9 Evaluation of Microleakage of a New Generation Nano-Ionomer in Class II Restoration of Primary Molars

Authors: Ghada Salem, Nihal Kabel

Abstract:

Objective: This in vitro study was carried out to assess the microleakage properties of nano-filled glass ionomer in comparison to resin-reinforced glass ionomers. Material and Methods: 40 deciduous molar teeth were included in this study. Class-II cavity was prepared in a standard form for all the specimens. The teeth were randomly distributed into two groups (20 per group) according to the restorative material used either nano-glass ionomer or Photac Fill glass ionomer restoration. All specimens were thermocycled for 1000 cycles between 5 and 55 °C. After that, the teeth were immersed in 2% methylene blue dye then sectioned and evaluated under a stereomicroscope. Microleakage was assessed using linear dye penetration and on a scale from zero to five. Results: Two way ANOVA test revealed a statistically significant lower degree of microleakage in both occlusal and gingival restorations (0.4±0.2), (0.9±0.1) for nano-filled glass ionomer group in comparison to resin modified glass ionomer (2.3±0.7), (2.4±0.5). No statistical difference was found between gingival and occlusal leakage regarding the effect of the measured site. Conclusion: Nano-filled glass ionomer shows superior sealing ability which enables this type of restoration to be used in minimum invasive treatment.

Keywords: microleakage, nanoionomer, resin-reinforced glass ionomer, proximal cavity preparation

Procedia PDF Downloads 235
8 Dependence of Ionomer Loading on the Hydrogen Generation Rate of a Proton Exchange Membrane Electrolyzer

Authors: Yingjeng James Li, Chih Chi Hsu, Chiao-Chih Hu

Abstract:

Membrane electrode assemblies MEAs for proton exchange membrane PEM water electrolyzers were prepared by employing 175um perfluorosulfonic acid PFSA membranes as the PEM, onto which iridium oxide catalyst was coated on one side as the anode and platinum catalyst was coated on the other side as the cathode. The cathode catalyst ink was prepared so that the weight ratio of the catalyst powder to ionomer was 75:25, 70:30, 65:35, 60:40, and 55:45, respectively. Whereas, the ratio of catalyst powder to ionomer of the anode catalyst ink keeps constant at 50:50. All the MEAs have a catalyst coated area of 5cm*5cm. The test cell employs a platinum plated titanium grid as anode gas diffusion media; whereas, carbon paper was employed as the cathode gas diffusion media. The measurements of the MEA gases production rate were carried out by holding the cell voltage ranging from 1.6 to 2.8 volts at room temperature. It was found that the MEA with cathode catalyst to ionomer ratio of 65:35 gives the largest hydrogen production rate which is 2.8mL/cm2*min.

Keywords: electrolyzer, membrane electrode assembly, proton exchange membrane, ionomer, hydrogen

Procedia PDF Downloads 255
7 The Differences on the Surface Roughness of Glass Ionomer Cement as the Results of Brushing with Whitening and Conventional Toothpaste

Authors: Aulina R. Rahmi, Farid Yuristiawan, Annisa Ibifadillah, Ummu H. Amri, Hidayati Gunawan

Abstract:

Glass ionomer cement is one of the filling material that often used on the field of dentistry because it is relatively less expensive and mostly available. Restoration materials could undergo changes in their clinical properties such as changes in roughness of the restoration`s surface. An increase of surface roughness accelerates bacterial colonization and plaque maturation. In the oral cavity, GIC was exposed to various substances, such as toothpaste, an oral care product used during toothbrushing. One of the popular toothpaste is whitening toothpaste. Abrasive and chemical agents such as hydrogen peroxide in whitening toothpaste could increase the surface roughness of restorative materials. Objective: To determine the differences on the surface roughness of glass ionomer cement that was brushed with whitening and conventional toothpaste. Method: This study was done using experimental laboratory method with pre and post test design. There were 36 samples which were divided into 2 groups. The first group was brushed with whitening toothpaste and the second group was brushed with conventional toothpaste, each for 2 minutes. Surface roughness value of the specimens was measured by using Roughness Tester test. Result: The data was analyzed by using independent t-test and the result of this study showed there was a significant difference between the surface of glass ionomer cement which was brushed with whitening and conventional toothpaste (p=0,000). Conclusion: Glass ionomer cement that was brushed with whitening toothpaste produced more roughness than conventional toothpaste.

