Search results for: Ni–base superalloy ŽS6K
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 2104

Search results for: Ni–base superalloy ŽS6K

64 Peculiarities of Absorption near the Edge of the Fundamental Band of Irradiated InAs-InP Solid Solutions

Authors: Nodar Kekelidze, David Kekelidze, Elza Khutsishvili, Bela Kvirkvelia

Abstract:

The semiconductor devices are irreplaceable elements for investigations in Space (artificial Earth satellite, interplanetary space craft, probes, rockets) and for investigation of elementary particles on accelerators, for atomic power stations, nuclear reactors, robots operating on heavily radiation contaminated territories (Chernobyl, Fukushima). Unfortunately, the most important parameters of semiconductors dramatically worsen under irradiation. So creation of radiation-resistant semiconductor materials for opto and microelectronic devices is actual problem, as well as investigation of complicated processes developed in irradiated solid states. Homogeneous single crystals of InP-InAs solid solutions were grown with zone melting method. There has been studied the dependence of the optical absorption coefficient vs photon energy near fundamental absorption edge. This dependence changes dramatically with irradiation. The experiments were performed on InP, InAs and InP-InAs solid solutions before and after irradiation with electrons and fast neutrons. The investigations of optical properties were carried out on infrared spectrophotometer in temperature range of 10K-300K and 1mkm-50mkm spectral area. Radiation fluencies of fast neutrons was equal to 2·1018neutron/cm2 and electrons with 3MeV, 50MeV up to fluxes of 6·1017electron/cm2. Under irradiation, there has been revealed the exponential type of the dependence of the optical absorption coefficient vs photon energy with energy deficiency. The indicated phenomenon takes place at high and low temperatures as well at impurity different concentration and practically in all cases of irradiation by various energy electrons and fast neutrons. We have developed the common mechanism of this phenomenon for unirradiated materials and implemented the quantitative calculations of distinctive parameter; this is in a satisfactory agreement with experimental data. For the irradiated crystals picture get complicated. In the work, the corresponding analysis is carried out. It has been shown, that in the case of InP, irradiated with electrons (Ф=1·1017el/cm2), the curve of optical absorption is shifted to lower energies. This is caused by appearance of the tails of density of states in forbidden band due to local fluctuations of ionized impurity (defect) concentration. Situation is more complicated in the case of InAs and for solid solutions with composition near to InAs when besides noticeable phenomenon there takes place Burstein effect caused by increase of electrons concentration as a result of irradiation. We have shown, that in certain conditions it is possible the prevalence of Burstein effect. This causes the opposite effect: the shift of the optical absorption edge to higher energies. So in given solid solutions there take place two different opposite directed processes. By selection of solid solutions composition and doping impurity we obtained such InP-InAs, solid solution in which under radiation mutual compensation of optical absorption curves displacement occurs. Obtained result let create on the base of InP-InAs, solid solution radiation-resistant optical materials. Conclusion: It was established the nature of optical absorption near fundamental edge in semiconductor materials and it was created radiation-resistant optical material.

Keywords: InAs-InP, electrons concentration, irradiation, solid solutions

Procedia PDF Downloads 202
63 Modelling of Reactive Methodologies in Auto-Scaling Time-Sensitive Services With a MAPE-K Architecture

Authors: Óscar Muñoz Garrigós, José Manuel Bernabeu Aubán

Abstract:

Time-sensitive services are the base of the cloud services industry. Keeping low service saturation is essential for controlling response time. All auto-scalable services make use of reactive auto-scaling. However, reactive auto-scaling has few in-depth studies. This presentation shows a model for reactive auto-scaling methodologies with a MAPE-k architecture. Queuing theory can compute different properties of static services but lacks some parameters related to the transition between models. Our model uses queuing theory parameters to relate the transition between models. It associates MAPE-k related times, the sampling frequency, the cooldown period, the number of requests that an instance can handle per unit of time, the number of incoming requests at a time instant, and a function that describes the acceleration in the service's ability to handle more requests. This model is later used as a solution to horizontally auto-scale time-sensitive services composed of microservices, reevaluating the model’s parameters periodically to allocate resources. The solution requires limiting the acceleration of the growth in the number of incoming requests to keep a constrained response time. Business benefits determine such limits. The solution can add a dynamic number of instances and remains valid under different system sizes. The study includes performance recommendations to improve results according to the incoming load shape and business benefits. The exposed methodology is tested in a simulation. The simulator contains a load generator and a service composed of two microservices, where the frontend microservice depends on a backend microservice with a 1:1 request relation ratio. A common request takes 2.3 seconds to be computed by the service and is discarded if it takes more than 7 seconds. Both microservices contain a load balancer that assigns requests to the less loaded instance and preemptively discards requests if they are not finished in time to prevent resource saturation. When load decreases, instances with lower load are kept in the backlog where no more requests are assigned. If the load grows and an instance in the backlog is required, it returns to the running state, but if it finishes the computation of all requests and is no longer required, it is permanently deallocated. A few load patterns are required to represent the worst-case scenario for reactive systems: the following scenarios test response times, resource consumption and business costs. The first scenario is a burst-load scenario. All methodologies will discard requests if the rapidness of the burst is high enough. This scenario focuses on the number of discarded requests and the variance of the response time. The second scenario contains sudden load drops followed by bursts to observe how the methodology behaves when releasing resources that are lately required. The third scenario contains diverse growth accelerations in the number of incoming requests to observe how approaches that add a different number of instances can handle the load with less business cost. The exposed methodology is compared against a multiple threshold CPU methodology allocating/deallocating 10 or 20 instances, outperforming the competitor in all studied metrics.

Keywords: reactive auto-scaling, auto-scaling, microservices, cloud computing

Procedia PDF Downloads 96
62 Bio-Hub Ecosystems: Investment Risk Analysis Using Monte Carlo Techno-Economic Analysis

Authors: Kimberly Samaha

Abstract:

In order to attract new types of investors into the emerging Bio-Economy, new methodologies to analyze investment risk are needed. The Bio-Hub Ecosystem model was developed to address a critical area of concern within the global energy market regarding the use of biomass as a feedstock for power plants. This study looked at repurposing existing biomass-energy plants into Circular Zero-Waste Bio-Hub Ecosystems. A Bio-Hub model that first targets a ‘whole-tree’ approach and then looks at the circular economics of co-hosting diverse industries (wood processing, aquaculture, agriculture) in the vicinity of the Biomass Power Plants facilities. This study modeled the economics and risk strategies of cradle-to-cradle linkages to incorporate the value-chain effects on capital/operational expenditures and investment risk reductions using a proprietary techno-economic model that incorporates investment risk scenarios utilizing the Monte Carlo methodology. The study calculated the sequential increases in profitability for each additional co-host on an operating forestry-based biomass energy plant in West Enfield, Maine. Phase I starts with the base-line of forestry biomass to electricity only and was built up in stages to include co-hosts of a greenhouse and a land-based shrimp farm. Phase I incorporates CO2 and heat waste streams from the operating power plant in an analysis of lowering and stabilizing the operating costs of the agriculture and aquaculture co-hosts. Phase II analysis incorporated a jet-fuel biorefinery and its secondary slip-stream of biochar which would be developed into two additional bio-products: 1) A soil amendment compost for agriculture and 2) A biochar effluent filter for the aquaculture. The second part of the study applied the Monte Carlo risk methodology to illustrate how co-location derisks investment in an integrated Bio-Hub versus individual investments in stand-alone projects of energy, agriculture or aquaculture. The analyzed scenarios compared reductions in both Capital and Operating Expenditures, which stabilizes profits and reduces the investment risk associated with projects in energy, agriculture, and aquaculture. The major findings of this techno-economic modeling using the Monte Carlo technique resulted in the masterplan for the first Bio-Hub to be built in West Enfield, Maine. In 2018, the site was designated as an economic opportunity zone as part of a Federal Program, which allows for Capital Gains tax benefits for investments on the site. Bioenergy facilities are currently at a critical juncture where they have an opportunity to be repurposed into efficient, profitable and socially responsible investments, or be idled and scrapped. The Bio-hub Ecosystems techno-economic analysis model is a critical model to expedite new standards for investments in circular zero-waste projects. Profitable projects will expedite adoption and advance the critical transition from the current ‘take-make-dispose’ paradigm inherent in the energy, forestry and food industries to a more sustainable Bio-Economy paradigm that supports local and rural communities.

Keywords: bio-economy, investment risk, circular design, economic modelling

Procedia PDF Downloads 101
61 Seismo-Volcanic Hazards in Great Ararat Region, Eastern Turkey

Authors: Mehmet Salih Bayraktutan, Emre Tokmak

Abstract:

Great Ararat Volcano is the highest peak in South Caucasus Volcanic Plateau. Uplifted by Quaternary basaltic pyroclastic and lava flows. Numerous volcanic cones formed along with the tensional fractures under N-S compressional geodynamic framework. Basaltic flows have fresh surface morphology give ages of 650-680 K years. Hyperstene andesites constitute a major mass of Greater Ararat gives ages of 450-490 K years. During the early eruption period, predominately pyroclastics, cinder, lapilly-ash volcanic bombs were extruded. Third-period eruptions dominantly basaltic lava flows. Andesitic domes aligned along with the NW-SE striking fractures. Hyalo basalt and hornblende basaltic lavas are the latest lava eruptions. Hyalo-basaltic eruptions occurred via parasitic cones distributed far from the center. Parasitic cones are most common at the foot of Mount covered by recent NW flowing basaltic lava. Some of the cones are distributed on a circular pattern. One of the most hazardous disasters recorded in Eastern Turkey was July 1840 Cehennem Canyon Flood. Volcanic activities seismically triggered resulted in melting of glacier cap, mixed with ash and pyroclastics, flowed down along the Valley. Mud rich Slush urged catastrophically northwards, crossed Ars River and damned Surmeli Basin, forming reservoir behind. Ararat volcanoes are located on NW-SE striking Agri Fault Zone. Right lateral extensional faults, along which a series of andesitic domes formed. Great Ararat, in general strato-type volcano. This huge structure, developed in two main parts with different topographic and morphological features. The large lower base covers a widespread area composed of predominantly pyroclastics, ignimbrites, aglomerates, thick pumice, perlite deposits. Approximately 1/3 of the Crest by height formed of this basement. And 2/3 of the upper part with a conic- shape composed of basaltic lava flows. The active tectonic structure consists of three different patterns. The first network is radially distributed fractures formed during the last stage of lava eruptions. The second group of active faults striking in NW direction, and continue in N30W strike, formes Igdir Fault Zone. The third set of faults, dipping in the northwest with 75-80 degrees, strikes NE- SW across the whole Mount, slicing Great Ararat into four segments. In the upper stage of Cehennem Canyon, this set cutting volcanic layers caused numerous Waterfalls, Rock Avalanches, Mud Flows along the canyon, threatens the Village of Yanidogan, at the apex of flood deposits. Great Ararat Region has high seismo-tectonic risk and by occurrence frequency and magnitude, which caused in history caused heavy disasters, at villages surrounding the Ararat Basement.

