄Fe₆₂.₆Al₄ composition was produced by arc melting under argon atmosphere. The Nd₃₃.₄Fe₆₂.₆Al₄ alloy has added to the 2:14:1 hard magnetic alloy with 48% by weight, and melted again by arc melting. Then, it was heat treated at 600, 700 and 800˚C for 3h under vacuum. In AC magnetic susceptibility measurements, for the as-cast sample, the signals decreased sharply at 101 ˚C and 313 ˚C corresponding to the Curie temperatures of the two ferromagnetic phases in addition to Fe phase. For the sample annealed at 600 ˚C, two Curie points were observed at about 257˚C and at 313˚C. However, the phase corresponding to the Curie temperature of 101 ˚C was disappeared. According to the magnetization measurements, the saturation magnetization has the highest value of 99.8 emu/g for the sample annealed at 600 ˚C, and decreased to 57.66 and 28.6 emu/g for the samples annealed at 700˚ and 800 ˚C respectively. Heat treatment resulted in an evolution of the new phase that caused changes in magnetic properties of the alloys. In order to have a clear picture, the identification of these phases are being under the investigation by XRD and SEM–EDX analysis.

Keywords: NdFeB hard magnets, bulk magnetic materials, arc melting, Curie temperature, heat treatment

Procedia PDF Downloads 263
1016 Isolation and Screening of Fungal Strains for β-Galactosidase Production

Authors: Parmjit S. Panesar, Rupinder Kaur, Ram S. Singh

Abstract:

Enzymes are the biocatalysts which catalyze the biochemical processes and thus have a wide variety of applications in the industrial sector. β-Galactosidase (E.C. 3.2.1.23) also known as lactase, is one of the prime enzymes, which has significant potential in the dairy and food processing industries. It has the capability to catalyze both the hydrolytic reaction for the production of lactose hydrolyzed milk and transgalactosylation reaction for the synthesis of prebiotics such as lactulose and galactooligosaccharides. These prebiotics have various nutritional and technological benefits. Although, the enzyme is naturally present in almonds, peaches, apricots and other variety of fruits and animals, the extraction of enzyme from these sources increases the cost of enzyme. Therefore, focus has been shifted towards the production of low cost enzyme from the microorganisms such as bacteria, yeast and fungi. As compared to yeast and bacteria, fungal β-galactosidase is generally preferred as being extracellular and thermostable in nature. Keeping the above in view, the present study was carried out for the isolation of the β-galactosidase producing fungal strain from the food as well as the agricultural wastes. A total of more than 100 fungal cultures were examined for their potential in enzyme production. All the fungal strains were screened using X-gal and IPTG as inducers in the modified Czapek Dox Agar medium. Among the various isolated fungal strains, the strain exhibiting the highest enzyme activity was chosen for further phenotypic and genotypic characterization. The strain was identified as Rhizomucor pusillus on the basis of 5.8s RNA gene sequencing data.

Keywords: beta-galactosidase, enzyme, fungal, isolation

Procedia PDF Downloads 229
1015 Formation of Protective Aluminum-Oxide Layer on the Surface of Fe-Cr-Al Sintered-Metal-Fibers via Multi-Stage Thermal Oxidation

Authors: Loai Ben Naji, Osama M. Ibrahim, Khaled J. Al-Fadhalah

Abstract:

The objective of this paper is to investigate the formation and adhesion of a protective aluminum-oxide (Al2O3, alumina) layer on the surface of Iron-Chromium-Aluminum Alloy (Fe-Cr-Al) sintered-metal-fibers. The oxide-scale layer was developed via multi-stage thermal oxidation at 930 oC for 1 hour, followed by 1 hour at 960 oC, and finally at 990 oC for 2 hours. Scanning Electron Microscope (SEM) images show that the multi-stage thermal oxidation resulted in the formation of predominantly Al2O3 platelets-like and whiskers. SEM images also reveal non-uniform oxide-scale growth on the surface of the fibers. Furthermore, peeling/spalling of the alumina protective layer occurred after minimum handling, which indicates weak adhesion forces between the protective layer and the base metal alloy.  Energy Dispersive Spectroscopy (EDS) analysis of the heat-treated Fe-Cr-Al sintered-metal-fibers confirmed the high aluminum content on the surface of the protective layer, and the low aluminum content on the exposed base metal alloy surface. In conclusion, the failure of the oxide-scale protective layer exposes the base metal alloy to further oxidation, and the fragile non-uniform oxide-scale is not suitable as a support for catalysts.