Keywords: glass ionomer cement, surface roughness, toothpaste, roughness tester

Procedia PDF Downloads 287
6 Comparison of Surface Hardness of Filling Material Glass Ionomer Cement Which Soaked in Alcohol Containing Mouthwash and Alcohol-Free Mouthwash

Authors: Farid Yuristiawan, Aulina R. Rahmi, Detty Iryani, Gunawan

Abstract:

Glass ionomer cement is one of the filling material that often used in the field of dentistry because it is relatively less expensive and mostly available. Surface hardness is one of the most important properties of restoration material; it is the ability of material to stand against indentation, which is directly connected to the material compressive strength and its ability to withstand abrasion. The higher surface hardness of a material means it is better to withstand abrasion. The existence of glass ionomer cement in the mouth makes it susceptible to any substance that comes into mouth, one of them is mouthwash which is a solution that used for many purposes such as antiseptic, astringent, to prevent caries, and bad breath. The presence of alcohol in mouthwash could affect the properties of glass ionomer cement, surface hardness. Objective: To determine the comparison of surface hardness of glass ionomer cement which soaked in alcohol containing mouthwash and alcohol-free mouthwash. Methods: This research is a laboratory experimental type study. There were 30 samples made from GC FUJI IX GP EXTRA and then soaked in artificial saliva for the first 24 hours inside incubator which temperature and humidity were controlled. Samples then divided into three groups. The first group will be soaked in alcohol-containing mouthwash; second group will be soaked alcohol-free mouthwash and control group will be soaked in artificial saliva for 6 hours inside incubator. Listerine is the mouthwash that was used on this research and surface hardness was examined using Vickers Hardness Tester. The result of this research shows mean value for surface hardness of the first group is 16.36 VHN, 24.04 VHN for second group, and 43.60 VHN for control group. The result one way ANOVA with post hoc Bonferroni comparing test show significant results p = 0.00. Conclusions: The data showed there were statistically significant differences of surface hardness between each group, which surface hardness of the first group is lower than the second group, and both surface hardness of the first (alcohol mouthwash) and second group (alcohol-free mouthwash) are lowered than control group (p = 0.00).

Keywords: glass ionomer cement, mouthwash, surface hardness, Vickers hardness tester

Procedia PDF Downloads 224
5 Optimization of Platinum Utilization by Using Stochastic Modeling of Carbon-Supported Platinum Catalyst Layer of Proton Exchange Membrane Fuel Cells

Authors: Ali Akbar, Seungho Shin, Sukkee Um

Abstract:

The composition of catalyst layers (CLs) plays an important role in the overall performance and cost of the proton exchange membrane fuel cells (PEMFCs). Low platinum loading, high utilization, and more durable catalyst still remain as critical challenges for PEMFCs. In this study, a three-dimensional material network model is developed to visualize the nanostructure of carbon supported platinum Pt/C and Pt/VACNT catalysts in pursuance of maximizing the catalyst utilization. The quadruple-phase randomly generated CLs domain is formulated using quasi-random stochastic Monte Carlo-based method. This unique statistical approach of four-phase (i.e., pore, ionomer, carbon, and platinum) model is closely mimic of manufacturing process of CLs. Various CLs compositions are simulated to elucidate the effect of electrons, ions, and mass transport paths on the catalyst utilization factor. Based on simulation results, the effect of key factors such as porosity, ionomer contents and Pt weight percentage in Pt/C catalyst have been investigated at the represented elementary volume (REV) scale. The results show that the relationship between ionomer content and Pt utilization is in good agreement with existing experimental calculations. Furthermore, this model is implemented on the state-of-the-art Pt/VACNT CLs. The simulation results on Pt/VACNT based CLs show exceptionally high catalyst utilization as compared to Pt/C with different composition ratios. More importantly, this study reveals that the maximum catalyst utilization depends on the distance spacing between the carbon nanotubes for Pt/VACNT. The current simulation results are expected to be utilized in the optimization of nano-structural construction and composition of Pt/C and Pt/VACNT CLs.

Keywords: catalyst layer, platinum utilization, proton exchange membrane fuel cell, stochastic modeling

Procedia PDF Downloads 121
4 A Furaneol-Containing Glass-Ionomer Cement for Enhanced Antibacterial Activity

Authors: Dong Xie, Yuling Xu, Leah Howard

Abstract:

Secondary caries is found to be one of the main reasons to the restoration failure of dental restoratives. To prevent secondary caries formation, dental restoratives ought to be made antibacterial. In this study, a natural fruit component furaneol was tethered onto polyacid, the formed polyacid was used to formulate the light-curable glass-ionomer cements, and then the effect of this new antibacterial compound on compressive strength (CS) and antibacterial activity of the formed cement was evaluated. Fuji II LC glass powders were used as fillers. Compressive strength (CS) and S. mutans viability were used to evaluate the mechanical strength and antibacterial activity of the formed cement. The experimental cement showed a significant antibacterial activity, accompanying with an initial CS reduction. Increasing the compound loading significantly decreased the S. mutans viability from 5 to 81% and also reduced the initial CS of the formed cements from 4 to 58%. The cement loading with 7% antibacterial polymer showed 168 MPa, 7.8 GPa, 243 MPa, 46 MPa, and 57 MPa in yield strength, modulus, CS, diametral tensile strength and flexural strength, respectively, as compared to 141, 6.9, 236, 42 and 53 for Fuji II LC. The cement also showed an antibacterial function to other bacteria. No human saliva effect was noticed. It is concluded that the experimental cement may potentially be developed to a permanent antibacterial cement.