Keywords: Eastern Turkey, geohazard, great ararat volcano, seismo-tectonic features

Procedia PDF Downloads 182
60 Global Winners versus Local Losers: Globalization Identity and Tradition in Spanish Club Football

Authors: Jim O'brien

Abstract:

Contemporary global representation and consumption of La Liga across a plethora of media platform outlets has resulted in significant implications for the historical, political and cultural developments which shaped the development of Spanish club football. This has established and reinforced a hierarchy of a small number of teams belonging to or aspiring to belong to a cluster of global elite clubs seeking to imitate the blueprint of the English Premier League in respect of corporate branding and marketing in order to secure a global fan base through success and exposure in La Liga itself and through the Champions League. The synthesis between globalization, global sport and the status of high profile clubs has created radical change within the folkloric iconography of Spanish football. The main focus of this paper is to critically evaluate the consequences of globalization on the rich tapestry at the core of the game’s distinctive history in Spain. The seminal debate underpinning the study considers whether the divergent aspects of globalization have acted as a malevolent force, eroding tradition, causing financial meltdown and reducing much of the fabric of club football to the status of by standers, or have promoted a renaissance of these traditions, securing their legacies through new fans and audiences. The study draws on extensive sources on the history, politics and culture of Spanish football, in both English and Spanish. It also uses primary and archive material derived from interviews and fieldwork undertaken with scholars, media professionals and club representatives in Spain. The paper has four main themes. Firstly, it contextualizes the key historical, political and cultural forces which shaped the landscape of Spanish football from the late nineteenth century. The seminal notions of region, locality and cultural divergence are pivotal to this discourse. The study then considers the relationship between football, ethnicity and identity as a barometer of continuity and change, suggesting that tradition is being reinvented and re-framed to reflect the shifting demographic and societal patterns within the Spanish state. Following on from this, consideration is given to the paradoxical function of ‘El Clasico’ and the dominant duopoly of the FC Barcelona – Real Madrid axis in both eroding tradition in the global nexus of football’s commodification and in protecting historic political rivalries. To most global consumers of La Liga, the mega- spectacle and hyperbole of ‘El Clasico’ is the essence of Spanish football, with cultural misrepresentation and distortion catapulting the event to the global media audience. Finally, the paper examines La Liga as a sporting phenomenon in which elite clubs, cult managers and galacticos serve as commodities on the altar of mass consumption in football’s global entertainment matrix. These processes accentuate a homogenous mosaic of cultural conformity which obscures local, regional and national identities and paradoxically fuses the global with the local to maintain the distinctive hue of La Liga, as witnessed by the extraordinary successes of Athletico Madrid and FC Eibar in recent seasons.

Keywords: Spanish football, globalization, cultural identity, tradition, folklore

Procedia PDF Downloads 302
59 Bacterial Exposure and Microbial Activity in Dental Clinics during Cleaning Procedures

Authors: Atin Adhikari, Sushma Kurella, Pratik Banerjee, Nabanita Mukherjee, Yamini M. Chandana Gollapudi, Bushra Shah

Abstract:

Different sharp instruments, drilling machines, and high speed rotary instruments are routinely used in dental clinics during dental cleaning. Therefore, these cleaning procedures release a lot of oral microorganisms including bacteria in clinic air and may cause significant occupational bioaerosol exposure risks for dentists, dental hygienists, patients, and dental clinic employees. Two major goals of this study were to quantify volumetric airborne concentrations of bacteria and to assess overall microbial activity in this type of occupational environment. The study was conducted in several dental clinics of southern Georgia and 15 dental cleaning procedures were targeted for sampling of airborne bacteria and testing of overall microbial activity in settled dusts over clinic floors. For air sampling, a Biostage viable cascade impactor was utilized, which comprises an inlet cone, precision-drilled 400-hole impactor stage, and a base that holds an agar plate (Tryptic soy agar). A high-flow Quick-Take-30 pump connected to this impactor pulls microorganisms in air at 28.3 L/min flow rate through the holes (jets) where they are collected on the agar surface for approx. five minutes. After sampling, agar plates containing the samples were placed in an ice chest with blue ice and plates were incubated at 30±2°C for 24 to 72 h. Colonies were counted and converted to airborne concentrations (CFU/m3) followed by positive hole corrections. Most abundant bacterial colonies (selected by visual screening) were identified by PCR amplicon sequencing of 16S rRNA genes. For understanding overall microbial activity in clinic floors and estimating a general cleanliness of the clinic surfaces during or after dental cleaning procedures, ATP levels were determined in swabbed dust samples collected from 10 cm2 floor surfaces. Concentration of ATP may indicate both the cell viability and the metabolic status of settled microorganisms in this situation. An ATP measuring kit was used, which utilized standard luciferin-luciferase fluorescence reaction and a luminometer, which quantified ATP levels as relative light units (RLU). Three air and dust samples were collected during each cleaning procedure (at the beginning, during cleaning, and immediately after the procedure was completed (n = 45). Concentrations at the beginning, during, and after dental cleaning procedures were 671±525, 917±1203, and 899±823 CFU/m3, respectively for airborne bacteria and 91±101, 243±129, and 139±77 RLU/sample, respectively for ATP levels. The concentrations of bacteria were significantly higher than typical indoor residential environments. Although an increasing trend for airborne bacteria was observed during cleaning, the data collected at three different time points were not significantly different (ANOVA: p = 0.38) probably due to high standard deviations of data. The ATP levels, however, demonstrated a significant difference (ANOVA: p <0.05) in this scenario indicating significant change in microbial activity on floor surfaces during dental cleaning. The most common bacterial genera identified were: Neisseria sp., Streptococcus sp., Chryseobacterium sp., Paenisporosarcina sp., and Vibrio sp. in terms of frequencies of occurrences, respectively. The study concluded that bacterial exposure in dental clinics could be a notable occupational biohazard, and appropriate respiratory protections for the employees are urgently needed.

Keywords: bioaerosols, hospital hygiene, indoor air quality, occupational biohazards

Procedia PDF Downloads 312
58 Speech and Swallowing Function after Tonsillo-Lingual Sulcus Resection with PMMC Flap Reconstruction: A Case Study

Authors: K. Rhea Devaiah, B. S. Premalatha

Abstract:

Background: Tonsillar Lingual sulcus is the area between the tonsils and the base of the tongue. The surgical resection of the lesions in the head and neck results in changes in speech and swallowing functions. The severity of the speech and swallowing problem depends upon the site and extent of the lesion, types and extent of surgery and also the flexibility of the remaining structures. Need of the study: This paper focuses on the importance of speech and swallowing rehabilitation in an individual with the lesion in the Tonsillar Lingual Sulcus and post-operative functions. Aim: Evaluating the speech and swallow functions post-intensive speech and swallowing rehabilitation. The objectives are to evaluate the speech intelligibility and swallowing functions after intensive therapy and assess the quality of life. Method: The present study describes a report of an individual aged 47years male, with the diagnosis of basaloid squamous cell carcinoma, left tonsillar lingual sulcus (pT2n2M0) and underwent wide local excision with left radical neck dissection with PMMC flap reconstruction. Post-surgery the patient came with a complaint of reduced speech intelligibility, and difficulty in opening the mouth and swallowing. Detailed evaluation of the speech and swallowing functions were carried out such as OPME, articulation test, speech intelligibility, different phases of swallowing and trismus evaluation. Self-reported questionnaires such as SHI-E(Speech handicap Index- Indian English), DHI (Dysphagia handicap Index) and SESEQ -K (Self Evaluation of Swallowing Efficiency in Kannada) were also administered to know what the patient feels about his problem. Based on the evaluation, the patient was diagnosed with pharyngeal phase dysphagia associated with trismus and reduced speech intelligibility. Intensive speech and swallowing therapy was advised weekly twice for the duration of 1 hour. Results: Totally the patient attended 10 intensive speech and swallowing therapy sessions. Results indicated misarticulation of speech sounds such as lingua-palatal sounds. Mouth opening was restricted to one finger width with difficulty chewing, masticating, and swallowing the bolus. Intervention strategies included Oro motor exercise, Indirect swallowing therapy, usage of a trismus device to facilitate mouth opening, and change in the food consistency to help to swallow. A practice session was held with articulation drills to improve the production of speech sounds and also improve speech intelligibility. Significant changes in articulatory production and speech intelligibility and swallowing abilities were observed. The self-rated quality of life measures such as DHI, SHI and SESE Q-K revealed no speech handicap and near-normal swallowing ability indicating the improved QOL after the intensive speech and swallowing therapy. Conclusion: Speech and swallowing therapy post carcinoma in the tonsillar lingual sulcus is crucial as the tongue plays an important role in both speech and swallowing. The role of Speech-language and swallowing therapists in oral cancer should be highlighted in treating these patients and improving the overall quality of life. With intensive speech-language and swallowing therapy post-surgery for oral cancer, there can be a significant change in the speech outcome and swallowing functions depending on the site and extent of lesions which will thereby improve the individual’s QOL.

Keywords: oral cancer, speech and swallowing therapy, speech intelligibility, trismus, quality of life

Procedia PDF Downloads 112
57 Baseline Data for Insecticide Resistance Monitoring in Tobacco Caterpillar, Spodoptera litura (Fabricius) (Lepidoptera: Noctuidae) on Cole Crops

Authors: Prabhjot Kaur, B.K. Kang, Balwinder Singh

Abstract:

The tobacco caterpillar, Spodoptera litura (Fabricius) (Lepidoptera: Noctuidae) is an agricultural important pest species. S. litura has a wide host range of approximately recorded 150 plant species worldwide. In Punjab, this pest attains sporadic status primarily on cauliflower, Brassica oleracea (L.). This pest destroys vegetable crop and particularly prefers the cruciferae family. However, it is also observed feeding on other crops such as arbi, Colocasia esculenta (L.), mung bean, Vigna radiata (L.), sunflower, Helianthus annuus (L.), cotton, Gossypium hirsutum (L.), castor, Ricinus communis (L.), etc. Larvae of this pest completely devour the leaves of infested plant resulting in huge crop losses which ranges from 50 to 70 per cent. Indiscriminate and continuous use of insecticides has contributed in development of insecticide resistance in insects and caused the environmental degradation as well. Moreover, a base line data regarding the toxicity of the newer insecticides would help in understanding the level of resistance developed in this pest and any possible cross-resistance there in, which could be assessed in advance. Therefore, present studies on development of resistance in S. litura against four new chemistry insecticides (emamectin benzoate, chlorantraniliprole, indoxacarb and spinosad) were carried out in the Toxicology laboratory, Department of Entomology, Punjab Agricultural University, Ludhiana, Punjab, India during the year 2011-12. Various stages of S. litura (eggs, larvae) were collected from four different locations (Malerkotla, Hoshiarpur, Amritsar and Samrala) of Punjab. Resistance is developed in third instars of lepidopterous pests. Therefore, larval bioassays were conducted to estimate the response of field populations of thirty third-instar larvae of S. litura under laboratory conditions at 25±2°C and 65±5 per cent relative humidity. Leaf dip bioassay technique with diluted insecticide formulations recommended by Insecticide Resistance Action Committee (IRAC) was performed in the laboratory with seven to ten treatments depending on the insecticide class, respectively. LC50 values were estimated by probit analysis after correction to record control mortality data which was used to calculate the resistance ratios (RR). The LC50 values worked out for emamectin benzoate, chlorantraniliprole, indoxacarb, spinosad are 0.081, 0.088, 0.380, 4.00 parts per million (ppm) against pest populations collected from Malerkotla; 0.051, 0.060, 0.250, 3.00 (ppm) of Amritsar; 0.002, 0.001, 0.0076, 0.10 ppm for Samrala and 0.000014, 0.00001, 0.00056, 0.003 ppm against pest population of Hoshiarpur, respectively. The LC50 values for populations collected from these four locations were in the order Malerkotla>Amritsar>Samrala>Hoshiarpur for the insecticides (emamectin benzoate, chlorantraniliprole, indoxacarb and spinosad) tested. Based on LC50 values obtained, emamectin benzoate (0.000014 ppm) was found to be the most toxic among all the tested populations, followed by chlorantraniliprole (0.00001 ppm), indoxacarb (0.00056 ppm) and spinosad (0.003 ppm), respectively. The pairwise correlation coefficients of LC50 values indicated that there was lack of cross resistance for emamectin benzoate, chlorantraniliprole, spinosad, indoxacarb in populations of S. litura from Punjab. These insecticides may prove to be promising substitutes for the effective control of insecticide resistant populations of S. litura in Punjab state, India.