Keywords: high-temperature oxidation, iron-chromium-aluminum alloy, alumina protective layer, sintered-metal-fibers

Procedia PDF Downloads 181
1014 Sintering Properties of Mechanically Alloyed Ti-5Al-2.5Fe

Authors: Ridvan Yamanoglu, Erdinc Efendi, Ismail Daoud

Abstract:

In this study, Ti-5Al-2.5Fe alloy was prepared by powder metallurgy. The elemental titanium, aluminum, and iron powders were mechanically alloyed for 10 h in a vacuum atmosphere. A stainless steel jar and stainless steel balls were used for mechanical alloying. The alloyed powders were then sintered by vacuum hot pressing at 950 °C for a soaking time of 30 minutes. Pure titanium was also sintered at the same conditions for comparison of mechanical properties and microstructural behavior. The samples were investigated by scanning electron microscopy, XRD analysis, and optical microscopy. Results showed that, after mechanical alloying, a homogeneous distribution of the elements was obtained, and desired a-b structure was determined. Ti-5Al-2.5Fe alloy was successfully produced, and the alloy showed enhanced mechanical properties compared to the commercial pure titanium.

Keywords: Ti5Al-2.5Fe, mechanical alloying, hot pressing, sintering

Procedia PDF Downloads 260
1013 Determination of Gross Alpha and Gross Beta Activity in Water Samples by iSolo Alpha/Beta Counting System

Authors: Thiwanka Weerakkody, Lakmali Handagiripathira, Poshitha Dabare, Thisari Guruge

Abstract:

The determination of gross alpha and beta activity in water is important in a wide array of environmental studies and these parameters are considered in international legislations on the quality of water. This technique is commonly applied as screening method in radioecology, environmental monitoring, industrial applications, etc. Measuring of Gross Alpha and Beta emitters by using iSolo alpha beta counting system is an adequate nuclear technique to assess radioactivity levels in natural and waste water samples due to its simplicity and low cost compared with the other methods. Twelve water samples (Six samples of commercially available bottled drinking water and six samples of industrial waste water) were measured by standard method EPA 900.0 consisting of the gas-less, firm wear based, single sample, manual iSolo alpha beta counter (Model: SOLO300G) with solid state silicon PIPS detector. Am-241 and Sr90/ Y90 calibration standards were used to calibrate the detector. The minimum detectable activities are 2.32mBq/L and 406mBq/L, for alpha and beta activity, respectively. Each of the 2L water samples was evaporated (at low heat) to a small volume and transferred into 50mm stainless steel counting planchet evenly (for homogenization) and heated by IR lamp and the constant weighted residue was obtained. Then the samples were counted for gross alpha and beta. Sample density on the planchet area was maintained below 5mg/cm. Large quantities of solid wastes sludges and waste water are generated every year due to various industries. This water can be reused for different applications. Therefore implementation of water treatment plants and measuring water quality parameters in industrial waste water discharge is very important before releasing them into the environment. This waste may contain different types of pollutants, including radioactive substances. All these measured waste water samples having gross alpha and beta activities, lower than the maximum tolerance limits for industrial waste water discharge of industrial waste in to inland surface water, that is 10-9µCi/mL and 10-8µCi/mL for gross alpha and beta respectively (National Environmental Act, No. 47 of 1980). This is according to extraordinary gazette of the democratic socialist republic of Sri Lanka in February 2008. The measured water samples were below the recommended radioactivity levels and do not pose any radiological hazard when releasing the environment. Drinking water is an essential requirement of life. All the drinking water samples were below the permissible levels of 0.5Bq/L for gross alpha activity and 1Bq/L for gross beta activity. The values have been proposed by World Health Organization in 2011; therefore the water is acceptable for consumption of humans without any further clarification with respect to their radioactivity. As these screening levels are very low, the individual dose criterion (IDC) would usually not be exceeded (0.1mSv y⁻¹). IDC is a criterion for evaluating health risks from long term exposure to radionuclides in drinking water. Recommended level of 0.1mSv/y expressed a very low level of health risk. This monitoring work will be continued further for environmental protection purposes.