Keywords: antibacterial, dental materials, strength, cell viability

Procedia PDF Downloads 317
3 Molecular Dynamics Studies of Main Factors Affecting Mass Transport Phenomena on Cathode of Polymer Electrolyte Membrane Fuel Cell

Authors: Jingjing Huang, Nengwei Li, Guanghua Wei, Jiabin You, Chao Wang, Junliang Zhang

Abstract:

In this work, molecular dynamics (MD) simulation is applied to analyze the mass transport process in the cathode of proton exchange membrane fuel cell (PEMFC), of which all types of molecules situated in the cathode is considered. a reasonable and effective MD simulation process is provided, and models were built and compared using both Materials Studio and LAMMPS. The mass transport is one of the key issues in the study of proton exchange membrane fuel cells (PEMFCs). In this report, molecular dynamics (MD) simulation is applied to analyze the influence of Nafion ionomer distribution and Pt nano-particle size on mass transport process in the cathode. It is indicated by the diffusion coefficients calculation that a larger quantity of Nafion, as well as a higher equivalent weight (EW) value, will hinder the transport of oxygen. In addition, medium-sized Pt nano-particles (1.5~2nm) are more advantageous in terms of proton transport compared with other particle sizes (0.94~2.55nm) when the center-to-center distance between two Pt nano-particles is around 5 nm. Then mass transport channels are found to be formed between the hydrophobic backbone and the hydrophilic side chains of Nafion ionomer according to the radial distribution function (RDF) curves. And the morphology of these channels affected by the Pt size is believed to influence the transport of hydronium ions and, consequently the performance of PEMFC.

Keywords: cathode catalytic layer, mass transport, molecular dynamics, proton exchange membrane fuel cell

Procedia PDF Downloads 242
2 The Effect of Tooth Brushing with Whitening and Non-Whitening Tooth Paste on Surface Roughness of Coated and Uncoated Glass Ionomer Cement

Authors: Hidayati, Eni Rahmi, Deli Mona, Cytha Nilam Chairani, Aulina Refri Rahmi

Abstract:

Background: Restoration materials could undergo changes in their clinical properties such as changes in roughness of the restoration's surface. An increase of surface roughness accelerates bacterial colonization and plaque maturation. It can be prevented by mechanically clean the tooth surface by brushing the teeth using toothpaste. Toothpaste may contain abrasives materials that usually found in whitening toothpaste. Those abrasive materials could increase the roughness of the restoration`s surface. Glass ionomer cement (GIC) is one of the restorative material widely used to this day. GC America has made an innovation called EQUIA to improve their wear resistance by coating the surface of GIC using G-Coat Plus. Objective: To determine the effect of teeth was brushing with whitening and non-whitening toothpaste to the surface roughness of coated and uncoated restoration (GIC). Methods: This research was a laboratory experimental with pretest-posttest group design. There were 28 samples which were divided into 2 groups. The first group was brushed with whitening toothpaste and the second group was brushed with non-whitening toothpaste. Each group was divided into group which coated by G-Coat Plus and group which left uncoated. The value of surface roughness was measured by using Roughness Tester. The data was analyzed by using independent t-test to determine differences between the surface roughness of coated samples and uncoated samples brushed with whitening and non-whitening toothpaste. Result: It was found that average roughness differences before and after being brushed by whitening toothpaste were smaller in coated samples than in uncoated samples (0.07 ± 0.09 < 0.12 ± 0.02). Similar results were also found in samples brushed by non-whitening toothpaste (0.02 ± 0.01 0.03 ± 0.01). The differences of average roughness in samples brushed with non-whitening toothpaste were smaller than samples brushed with whitening toothpaste. Conclusion: The data showed there were statistically significant differences between the surface roughness of coated samples and uncoated samples brushed with non-whitening toothpaste (p < 0.05) but the was no statistically significant to samples brushed with whitening toothpaste (p > 0.05).

Keywords: surface roughness, toothpaste, EQUIA, coating

Procedia PDF Downloads 247
1 Investigation of Mechanical and Rheological Properties of Poly (trimethylene terephthalate) (PTT)/Polyethylene Blend Using Carboxylate and Ionomer as Compatibilizers

Authors: Wuttikorn Chayapanja, Sutep Charoenpongpool, Manit Nithitanakul, Brian P. Grady

Abstract:

Poly (trimethylene terephthalate) (PTT) is a linear aromatic polyester with good strength and stiffness, good surface appearance, low shrinkage and war page, and good dimensional stability. However, it has low impact strength which is a problem in automotive application. Thus, modification of PTT with the other polymer or polymer blending is a one way to develop a new material with excellence properties. In this study, PTT/High Density Polyethylene (HDPE) blends and PTT/Linear Low Density Polyethylene (LLDPE) blends with and without compatibilizers base on maleic anhydride grafted HDPE (MAH-g-HDPE) and ethylene-methacrylic acid neutralized sodium metal (Na-EMAA) were prepared by a twin-screw extruder. The blended samples with different ratios of polymers and compatibilizers were characterized on mechanical and rheological properties. Moreover, the phase morphology and dispersion size were studied by using SEM to give better understanding of the compatibility of the blends.

Keywords: poly trimethylene terephthalate, polyethylene, compatibilizer, polymer blend

Procedia PDF Downloads 414