415 Dissolution of South African Limestone for Wet Flue Gas Desulphurization
Authors: Lawrence Koech, Ray Everson, Hein Neomagus, Hilary Rutto
Abstract:
Wet Flue gas desulphurization (FGD) systems are commonly used to remove sulphur dioxide from flue gas by contacting it with limestone in aqueous phase which is obtained by dissolution. Dissolution is important as it affects the overall performance of a wet FGD system. In the present study, effects of pH, stirring speed, solid to liquid ratio and acid concentration on the dissolution of limestone using an organic acid (adipic acid) were investigated. This was investigated using the pH stat apparatus. Calcium ions were analyzed at the end of each experiment using Atomic Absorption (AAS) machine.Keywords: desulphurization, limestone, dissolution, pH stat apparatus
Procedia PDF Downloads 460414 Geomorphology of Karst Features of Shiraz City and Arjan Plain and Development Limitations
Authors: Meysam Jamali, Ebrahim Moghimi, Zean Alabden Jafarpour
Abstract:
Karst term is the determiner of a variety of areas or landforms and unique perspectives that have been formed in result of the ingredients dissolution of rocks constituter by natural waters. Shiraz area with an area of 5322km2 is located in the simple folded belt in the southern part of Zagros Mountain of Fars, and is surrounded with Limestone Mountains (Asmari formation). Shiraz area is located in Calcareous areas. The Infrastructure of this city is lime and absorbing wells that the city has, can influence on the Limestone dissolution and those accelerate its rate and increases the cavitation below the surface. Dasht-e Arjan is a graben, which has been created as the result of activity of two normal faults in its east and west sides. It is a complete sample of Karst plains (Polje) which has been created with the help of tectonic forces (fault) and dissolution process of water in Asmari limestone formation. It is located 60km. off south west of Shiraz (on Kazeroon-Shiraz road). In 1971, UNESCO has recognized this plain as a reserve of biosphere. It is considered as one of the world’s most beautiful geological phenomena, so that most of the world’s geologists are interested in visiting this place. The purpose of this paper is to identify and introduce landscapes of Karst features shiraz city and Dasht-e Arjan including Karst dissolution features (Lapiez, Karst springs, dolines, caves, underground caves, ponors, and Karst valleys), anticlines and synclines, and Arjan Lake, which are studied in this paper.Keywords: Dasht-eArjan, fault, Karst features, polje, Shiraz city, Zagros
Procedia PDF Downloads 420413 Controlling Differential Settlement of Large Reservoir through Soil Structure Interaction Approach
Authors: Madhav Khadilkar
Abstract:
Construction of a large standby reservoir was required to provide secure water supply. The new reservoir was required to be constructed at the same location of an abandoned old open pond due to space constraints. Some investigations were carried out earlier to improvise and re-commission the existing pond. But due to a lack of quantified risk of settlement from voids in the underlying limestone, the shallow foundations were not found feasible. Since the reservoir was resting on hard strata for about three-quarter of plan area and one quarter was resting on soil underlying with limestone and considerably low subgrade modulus. Further investigations were carried out to ascertain the locations and extent of voids within the limestone. It was concluded that the risk due to lime dissolution was acceptably low, and the site was found geotechnically feasible. The hazard posed by limestone dissolution was addressed through the integrated structural and geotechnical analysis and design approach. Finite Element Analysis was carried out to quantify the stresses and differential settlement due to various probable loads and soil-structure interaction. Walls behaving as cantilever under operational loads were found undergoing in-plane bending and tensile forces due to soil-structure interaction. Sensitivity analysis for varying soil subgrade modulus was carried out to check the variation in the response of the structure and magnitude of stresses developed. The base slab was additionally checked for the loss of soil contact due to lime pocket formations at random locations. The expansion and contraction joints were planned to receive minimal additional forces due to differential settlement. The reservoir was designed to sustain the actions corresponding to allowable deformation limits per code, and geotechnical measures were proposed to achieve the soil parameters set in structural analysis.Keywords: differential settlement, limestone dissolution, reservoir, soil structure interaction
Procedia PDF Downloads 154412 Microfacies Analysis, Depositional Environment, and Diagentic Process of the Antalo Limestone Successions in the Mekelle Outlier (Hagere-Selam, Messobo and Wukro Sections), Northern Ethiopia
Authors: Werede Girmay Tesfasilasiea
Abstract:
Three stratigraphic sections of the Antalo Limestone successions in Mekelle Outlier, northern Ethiopia (at Hagere-Selam, Messobo, and Wukro sections) have been investigated to distinguish their microfacies features, reservoir characterization, and their equivalent depositional environments. The Antalo Limestone successions were deposited in the Mekelle Outlier during the Upper Jurassic period as a result of flooding of the area by the Tethys Ocean toward the southeast direction. This study is based on field description and petrographic analysis to determine the depositional environment, age, and reservoir characteristics of the carbonate units. According to petrographical studies of 100 thin sections and field investigation, 14 microfacies types are recognized. These are grouped into 4 microfacies association of a tidal flat (MFT1-2), lagoons (MFL1-2), shoal (MFS1-4), and open marine environment (MFO1-6). Hence, the Antalo limestone successions are deposited in shallow carbonate ramps with a wide lateral and vertical distribution of facies. The carbonate units in the studied sections are affected by bioturbation, micritization, cementation, dolomitization, dissolution, silicification, and compaction type of early diagenetic alteration. Dissolution and dolomitization affected the type of rock, showing good reservoir quality, while cementation and compaction affected the type of rock, resulting in poor reservoir quality in the Antalo Limestone successions of the Mekelle outlier. Based on the abundant distribution of the Alveosepta jaccardi (Schrodt), Pseudocyclammina lituus (Yokoyama), Kurnubia palestiniensis (Henson), and Somalirhynchia africana in the studied sections the Antalo Limestone successions assigned to the Late Oxfordian-Kimmeridgian age.Keywords: Antelo limestone successions, depositional environment, Mekelle outlier, microfacies analysis, diagenesis, reservoir quality
Procedia PDF Downloads 54411 Experimental Investigation on Correlation Between Permeability Variation and Sabkha Soil Salts Dissolution
Authors: Fahad A. Alotaibi
Abstract:
An increase in salt dissolution rate with continuous water flow is expected to lead to the progressive collapse of the soil structure. Evaluation of the relationship between soil salt dissolution and the variation of sabkha soil permeability in terms of type, rate, and quantity in order to assure construction safety in these environments. The current study investigates the relationship of soil permeability with the rate of dissolution of calcium (Ca2+), sulfate (SO4-2), chloride (CL−1), magnesium (Mg2+), sodium (Na+), and potassium (K+1) ions. Results revealed an increase in sabkha soil permeability with the rate of ions dissolution. This makes the efficiency of using a waterproofing stabilization agent in the reduction of sabkha salts dissolution the main criterion is selecting suitable stabilizing method.Keywords: sabkha, permeability, salts, dissolution
Procedia PDF Downloads 105410 Prediction of in situ Permeability for Limestone Rock Using Rock Quality Designation Index
Authors: Ahmed T. Farid, Muhammed Rizwan
Abstract:
Geotechnical study for evaluating soil or rock permeability is a highly important parameter. Permeability values for rock formations are more difficult for determination than soil formation as it is an effect of the rock quality and its fracture values. In this research, the prediction of in situ permeability of limestone rock formations was predicted. The limestone rock permeability was evaluated using Lugeon tests (in-situ packer permeability). Different sites which spread all over the Riyadh region of Saudi Arabia were chosen to conduct our study of predicting the in-situ permeability of limestone rock. Correlations were deducted between the values of in-situ permeability of the limestone rock with the value of the rock quality designation (RQD) calculated during the execution of the boreholes of the study areas. The study was performed for different ranges of RQD values measured during drilling of the sites boreholes. The developed correlations are recommended for the onsite determination of the in-situ permeability of limestone rock only. For the other sedimentary formations of rock, more studies are needed for predicting the actual correlations related to each type.Keywords: In situ, packer, permeability, rock, quality
Procedia PDF Downloads 371409 Investigation of Dissolution in Diammonium Hydrogen Phosphate Solutions of Gypsum
Authors: Turan Çalban, Nursel Keskin, Sabri Çolak, Soner Kuşlu
Abstract:
Gypsum (CaSO4.2H2O) is a mineral that is found in large quantities in the Turkey and in the World. The dissolution of this mineral in the diammonium hydrogen phosphate solutions has not been studied so far. Investigation of the dissolution and dissolution kinetics gypsum in diammonium hydrogen phosphate solutions will be useful for evaluating of solid wastes containing gypsum. In this study, parameters such as diammonium hydrogen phosphate concentration, temperature and stirring speed affecting on the dissolution rate of the gypsum in diammonium hydrogen phosphate solutions were investigated. In experimental studies have researched effectiveness of the selected parameters. The dissolution of gypsum were examined in two parts at low and high temperatures. The experimental results were successfully correlated by linear regression using Statistica program. Dissolution curves were evaluated shrinking core models for solid-fluid systems. The activation energy was found to be 34.58 kJ/mol and 44.45 kJ/mol for the low and the high temperatures. The dissolution of gypsum was controlled by chemical reaction both low temperatures and high temperatures. Reaction rate expressions of dissolution of gypsum at the low temperatures and the high temperatures controlled by chemical reaction are as follows, respectively. = k1.e-5159.5/T.t = k2.e-5346.8/T.t Where k1 and k2 are constants depending on the diammonium hydrogen phosphate solution concentration, the solid/liquid ratio, the stirring speed and the particle size.Keywords: diammonium hydrogen phosphate, dissolution kinetics, gypsum, kinetics.