Keywords: Spodoptera litura, insecticides, toxicity, resistance

Procedia PDF Downloads 343
56 Amyloid Angiopathy and Golf: Two Opposite but Close Worlds

Authors: Andrea Bertocchi, Alessio Barnaba Di Fonzo, Davide Talarico, Simone Rivaroli, Jeff Konin

Abstract:

The patient is a 89 years old male (180cm/85kg) retired notary former golfer with no past medical history. He describes a progressive ideomotor slowdown for 14 months. The disorder is characterized by short-term memory deficits and, for some months, also by unstable walking with a broad base with skidding and risk of falling at directional changes and urinary urgency. There were also episodes of aggression towards his wife and staff. At the time, the patient takes no prescribed medications. He has difficulty eating, dressing, and some problems with personal hygiene. In the initial visit, the patient was alert, cooperating, and performed simple tasks; however, he has a hearing impairment, slowed spontaneous speech, and amnestic deficit to the short story. Ideomotor apraxia is not present. He scored 20 points in the MMSE. From a motor function, he has deficits using Medical Research Council (MRC) 3-/5 in bilateral lower limbs and requires maximum assistance from sit to stand with existing premature fatigue. He’s unable to walk for about 1 month. Tremors and hypertonia are absent. BERG was unable to be administered, and BARTHEL was obtained 45/100. An Amyloid Angiopathy is suspected and then confirmed at the neurological examination. Therehabilitation objectives were the recovery of mobility and reinforcement of the UE/LE, especially legs, for recovery of standing and walking. The cognitive aspect was also an essential factor for the patient's recovery. The literature doesn’t demonstrate any particular studies regarding motor and cognitive rehabilitation on this pathology. Failing to manage his attention on exercise and tending to be disinterested and falling asleep constantly, we used golf-specific gestures to stimulate his mind to work and get results because the patient has memory recall of golf related movement. We worked for 4 months with a frequency of 3 sessions per week. Every session lasted for 45 minutes. After 4 months of work, the patient walked independently with the use of a stick for about 120 meters without stopping. MRC 4/5 AI bilaterally andpostural steps performed independently with supervision. BERG 36/56. BARTHEL 65/100. 6 Minutes Walking Test (6MWT), at the beginning, it wasn’t measurable, now, he performs 151,5m with Numeric Rating Scale 4 at the beginning and 7 at the end. Cognitively, he no longer has episodes of aggression, although the short-term memory and concentration deficit remains. Amyloid Angiopathy is a mix of motor and cognitive disorder. It is worth the thought that cerebral amyloid angiopathy manifests with functional deficits due to strokes and bleedings and, as such, has an important rehabilitation indication, as classical stroke is not associated with amyloidosis. Exploring the motor patterns learned at a young age and remained in the implicit and explicit memory of the patient allowed us to set up effective work and to obtain significant results in the short-middle term. Surely many studies will still be done regarding this pathology and its rehabilitation, but the importance of the cognitive sphere applied to the motor sphere could represent an important starting point.

Keywords: amyloid angiopathy, cognitive rehabilitation, golf, motor disorder

Procedia PDF Downloads 139
55 Teachers Engagement to Teaching: Exploring Australian Teachers’ Attribute Constructs of Resilience, Adaptability, Commitment, Self/Collective Efficacy Beliefs

Authors: Lynn Sheridan, Dennis Alonzo, Hoa Nguyen, Andy Gao, Tracy Durksen

Abstract:

Disruptions to teaching (e.g., COVID-related) have increased work demands for teachers. There is an opportunity for research to explore evidence-informed steps to support teachers. Collective evidence informs data on teachers’ personal attributes (e.g., self-efficacy beliefs) in the workplace are seen to promote success in teaching and support teacher engagement. Teacher engagement plays a role in students’ learning and teachers’ effectiveness. Engaged teachers are better at overcoming work-related stress, burnout and are more likely to take on active roles. Teachers’ commitment is influenced by a host of personal (e.g., teacher well-being) and environmental factors (e.g., job stresses). The job demands-resources model provided a conceptual basis for examining how teachers’ well-being, and is influenced by job demands and job resources. Job demands potentially evoke strain and exceed the employee’s capability to adapt. Job resources entail what the job offers to individual teachers (e.g., organisational support), helping to reduce job demands. The application of the job demands-resources model involves gathering an evidence-base of and connection to personal attributes (job resources). The study explored the association between constructs (resilience, adaptability, commitment, self/collective efficacy) and a teacher’s engagement with the job. The paper sought to elaborate on the model and determine the associations between key constructs of well-being (resilience, adaptability), commitment, and motivation (self and collective-efficacy beliefs) to teachers’ engagement in teaching. Data collection involved online a multi-dimensional instrument using validated items distributed from 2020-2022. The instrument was designed to identify construct relationships. The participant number was 170. Data Analysis: The reliability coefficients, means, standard deviations, skewness, and kurtosis statistics for the six variables were completed. All scales have good reliability coefficients (.72-.96). A confirmatory factor analysis (CFA) and structural equation model (SEM) were performed to provide measurement support and to obtain latent correlations among factors. The final analysis was performed using structural equation modelling. Several fit indices were used to evaluate the model fit, including chi-square statistics and root mean square error of approximation. The CFA and SEM analysis was performed. The correlations of constructs indicated positive correlations exist, with the highest found between teacher engagement and resilience (r=.80) and the lowest between teacher adaptability and collective teacher efficacy (r=.22). Given the associations; we proceeded with CFA. The CFA yielded adequate fit: CFA fit: X (270, 1019) = 1836.79, p < .001, RMSEA = .04, and CFI = .94, TLI = .93 and SRMR = .04. All values were within the threshold values, indicating a good model fit. Results indicate that increasing teacher self-efficacy beliefs will increase a teacher’s level of engagement; that teacher ‘adaptability and resilience are positively associated with self-efficacy beliefs, as are collective teacher efficacy beliefs. Implications for school leaders and school systems: 1. investing in increasing teachers’ sense of efficacy beliefs to manage work demands; 2. leadership approaches can enhance teachers' adaptability and resilience; and 3. a culture of collective efficacy support. Preparing teachers for now and in the future offers an important reminder to policymakers and school leaders on the importance of supporting teachers’ personal attributes when faced with the challenging demands of the job.

Keywords: collective teacher efficacy, teacher self-efficacy, job demands, teacher engagement

Procedia PDF Downloads 130
54 The Impact of the Media in the Implementation of Qatar’s Foreign Policy on the Public Opinion of the People of the Middle East (2011-2023)

Authors: Negar Vkilbashi, Hassan Kabiri

Abstract:

Modern diplomacy, in its general form, refers to the people and not the governments, and diplomacy tactics are more addressed to the people than to the governments. Media diplomacy and cyber diplomacy are also one of the sub-branches of public diplomacy and, in fact, the role of media in the process of influencing public opinion and directing foreign policy. Mass media, including written, radio and television, theater, satellite, internet, and news agencies, transmit information and demands. What the Qatari government tried to implement in the countries of the region during the Arab Spring and after was through its important media, Al Jazeera. The embargo on Qatar began in 2017, when Saudi Arabia, the United Arab Emirates, Bahrain, and Egypt imposed a land, sea, and air blockade against the country. The media tool constitutes the cornerstone of soft power in the field of foreign policy, which Qatari leaders have consistently resorted to over the past two decades. Undoubtedly, the role it played in covering the events of the Arab Spring has created geopolitical tensions. The United Arab Emirates and other neighboring countries sometimes criticize Al Jazeera for providing a platform for the Muslim Brotherhood, Hamas, and other Islamists to promote their ideology. In 2011, at the same time as the Arab Spring, Al Jazeera reached the peak of its popularity. Al Jazeera's live coverage of protests in Tunisia, Egypt, Yemen, Libya, and Syria helped create a unified narrative of the Arab Spring, with audiences tuning in every Friday to watch simultaneous protests across the Middle East. Al Jazeera operates in three groups: First, it is a powerful base in the hands of the government so that it can direct and influence Arab public opinion. Therefore, this network has been able to benefit from the unlimited financial support of the Qatar government to promote its desired policies and culture. Second, it has provided an attractive platform for politicians and scientific and intellectual elites, thus attracting their support and defense from the government and its rulers. Third, during the last years of Prince Hamad's reign, the Al Jazeera network formed a deterrent weapon to counter the media and political struggle campaigns. The importance of the research is that this network covers a wide range of people in the Middle East and, therefore, has a high influence on the decision-making of countries. On the other hand, Al Jazeera is influential as a tool of public diplomacy and soft power in Qatar's foreign policy, and by studying it, the results of its effectiveness in the past years can be examined. Using a qualitative method, this research analyzes the impact of the media on the implementation of Qatar's foreign policy on the public opinion of the people of the Middle East. Data collection has been done by the secondary method, that is, reading related books, magazine articles, newspaper reports and articles, and analytical reports of think tanks. The most important findings of the research are that Al Jazeera plays an important role in Qatar's foreign policy in Qatar's public diplomacy. So that, in 2011, 2017 and 2023, it played an important role in Qatar's foreign policy in various crises. Also, the people of Arab countries use Al-Jazeera as their first reference.