Keywords: drinking water, gross alpha, gross beta, waste water

Procedia PDF Downloads 174
1012 Hybrid Sol-Gel Coatings for Corrosion Protection of AA6111-T4 Aluminium Alloy

Authors: Shadatul Hanom Rashid, Xiaorong Zhou

Abstract:

Hybrid sol-gel coatings are the blend of both advantages of inorganic and organic networks have been reported as environmentally friendly anti-corrosion surface pre-treatment for several metals, including aluminum alloys. In this current study, Si-Zr hybrid sol-gel coatings were synthesized from (3-glycidoxypropyl)trimethoxysilane (GPTMS), tetraethyl orthosilicate (TEOS) and zirconium(IV) propoxide (TPOZ) precursors and applied on AA6111 aluminum alloy by dip coating technique. The hybrid sol-gel coatings doped with different concentrations of cerium nitrate (Ce(NO3)3) as a corrosion inhibitor were also prepared and the effect of Ce(NO3)3 concentrations on the morphology and corrosion resistance of the coatings were examined. The surface chemistry and morphology of the hybrid sol-gel coatings were analyzed by Fourier transform infrared (FTIR) spectroscopy and scanning electron microscopy (SEM). The corrosion behavior of the coated aluminum alloy samples was evaluated by electrochemical impedance spectroscopy (EIS). Results revealed that good corrosion resistance of hybrid sol-gel coatings were prepared from hydrolysis and condensation reactions of GPTMS, TEOS and TPOZ precursors deposited on AA6111 aluminum alloy. When the coating doped with cerium nitrate, the properties were improved significantly. The hybrid sol-gel coatings containing lower concentration of cerium nitrate offer the best inhibition performance. A proper doping concentration of Ce(NO3)3 can effectively improve the corrosion resistance of the alloy, while an excessive concentration of Ce(NO3)3 would reduce the corrosion protection properties, which is associated with defective morphology and instability of the sol-gel coatings.

Keywords: AA6111, Ce(NO3)3, corrosion, hybrid sol-gel coatings

Procedia PDF Downloads 133
1011 Pyrroloquinoline Quinone Enhances the Mitochondrial Function by Increasing Beta-Oxidation and a Balanced Mitochondrial Recycling in Mice Granulosa Cells

Authors: Moustafa Elhamouly, Masayuki Shimada

Abstract:

The production of competent oocytes is essential for reproductivity in mammals. Maintenance of mitochondrial efficiency is required to supply the ATP necessary for granulosa cell proliferation during the follicular development process. Treatment with Pyrroloquinoline quinone (PQQ) has been reported to increase the number of ovulated oocytes and pups per delivery in mice by maintaining healthy mitochondrial function. This study aimed to elucidate how PQQ maintains mitochondrial function during ovarian follicle growth. To do this, both in vitro and in vivo experiments were performed with granulosa cells from superovulated immature (3-week-old) mice that were pretreated with or without PQQ. The effects of PQQ on beta-oxidation, mitochondrial function, mitophagy, and mitochondrial biogenesis were examined. PQQ increased beta-oxidation-related genes and CPT1 protein content in granulosa cells and this was associated with a decreased phosphorylation of P38 signaling protein. Using the fatty acid oxidation assay on the flux analyzer, PQQ increased the reliance of beta-oxidation on the endogenous fatty acids and was associated with a mild UCP-dependant mitochondrial uncoupling, ATP production, mitophagy, and mitochondrial biogenesis. PQQ also increased the expression of endogenous antioxidant enzymes. Thus, PQQ induced beta-oxidation in growing granulosa cells relying on endogenous fatty acids. And reduced the Reactive oxygen species (ROS) production by inducing a mild mitochondrial uncoupling with keeping high mitochondrial function. Damaged mitochondria were recycled by the induced mitophagy and replaced by the increased mitochondrial biogenesis. Collectively, PQQ may enhance reproductivity by maintaining the efficiency of mitochondria to produce enough ATP required for normal folliculogenesis.