Procedia PDF Downloads 387408 Microfacies and Diagenetic Study of Rembang Limestone, Central Java, Indonesia
Authors: Evalita Amrita, Abdurrokhim, Ildrem Syafri
Abstract:
Research area is located in Pasedan District, Rembang Regency, Central Java Province. This research is being held for the purpose of microfacies and diagenetic study of carbonate rocks. The study area is dominated by deformed carbonate rocks, folded and faulted. The research method is petrographic analysis with red alizarin staining to differentiate mineral types. Microfacies types and diagenetic processes can be known from petrographic analysis of rock texture, rock structure, type of grain, and fossils. Carbonate rocks in the study area can be divided into 4 types of microfacies: Reef Microfacies (SMF 7), Shallow Water Microfacies (SMF 9), and Textural Inversion Microfacies (SMF 10). Diagenetic processes that take place in carbonate rocks are microbial micritization, compaction, neomorphism, cementation, and dissolution.Keywords: diagenetic, limestone, microfacies, Rembang
Procedia PDF Downloads 239407 Influence of Surface Area on Dissolution of Additively Manufactured Polyvinyl Alcohol Tablets
Authors: Seyedebrahim Afkhami, Meisam Abdi, Reza Baserinia
Abstract:
Additive manufacturing is revolutionising production in different industries, including pharmaceuticals. This case study explores the influence of surface area on the dissolution of additively manufactured polyvinyl alcohol parts as a polymer candidate. Specimens of different geometries and constant mass were fabricated using a Fused Deposition Modelling 3D printer. The dissolution behaviour of these samples was compared with respect to their surface area. Improved and accelerated dissolution was observed for samples with a larger surface area. This study highlights the capabilities of additive manufacturing to produce samples of complex geometries that cannot be manufactured otherwise to control the dissolution behaviour for pharmaceutical and biopharmaceutical applications.Keywords: additive manufacturing, polymer dissolution, fused deposition modelling, geometry optimization
Procedia PDF Downloads 101406 Adhesion Study of Repair Mortar Based in Dune and Crushed Limestone Sand
Authors: Krobba Benharzallah, Kenai Said, Bouhicha Mohamed, Lakhdari Mohammed Fatah, Merah Ahmed
Abstract:
In recent years, great interest has been directed towards the use of local materials and natural resources in building and public works. This is to satisfy the enormous need for these materials and contribute to sustainable development. Among these resources, dune sand and limestone crushed sand, which can be an interesting alternative to the replacement of siliceous alluvial sands for the formulation of a repair mortar. The results found show that the particle size correction of dune sand by limestone sand and the addition of a superplasticizer are very beneficial in terms of adhesion and mechanical strength.Keywords: repair mortar, dune sand, crushed limestone sand, adhesion, mechanical strength
Procedia PDF Downloads 161405 Development of Green Cement, Based on Partial Replacement of Clinker with Limestone Powder
Authors: Yaniv Knop, Alva Peled
Abstract:
Over the past few years there has been a growing interest in the development of Portland Composite Cement, by partial replacement of the clinker with mineral additives. The motivations to reduce the clinker content are threefold: (1) Ecological - due to lower emission of CO2 to the atmosphere; (2) Economical - due to cost reduction; and (3) Scientific\Technology – improvement of performances. Among the mineral additives being used and investigated, limestone is one of the most attractive, as it is considered natural, available, and with low cost. The goal of the research is to develop green cement, by partial replacement of the clinker with limestone powder while improving the performances of the cement paste. This work studied blended cements with three limestone powder particle diameters: smaller than, larger than, and similarly sized to the clinker particle. Blended cement with limestone consisting of one particle size distribution and limestone consisting of a combination of several particle sizes were studied and compared in terms of hydration rate, hydration degree, and water demand to achieve normal consistency. The performances of these systems were also compared with that of the original cement (without added limestone). It was found that the ability to replace an active material with an inert additive, while achieving improved performances, can be obtained by increasing the packing density of the cement-based particles. This may be achieved by replacing the clinker with limestone powders having a combination of several different particle size distributions. Mathematical and physical models were developed to simulate the setting history from initial to final setting time and to predict the packing density of blended cement with limestone having different sizes and various contents. Besides the effect of limestone, as inert additive, on the packing density of the blended cement, the influence of the limestone particle size on three different chemical reactions were studied; hydration of the cement, carbonation of the calcium hydroxide and the reactivity of the limestone with the hydration reaction products. The main results and developments will be presented.Keywords: packing density, hydration degree, limestone, blended cement
Procedia PDF Downloads 285404 Heavy Metal Reduction in Plant Using Soil Amendment
Authors: C. Chaiyaraksa, T. Khamko
Abstract:
This study investigated the influence of limestone and sepiolite on heavy metals accumulation in the soil and soybean. The soil was synthesized to contaminate with zinc 150 mg/kg, copper 100 mg/kg, and cadmium 1 mg/kg. The contaminated soil was mixed with limestone and sepiolite at the ratio of 1:0, 0:1, 1:1, and 2:1. The amount of soil modifier added to soil was 0.2%, 0.4%, and 0.8%. The metals determination was performed on soil both before and after soybean planting and in the root, shoot, and seed of soybean after harvesting. The study was also on metal translocate from root to seed and on bioaccumulation factor. Using of limestone and sepiolite resulted in a reduction of metals accumulated in soybean. For soil containing a high concentration of copper, cadmium, and zinc, a mixture of limestone and sepiolite (1:1) was recommended to mix with soil with the amount of 0.2%. Zinc could translocate from root to seed more than copper, and cadmium. From studying the movement of metals from soil to accumulate in soybean, the result was that soybean could absorb the highest amount of cadmium, followed by zinc, and copper, respectively.Keywords: heavy metals, limestone, sepiolite, soil, soybean
Procedia PDF Downloads 153403 Evaluation of the Efficiency of Nanomaterials in the Consolidation of Limestone
Authors: Mohamed Saad Gad Elzoghby
Abstract:
Nanomaterials are widely used nowadays for the consolidation of degraded archaeological limestone. It’s one of the most predominant stones in monumental buildings and statuary works. It is exposed to different weathering processes that cause degradation and the presence of deterioration pattern as cracks, fissures, and granular disintegration. Nanomaterials have been applied to limestone consolidation. Among these nanomaterials are nanolimes, i.e., dispersions of lime nanoparticles in alcohols, and nano-silica, i.e., dispersions of silica nanoparticles in water, promising consolidating products for limestone. It was investigated and applied to overcome the disadvantages of traditional consolidation materials such as lime water, water glass, and paraliod. So, researchers investigated and tested the effectiveness of nanomaterials as consolidation materials for limestone. The present study includes an evaluation of some nanomaterials in consolidation limestone stone in comparison with traditional consolidants. These consolidation materials are nano calcium hydroxide nanolime, and nanosilica. The latter is known commercially as Nano Estel and the former Known as Nanorestore compared to traditional consolidants Wacker OH (ethyl silicate) and Paraloid B72 (a copolymer of ethyl methacrylate and methyl acrylate). The study evaluated the consolidation effectiveness of nanomaterials and traditional consolidants by using followed methods, characterization of physical properties of stone, scanning electron microscopy (SEM), X-ray diffractometry, Fourier transforms infrared spectroscopy, and mechanical properties. The study confirmed that nanomaterials were better in the distribution and encapsulation of calcite grains in limestone, and traditional materials were better in improving the physical properties of limestone. It demonstrated that good results could be achieved through mixtures of nanomaterials and traditional consolidants.Keywords: nanomaterials, limestone, consolidation, evaluation, weathering, nanolime, nanosilica, scanning electron microscope
Procedia PDF Downloads 80402 Evaluation of the Efficiency of Nanomaterials in Consolidation of Limestone
Authors: Mohamed Saad Gad Eloghby
Abstract:
Nanomaterials are widely used nowadays for the consolidation of degraded archaeological limestone. It’s one of the most predominant stones in monumental buildings and statuary works. Exposure to different weathering processes caused degradation and the presence of deterioration pattern as cracks, fissures, and granular disintegration. Nanomaterials have been applied to limestone consolidation. Among these nanomaterials are nanolimes, i.e., dispersions of lime nanoparticles in alcohols and nanosilica, i.e., dispersions of silica nanoparticles in water promising consolidating products for limestone. It was investigated and applied to overcome the disadvantages of traditional consolidation materials such as lime water, water glass and paraliod. So, researchers investigated and tested the effectiveness of nanomaterials as consolidation materials for limestone. The present study includes the evaluation of some nano materials in consolidation limestone stone in comparison with traditional consolidantes. These consolidation materials are nano calcium hydroxide nanolime and nanosilica. The latter is known commercially as Nano Estel and the former is known as Nanorestore compared to traditional consolidantes Wacker OH (ethyl silicate) and Paraloid B72 (a copolymer of ethyl methacrylate and methyl acrylate). The study evaluated the consolidation effectiveness of nanomaterials and traditional consolidantes by using followed methods, Characterization of physical properties of stone, Scanning electron microscopy (SEM), X-ray diffractometry, Fourier transform infrared spectroscopy and Mechanical properties. The study confirmed that nanomaterials were better in the distribution and encapsulation of calcite grains in limestone, and traditional materials were better in improving the physical properties of limestone. It demonstrated that good results can be achieved through mixtures of nanomaterials and traditional consolidants.Keywords: nanomaterials, limestone, consolidation, evaluation, weathering, nanolime, nanosilica, scanning electron microscope
Procedia PDF Downloads 73401 Effects of Particle Size Distribution of Binders on the Performance of Slag-Limestone Ternary Cement
Authors: Zhuomin Zou, Thijs Van Landeghem, Elke Gruyaert
Abstract:
Using supplementary cementitious materials, such as blast-furnace slag and limestone, to replace cement clinker is a promising method to reduce the carbon emissions from cement production. To efficiently use slag and limestone, it is necessary to carefully select the particle size distribution (PSD) of the binders. This study investigated the effects of the PSD of binders on the performance of slag-limestone ternary cement. The Portland cement (PC) was prepared by grinding 95% clinker + 5% gypsum. Based on the PSD parameters of the binders, three types of ternary cements with a similar overall PSD were designed, i.e., NO.1 fine slag, medium PC, and coarse limestone; NO.2 fine limestone, medium PC, and coarse slag; NO.3. fine PC, medium slag, and coarse limestone. The binder contents in the ternary cements were (a) 50 % PC, 40 % slag, and 10 % limestone (called high cement group) or (b) 35 % PC, 55 % slag, and 10 % limestone (called low cement group). The pure PC and binary cement with 50% slag and 50% PC prepared with the same binders as the ternary cement were considered as reference cements. All these cements were used to investigate the mortar performance in terms of workability, strength at 2, 7, 28, and 90 days, carbonation resistance, and non-steady state chloride migration resistance at 28 and 56 days. Results show that blending medium PC with fine slag could exhibit comparable performance to blending fine PC with medium/coarse slag in binary cement. For the three ternary cements in the high cement group, ternary cement with fine limestone (NO.2) shows the lowest strength, carbonation, and chloride migration performance. Ternary cements with fine slag (NO.1) and with fine PC (NO.3) show the highest flexural strength at early and late ages, respectively. In addition, compared with ternary cement with fine PC (NO.3), ternary cement with fine slag (NO.1) has a similar carbonation resistance and a better chloride migration resistance. For the low cement group, three ternary cements have a similar flexural and compressive strength before 7 days. After 28 days, ternary cement with fine limestone (NO.2) shows the highest flexural strength while fine PC (NO.3) has the highest compressive strength. In addition, ternary cement with fine slag (NO.1) shows a better chloride migration resistance but a lower carbonation resistance compared with the other two ternary cements. Moreover, the durability performance of ternary cement with fine PC (NO.3) is better than that of fine limestone (NO.2).Keywords: limestone, particle size distribution, slag, ternary cement
Procedia PDF Downloads 125400 Improved Wetting for Improved Solubility and Dissolution of Candesartan Cilexetil
Authors: Shilpa Bhilegaonkar, Ram Gaud
Abstract:
Candesartan cilexetil is a poorly soluble antihypertensive agent with solubility limited bioavailability (15%). To initiate process of solubilisation, it is very much necessary to displace the air at the surface and wet the drug surface with a solvent, with which drug is compatible. Present research adopts the same principle to improve solubility and dissolution of candesartan cilexetil. Solvents used here are surfactant and modified surfactant in different drug: solvent (1:1-1:9) ratio’s for preparation of adsorbates. Adsorbates were then converted into free flowing powders as liquisolid compacts and compressed to form tablets. Liquisolid compacts were evaluated for improvement in saturation solubility and dissolution of candesartan cilexetil. All systems were evaluated for improvement in saturation solubility and dissolution in different medias such as water, 0.1 N HCl, Phosphate buffer pH 6.8 and media given by office of generic drugs along with other physicochemical testing. All systems exhibited a promising advantage in terms of solubility and dissolution without affecting the drug structure as confirmed by IR and XRD. No considerable advantage was seen of increasing solvent ratio with drug.Keywords: candesartan cilexetil, improved dissolution, solubility, liquisolid
Procedia PDF Downloads 325399 PM10 Concentration Emitted from Blasting and Crushing Processes of Limestone Mines in Saraburi Province, Thailand
Authors: Kanokrat Makkwao, Tassanee Prueksasit
Abstract:
This study aimed to investigate PM10 emitted from different limestone mines in Saraburi province, Thailand. The blasting and crushing were the main processes selected for PM10 sampling. PM10 was collected in two mines including, a limestone mine for cement manufacturing (mine A) and a limestone mine for construction (mine B). The IMPACT samplers were used to collect PM10. At blasting, the points aligning with the upwind and downwind direction were assigned for the sampling. The ranges of PM10 concentrations at mine A and B were 0.267-5.592 and 0.130-0.325 mg/m³, respectively, and the concentration at blasting from mine A was significantly higher than mine B (p < 0.05). During crushing at mine A, the PM10 concentration with the range of 1.153-3.716 and 0.085-1.724 mg/m³ at crusher and piles in respectively were observed whereas the PM10 concentration measured at four sampling points in mine B, including secondary crusher, tertiary crusher, screening point, and piles, were ranged 1.032-16.529, 10.957-74.057, 0.655-4.956, and 0.169-1.699 mg/m³, respectively. The emission of PM10 concentration at the crushing units was different in the ranges depending on types of machine, its operation, dust collection and control system, and environmental conditions.Keywords: PM₁₀ concentration, limestone mines, blasting, crushing
Procedia PDF Downloads 142398 Estimation of Opc, Fly Ash and Slag Contents in Blended and Composite Cements by Selective Dissolution Method
Authors: Suresh Palla
Abstract:
This research paper presents the results of the study on the estimation of fly ash, slag and cement contents in blended and composite cements by novel selective dissolution method. Types of cement samples investigated include OPC with fly ash as performance improver, OPC with slag as performance improver, PPC, PSC and Composite cement confirming to respective Indian Standards. Slag and OPC contents in PSC were estimated by selectively dissolving OPC in stage 1 and selectively dissolving slag in stage 2. In the case of composite cement sample, the percentage of cement, slag and fly ash were estimated systematically by selective dissolution of cement, slag and fly ash in three stages. In the first stage, cement dissolved and separated by leaving the residue of slag and fly ash, designated as R1. The second stage involves gravimetric estimation of fractions of OPC, residue and selective dissolution of fly ash and slag contents. Fly ash content, R2 was estimated through gravimetric analysis. Thereafter, the difference between the R1 and R2 is considered as slag content. The obtained results of cement, fly ash and slag using selective dissolution method showed 10% of standard deviation with the corresponding percentage of respective constituents. The results suggest that this novel selective dissolution method can be successfully used for estimation of OPC and SCMs contents in different types of cements.Keywords: selective dissolution method , fly ash, ggbfs slag, edta