Keywords: Al Jazeera, Qatar, media, diplomacy

Procedia PDF Downloads 80
53 A Comprehensive Planning Model for Amalgamation of Intensification and Green Infrastructure

Authors: Sara Saboonian, Pierre Filion

Abstract:

The dispersed-suburban model has been the dominant one across North America for the past seventy years, characterized by automobile reliance, low density, and land-use specialization. Two planning models have emerged as possible alternatives to address the ills inflicted by this development pattern. First, there is intensification, which promotes efficient infrastructure by connecting high-density, multi-functional, and walkable nodes with public transit services within the suburban landscape. Second is green infrastructure, which provides environmental health and human well-being by preserving and restoring ecosystem services. This research studies incompatibilities and the possibility of amalgamating the two alternatives in an attempt to develop a comprehensive alternative to suburban model that advocates density, multi-functionality and transit- and pedestrian-conduciveness, with measures capable of mitigating the adverse environmental impacts of compactness. The research investigates three Canadian urban growth centers, where intensification is the current planning practice, and the awareness of green infrastructure benefits is on the rise. However, these three centers are contrasted by their development stage, the presence or absence of protected natural land, their environmental approach, and their adverse environmental consequences according to the planning cannons of different periods. The methods include reviewing the literature on green infrastructure planning, criticizing the Ontario provincial plans for intensification, surveying residents’ preferences for alternative models, and interviewing officials who deal with the local planning for the centers. Moreover, the research draws on recalling debates between New Urbanism and Landscape/Ecological Urbanism. The case studies expose the difficulties in creating urban growth centres that accommodate green infrastructure while adhering to intensification principles. First, the dominant status of intensification and the obstacles confronting intensification have monopolized the planners’ concerns. Second, the tension between green infrastructure and intensification explains the absence of the green infrastructure typologies that correspond to intensification-compatible forms and dynamics. Finally, the lack of highlighted social-economic benefits of green infrastructure reduces residents’ participation. Moreover, the results from the research provide insight into predominating urbanization theories, New Urbanism and Landscape/Ecological Urbanism. In order to understand political, planning, and ecological dynamics of such blending, dexterous context-specific planning is required. Findings suggest the influence of the following factors on amalgamating intensification and green infrastructure. Initially, producing ecosystem services-based justifications for green infrastructure development in the intensification context provides an expert-driven backbone for the implementation programs. This knowledge-base should be translated to effectively imbue different urban stakeholders. Moreover, due to the limited greenfields in intensified areas, spatial distribution and development of multi-level corridors such as pedestrian-hospitable settings and transportation networks along green infrastructure measures are required. Finally, to ensure the long-term integrity of implemented green infrastructure measures, significant investment in public engagement and education, as well as clarification of management responsibilities is essential.

Keywords: ecosystem services, green infrastructure, intensification, planning

Procedia PDF Downloads 356
52 The Use of STIMULAN Resorbable Antibiotic Beads in Conjunction with Autologous Tissue Transfer to Treat Recalcitrant Infections and Osteomyelitis in Diabetic Foot Wounds

Authors: Hayden R Schott, John M Felder III

Abstract:

Introduction: Chronic lower extremity wounds in the diabetic and vasculopathic populations are associated with a high degree of morbidity.When wounds require more extensive treatment than can be offered by wound care centers, more aggressive solutions involve local tissue transfer and microsurgical free tissue transfer for achieving definitive soft tissue coverage. These procedures of autologous tissue transfer (ATT) offer resilient, soft tissue coverage of limb-threatening wounds and confer promising limb salvage rates. However, chronic osteomyelitis and recalcitrant soft tissue infections are common in severe diabetic foot wounds and serve to significantly complicate ATT procedures. Stimulan is a resorbable calcium sulfate antibiotic carrier. The use of stimulan antibiotic beads to treat chronic osteomyelitis is well established in the orthopedic and plastic surgery literature. In these procedures, the beads are placed beneath the skin flap to directly deliver antibiotics to the infection site. The purpose of this study was to quantify the success of Stimulan antibiotic beads in treating recalcitrant infections in patients with diabetic foot wounds receiving ATT. Methods: A retrospective review of clinical and demographic information was performed on patients who underwent ATT with the placement of Stimulan antibiotic beads for attempted limb salvage from 2018-21. Patients were analyzed for preoperative wound characteristics, demographics, infection recurrence, and adverse outcomes as a result of product use. The primary endpoint was 90 day infection recurrence, with secondary endpoints including 90 day complications. Outcomes were compared using basic statistics and Fisher’s exact tests. Results: In this time span, 14 patients were identified. At the time of surgery, all patients exhibited clinical signs of active infection, including positive cultures and erythema. 57% of patients (n=8) exhibited chronic osteomyelitis prior to surgery, and 71% (n=10) had exposed bone at the wound base. In 57% of patients (n=8), Stimulan beads were placed beneath a free tissue flap and beneath a pedicle tissue flap in 42% of patients (n=6). In all patients, Stimulan beads were only applied once. Recurrent infections were observed in 28% of patients (n=4) at 90 days post-op, and flap nonadherence was observed in 7% (n=1). These were the only Stimulan related complications observed. Ultimately, lower limb salvage was successful in 85% of patients (n=12). Notably, there was no significant association between the preoperative presence of osteomyelitis and recurrent infections. Conclusions: The use of Stimulanantiobiotic beads to treat recalcitrant infections in patients receiving definitive skin coverage of diabetic foot wounds does not appear to demonstrate unnecessary risk. Furthermore, the lack of significance between the preoperative presence of osteomyelitis and recurrent infections indicates the successful use of Stimulan to dampen infection in patients with osteomyelitis, as is consistent with the literature. Further research is needed to identify Stimulan as the significant contributor to infection treatment using future cohort and case control studies with more patients. Nonetheless, the use of Stimulan antibiotic beads in patients with diabetic foot wounds demonstrates successful infection suppression and maintenance of definitive soft tissue coverage.

Keywords: wound care, stimulan antibiotic beads, free tissue transfer, plastic surgery, wound, infection

Procedia PDF Downloads 91
51 Synthesis, Growth, Characterization and Quantum Chemical Investigations of an Organic Single Crystal: 2-Amino- 4-Methylpyridinium Quinoline- 2-Carboxylate

Authors: Anitha Kandasamy, Thirumurugan Ramaiah

Abstract:

Interestingly, organic materials exhibit large optical nonlinearity with quick responses and having the flexibility of molecular tailoring using computational modelling and favourable synthetic methodologies. Pyridine based organic compounds and carboxylic acid contained aromatic compounds play a crucial role in crystal engineering of NCS complexes that displays admirable optical nonlinearity with fast response and favourable physicochemical properties such as low dielectric constant, wide optical transparency and large laser damage threshold value requires for optoelectronics device applications. Based on these facts, it was projected to form an acentric molecule of π-conjugated system interaction with appropriately replaced electron donor and acceptor groups for achieving higher SHG activity in which quinoline-2-carboyxlic acid is chosen as an electron acceptor and capable of acting as an acid as well as a base molecule, while 2-amino-4-methylpyridine is used as an electron donor and previously employed in numerous proton transfer complexes for synthesis of NLO materials for optoelectronic applications. 2-amino-4-mehtylpyridinium quinoline-2-carboxylate molecular complex (2AQ) is having π-donor-acceptor groups in which 2-amino-4-methylpyridine donates one of its electron to quinoline -2-carboxylic acid thereby forming a protonated 2-amino-4-methyl pyridinium moiety and mono ionized quinoline-2-carboxylate moiety which are connected via N-H…O intermolecular interactions with non-centrosymmetric crystal packing arrangement at microscopic scale is accountable to the enhancement of macroscopic second order NLO activity. The 2AQ crystal was successfully grown by a slow evaporation solution growth technique and its structure was determined in orthorhombic crystal system with acentric, P212121, space group. Hirshfeld surface analysis reveals that O…H intermolecular interactions primarily contributed with 31.0 % to the structural stabilization of 2AQ. The molecular structure of title compound has been confirmed by 1H and 13C NMR spectral studies. The vibrational modes of functional groups present in 2AQ have been assigned by using FTIR and FT-Raman spectroscopy. The grown 2AQ crystal exhibits high optical transparency with lower cut-off wavelength (275 nm) within the region of 275-1500 nm. The laser study confirmed that 2AQ exhibits high SHG efficiency of 12.6 times greater than that of KDP. TGA-DTA analysis revealed that 2AQ crystal had a thermal stability of 223 °C. The low dielectric constant and low dielectric loss at higher frequencies confirmed good crystalline nature with fewer defects of grown 2AQ crystal. The grown crystal exhibits soft material and positive photoconduction behaviour. Mulliken atomic distribution and FMOs analysis suggested that the strong intermolecular hydrogen bonding which lead to the enhancement of NLO activity. These properties suggest that 2AQ crystal is a suitable material for optoelectronic and laser frequency conversion applications.

Keywords: crystal growth, NLO activity, proton transfer complex, quantum chemical investigation

Procedia PDF Downloads 123
50 Absorptive Capabilities in the Development of Biopharmaceutical Industry: The Case of Bioprocess Development and Research Unit, National Polytechnic Institute

Authors: Ana L. Sánchez Regla, Igor A. Rivera González, María del Pilar Monserrat Pérez Hernández

Abstract:

The ability of an organization to identify and get useful information from external sources, assimilate it, transform and apply to generate products or services with added value is called absorptive capacity. Absorptive capabilities contribute to have market opportunities to firms and get a leader position with respect to others competitors. The Bioprocess Development and Research Unit (UDIBI) is a Research and Development (R&D) laboratory that belongs to the National Polytechnic Institute (IPN), which is a higher education institute in Mexico. The UDIBI was created with the purpose of carrying out R and D activities for the Transferon®, a biopharmaceutical product developed and patented by IPN. The evolution of competence and scientific and technological platform made UDIBI expand its scope by providing technological services (preclínical studies and bio-compatibility evaluation) to the national pharmaceutical industry and biopharmaceutical industry. The relevance of this study is that those industries are classified as high scientific and technological intensity, and yet, after a review of the state of the art, there is only one study of absorption capabilities in biopharmaceutical industry with a similar scope to this research; in the case of Mexico, there is none. In addition to this, UDIBI belongs to a public university and its operation does not depend on the federal budget, but on the income generated by its external technological services. This fact represents a highly remarkable case in Mexico's public higher education context. This current doctoral research (2015-2019) is contextualized within a case study, its main objective is to identify and analyze the absorptive capabilities that characterise the UDIBI that allows it had become in a one of two third authorized laboratory by the sanitary authority in Mexico for developed bio-comparability studies to bio-pharmaceutical products. The development of this work in the field is divided into two phases. In a first phase, 15 interviews were conducted with the UDIBI personnel, covering management levels, heads of services, project leaders and laboratory personnel. These interviews were structured under a questionnaire, which was designed to integrate open questions and to a lesser extent, others, whose answers would be answered on a Likert-type rating scale. From the information obtained in this phase, a scientific article was made (in review and a proposal of presentation was submitted in different academic forums. A second stage will be made from the conduct of an ethnographic study within this organization under study that will last about 3 months. On the other hand, it is intended to carry out interviews with external actors around the UDIBI (suppliers, advisors, IPN officials, including contact with an academic specialized in absorption capacities to express their comments on this thesis. The inicial findings had shown two lines: i) exist institutional, technological and organizational management elements that encourage and/or limit the creation of absorption capacities in this scientific and technological laboratory and, ii) UDIBI has had created a set of multiple transfer technology of knowledge mechanisms which have had permitted to build a huge base of prior knowledge.