Keywords: granulosa cells, mitochondrial uncoupling, mitophagy, pyrroloquinoline quinone (PQQ), reactive oxygen species (ROS).

Procedia PDF Downloads 61
1010 Postpartum Depression and Its Association with Food Insecurity and Social Support among Women in Post-Conflict Northern Uganda

Authors: Kimton Opiyo, Elliot M. Berry, Patil Karamchand, Barnabas K. Natamba

Abstract:

Background: Postpartum depression (PPD) is a major psychiatric disorder that affects women soon after birth and in some cases, is a continuation of antenatal depression. Food insecurity (FI) and social support (SS) are known to be associated with major depressive disorder, and vice versa. This study was conducted to examine the interrelationships among FI, SS, and PPD among postpartum women in Gulu, a post-conflict region in Uganda. Methods: Cross-sectional data from postpartum women on depression symptoms, FI and SS were, respectively, obtained using the Center for Epidemiologic Studies-Depression (CES-D) scale, Individually Focused FI Access scale (IFIAS) and Duke-UNC functional social support scale. Standard regression methods were used to assess associations among FI, SS, and PPD. Results: A total of 239 women were studied, and 40% were found to have any PPD, i.e., with depressive symptom scores of ≥ 17. The mean ± standard deviation (SD) for FI score and SS scores were 6.47 ± 5.02 and 19.11 ± 4.23 respectively. In adjusted analyses, PPD symptoms were found to be positively associated with FI (unstandardized beta and standardized beta of 0.703 and 0.432 respectively, standard errors =0.093 and p-value < 0.0001) and negatively associated with SS (unstandardized beta and standardized beta of -0.263 and -0.135 respectively, standard errors = 0.111 and p-value = 0.019). Conclusions: Many women in this post-conflict region reported experiencing PPD. In addition, this data suggest that food security and psychosocial support interventions may help mitigate women’s experience of PPD or its severity.

Keywords: postpartum depression, food insecurity, social support, post-conflict region

Procedia PDF Downloads 147
1009 The Influence of Beta Shape Parameters in Project Planning

Authors: Αlexios Kotsakis, Stefanos Katsavounis, Dimitra Alexiou

Abstract:

Networks can be utilized to represent project planning problems, using nodes for activities and arcs to indicate precedence relationship between them. For fixed activity duration, a simple algorithm calculates the amount of time required to complete a project, followed by the activities that comprise the critical path. Program Evaluation and Review Technique (PERT) generalizes the above model by incorporating uncertainty, allowing activity durations to be random variables, producing nevertheless a relatively crude solution in planning problems. In this paper, based on the findings of the relevant literature, which strongly suggests that a Beta distribution can be employed to model earthmoving activities, we utilize Monte Carlo simulation, to estimate the project completion time distribution and measure the influence of skewness, an element inherent in activities of modern technical projects. We also extract the activity criticality index, with an ultimate goal to produce more accurate planning estimations.

Keywords: beta distribution, PERT, Monte Carlo simulation, skewness, project completion time distribution

Procedia PDF Downloads 127
1008 Hot Deformability of Si-Steel Strips Containing Al

Authors: Mohamed Yousef, Magdy Samuel, Maha El-Meligy, Taher El-Bitar

Abstract:

The present work is dealing with 2% Si-steel alloy. The alloy contains 0.05% C as well as 0.85% Al. The alloy under investigation would be used for electrical transformation purposes. A heating (expansion) - cooling (contraction) dilation investigation was executed to detect the a, a+g, and g transformation temperatures at the inflection points of the dilation curve. On heating, primary a  was detected at a temperature range between room temperature and 687 oC. The domain of a+g was detected in the range between 687 oC and 746 oC. g phase exists in the closed g region at the range between 746 oC and 1043 oC. The domain of a phase appears again at a temperature range between 1043 and 1105 oC, and followed by secondary a at temperature higher than 1105 oC. A physical simulation of thermo-mechanical processing on the as-cast alloy was carried out. The simulation process took into consideration the hot flat rolling pilot plant parameters. The process was executed on the thermo-mechanical simulator (Gleeble 3500). The process was designed to include seven consecutive passes. The 1st pass represents the roughing stage, while the remaining six passes represent finish rolling stage. The whole process was executed at the temperature range from 1100 oC to 900 oC. The amount of strain starts with 23.5% at the roughing pass and decreases continuously to reach 7.5 % at the last finishing pass. The flow curve of the alloy can be abstracted from the stress-strain curves representing simulated passes. It shows alloy hardening from a pass to the other up to pass no. 6, as a result of decreasing the deformation temperature and increasing of cumulative strain. After pass no. 6, the deformation process enhances the dynamic recrystallization phenomena to appear, where the z-parameter would be high.