Procedia PDF Downloads 156397 Limestone Briquette Production and Characterization
Authors: André C. Silva, Mariana R. Barros, Elenice M. S. Silva, Douglas. Y. Marinho, Diego F. Lopes, Débora N. Sousa, Raphael S. Tomáz
Abstract:
Modern agriculture requires productivity, efficiency and quality. Therefore, there is need for agricultural limestone implementation that provides adequate amounts of calcium and magnesium carbonates in order to correct soil acidity. During the limestone process, fine particles (with average size under 400#) are generated. These particles do not have economic value in agricultural and metallurgical sectors due their size. When limestone is used for agriculture purposes, these fine particles can be easily transported by wind generated air pollution. Therefore, briquetting, a mineral processing technique, was used to mitigate this problem resulting in an agglomerated product suitable for agriculture use. Briquetting uses compressive pressure to agglomerate fine particles. It can be aided by agglutination agents, allowing adjustments in shape, size and mechanical parameters of the mass. Briquettes can generate extra profits for mineral industry, presenting as a distinct product for agriculture, and can reduce the environmental liabilities of the fine particles storage or disposition. The produced limestone briquettes were subjected to shatter and water action resistance tests. The results show that after six minutes completely submerged in water, the briquettes where fully diluted, a highly favorable result considering its use for soil acidity correction.Keywords: agglomeration, briquetting, limestone, soil acidity correction
Procedia PDF Downloads 389396 In vitro Disaggregation and Dissolution of Four IR Lamotrigine Solid Dosage Forms
Authors: Ilaria Manca, Ilaria Manca, Francesca Pettinau, Ignazia Mocci, Elisabetta M. Usai, Barbara Pittau
Abstract:
Lamotrigine is a phenyltriazine used in the treatment of epilepsy and bipolar disorder type I. The purpose of this study was to test and compare various solid forms of immediate release (IR) lamotrigine products, at different strenghts, in order to study their disaggregation and dissolution behavior. IR products are designed to release their active substance promptly after administration. Concentration of hydrochloric acid in gastric juice is about 0.1-0.001 M, so FDA (Food and Drug Administration) recommends, for lamotrigine regular tablets, dissolution tests in HCl 0.1 M.Toinvestigate the pH dependency of drug release in the entire gastrointestinal tract, we worked at two additional media with different pH values (4.5 and 6.8), that reflect conditions in it. To afford acceptable dissolution rates, tablets must disintegrate. Disaggregation of constituent particles increases the surface area and substantially increases the dissolution rate. For this reason availability of an active substance from tablets depends on its ability to disintegrate fast in dissolution media. pH of gastrointestinal fluid affects drug absorption by conditioning its solubility and dissolution, but also tablet disintegration may be influenced by it. To obtain information about the quantitative relationship between different mixture components, Nuclear Magnetic Resonance (NMR) spectroscopy was used. We also investigate tablet hardness. The investigation carried out confirms pH 1.2 as the ideal environment for the immediate availability of the active substance.Keywords: dissolution, disaggregation, Lamotrigine, bioequivalence
Procedia PDF Downloads 452395 Influence of Physical Properties on Estimation of Mechanical Strength of Limestone
Authors: Khaled Benyounes
Abstract:
Determination of the rock mechanical properties such as unconfined compressive strength UCS, Young’s modulus E, and tensile strength by the Brazilian test Rtb is considered to be the most important component in drilling and mining engineering project. Research related to establishing correlation between strength and physical parameters of rocks has always been of interest to mining and reservoir engineering. For this, many rock blocks of limestone were collected from the quarry located in Meftah(Algeria), the cores were crafted in the laboratory using a core drill. This work examines the relationships between mechanical properties and some physical properties of limestone. Many empirical equations are established between UCS and physical properties of limestone (such as dry bulk density, velocity of P-waves, dynamic Young’s modulus, alteration index, and total porosity). Others correlations UCS-tensile strength, dynamic Young’s modulus-static Young’s modulus have been find. Based on the Mohr-Coulomb failure criterion, we were able to establish mathematical relationships that will allow estimating the cohesion and internal friction angle from UCS and indirect tensile strength. Results from this study can be useful for mining industry for resolve range of geomechanical problems such as slope stability.Keywords: limestone, mechanical strength, Young’s modulus, porosity
Procedia PDF Downloads 453394 Carbonate Microfacies and Diagenesis of Klapanunggal Formation in Cileungsi District, Bogor Regency, West Java Province, Indonesia
Authors: Reghina Karyadi, Abdurrokhim, Lili Fauzielly
Abstract:
Administratively, the research area is located in Cileungsi District, Bogor Regency, West Java Province, Indonesia. Geographically, it located at 106° 56’ 1,9392” - 107° 1’ 27,8112” East Longitude and 6° 32’ 29,3712” - 6° 27’ 5,6124” South Latitude. This research is being held as a purpose to observe microfacies and limestone diagenesis that happened in the study area. Dominantly, the area fulfills of various hills that formed by carbonate and sediment stones which folded and faulted. The method that using in this research is analysis the outcrop data and petrography by using red alizarin for differentiating of minerals type. Microfacies type and diagenesis processes can be known from petrography analysis results like rock texture, rock structure, porosity, type of grain and fossils. The result of research shows that carbonate rocks in the study area can be divided into 3 types microfasies, which is Reef Microfacies (SMF 7), Shallow Water Microfacies (SMF 9), and Textural Inversion Microfacies (SMF 10). Whereas diagenesis process that happened is microbial micritization, compaction, neomorphism, cementation and dissolution process.Keywords: carbonate, limestone, microfacies, diagenesis