Keywords: absorptive capabilities, biopharmaceutical industry, high research and development intensity industries, knowledge management, transfer of knowledge

Procedia PDF Downloads 226
49 Differential Expression Analysis of Busseola fusca Larval Transcriptome in Response to Cry1Ab Toxin Challenge

Authors: Bianca Peterson, Tomasz J. Sańko, Carlos C. Bezuidenhout, Johnnie Van Den Berg

Abstract:

Busseola fusca (Fuller) (Lepidoptera: Noctuidae), the maize stem borer, is a major pest in sub-Saharan Africa. It causes economic damage to maize and sorghum crops and has evolved non-recessive resistance to genetically modified (GM) maize expressing the Cry1Ab insecticidal toxin. Since B. fusca is a non-model organism, very little genomic information is publicly available, and is limited to some cytochrome c oxidase I, cytochrome b, and microsatellite data. The biology of B. fusca is well-described, but still poorly understood. This, in combination with its larval-specific behavior, may pose problems for limiting the spread of current resistant B. fusca populations or preventing resistance evolution in other susceptible populations. As part of on-going research into resistance evolution, B. fusca larvae were collected from Bt and non-Bt maize in South Africa, followed by RNA isolation (15 specimens) and sequencing on the Illumina HiSeq 2500 platform. Quality of reads was assessed with FastQC, after which Trimmomatic was used to trim adapters and remove low quality, short reads. Trinity was used for the de novo assembly, whereas TransRate was used for assembly quality assessment. Transcript identification employed BLAST (BLASTn, BLASTp, and tBLASTx comparisons), for which two libraries (nucleotide and protein) were created from 3.27 million lepidopteran sequences. Several transcripts that have previously been implicated in Cry toxin resistance was identified for B. fusca. These included aminopeptidase N, cadherin, alkaline phosphatase, ATP-binding cassette transporter proteins, and mitogen-activated protein kinase. MEGA7 was used to align these transcripts to reference sequences from Lepidoptera to detect mutations that might potentially be contributing to Cry toxin resistance in this pest. RSEM and Bioconductor were used to perform differential gene expression analysis on groups of B. fusca larvae challenged and unchallenged with the Cry1Ab toxin. Pairwise expression comparisons of transcripts that were at least 16-fold expressed at a false-discovery corrected statistical significance (p) ≤ 0.001 were extracted and visualized in a hierarchically clustered heatmap using R. A total of 329,194 transcripts with an N50 of 1,019 bp were generated from the over 167.5 million high-quality paired-end reads. Furthermore, 110 transcripts were over 10 kbp long, of which the largest one was 29,395 bp. BLAST comparisons resulted in identification of 157,099 (47.72%) transcripts, among which only 3,718 (2.37%) were identified as Cry toxin receptors from lepidopteran insects. According to transcript expression profiles, transcripts were grouped into three subclusters according to the similarity of their expression patterns. Several immune-related transcripts (pathogen recognition receptors, antimicrobial peptides, and inhibitors) were up-regulated in the larvae feeding on Bt maize, indicating an enhanced immune status in response to toxin exposure. Above all, extremely up-regulated arylphorin genes suggest that enhanced epithelial healing is one of the resistance mechanisms employed by B. fusca larvae against the Cry1Ab toxin. This study is the first to provide a resource base and some insights into a potential mechanism of Cry1Ab toxin resistance in B. fusca. Transcriptomic data generated in this study allows identification of genes that can be targeted by biotechnological improvements of GM crops.

Keywords: epithelial healing, Lepidoptera, resistance, transcriptome

Procedia PDF Downloads 204
48 OpenFOAM Based Simulation of High Reynolds Number Separated Flows Using Bridging Method of Turbulence

Authors: Sagar Saroha, Sawan S. Sinha, Sunil Lakshmipathy

Abstract:

Reynolds averaged Navier-Stokes (RANS) model is the popular computational tool for prediction of turbulent flows. Being computationally less expensive as compared to direct numerical simulation (DNS), RANS has received wide acceptance in industry and research community as well. However, for high Reynolds number flows, the traditional RANS approach based on the Boussinesq hypothesis is incapacitated to capture all the essential flow characteristics, and thus, its performance is restricted in high Reynolds number flows of practical interest. RANS performance turns out to be inadequate in regimes like flow over curved surfaces, flows with rapid changes in the mean strain rate, duct flows involving secondary streamlines and three-dimensional separated flows. In the recent decade, partially averaged Navier-Stokes (PANS) methodology has gained acceptability among seamless bridging methods of turbulence- placed between DNS and RANS. PANS methodology, being a scale resolving bridging method, is inherently more suitable than RANS for simulating turbulent flows. The superior ability of PANS method has been demonstrated for some cases like swirling flows, high-speed mixing environment, and high Reynolds number turbulent flows. In our work, we intend to evaluate PANS in case of separated turbulent flows past bluff bodies -which is of broad aerodynamic research and industrial application. PANS equations, being derived from base RANS, continue to inherit the inadequacies from the parent RANS model based on linear eddy-viscosity model (LEVM) closure. To enhance PANS’ capabilities for simulating separated flows, the shortcomings of the LEVM closure need to be addressed. Inabilities of the LEVMs have inspired the development of non-linear eddy viscosity models (NLEVM). To explore the potential improvement in PANS performance, in our study we evaluate the PANS behavior in conjugation with NLEVM. Our work can be categorized into three significant steps: (i) Extraction of PANS version of NLEVM from RANS model, (ii) testing the model in the homogeneous turbulence environment and (iii) application and evaluation of the model in the canonical case of separated non-homogeneous flow field (flow past prismatic bodies and bodies of revolution at high Reynolds number). PANS version of NLEVM shall be derived and implemented in OpenFOAM -an open source solver. Homogeneous flows evaluation will comprise the study of the influence of the PANS’ filter-width control parameter on the turbulent stresses; the homogeneous analysis performed over typical velocity fields and asymptotic analysis of Reynolds stress tensor. Non-homogeneous flow case will include the study of mean integrated quantities and various instantaneous flow field features including wake structures. Performance of PANS + NLEVM shall be compared against the LEVM based PANS and LEVM based RANS. This assessment will contribute to significant improvement of the predictive ability of the computational fluid dynamics (CFD) tools in massively separated turbulent flows past bluff bodies.

Keywords: bridging methods of turbulence, high Re-CFD, non-linear PANS, separated turbulent flows

Procedia PDF Downloads 145
47 Gas-Phase Noncovalent Functionalization of Pristine Single-Walled Carbon Nanotubes with 3D Metal(II) Phthalocyanines

Authors: Vladimir A. Basiuk, Laura J. Flores-Sanchez, Victor Meza-Laguna, Jose O. Flores-Flores, Lauro Bucio-Galindo, Elena V. Basiuk

Abstract:

Noncovalent nanohybrid materials combining carbon nanotubes (CNTs) with phthalocyanines (Pcs) is a subject of increasing research effort, with a particular emphasis on the design of new heterogeneous catalysts, efficient organic photovoltaic cells, lithium batteries, gas sensors, field effect transistors, among other possible applications. The possibility of using unsubstituted Pcs for CNT functionalization is very attractive due to their very moderate cost and easy commercial availability. However, unfortunately, the deposition of unsubstituted Pcs onto nanotube sidewalls through the traditional liquid-phase protocols turns to be very problematic due to extremely poor solubility of Pcs. On the other hand, unsubstituted free-base H₂Pc phthalocyanine ligand, as well as many of its transition metal complexes, exhibit very high thermal stability and considerable volatility under reduced pressure, which opens the possibility for their physical vapor deposition onto solid surfaces, including nanotube sidewalls. In the present work, we show the possibility of simple, fast and efficient noncovalent functionalization of single-walled carbon nanotubes (SWNTs) with a series of 3d metal(II) phthalocyanines Me(II)Pc, where Me= Co, Ni, Cu, and Zn. The functionalization can be performed in a temperature range of 400-500 °C under moderate vacuum and requires about 2-3 h only. The functionalized materials obtained were characterized by means of Fourier-transform infrared (FTIR), Raman, UV-visible and energy-dispersive X-ray spectroscopy (EDS), scanning and transmission electron microscopy (SEM and TEM, respectively) and thermogravimetric analysis (TGA). TGA suggested that Me(II)Pc weight content is 30%, 17% and 35% for NiPc, CuPc, and ZnPc, respectively (CoPc exhibited anomalous thermal decomposition behavior). The above values are consistent with those estimated from EDS spectra, namely, of 24-39%, 27-36% and 27-44% for CoPc, CuPc, and ZnPc, respectively. A strong increase in intensity of D band in the Raman spectra of SWNT‒Me(II)Pc hybrids, as compared to that of pristine nanotubes, implies very strong interactions between Pc molecules and SWNT sidewalls. Very high absolute values of binding energies of 32.46-37.12 kcal/mol and the highest occupied and lowest unoccupied molecular orbital (HOMO and LUMO, respectively) distribution patterns, calculated with density functional theory by using Perdew-Burke-Ernzerhof general gradient approximation correlation functional in combination with the Grimme’s empirical dispersion correction (PBE-D) and the double numerical basis set (DNP), also suggested that the interactions between Me(II) phthalocyanines and nanotube sidewalls are very strong. The authors thank the National Autonomous University of Mexico (grant DGAPA-IN200516) and the National Council of Science and Technology of Mexico (CONACYT, grant 250655) for financial support. The authors are also grateful to Dr. Natalia Alzate-Carvajal (CCADET of UNAM), Eréndira Martínez (IF of UNAM) and Iván Puente-Lee (Faculty of Chemistry of UNAM) for technical assistance with FTIR, TGA measurements, and TEM imaging, respectively.

Keywords: carbon nanotubes, functionalization, gas-phase, metal(II) phthalocyanines

Procedia PDF Downloads 132
46 Finite Element Analysis of Mini-Plate Stabilization of Mandible Fracture

Authors: Piotr Wadolowski, Grzegorz Krzesinski, Piotr Gutowski

Abstract:

The aim of the presented investigation is to recognize the possible mechanical issues of mini-plate connection used to treat mandible fractures and to check the impact of different factors for the stresses and displacements within the bone-stabilizer system. The mini-plate osteosynthesis technique is a common type of internal fixation using metal plates connected to the fractured bone parts by a set of screws. The selected two types of plate application methodology used by maxillofacial surgeons were investigated in the work. Those patterns differ in location and number of plates. The bone geometry was modeled on the base of computed tomography scans of hospitalized patient done just after mini-plate application. The solid volume geometry consisting of cortical and cancellous bone was created based on gained cloud of points. Temporomandibular joint and muscle system were simulated to imitate the real masticatory system behavior. Finite elements mesh and analysis were performed by ANSYS software. To simulate realistic connection behavior nonlinear contact conditions were used between the connecting elements and bones. The influence of the initial compression of the connected bone parts or the gap between them was analyzed. Nonlinear material properties of the bone tissues and elastic-plastic model of titanium alloy were used. The three cases of loading assuming the force of magnitude of 100N acting on the left molars, the right molars and the incisors were investigated. Stress distribution within connecting plate shows that the compression of the bone parts in the connection results in high stress concentration in the plate and the screws, however the maximum stress levels do not exceed material (titanium) yield limit. There are no significant differences between negative offset (gap) and no-offset conditions. The location of the external force influences the magnitude of stresses around both the plate and bone parts. Two-plate system gives generally lower von Misses stress under the same loading than the one-plating approach. Von Mises stress distribution within the cortical bone shows reduction of high stress field for the cases without the compression (neutral initial contact). For the initial prestressing there is a visible significant stress increase around the fixing holes at the bottom mini-plate due to the assembly stress. The local stress concentration may be the reason of bone destruction in those regions. The performed calculations prove that the bone-mini-plate system is able to properly stabilize the fractured mandible bone. There is visible strong dependency between the mini-plate location and stress distribution within the stabilizer structure and the surrounding bone tissue. The results (stresses within the bone tissues and within the devices, relative displacements of the bone parts at the interface) corresponding to different models of the connection provide a basis for the mechanical optimization of the mini-plate connections. The results of the performed numerical simulations were compared to clinical observation. They provide information helpful for better understanding of the load transfer in the mandible with the stabilizer and for improving stabilization techniques.