Keywords: si- steel, hot deformability, critical transformation temperature, physical simulation, thermo-mechanical processing, flow curve, dynamic softening.

Procedia PDF Downloads 224
1007 Influence of the Growth Rate on Eutectic Microstructures and Physical Properties of Aluminum–Silicon-Cobalt Alloy

Authors: Aynur Aker, Hasan Kaya

Abstract:

Al-12.6wt.%Si-%2wt.Co alloy was prepared in a graphite crucible under vacuum atmosphere. The samples were directionally solidified upwards with different growth rate at constant temperature gradient using by Bridgman–type growth apparatus. The values of microstructures (λ) was measured from transverse sections of the samples. The microhardness (HV), ultimate tensile strength (σ) and electrical resistivity (ρ) of the directional solidification samples were also measured. Influence of the growth rate and spacings on microhardness, ultimate tensile strength and electrical resistivity were investigated and the relationships between them were experimentally obtained by using regression analysis. The results obtained in present work were compared with the previous similar experimental results obtained for binary and ternary alloys.

Keywords: directional solidification, Al-Si-Co alloy, mechanical properties, electrical properties

Procedia PDF Downloads 268
1006 Surface Modification of Titanium Alloy with Laser Treatment

Authors: Nassier A. Nassir, Robert Birch, D. Rico Sierra, S. P. Edwardson, G. Dearden, Zhongwei Guan

Abstract:

The effect of laser surface treatment parameters on the residual strength of titanium alloy has been investigated. The influence of the laser surface treatment on the bonding strength between the titanium and poly-ether-ketone-ketone (PEKK) surfaces was also evaluated and compared to those offered by titanium foils without surface treatment to optimize the laser parameters. Material characterization using an optical microscope was carried out to study the microstructure and to measure the mean roughness value of the titanium surface. The results showed that the surface roughness shows a significant dependency on the laser power parameters in which surface roughness increases with the laser power increment. Moreover, the results of the tensile tests have shown that there is no significant dropping in tensile strength for the treated samples comparing to the virgin ones. In order to optimize the laser parameter as well as the corresponding surface roughness, single-lap shear tests were conducted on pairs of the laser treated titanium stripes. The results showed that the bonding shear strength between titanium alloy and PEKK film increased with the surface roughness increment to a specific limit. After this point, it is interesting to note that there was no significant effect for the laser parameter on the bonding strength. This evidence suggests that it is not necessary to use very high power of laser to treat titanium surface to achieve a good bonding strength between titanium alloy and the PEKK film.

Keywords: bonding strength, laser surface treatment, PEKK, poly-ether-ketone-ketone, titanium alloy

Procedia PDF Downloads 320
1005 Effect of thermal aging on Low Cycle Fatigue of Alloy 690

Authors: Kushal Gowda Jayaram, Joseph Huret, Jonathan Quibel, Walter-John Chitty, Gilbert Henaff

Abstract:

Thermal aging is one of the concerns for the long-term operation of nuclear power plants. Indeed, components in the primary circuit undergo thermal aging while exposed to the chemically active environment of Pressurized Water Reactors (PWRs) over time. Among the materials used in the reactor components, Alloy 690 can be found in some critical components for nuclear safety. Despite its importance, research on the effect of thermal aging on the microstructural changes and low cycle fatigue (LCF) behavior of Alloy 690 remains limited. This study aims to assess the impact of thermal aging on the fatigue life of Alloy 690. The as-received sample underwent aging at 420°C for 4000 hours, representing the equivalent aging of 60 years in reactor working conditions. First, the characterization of the area and density of intergranular and intragranular precipitates was performed to understand the microstructural changes in the aged specimen. Then, low cycle fatigue tests were conducted on the as received and aged samples at varying strain amplitudes. To investigate the influence of thermal aging on the fatigue behavior of Alloy 690, fracture surfaces were analyzed to estimate fatigue crack growth rates based on striation spacing measurements. Additionally, the axially cut fractured samples have undergone analysis using Electron Backscatter Diffraction (EBSD) to understand the effect of aging on strain localization near the crack path. Results indicate that while the characterization of the area and density of intergranular precipitates in the aged specimen (for 2000 hours, approximately 30 years) showed no significant changes, there was a slight increase in the area and density of intragranular precipitates under the same conditions.

Keywords: alloy 690, thermal aging, low cycle fatigue, precipitates

Procedia PDF Downloads 21
1004 Specific Frequency of Globular Clusters in Different Galaxy Types

Authors: Ahmed H. Abdullah, Pavel Kroupa

Abstract:

Globular clusters (GC) are important objects for tracing the early evolution of a galaxy. We study the correlation between the cluster population and the global properties of the host galaxy. We found that the correlation between cluster population (NGC) and the baryonic mass (Mb) of the host galaxy are best described as 10 −5.6038Mb. In order to understand the origin of the U -shape relation between the GC specific frequency (SN) and Mb (caused by the high value of SN for dwarfs galaxies and giant ellipticals and a minimum SN for intermediate mass galaxies≈ 1010M), we derive a theoretical model for the specific frequency (SNth). The theoretical model for SNth is based on the slope of the power-law embedded cluster mass function (β) and different time scale (Δt) of the forming galaxy. Our results show a good agreement between the observation and the model at a certain β and Δt. The model seems able to reproduce higher value of SNth of β = 1.5 at the midst formation time scale.

Keywords: galaxies: dwarf, globular cluster: specific frequency, number of globular clusters, formation time scale

Procedia PDF Downloads 310
1003 Effects of Kolavironon Liver Oxidative Stress and Beta-Cell Damage in Streptozotocin-Induced Diabetic Rats

Authors: Omolola R. Ayepola, Nicole L. Brooks, Oluwafemi O. Oguntibeju

Abstract:

The liver plays an important role in the regulation of blood glucose and is a target organ of hyperglycaemia. Hyperglycemia plays a crucial role in the onset of various liver diseases and may culminate into hepatopathy if untreated. Alteration in antioxidant defense and increase in oxidative stress that results in tissue injury is characteristic of diabetes. We evaluated the protective effects of kolaviron-a biflavonoid complex, on hepatic antioxidants, lipid peroxidation and apoptosis in the liver of diabetic rats. To induce type I diabetes, rats were injected with streptozotocin intraperitoneally at a single dose of 50 mg/kg. Oral treatment of diabetic rats with kolaviron (100 mg/kg) started on the 6th day after diabetes induction and continued for 6 weeks (5 times weekly). Diabetic rats exhibited a significant increase in the peroxidation of hepatic lipids as observed from the elevated level of malondialdehyde (MDA) estimated by High-Performance Liquid Chromatography. In addition, Oxygen Radical Absorbance Capacity (ORAC), ratio of reduced to oxidized glutathione (GSH/GSSG) and catalase (CAT) activity was decreased in the liver of diabetic rats. TUNEL assay revealed increased apoptotic cell death in the liver of diabetic rats. Examination of Pancreatic beta-cells by immunohistochemical methods revealed beta cell degeneration and reduction in beta cell/ islet area in the diabetic controls. Kolaviron-treatment increased the area of insulin immunoreactive beta-cells significantly. Kolaviron attenuated lipid peroxidation and apoptosis in the liver of diabetic rats, increased CAT activity GSH levels and the resultant GSH: GSSG. The ORAC of kolaviron-treated diabetic liver was restored to near-normal values. Kolaviron protects the liver against oxidative and apoptotic damage induced by hyperglycemia. The antidiabetic effect of kolaviron may also be related to its beneficial effects on beta-cell function.

Keywords: diabetes mellitus, kolaviron, oxidative stress, liver, apoptosis

Procedia PDF Downloads 371