Procedia PDF Downloads 387393 Rupture Probability of Type of Coarse Aggregate on Fracture Surface of Concrete
Authors: B. Ramakrishna, S. Sivamurthy Reddy
Abstract:
The various types of aggregates such as granite, dolerite, Quartzite, dolomitic limestone, limestone and river gravel were used to produce the concrete with 28-day target compressive strength of 35, 60, and 80 Mpa. The compressive strength of concrete, as well as aggregates, was measured to study the effect of rupture probability of aggregate on the fracture surface of the concrete. Also, the petrographic studies were carried out to study the texture, type of minerals present and their relative proportions in various types of aggregates. The concrete of various grades produced with the same aggregate has shown a rise in RPCA with strength. However, the above relationship has ceased to exist in the concretes of the same grade, made of different types of aggregates. The carbonate aggregates namely Limestone and Dolomitic limestone have produced concrete with higher RPCA irrespective of the strength of concrete. The mode of origin, texture and mineralogical composition of aggregates have a significant impact on their pulse velocity and thereby the pulse velocity of concrete. Procedia PDF Downloads 292392 Physical and Mechanical Characterization of Limestone in the Quarry of Meftah (Algeria)
Authors: Khaled Benyounes
Abstract:
Determination of the rock mechanical properties such as unconfined compressive strength UCS, Young’s modulus E, and tensile strength by the Brazilian test Rtb is considered to be the most important component in drilling and mining engineering project. Research related to establishing correlation between strength and physical parameters of rocks has always been of interest to mining and reservoir engineering. For this, many rock blocks of limestone were collected from the quarry located in Meftah (Algeria), the cores were crafted in the laboratory using a core drill. This work examines the relationships between mechanical properties and some physical properties of limestone. Many empirical equations are established between UCS and physical properties of limestone (such as dry bulk density, velocity of P-waves, dynamic Young’s modulus, alteration index, and total porosity). Other correlations, UCS - tensile strength, dynamic Young’s modulus - static Young’s modulus have been find. Based on the Mohr-Coulomb failure criterion, we were able to establish mathematical relationships that will allow estimating the cohesion and internal friction angle from UCS and indirect tensile strength. Results from this study can be useful for mining industry for resolve range of geomechanical problems such as slope stability.Keywords: limestone, mechanical strength, Young’s modulus, porosity
Procedia PDF Downloads 636391 Foraminiferal Description and Biostratigraphy of Eocene Deposits in Zagros Basin (Izeh and Interior Fars Sub-Basins) in South-West of Iran
Authors: Ronak Gravand
Abstract:
Eocene deposits in Zagros basin in tow zones of interior Fars and Izeh include limestone and marly limestone succession along with abundant fossils. The significance of this area is due to its hydro carbonic resources. In Dashte Kuh section, limestone and marly limestone deposits with medium to thick creamy layers containing benthic foraminifera could be seen. Bio-zones identified in such deposits include Opertorbitolites Subzone, Somalina Subzone, Alveolina Nummulites Assemblage Subzone and Nummulites fabianii Silvestriella tetraedra Assembelage Zone. In Nil Kuh section, marly limestone of the succession contain abundant plagic foraminifera. The zones identified in this succession include Morozovella aragonesis Range Zone, Hantkenina nuttalli Range Zone, Hantkenina nuttalli Turborotalia cerro-azulensis Interval Zone, Turborotalia cerro-azulensis Range Zone and Morozovella aragonesis Range Zone.Keywords: zagros basin, foraminifera , biozone, Iran
Procedia PDF Downloads 500390 Passive Neutralization of Acid Mine Drainage Using Locally Produced Limestone
Authors: Reneiloe Seodigeng, Malwandla Hanabe, Haleden Chiririwa, Hilary Rutto, Tumisang Seodigeng
Abstract:
Neutralisation of acid-mine drainage (AMD) using limestone is cost effective, and good results can be obtained. However, this process has its limitations; it cannot be used for highly acidic water which consists of Fe(III). When Fe(III) reacts with CaCO3, it results in armoring. Armoring slows the reaction, and additional alkalinity can no longer be generated. Limestone is easily accessible, so this problem can be easily dealt with. Experiments were carried out to evaluate the effect of PVC pipe length on ferric and ferrous ions. It was found that the shorter the pipe length the more these dissolved metals precipitate. The effect of the pipe length on the hydrogen ions was also studied, and it was found that these two have an inverse relationship. Experimental data were further compared with the model prediction data to see if they behave in a similar fashion. The model was able to predict the behaviour of 1.5m and 2 m pipes in ferric and ferrous ion precipitation.Keywords: acid mine drainage, neutralisation, limestone, mathematical modelling
Procedia PDF Downloads 364389 Dissolution Kinetics of Chevreul’s Salt in Ammonium Cloride Solutions
Authors: Mustafa Sertçelik, Turan Çalban, Hacali Necefoğlu, Sabri Çolak
Abstract:
In this study, Chevreul’s salt solubility and its dissolution kinetics in ammonium chloride solutions were investigated. Chevreul’s salt that we used in the studies was obtained by using the optimum conditions (ammonium sulphide concentration; 0,4 M, copper sulphate concentration; 0,25 M, temperature; 60°C, stirring speed; 600 rev/min, pH; 4 and reaction time; 15 mins) determined by T. Çalban et al. Chevreul’s salt solubility in ammonium chloride solutions and the kinetics of dissolution were investigated. The selected parameters that affect solubility were reaction temperature, concentration of ammonium chloride, stirring speed, and solid/liquid ratio. Correlation of experimental results had been achieved using linear regression implemented in the statistical package program statistica. The effect of parameters on Chevreul’s salt solubility was examined and integrated rate expression of dissolution rate was found using kinetic models in solid-liquid heterogeneous reactions. The results revealed that the dissolution rate of Chevreul’s salt was decreasing while temperature, concentration of ammonium chloride and stirring speed were increasing. On the other hand, dissolution rate was found to be decreasing with the increase of solid/liquid ratio. Based on result of the applications of the obtained experimental results to the kinetic models, we can deduce that Chevreul’s salt dissolution rate is controlled by diffusion through the ash (or product layer). Activation energy of the reaction of dissolution was found as 74.83 kJ/mol. The integrated rate expression along with the effects of parameters on Chevreul's salt solubility was found to be as follows: 1-3(1-X)2/3+2(1-X)= [2,96.1013.(CA)3,08 .(S/L)-038.(W)1,23 e-9001,2/T].tKeywords: Chevreul's salt, copper, ammonium chloride, ammonium sulphide, dissolution kinetics
Procedia PDF Downloads 306388 Improving the Dissolution Rate of Folic Acid via the Antisolvent Vapour Precipitation
Authors: J. Y. Tan, L. C. Lum, M. G. Lee, S. Mansouri, K. Hapgood, X. D. Chen, M. W. Woo
Abstract:
Folic acid (FA) is known to be an important supplement to prevent neural tube defect (NTD) in pregnant women. Similar to some commercial formulations, sodium bicarbonate solution is used as a solvent for FA. This work uses the antisolvent vapor precipitation (AVP), incorporating ethanol vapor as the convective drying medium in place of air to produce branch-like micro-structure FA particles. Interestingly, the dissolution rate of the resultant particle is 2-3 times better than the particle produce from conventional air drying due to the higher surface area of particles produced. The higher dissolution rate could possibly improve the delivery and absorption of FA in human body. This application could potentially be extended to other commercial products, particularly in less soluble drugs to improve its solubility.Keywords: absorption, antisolvent vapor precipitation, dissolution rate, folic acid
Procedia PDF Downloads 443387 3D Scanning Documentation and X-Ray Radiography Examination for Ancient Egyptian Canopic Jar
Authors: Abdelrahman Mohamed Abdelrahman
Abstract:
Canopic jars are one of the vessels of funerary nature used by the ancient Egyptian in mummification process that were used to save the viscera of the mummified body after being extracted from the body and treated. Canopic jars are made of several types of materials like Limestone, Alabaster, and Pottery. The studied canopic jar dates back to Late period, located in the Grand Egyptian Museum (GEM), Giza, Egypt. This jar carved from limestone with carved hieroglyphic inscriptions, and it filled and closed by mortar from inside. Some aspects of damage appeared in the jar, such as dust, dirts, classification, wide crack, weakness of limestone. In this study, we used documentation and investigation modern techniques to document and examine the jar. 3D scanning and X-ray Radiography imaging used in applied study. X-ray imaging showed that the mortar was placed at a time when the jar contained probably viscera where the mortar appeared that not reach up to the base of the inner jar. Through the three-dimensional photography, the jar was documented, and we have 3D model of the jar, and now we have the ability through the computer to see any part of the jar in all its details. After that, conservation procedures have been applied with high accuracy to conserve the jar, including mechanical, wet, and chemical cleaning, filling wide crack in the body of the jar using mortar consisting of calcium carbonate powder mixing with primal E330 S, and consolidation, so the limestone became strong after using paraloid B72 2% concentrate as a consolidate material.Keywords: vessel, limestone, canopic jar, mortar, 3D scanning, X-ray radiography
Procedia PDF Downloads 75386 Reduction of Toxic Matter from Marginal Water Treatment Using Sludge Recycling from Combination of Stepped Cascade Weir with Limestone Trickling Filter
Authors: Dheyaa Wajid Abbood, Ali Mohammed Tawfeeq Baqer, Eitizaz Awad Jasim
Abstract:
The aim of this investigation is to confirm the activity of a sludge recycling process in trickling filter filled with limestone as an alternative biological process over conventional high-cost treatment process with regard to toxic matter reduction from marginal water. The combination system of stepped cascade weir with limestone trickling filter has been designed and constructed in the Environmental Hydraulic Laboratory, Al-Mustansiriya University, College of Engineering. A set of experiments has been conducted during the period from August 2013 to July 2014. Seven days of continuous operation with different continuous flow rates (0.4m3/hr, 0.5 m3/hr, 0.6 m3/hr, 0.7m3/hr,0.8 m3/hr, 0.9 m3/hr, and 1m3/hr) after ten days of acclimatization experiments were carried out. Results indicate that the concentrations of toxic matter were decreasing with increasing of operation time, sludge recirculation ratio, and flow rate. The toxic matter measured includes (Mineral oils, Petroleum products, Phenols, Biocides, Polychlorinated biphenyls (PCBs), and Surfactants) which are used in these experiments were ranged between (0.074 nm-0.156 nm). Results indicated that the overall reduction efficiency after 4, 28, 52, 76, 100, 124, and 148 hours of operation were (55%, 48%, 42%, 50%, 59%, 61%, and 64%) when the combination of stepped cascade weir with limestone trickling filter is used.Keywords: Marginal water , Toxic matter, Stepped Cascade weir, limestone trickling filter