Keywords: finite element modeling, mandible fracture, mini-plate connection, osteosynthesis

Procedia PDF Downloads 247
45 3D Structuring of Thin Film Solid State Batteries for High Power Demanding Applications

Authors: Alfonso Sepulveda, Brecht Put, Nouha Labyedh, Philippe M. Vereecken

Abstract:

High energy and power density are the main requirements of today’s high demanding applications in consumer electronics. Lithium ion batteries (LIB) have the highest energy density of all known systems and are thus the best choice for rechargeable micro-batteries. Liquid electrolyte LIBs present limitations in safety, size and design, thus thin film all-solid state batteries are predominantly considered to overcome these restrictions in small devices. Although planar all-solid state thin film LIBs are at present commercially available they have low capacity (<1mAh/cm2) which limits their application scenario. By using micro-or nanostructured surfaces (i.e. 3D batteries) and appropriate conformal coating technology (i.e. electrochemical deposition, ALD) the capacity can be increased while still keeping a high rate performance. The main challenges in the introduction of solid-state LIBs are low ionic conductance and limited cycle life time due to mechanical stress and shearing interfaces. Novel materials and innovative nanostructures have to be explored in order to overcome these limitations. Thin film 3D compatible materials need to provide with the necessary requirements for functional and viable thin-film stacks. Thin film electrodes offer shorter Li-diffusion paths and high gravimetric and volumetric energy densities which allow them to be used at ultra-fast charging rates while keeping their complete capacities. Thin film electrolytes with intrinsically high ion conductivity (~10-3 S.cm) do exist, but are not electrochemically stable. On the other hand, electronically insulating electrolytes with a large electrochemical window and good chemical stability are known, but typically have intrinsically low ionic conductivities (<10-6 S cm). In addition, there is the need for conformal deposition techniques which can offer pinhole-free coverage over large surface areas with large aspect ratio features for electrode, electrolyte and buffer layers. To tackle the scaling of electrodes and the conformal deposition requirements on future 3D batteries we study LiMn2O4 (LMO) and Li4Ti5O12 (LTO). These materials are among the most interesting electrode candidates for thin film batteries offering low cost, low toxicity, high voltage and high capacity. LMO and LTO are considered 3D compatible materials since they can be prepared through conformal deposition techniques. Here, we show the scaling effects on rate performance and cycle stability of thin film cathode layers of LMO created by RF-sputtering. Planar LMO thin films below 100 nm have been electrochemically characterized. The thinnest films show the highest volumetric capacity and the best cycling stability. The increased stability of the films below 50 nm allows cycling in both the 4 and 3V potential region, resulting in a high volumetric capacity of 1.2Ah/cm3. Also, the creation of LTO anode layers through a post-lithiation process of TiO2 is demonstrated here. Planar LTO thin films below 100 nm have been electrochemically characterized. A 70 nm film retains 85% of its original capacity after 100 (dis)charging cycles at 10C. These layers can be implemented into a high aspect ratio structures. IMEC develops high aspect Si pillars arrays which is the base for the advance of 3D thin film all-solid state batteries of future technologies.

Keywords: Li-ion rechargeable batteries, thin film, nanostructures, rate performance, 3D batteries, all-solid state

Procedia PDF Downloads 338
44 How Can Personal Protective Equipment Be Best Used and Reused: A Human Factors based Look at Donning and Doffing Procedures

Authors: Devin Doos, Ashley Hughes, Trang Pham, Paul Barach, Rami Ahmed

Abstract:

Over 115,000 Health Care Workers (HCWs) have died from COVID-19, and millions have been infected while caring for patients. HCWs have filed thousands of safety complaints surrounding safety concerns due to Personal Protective Equipment (PPE) shortages, which included concerns around inadequate and PPE reuse. Protocols for donning and doffing PPE remain ambiguous, lacking an evidence-base, and often result in wide deviations in practice. PPE donning and doffing protocol deviations commonly result in self-contamination but have not been thoroughly addressed. No evidence-driven protocols provide guidance on protecting HCW during periods of PPE reuse. Objective: The aim of this study was to examine safety-related threats and risks to Health Care Workers (HCWs) due to the reuse of PPE among Emergency Department personnel. Method: We conducted a prospective observational study to examine the risks of reusing PPE. First, ED personnel were asked to don and doff PPE in a simulation lab. Each participant was asked to don and doff PPE five times, according to the maximum reuse recommendation set by the Centers for Disease Control and Prevention (CDC). Each participant was videorecorded; video recordings were reviewed and coded independently by at least 2 of the 3trained coders for safety behaviors and riskiness of actions. A third coder was brought in when the agreement between the 2 coders could not be reached. Agreement between coders was high (81.9%), and all disagreements (100%) were resolved via consensus. A bowtie risk assessment chart was constructed analyzing the factors that contribute to increased risks HCW are faced with due to PPE use and reuse. Agreement amongst content experts in the field of Emergency Medicine, Human Factors, and Anesthesiology was used to select aspects of health care that both contribute and mitigate risks associated with PPE reuse. Findings: Twenty-eight clinician participants completed five rounds of donning/doffing PPE, yielding 140 PPE donning/doffing sequences. Two emerging threats were associated with behaviors in donning, doffing, and re-using PPE: (i) direct exposure to contaminant, and (ii) transmission/spread of contaminant. Protective behaviors included: hand hygiene, not touching the patient-facing surface of PPE, and ensuring a proper fit and closure of all PPE materials. 100% of participants (n= 28) deviated from the CDC recommended order, and most participants (92.85%, n=26) self-contaminated at least once during reuse. Other frequent errors included failure to tie all ties on the PPE (92.85%, n=26) and failure to wash hands after a contamination event occurred (39.28%, n=11). Conclusions: There is wide variation and regular errors in how HCW don and doffPPE while including in reusing PPE that led to self-contamination. Some errors were deemed “recoverable”, such as hand washing after touching a patient-facing surface to remove the contaminant. Other errors, such as using a contaminated mask and accidentally spreading to the neck and face, can lead to compound risks that are unique to repeated PPE use. A more comprehensive understanding of the contributing threats to HCW safety and complete approach to mitigating underlying risks, including visualizing with risk management toolsmay, aid future PPE designand workflow and space solutions.

Keywords: bowtie analysis, health care, PPE reuse, risk management

Procedia PDF Downloads 92
43 Medicompills Architecture: A Mathematical Precise Tool to Reduce the Risk of Diagnosis Errors on Precise Medicine

Authors: Adriana Haulica

Abstract:

Powered by Machine Learning, Precise medicine is tailored by now to use genetic and molecular profiling, with the aim of optimizing the therapeutic benefits for cohorts of patients. As the majority of Machine Language algorithms come from heuristics, the outputs have contextual validity. This is not very restrictive in the sense that medicine itself is not an exact science. Meanwhile, the progress made in Molecular Biology, Bioinformatics, Computational Biology, and Precise Medicine, correlated with the huge amount of human biology data and the increase in computational power, opens new healthcare challenges. A more accurate diagnosis is needed along with real-time treatments by processing as much as possible from the available information. The purpose of this paper is to present a deeper vision for the future of Artificial Intelligence in Precise medicine. In fact, actual Machine Learning algorithms use standard mathematical knowledge, mostly Euclidian metrics and standard computation rules. The loss of information arising from the classical methods prevents obtaining 100% evidence on the diagnosis process. To overcome these problems, we introduce MEDICOMPILLS, a new architectural concept tool of information processing in Precise medicine that delivers diagnosis and therapy advice. This tool processes poly-field digital resources: global knowledge related to biomedicine in a direct or indirect manner but also technical databases, Natural Language Processing algorithms, and strong class optimization functions. As the name suggests, the heart of this tool is a compiler. The approach is completely new, tailored for omics and clinical data. Firstly, the intrinsic biological intuition is different from the well-known “a needle in a haystack” approach usually used when Machine Learning algorithms have to process differential genomic or molecular data to find biomarkers. Also, even if the input is seized from various types of data, the working engine inside the MEDICOMPILLS does not search for patterns as an integrative tool. This approach deciphers the biological meaning of input data up to the metabolic and physiologic mechanisms, based on a compiler with grammars issued from bio-algebra-inspired mathematics. It translates input data into bio-semantic units with the help of contextual information iteratively until Bio-Logical operations can be performed on the base of the “common denominator “rule. The rigorousness of MEDICOMPILLS comes from the structure of the contextual information on functions, built to be analogous to mathematical “proofs”. The major impact of this architecture is expressed by the high accuracy of the diagnosis. Detected as a multiple conditions diagnostic, constituted by some main diseases along with unhealthy biological states, this format is highly suitable for therapy proposal and disease prevention. The use of MEDICOMPILLS architecture is highly beneficial for the healthcare industry. The expectation is to generate a strategic trend in Precise medicine, making medicine more like an exact science and reducing the considerable risk of errors in diagnostics and therapies. The tool can be used by pharmaceutical laboratories for the discovery of new cures. It will also contribute to better design of clinical trials and speed them up.

Keywords: bio-semantic units, multiple conditions diagnosis, NLP, omics

Procedia PDF Downloads 70
42 Admissibility as a Property of Evidence in Modern Conditions

Authors: Iryna Teslenko

Abstract:

According to the provisions of the current criminal procedural legislation of Ukraine, the issue of admissibility of evidence is closely related to both the right to a fair trial and the presumption of innocence. The general rule is that evidence obtained improperly or illegally cannot be taken into account in a court case. Therefore, the evidence base of the prosecution, collected at the stage of the pre-trial investigation, compliance with the requirements of the law during the collection of evidence, is of crucial importance for the criminal process, the violation of which entails the recognition of the relevant evidence as inadmissible, which can nullify all the efforts of the pre-trial investigation body and the prosecution. Therefore, the issue of admissibility of evidence in criminal proceedings is fundamentally important and decisive for the entire process. Research on this issue began in December 2021. At that time, there was still no clear understanding of what needed to be conveyed to the scientific community. In February 2022, the lives of all citizens of Ukraine have totally changed. A war broke out in the country. At a time when the entire world community is on the path of humanizing society, respecting the rights and freedoms of man and citizen, a military conflict has arisen in the middle of Europe - one country attacked another, war crimes are being committed. The world still cannot believe it, but it is happening here and now, people are dying, infrastructure is being destroyed, war crimes are being committed, contrary to the signed and ratified international conventions, and contrary to all the acquisitions and development of world law. At this time, the life of the world has divided into before and after February 24, 2022, the world cannot be the same as it was before, and the approach to solving legal issues in the criminal process, in particular, issues of proving the commission of crimes and the involvement of certain persons in their commission. An international criminal has appeared in the humane European world, who disregards all norms of law and morality, and does not adhere to any principles. Until now, the practice of the European Court of Human Rights and domestic courts of Ukraine treated with certain formalism, such a property of evidence in criminal proceedings as the admissibility of evidence. Currently, we have information that the Office of the Prosecutor of the International Criminal Court in The Hague has started an investigation into war crimes in Ukraine and is documenting them. In our opinion, the world cannot allow formalism in bringing a war criminal to justice. There is a war going on in Ukraine, the cities are under round-the-clock missile fire from the aggressor country, which makes it impossible to carry out certain investigative actions. If due to formal deficiencies, the collected evidence is declared inadmissible, it may lead to the fact that the guilty people will not be punished. And this, in turn, sends a message to other terrorists in the world about the impunity of their actions, the system of deterring criminals from committing criminal offenses (crimes) will collapse due to the understanding of the inevitability of punishment, and this will affect the entire world security and European security in particular. Therefore, we believe that the world cannot allow chaos in the issue of general security, there should be a transformation of the approach in general to such a property of evidence in the criminal process as admissibility in order to ensure the inevitability of the punishment of criminals. We believe that the scientific and legal community should not allow criminals to avoid responsibility. The evil that is destroying Ukraine should be punished. We must all together prove that legal norms are not just words written on paper but rules of behavior of all members of society, their non-observance leads to mandatory responsibility. Everybody who commits crimes will be punished, which is inevitable, and this principle is the guarantor of world security in the future.

Keywords: admissibility of evidence, criminal process, war, Ukraine

Procedia PDF Downloads 88
41 Differential Expression Profile Analysis of DNA Repair Genes in Mycobacterium Leprae by qPCR

Authors: Mukul Sharma, Madhusmita Das, Sundeep Chaitanya Vedithi

Abstract:

Leprosy is a chronic human disease caused by Mycobacterium leprae, that cannot be cultured in vitro. Though treatable with multidrug therapy (MDT), recently, bacteria reported resistance to multiple antibiotics. Targeting DNA replication and repair pathways can serve as the foundation of developing new anti-leprosy drugs. Due to the absence of an axenic culture medium for the propagation of M. leprae, studying cellular processes, especially those belonging to DNA repair pathways, is challenging. Genomic understanding of M. Leprae harbors several protein-coding genes with no previously assigned function known as 'hypothetical proteins'. Here, we report identification and expression of known and hypothetical DNA repair genes from a human skin biopsy and mouse footpads that are involved in base excision repair, direct reversal repair, and SOS response. Initially, a bioinformatics approach was employed based on sequence similarity, identification of known protein domains to screen the hypothetical proteins in the genome of M. leprae, that are potentially related to DNA repair mechanisms. Before testing on clinical samples, pure stocks of bacterial reference DNA of M. leprae (NHDP63 strain) was used to construct standard graphs to validate and identify lower detection limit in the qPCR experiments. Primers were designed to amplify the respective transcripts, and PCR products of the predicted size were obtained. Later, excisional skin biopsies of newly diagnosed untreated, treated, and drug resistance leprosy cases from SIHR & LC hospital, Vellore, India were taken for the extraction of RNA. To determine the presence of the predicted transcripts, cDNA was generated from M. leprae mRNA isolated from clinically confirmed leprosy skin biopsy specimen across all the study groups. Melting curve analysis was performed to determine the integrity of the amplification and to rule out primer‑dimer formation. The Ct values obtained from qPCR were fitted to standard curve to determine transcript copy number. Same procedure was applied for M. leprae extracted after processing a footpad of nude mice of drug sensitive and drug resistant strains. 16S rRNA was used as positive control. Of all the 16 genes involved in BER, DR, and SOS, differential expression pattern of the genes was observed in terms of Ct values when compared to human samples; this was because of the different host and its immune response. However, no drastic variation in gene expression levels was observed in human samples except the nth gene. The higher expression of nth gene could be because of the mutations that may be associated with sequence diversity and drug resistance which suggests an important role in the repair mechanism and remains to be explored. In both human and mouse samples, SOS system – lexA and RecA, and BER genes AlkB and Ogt were expressing efficiently to deal with possible DNA damage. Together, the results of the present study suggest that DNA repair genes are constitutively expressed and may provide a reference for molecular diagnosis, therapeutic target selection, determination of treatment and prognostic judgment in M. leprae pathogenesis.

Keywords: DNA repair, human biopsy, hypothetical proteins, mouse footpads, Mycobacterium leprae, qPCR

Procedia PDF Downloads 104
40 Unpacking the Spatial Outcomes of Public Transportation in a Developing Country Context: The Case of Johannesburg

Authors: Adedayo B. Adegbaju, Carel B. Schoeman, Ilse M. Schoeman

Abstract:

The unique urban contexts that emanated from the apartheid history of South Africa informed the transport landscape of the City of Johannesburg. Apartheid‘s divisive spatial planning and land use management policies promoted sprawling and separated workers from job opportunities. This was further exacerbated by poor funding of public transport and road designs that encouraged the use of private cars. However, the democratization of the country in 1994 and the hosting of the 2010 FIFA World Cup provided a new impetus to the city’s public transport-oriented urban planning inputs. At the same time, the state’s new approach to policy formulations that entails the provision of public transport as one of the tools to end years of marginalization and inequalities soon began to largely reflect in planning decisions of other spheres of government. The Rea Vaya BRT and the Gautrain were respectively implemented by the municipal and provincial governments to demonstrate strong political will and commitment to the new policy direction. While the Gautrain was implemented to facilitate elite movement within Gauteng and to crowd investments and economic growths around station nodes, the BRT was provided for previously marginalized public transport users to provide a sustainable alternative to the dominant minibus taxi. The aim of this research is to evaluate the spatial impacts of the Gautrain and Rea Vaya BRT on the City of Johannesburg and to inform future outcomes by determining the existing potentials. By using the case study approach with a focus on the BRT and fast rail in a metropolitan context, the triangulation research method, which combines various data collection methods, was used to determine the research outcomes. The use of interviews, questionnaires, field observation, and databases such as REX, Quantec, StatsSA, GCRO observatory, national and provincial household travel surveys, and the quality of life surveys provided the basis for data collection. The research concludes that the Gautrain has demonstrated that viable alternatives to the private car can be provided, with its satisfactory feedbacks from users; while some of its station nodes (Sandton, Rosebank) have shown promises of transit-oriented development, one of the project‘s key objectives. The other stations have been unable to stimulate growth due to reasons like non-implementation of their urban design frameworks and lack of public sector investment required to attract private investors. The Rea Vaya BRT continues to be expanded in spite of both its inability to induce modal change and its low ridership figures. The research identifies factors like the low peak to base ratio, pricing, and the city‘s disjointed urban fabric as some of the reasons for its below-average performance. By drawing from the highlights and limitations, the study recommends that public transport provision should be institutionally integrated across and within spheres of government. Similarly, harmonization of the funding structure, better understanding of users’ needs, and travel patterns, underlined with continuity of policy direction and objectives, will equally promote optimal outcomes.

Keywords: bus rapid transit, Gautrain, Rea Vaya, sustainable transport, spatial and transport planning, transit oriented development

Procedia PDF Downloads 115
39 From Modelled Design to Reality through Material and Machinery Lab and Field Tests: Porous Concrete Carparks at the Wanda Metropolitano Stadium in Madrid

Authors: Manuel de Pazos-Liano, Manuel Cifuentes-Antonio, Juan Fisac-Gozalo, Sara Perales-Momparler, Carlos Martinez-Montero

Abstract:

The first-ever game in the Wanda Metropolitano Stadium, the new home of the Club Atletico de Madrid, was played on September 16, 2017, thanks to the work of a multidisciplinary team that made it possible to combine urban development with sustainability goals. The new football ground sits on a 1.2 km² land owned by the city of Madrid. Its construction has dramatically increased the sealed area of the site (transforming the runoff coefficient from 0.35 to 0.9), and the surrounding sewer network has no capacity for that extra flow. As an alternative to enlarge the existing 2.5 m diameter pipes, it was decided to detain runoff on site by means of an integrated and durable infrastructure that would not blow up the construction cost nor represent a burden on the municipality’s maintenance tasks. Instead of the more conventional option of building a large concrete detention tank, the decision was taken on the use of pervious pavement on the 3013 car parking spaces for sub-surface water storage, a solution aligned with the city water ordinance and the Madrid + Natural project. Making the idea a reality, in only five months and during the summer season (which forced to pour the porous concrete only overnight), was a challenge never faced before in Spain, that required of innovation both at the material as well as the machinery side. The process consisted on: a) defining the characteristics required for the porous concrete (compressive strength of 15 N/mm2 and 20% voids); b) testing of different porous concrete dosages at the construction company laboratory; c) stablishing the cross section in order to provide structural strength and sufficient water detention capacity (20 cm porous concrete over a 5 cm 5/10 gravel, that sits on a 50 cm coarse 40/50 aggregate sub-base separated by a virgin fiber polypropylene geotextile fabric); d) hydraulic computer modelling (using the Full Hydrograph Method based on the Wallingford Procedure) to estimate design peak flows decrease (an average of 69% at the three car parking lots); e) use of a variety of machinery for the application of the porous concrete to achieve both structural strength and permeable surface (including an inverse rotating rolling imported from USA, and the so-called CMI, a sliding concrete paver used in the construction of motorways with rigid pavements); f) full-scale pilots and final construction testing by an accredited laboratory (pavement compressive strength average value of 15 N/mm2 and 0,0032 m/s permeability). The continuous testing and innovating construction process explained in detail within this article, allowed for a growing performance with time, finally proving the use of the CMI valid also for large porous car park applications. All this process resulted in a successful story that converts the Wanda Metropolitano Stadium into a great demonstration site that will help the application of the Spanish Royal Decree 638/2016 (it also counts with rainwater harvesting for grass irrigation).

Keywords: construction machinery, permeable carpark, porous concrete, SUDS, sustainable develpoment

Procedia PDF Downloads 145
38 Texture Characteristics and Depositional Environment of the Lower Mahi River Sediment, Mainland Gujarat, India

Authors: Shazi Farooqui, Anupam Sharma

Abstract:

The Mahi River (~600km long) is an important west flowing the river of Central India. It originates in Madhya Pradesh and starts flowing in NW direction and enters into the state of Rajasthan. It flows across southern Rajasthan and then enters into Gujarat and finally debouches in the Gulf of Cambay. In Gujarat state, it flows through all four geomorphic zones i.e. eastern upland zone, shallow buried piedmont zone, alluvial zone and coastal zone. In lower reaches and particularly when it is flowing under the coastal regime, it provides an opportunity to study – 1. Land–Sea interaction and role of relative sea level changes, 2. Coastal/estuarine geological process, 3. Landscape evolution in marginal areas and so on. The Late Quaternary deposits of Mainland Gujarat is appreciably studied by Chamyal and his group of MS University of Baroda, and they have established that the 30-35m thick sediment package of the Mainland Gujarat is comprised of marine, fluvial and aeolian sediments. It is also established that in the estuarine zone, the upper few meter thick sediments package is of marine nature. However, its thickness, characters and the depositional environment including the role of climate and tectonics is still not clearly defined. To understand few aspects of the above mentioned, in the present study, a 17m subsurface sediment core has been retrieved from the estuarine zone of Mahi river basin. The Multiproxy studies which include the textural analysis (grain size), Loss on ignition (LOI), Bulk and clay mineralogy and geochemical studies have been carried out. In the entire sedimentary sequence, the grain size largely varies from coarse sand to clay; however, a solitary gravel bed is also noticed. The lower part (depth 9-17m), is mainly comprised of sub equal proportion of sand and silt. The sediments mainly have bimodal and leptokurtic distribution and deposited in alternate sand-silt package, probably indicating flood deposits. Relatively low moisture (1.8%) and organic carbon (2.4%) with increased carbonate values (12%) indicate that conditions must have to remain oxidizing. The middle part (depth 9–6m) has a 1m thick gravel bed at the bottom and overlain by coarse sand to very fine sand showing fining upward sequence. The presence of gravel bed suggests some kind of tectonic activity resulting into change in base level or enhanced precipitation in the catchment region. The upper part (depth 6–0m; top part of sequence) mainly comprised of fine sand to silt size grains (with appreciable clay content). The sediment of this part is Unimodal and very leptokurtic in nature suggesting wave and winnowing process and deposited in low energy suspension environment. This part has relatively high moisture (2.1%) and organic carbon (2.7%) with decreased carbonate content (4.2%) indicating change in the depositional environment probably under estuarine conditions. The presence of chlorite along with smectite clay mineral further supports the significant marine contribution in the formation of upper part of the sequence.

Keywords: grain size, statistical analysis, clay minerals, late quaternary, LOI

Procedia PDF Downloads 181
37 Analysis of Short Counter-Flow Heat Exchanger (SCFHE) Using Non-Circular Micro-Tubes Operated on Water-CuO Nanofluid

Authors: Avdhesh K. Sharma

Abstract:

Key, in the development of energy-efficient micro-scale heat exchanger devices, is to select large heat transfer surface to volume ratio without much expanse on re-circulated pumps. The increased interest in short heat exchanger (SHE) is due to accessibility of advanced technologies for manufacturing of micro-tubes in range of 1 micron m - 1 mm. Such SHE using micro-tubes are highly effective for high flux heat transfer technologies. Nanofluids, are used to enhance the thermal conductivity of re-circulated coolant and thus enhances heat transfer rate further. Higher viscosity associated with nanofluid expands more pumping power. Thus, there is a trade-off between heat transfer rate and pressure drop with geometry of micro-tubes. Herein, a novel design of short counter flow heat exchanger (SCFHE) using non-circular micro-tubes flooded with CuO-water nanofluid is conceptualized by varying the ratio of surface area to cross-sectional area of micro-tubes. A framework for comparative analysis of SCFHE using micro-tubes non-circular shape flooded by CuO-water nanofluid is presented. In SCFHE concept, micro-tubes having various geometrical shapes (viz., triangular, rectangular and trapezoidal) has been arranged row-wise to facilitate two aspects: (1) allowing easy flow distribution for cold and hot stream, and (2) maximizing the thermal interactions with neighboring channels. Adequate distribution of rows for cold and hot flow streams enables above two aspects. For comparative analysis, a specific volume or cross-section area is assigned to each elemental cell (which includes flow area and area corresponds to half wall thickness). A specific volume or cross-section area is assumed to be constant for each elemental cell (which includes flow area and half wall thickness area) and variation in surface area is allowed by selecting different geometry of micro-tubes in SCFHE. Effective thermal conductivity model for CuO-water nanofluid has been adopted, while the viscosity values for water based nanofluids are obtained empirically. Correlations for Nusselt number (Nu) and Poiseuille number (Po) for micro-tubes have been derived or adopted. Entrance effect is accounted for. Thermal and hydrodynamic performances of SCFHE are defined in terms of effectiveness and pressure drop or pumping power, respectively. For defining the overall performance index of SCFHE, two links are employed. First one relates heat transfer between the fluid streams q and pumping power PP as (=qj/PPj); while another link relates effectiveness eff and pressure drop dP as (=effj/dPj). For analysis, the inlet temperatures of hot and cold streams are varied in usual range of 20dC-65dC. Fully turbulent regime is seldom encountered in micro-tubes and transition of flow regime occurs much early (i.e., ~Re=1000). Thus, Re is fixed at 900, however, the uncertainty in Re due to addition of nanoparticles in base fluid is quantified by averaging of Re. Moreover, for minimizing error, volumetric concentration is limited to range 0% to ≤4% only. Such framework may be helpful in utilizing maximum peripheral surface area of SCFHE without any serious severity on pumping power and towards developing advanced short heat exchangers.

Keywords: CuO-water nanofluid, non-circular micro-tubes, performance index, short counter flow heat exchanger

Procedia PDF Downloads 216
36 Origin of the Eocene Volcanic Rocks in Muradlu Village, Azerbaijan Province, Northwest of Iran

Authors: A. Shahriari, M. Khalatbari Jafari, M. Faridi

Abstract:

Abstract The Muradlu volcanic area is located in Azerbaijan province, NW Iran. The studied area exposed in a vast region includes lesser Caucasus, Southeastern Turkey, and northwestern Iran, comprising Cenozoic volcanic and plutonic massifs. The geology of this extended region was under the influence of the Alpine-Himalayan orogeny. Cenozoic magmatic activities in this vast region evolved through the northward subduction of the Neotethyan subducted slab and subsequence collision of the Arabian and Eurasian plates. Based on stratigraphy and paleontology data, most of the volcanic activities in the Muradlu area occurred in the Eocene period. The Studied volcanic rocks overly late Cretaceous limestone with disconformity. The volcanic sequence includes thick epiclastic and hyaloclastite breccia at the base, laterally changed to pillow lava and continued by hyaloclastite and lave flows at the top of the series. The lava flows display different textures from megaporphyric-phyric to fluidal and microlithic textures. The studied samples comprise picrobasalt basalt, tephrite basanite, trachybasalt, basaltic trachyandesite, phonotephrite, tephrophonolite, trachyandesite, and trachyte in compositions. Some xenoliths with lherzolitic composition are found in picrobasalt. These xenoliths are made of olivine, cpx (diopside), and opx (enstatite), probably the remain of mantle origin. Some feldspathoid minerals such as sodalite presence in the phonotephrite confirm an alkaline trend. Two types of augite phenocrysts are found in picrobasalt, basalt and trachybasalt. The first types are shapeless, with disharmony zoning and sponge texture with reaction edges probably resulted from sodic magma, which is affected by a potassic magma. The second shows a glomerocryst shape. In discriminative diagrams, the volcanic rocks show alkaline-shoshonitic trends. They contain (0.5-7.7) k2O values and plot in the shoshonitic field. Most of the samples display transitional to potassic alkaline trends, and some samples reveal sodic alkaline trends. The transitional trend probably results from the mixing of the sodic alkaline and potassic magmas. The Rare Earth Elements (REE) patterns and spider diagrams indicate enrichment of Large-Ione Lithophile Element (LILE) and depletion of High Field Strength Elements (HFSE) relative to Heavy Rare Earth Elements (HREE). Enrichment of K, Rb, Sr, Ba, Zr, Th, and U and the enrichment of Light Rare Earth Elements (LREE) relative to Heavy Rare Earth Elements (HREE) indicate the effect of subduction-related fluids over the mantle source, which has been reported in the arc and continental collision zones. The studied samples show low Nb/La ratios. Our studied samples plot in the lithosphere and lithosphere-asthenosphere fields in the Nb/La versus La/Yb ratios diagram. These geochemical characters allow us to conclude that a lithospheric mantle source previously metasomatized by subduction components was the origin of the Muradlu volcanic rocks.

Keywords: alkaline, asthenosphere, lherzolite, lithosphere, Muradlu, potassic, shoshonitic, sodic, volcanism

Procedia PDF Downloads 172
35 Fine Characterization of Glucose Modified Human Serum Albumin by Different Biophysical and Biochemical Techniques at a Range

Authors: Neelofar, Khursheed Alam, Jamal Ahmad

Abstract:

Protein modification in diabetes mellitus may lead to early glycation products (EGPs) or amadori product as well as advanced glycation end products (AGEs). Early glycation involves the reaction of glucose with N-terminal and lysyl side chain amino groups to form Schiff’s base which undergoes rearrangements to form more stable early glycation product known as Amadori product. After Amadori, the reactions become more complicated leading to the formation of advanced glycation end products (AGEs) that interact with various AGE receptors, thereby playing an important role in the long-term complications of diabetes. Millard reaction or nonenzymatic glycation reaction accelerate in diabetes due to hyperglycation and alter serum protein’s structure, their normal functions that lead micro and macro vascular complications in diabetic patients. In this study, Human Serum Albumin (HSA) with a constant concentration was incubated with different concentrations of glucose at 370C for a week. At 4th day, Amadori product was formed that was confirmed by colorimetric method NBT assay and TBA assay which both are authenticate early glycation product. Conformational changes in native as well as all samples of Amadori albumin with different concentrations of glucose were investigated by various biophysical and biochemical techniques. Main biophysical techniques hyperchromacity, quenching of fluorescence intensity, FTIR, CD and SDS-PAGE were used. Further conformational changes were observed by biochemical assays mainly HMF formation, fructoseamine, reduction of fructoseamine with NaBH4, carbonyl content estimation, lysine and arginine residues estimation, ANS binding property and thiol group estimation. This study find structural and biochemical changes in Amadori modified HSA with normal to hyperchronic range of glucose with respect to native HSA. When glucose concentration was increased from normal to chronic range biochemical and structural changes also increased. Highest alteration in secondary and tertiary structure and conformation in glycated HSA was observed at the hyperchronic concentration (75mM) of glucose. Although it has been found that Amadori modified proteins is also involved in secondary complications of diabetes as AGEs but very few studies have been done to analyze the conformational changes in Amadori modified proteins due to early glycation. Most of the studies were found on the structural changes in Amadori protein at a particular glucose concentration but no study was found to compare the biophysical and biochemical changes in HSA due to early glycation with a range of glucose concentration at a constant incubation time. So this study provide the information about the biochemical and biophysical changes occur in Amadori modified albumin at a range of glucose normal to chronic in diabetes. Although many implicates currently in use i.e. glycaemic control, insulin treatment and other chemical therapies that can control many aspects of diabetes. However, even with intensive use of current antidiabetic agents more than 50 % of diabetic patient’s type 2 suffers poor glycaemic control and 18 % develop serious complications within six years of diagnosis. Experimental evidence related to diabetes suggests that preventing the nonenzymatic glycation of relevant proteins or blocking their biological effects might beneficially influence the evolution of vascular complications in diabetic patients or quantization of amadori adduct of HSA by authentic antibodies against HSA-EGPs can be used as marker for early detection of the initiation/progression of secondary complications of diabetes. So this research work may be helpful for the same.

Keywords: diabetes mellitus, glycation, albumin, amadori, biophysical and biochemical techniques

Procedia PDF Downloads 273