Search results for: combined anaerobic-aerobic degradation
4214 Azadrachea indica Leaves Extract Assisted Green Synthesis of Ag-TiO₂ for Degradation of Dyes in Aqueous Medium
Authors: Muhammad Saeed, Sheeba Khalid
Abstract:
Aqueous pollution due to the textile industry is an important issue. Photocatalysis using metal oxides as catalysts is one of the methods used for eradication of dyes from textile industrial effluents. In this study, the synthesis, characterization, and evaluation of photocatalytic activity of Ag-TiO₂ are reported. TiO₂ catalysts with 2, 4, 6 and 8% loading of Ag were prepared by green methods using Azadrachea indica leaves' extract as reducing agent and titanium dioxide and silver nitrate as precursor materials. The 4% Ag-TiO₂ exhibited the best catalytic activity for degradation of dyes. Prepared catalyst was characterized by advanced techniques. Catalytic degradation of methylene blue and rhodamine B were carried out in Pyrex glass batch reactor. Deposition of Ag greatly enhanced the catalytic efficiency of TiO₂ towards degradation of dyes. Irradiation of catalyst excites electrons from conduction band of catalyst to valence band yielding an electron-hole pair. These photoexcited electrons and positive hole undergo secondary reaction and produce OH radicals. These active radicals take part in the degradation of dyes. More than 90% of dyes were degraded in 120 minutes. It was found that there was no loss catalytic efficiency of prepared Ag-TiO₂ after recycling it for two times. Photocatalytic degradation of methylene blue and rhodamine B followed Eley-Rideal mechanism which states that dye reacts in fluid phase with adsorbed oxygen. 27 kJ/mol and 20 kJ/mol were found as activation energy for photodegradation of methylene blue and rhodamine B dye respectively.Keywords: TiO₂, Ag-TiO₂, methylene blue, Rhodamine B., photo degradation
Procedia PDF Downloads 1654213 Zeolite Supported Iron-Sensitized TIO₂ for Tetracycline Photocatalytic Degradation under Visible Light: A Comparison between Doping and Ion Exchange
Authors: Ghadeer Jalloul, Nour Hijazi, Cassia Boyadjian, Hussein Awala, Mohammad N. Ahmad, Ahmad Albadarin
Abstract:
In this study, we applied Fe-sensitized TiO₂ supported over embryonic Beta zeolite (BEA) zeolite for the photocatalytic degradation of Tetracycline (TC) antibiotic under visible light. Four different samples having 20, 40, 60, and 100% w/w as a ratio of TiO₂/BEA were prepared. The immobilization of solgel TiO₂ (33 m²/g) over BEA (390 m²/g) increased its surface area to (227 m²/g) and enhanced its adsorption capacity from 8% to 19%. To expand the activity of TiO₂ photocatalyst towards the visible light region (λ>380 nm), we explored two different metal sensitization techniques with Iron ions (Fe³⁺). In the ion-exchange method, the substitutional cations in the zeolite in TiO₂/BEA were exchanged with (Fe³⁺) in an aqueous solution of FeCl₃. In the doping technique, solgel TiO₂ was doped with (Fe³⁺) from FeCl₃ precursor during its synthesis and before its immobilization over BEA. (Fe-TiO₂/BEA) catalysts were characterized using SEM, XRD, BET, UV-VIS DRS, and FTIR. After testing the performance of the various ion-exchanged catalysts under blue and white lights, only (Fe-TiO₂/BEA 60%) showed better activity as compared to pure TiO₂ under white light with 100 ppm initial catalyst concentration and 20 ppm TC concentration. As compared to ion-exchanged (Fe-TiO₂/BEA), doped (Fe-TiO₂/BEA) resulted in higher photocatalytic efficiencies under blue and white lights. The 3%-Fe-doped TiO₂/BEA removed 92% of TC compared to 54% by TiO₂ under white light. The catalysts were also tested under real solar irradiations. This improvement in the photocatalytic performance of TiO₂ was due to its higher adsorption capacity due to BEA support combined with the presence of Iron ions that enhance the visible light absorption and minimize the recombination effect by the charge carriers. Keywords: Tetracycline, photocatalytic degradation, immobilized TiO₂, zeolite, iron-doped TiO₂, ion-exchange
Procedia PDF Downloads 1084212 Mapping Man-Induced Soil Degradation in Armenia's High Mountain Pastures through Remote Sensing Methods: A Case Study
Authors: A. Saghatelyan, Sh. Asmaryan, G. Tepanosyan, V. Muradyan
Abstract:
One of major concern to Armenia has been soil degradation emerged as a result of unsustainable management and use of grasslands, this in turn largely impacting environment, agriculture and finally human health. Hence, assessment of soil degradation is an essential and urgent objective set out to measure its possible consequences and develop a potential management strategy. Since recently, an essential tool for assessing pasture degradation has been remote sensing (RS) technologies. This research was done with an intention to measure preciseness of Linear spectral unmixing (LSU) and NDVI-SMA methods to estimate soil surface components related to degradation (fractional vegetation cover-FVC, bare soils fractions, surface rock cover) and determine appropriateness of these methods for mapping man-induced soil degradation in high mountain pastures. Taking into consideration a spatially complex and heterogeneous biogeophysical structure of the studied site, we used high resolution multispectral QuickBird imagery of a pasture site in one of Armenia’s rural communities - Nerkin Sasoonashen. The accuracy assessment was done by comparing between the land cover abundance data derived through RS methods and the ground truth land cover abundance data. A significant regression was established between ground truth FVC estimate and both NDVI-LSU and LSU - produced vegetation abundance data (R2=0.636, R2=0.625, respectively). For bare soil fractions linear regression produced a general coefficient of determination R2=0.708. Because of poor spectral resolution of the QuickBird imagery LSU failed with assessment of surface rock abundance (R2=0.015). It has been well documented by this particular research, that reduction in vegetation cover runs in parallel with increase in man-induced soil degradation, whereas in the absence of man-induced soil degradation a bare soil fraction does not exceed a certain level. The outcomes show that the proposed method of man-induced soil degradation assessment through FVC, bare soil fractions and field data adequately reflects the current status of soil degradation throughout the studied pasture site and may be employed as an alternate of more complicated models for soil degradation assessment.Keywords: Armenia, linear spectral unmixing, remote sensing, soil degradation
Procedia PDF Downloads 3284211 Field Study of Chlorinated Aliphatic Hydrocarbons Degradation in Contaminated Groundwater via Micron Zero-Valent Iron Coupled with Biostimulation
Authors: Naijin Wu, Peizhong Li, Haijian Wang, Wenxia Wei, Yun Song
Abstract:
Chlorinated aliphatic hydrocarbons (CAHs) pollution poses a severe threat to human health and is persistent in groundwater. Although chemical reduction or bioremediation is effective, it is still hard to achieve their complete and rapid dechlorination. Recently, the combination of zero-valent iron and biostimulation has been considered to be one of the most promising strategies, but field studies of this technology are scarce. In a typical site contaminated by various types of CAHs, basic physicochemical parameters of groundwater, CAHs and their product concentrations, and microbial abundance and diversity were monitored after a remediation slurry containing both micron zero-valent iron (mZVI) and biostimulation components were directly injected into the aquifer. Results showed that groundwater could form and keep low oxidation-reduction potential (ORP), a neutral pH, and anoxic conditions after different degrees of fluctuations, which was benefit for the reductive dechlorination of CAHs. The injection also caused an obvious increase in the total organic carbon (TOC) concentration and sulfate reduction. After 253 days post-injection, the mean concentration of total chlorinated ethylene (CEE) from two monitoring wells decreased from 304 μg/L to 8 μg/L, and total chlorinated ethane (CEA) decreased from 548 μg/L to 108 μg/L. Occurrence of chloroethane (CA) suggested that hydrogenolysis dechlorination was one of the main degradation pathways for CEA, and also hints that biological dechlorination was activated. A significant increase of ethylene at day 67 post-injection indicated that dechlorination was complete. Additionally, the total bacterial counts increased by 2-3 orders of magnitude after 253 days post-injection. And the microbial species richness decreased and gradually changed to anaerobic/fermentative bacteria. The relative abundance of potential degradation bacteria increased corresponding to the degradation of CAHs. This work demonstrates that mZVI and biostimulation can be combined to achieve the efficient removal of various CAHs from contaminated groundwater sources.Keywords: chlorinated aliphatic hydrocarbons, groundwater, field study, zero-valent iron, biostimulation
Procedia PDF Downloads 1654210 Degradation of Polycyclic Aromatic Hydrocarbons-Contaminated Soil by Proxy-Acid Method
Authors: Reza Samsami
Abstract:
The aim of the study was to degradation of polycyclic aromatic hydrocarbons (PAHs) by proxy-acid method. The amounts of PAHs were determined in a silty-clay soil sample of an aged oil refinery field in Abadan, Iran. Proxy-acid treatment method was investigated. The results have shown that the proxy-acid system is an effective method for degradation of PAHs. The results also demonstrated that the number of fused aromatic rings have not significant effects on PAH removal by proxy-acid method. The results also demonstrated that the number of fused aromatic rings have not significant effects on PAH removal by proxy-acid method.Keywords: proxy-acid treatment, silty-clay soil, PAHs, degradation
Procedia PDF Downloads 2674209 Degradation of Petroleum Hydrocarbons Using Pseudomonas Aeruginosa Isolated from Oil Contaminated Soil Incorporated into E. coli DH5α Host
Authors: C. S. Jeba Samuel
Abstract:
Soil, especially from oil field has posed a great hazard for terrestrial and marine ecosystems. The traditional treatment of oil contaminated soil cannot degrade the crude oil completely. So far, biodegradation proves to be an efficient method. During biodegradation, crude oil is used as the carbon source and addition of nitrogenous compounds increases the microbial growth, resulting in the effective breakdown of crude oil components to low molecular weight components. The present study was carried out to evaluate the biodegradation of crude oil by hydrocarbon-degrading microorganism Pseudomonas aeruginosa isolated from natural environment like oil contaminated soil. Pseudomonas aeruginosa, an oil degrading microorganism also called as hydrocarbon utilizing microorganism (or “HUM” bug) can utilize crude oil as sole carbon source. In this study, the biodegradation of crude oil was conducted with modified mineral basal salt medium and nitrogen sources so as to increase the degradation. The efficacy of the plasmid from the isolated strain was incorporated into E.coli DH5 α host to speed up the degradation of oil. The usage of molecular techniques has increased oil degradation which was confirmed by the degradation of aromatic and aliphatic rings of hydrocarbons and was inferred by the lesser number of peaks in Fourier Transform Infrared Spectroscopy (FTIR). The gas chromatogram again confirms better degradation by transformed cells by the lesser number of components obtained in the oil treated with transformed cells. This study demonstrated the technical feasibility of using direct inoculation of transformed cells onto the oil contaminated region thereby leading to the achievement of better oil degradation in a shorter time than the degradation caused by the wild strain.Keywords: biodegradation, aromatic rings, plasmid, hydrocarbon, Fourier Transform Infrared Spectroscopy (FTIR)
Procedia PDF Downloads 3724208 Environmental Degradation in Niger-Delta and Sustainable Development in Nigeria: Issues for Consideration
Authors: Peter Okpamen
Abstract:
The issue of environmental degradation in Nigeria is of serious concern. The colonial period brought a major change in environmental awareness and relationship with the environment. This period introduced a model of development, the major thrust of which was the exploration and transformation of natural and human resources for the benefit of the colonial masters. There is abundant evidence in the literature that there are various manifestations of environmental degradation in Nigeria, which have resulted in the various problems found throughout the Nigeria national space. The idea of the environment acting as a constraint to the growth of human activity has given way to the contrary. Environmental education, going by the literature, exists at the primary, secondary and tertiary institutions. In short, the 1st National conference on environmental education gave several suggestions on how it could be realised. Thus, to realise sustainable environmental development we need to accelerate the process of providing basic education for both the old and young. Environmental education should cover the whole federation, and resources should be made available for the training of environmental education teachers and research into environmental education for the development of appropriate learning resources.Keywords: degradation, development, education, environment, sustainable
Procedia PDF Downloads 4144207 Catalytic Degradation of Tetracycline in Aqueous Solution by Magnetic Ore Pyrite Nanoparticles
Authors: Allah Bakhsh Javid, Ali Mashayekh-Salehi, Fatemeh Davardoost
Abstract:
This study presents the preparation, characterization and catalytic activity of a novel natural mineral-based catalyst for destructive adsorption of tetracycline (TTC) as water emerging compounds. Degradation potential of raw and calcined magnetite catalyst was evaluated at different experiments situations such as pH, catalyst dose, reaction time and pollutant concentration. Calcined magnetite attained greater catalytic potential than the raw ore in the degradation of tetracycline, around 69% versus 3% at reaction time of 30 min and TTC aqueous solution of 50 mg/L, respectively. Complete removal of TTC could be obtained using 2 g/L calcined nanoparticles at reaction time of 60 min. The removal of TTC increased with the increase in solution temperature. Accordingly, considering its abundance in nature together with its very high catalytic potential, calcined pyrite is a promising and reliable catalytic material for destructive decomposition for catalytic decomposition and mineralization of such pharmaceutical compounds as TTC in water and wastewater.Keywords: catalytic degradation, tetracycline, pyrite, emerging pollutants
Procedia PDF Downloads 1924206 Degradation of Neonicotinoid Insecticides (Acetamiprid and Imidacloprid) Using Biochar of Rice Husk and Fruit Peels
Authors: Mateen Abbas, Abdul Muqeet Khan, Sadia Bashir, Muhammad Awais Khalid, Aamir Ghafoor, Zara Hussain, Mashal Shahid
Abstract:
The irrational use of insecticides in everyday life has drawn attention worldwide towards its harmful effects. To mitigate the toxic effects of insecticides to humans, present study was planned on the degradation/detoxification of the neonicotinoid insecticides including imidacloprid and acetamiprid. Biocarbon of fruit peels (Banana & Watermelon) and biochar (activated or non-activated) of rice husk was utilized as adsorbents for degradation of selected pesticides. Both activated and non-activated biochar were prepared for treatment and then applied in different concentrations (0.5 to 2.0 ppm) and dosage (1.0 to 2.5g) to insecticides (Acetamiprid & Imidacloprid) as well as studied at different times (30-120 minutes). Reverse Phase-High Performance Liquid Chromatography (RP-HPLC) coupled with Photodiode array detector was used to quantify the insecticides. Results depicted that activated biochar of rice husk minimized the 73% concentrations of both insecticides however, watermelon activated biocarbon degraded 72% of imidacloprid and 56% of acetamiprid. Results proved the efficiency of the method employed and it was also inferred that high concentration of biocarbon resulted in larger percentage of degradation. The applied method is cheaper, easy and accessible that can be used to minimize the pesticide residues in animal feed. Degradation using biochar proved significant degradation, eco-friendly and economic method to reduce toxicity of insecticides.Keywords: insecticides, acetamiprid, imidacloprid, biochar, HPLC
Procedia PDF Downloads 1534205 Monitoring of Humoral Immune Response of Monovalent and Combined PPR and FMD Serotype 'O' Virus Vaccines in Goats
Authors: Mudassar Hameed, Khushi Muhammad, Aamir Ghafoor, Masood Rabbani, Momena Habib, Jawad Nazir
Abstract:
Comparative efficacy of three formulations (non-adjuvant, gel, and oil adjuvant) of monovalent and combined PPR and FMD virus vaccines was evaluated in goats. All kinds of monovalent PPRV vaccines elicited protective antibody titers at one-month post vaccination (PV) that remained so till six months PV. Monovalent non-adjuvant (NA) FMDV vaccine provoked non-protective antibody titers that declined to undetectable levels after three months. In case of combined vaccines, all of the formulations elicited protective antibody titers against PPRV in vaccinated animals which remained above that limit for six months. However, an exceptional immune response against FMDV was observed in combined NA vaccine group where antibody titers were extremely high and remained above protective level till 4 months PV in animals who received a single vaccine shot and till six months PV in booster group. Although, adjuvant or NA combined vaccines can induce protective antibody titers against both of the viruses within one month PV, but a booster vaccine shot is needed to retain protective antibody level for 6 months duration. Immune response elicited by combined vaccines is comparable or superior to the monovalent vaccines. Hence combined vaccine can be effectively used for the control and prevention of both of the diseases.Keywords: antibody titer, protective, combined vaccine, non adjuvant
Procedia PDF Downloads 2044204 Microbial Degradation of Lignin for Production of Valuable Chemicals
Authors: Fnu Asina, Ivana Brzonova, Keith Voeller, Yun Ji, Alena Kubatova, Evguenii Kozliak
Abstract:
Lignin, a heterogeneous three-dimensional biopolymer, is one of the building blocks of lignocellulosic biomass. Due to its limited chemical reactivity, lignin is currently processed as a low-value by-product in pulp and paper mills. Among various industrial lignins, Kraft lignin represents a major source of by-products generated during the widely employed pulping process across the pulp and paper industry. Therefore, valorization of Kraft lignin holds great potential as this would provide a readily available source of aromatic compounds for various industrial applications. Microbial degradation is well known for using both highly specific ligninolytic enzymes secreted by microorganisms and mild operating conditions compared with conventional chemical approaches. In this study, the degradation of Indulin AT lignin was assessed by comparing the effects of Basidiomycetous fungi (Coriolus versicolour and Trametes gallica) and Actinobacteria (Mycobacterium sp. and Streptomyces sp.) to two commercial laccases, T. versicolour ( ≥ 10 U/mg) and C. versicolour ( ≥ 0.3 U/mg). After 54 days of cultivation, the extent of microbial degradation was significantly higher than that of commercial laccases, reaching a maximum of 38 wt% degradation for C. versicolour treated samples. Lignin degradation was further confirmed by thermal carbon analysis with a five-step temperature protocol. Compared with commercial laccases, a significant decrease in char formation at 850ºC was observed among all microbial-degraded lignins with a corresponding carbon percentage increase from 200ºC to 500ºC. To complement the carbon analysis result, chemical characterization of the degraded products at different stages of the delignification by microorganisms and commercial laccases was performed by Pyrolysis-GC-MS.Keywords: lignin, microbial degradation, pyrolysis-GC-MS, thermal carbon analysis
Procedia PDF Downloads 4124203 Automating and Optimization Monitoring Prognostics for Rolling Bearing
Authors: H. Hotait, X. Chiementin, L. Rasolofondraibe
Abstract:
This paper presents a continuous work to detect the abnormal state in the rolling bearing by studying the vibration signature analysis and calculation of the remaining useful life. To achieve these aims, two methods; the first method is the classification to detect the degradation state by the AOM-OPTICS (Acousto-Optic Modulator) method. The second one is the prediction of the degradation state using least-squares support vector regression and then compared with the linear degradation model. An experimental investigation on ball-bearing was conducted to see the effectiveness of the used method by applying the acquired vibration signals. The proposed model for predicting the state of bearing gives us accurate results with the experimental and numerical data.Keywords: bearings, automatization, optimization, prognosis, classification, defect detection
Procedia PDF Downloads 1204202 Preparation of Fe, Cr Codoped TiO2 Nanostructure for Phenol Removal from Wastewaters
Authors: N. Nowzari-Dalini, S. Sabbaghi
Abstract:
Phenol is a hazardous material found in many industrial wastewaters. Photocatalytic degradation and furthermore catalyst doping are promising techniques in purpose of effective phenol removal, which have been studied comprehensively in this decade. In this study, Fe, Cr codoped TiO2 were prepared by sol-gel method, and its photocatalytic activity was investigated through degradation of phenol under visible light. The catalyst was characterized by XRD, SEM, FT-IR, BET, and EDX. The results showed that nanoparticles possess anatase phase, and the average size of nanoparticles was about 21 nm. Also, photocatalyst has significant surface area. Effect of experimental parameters such as pH, irradiation time, pollutant concentration, and catalyst concentration were investigated by using Design-Expert® software. 98% of phenol degradation was achieved after 6h of irradiation.Keywords: doping, metals, sol-gel, titanium dioxide, wastewater
Procedia PDF Downloads 3284201 Preparation and Characterization of the TiO₂ Photocatalytic Membrane for the Degradation of Reactive Orange 16 Dye
Authors: Shruti Sakarkar, Jega Jegatheesan, Srinivasan Madapusi
Abstract:
Photocatalytic membranes have shown great potential for the removal of an organic and inorganic pollutant from wastewater as it combines the degradation and antibacterial properties from photocatalysis and physical separation by the membrane in a single unit. Incorporation of the semiconductor in membrane structure results in enhancing the performance and the properties of the membrane. In this study porous ultrafiltration polyvinylidene fluoride (PVDF) membranes with entrapped TiO₂ nanoparticle were prepared by phase inversion method and further used for the degradation of reactive orange 16 (RO16). Prepared photocatalytic membranes were characterized by the scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), contact angle, and atomic force microscope (AFM). The addition of TiO₂ nanopartparticles improves the strength and thermal stability of the membrane. In particular hydrophilicity and permeability increases with the increase of TiO₂ nanoparticles into the membrane. The photocatalytic membrane achieves 80-85% degrdation of RO16. The impact of different parameters such as pH, concentration of photocatalyst, dye concentration and effect of H₂O₂ were analysed. The best conditions for dye degradation were an initial dye concentration of 50 mg/L, with a membrane containing TiO₂ loading of 2wt%. It was observed that in the presence of H₂O₂, degradation increases with increasing H₂O₂ concentration and reached up to 95-98%. The high quality permeates obtained from the photocatalytic membrane can be reused.Keywords: photocatalytic membrane, TiO₂, PVDF, nanoparticles
Procedia PDF Downloads 1664200 Fast Reductive Defluorination of Branched Perfluorooctane Sulfonic Acids by Cobalt Phthalocyanine: Electrochemical Studies and Mechanistic Insights
Authors: Maryam Mirabediny, Tsz Tin Yu, Jun Sun, Matthew Lee, Denis M. O’Carroll, Michael J. Manefield, Björn Akermark, Biswanath Das, Naresh Kumar
Abstract:
Branched perfluorooctane sulfonic acid (PFOS) is recognized as a threatening environmental pollutant due to its high persistence and bioaccumulation in various environmental matrices as well as for its toxic effects on humans and wildlife, even at very low concentrations. This study reports the first investigation of branched PFOS defluorination catalyzed by metal phthalocyanines. The reaction conditions were optimized using the different reductants and temperatures. Cobalt phthalocyanine, when combined with Ti citrate as a reducing agent, was able to defluorinate 10.9% of technical PFOS within 8 hours. In contrast, vitamin B12 only showed 2.4% defluorination during the same period under similar conditions. The defluorination mediated by cobalt phthalocyanine and Ti citrate system corresponds to 54.5% of all branched PFOS isomers (br-PFOS isomers). Isomer-specific degradation was also investigated via high-resolution LC-orbitrap, followed by their relative rates. The difference in catalytic efficacy of various phthalocyanine complexes is rationalized by their structures and electrochemical response. Lastly, a new defluorination mechanism is proposed based on the newly detected degradation products after the phthalocyanines treatment and the previous studies.Keywords: branched isomers, catalyst, reductive defluorination, water remediation
Procedia PDF Downloads 1004199 Offline Parameter Identification and State-of-Charge Estimation for Healthy and Aged Electric Vehicle Batteries Based on the Combined Model
Authors: Xiaowei Zhang, Min Xu, Saeid Habibi, Fengjun Yan, Ryan Ahmed
Abstract:
Recently, Electric Vehicles (EVs) have received extensive consideration since they offer a more sustainable and greener transportation alternative compared to fossil-fuel propelled vehicles. Lithium-Ion (Li-ion) batteries are increasingly being deployed in EVs because of their high energy density, high cell-level voltage, and low rate of self-discharge. Since Li-ion batteries represent the most expensive component in the EV powertrain, accurate monitoring and control strategies must be executed to ensure their prolonged lifespan. The Battery Management System (BMS) has to accurately estimate parameters such as the battery State-of-Charge (SOC), State-of-Health (SOH), and Remaining Useful Life (RUL). In order for the BMS to estimate these parameters, an accurate and control-oriented battery model has to work collaboratively with a robust state and parameter estimation strategy. Since battery physical parameters, such as the internal resistance and diffusion coefficient change depending on the battery state-of-life (SOL), the BMS has to be adaptive to accommodate for this change. In this paper, an extensive battery aging study has been conducted over 12-months period on 5.4 Ah, 3.7 V Lithium polymer cells. Instead of using fixed charging/discharging aging cycles at fixed C-rate, a set of real-world driving scenarios have been used to age the cells. The test has been interrupted every 5% capacity degradation by a set of reference performance tests to assess the battery degradation and track model parameters. As battery ages, the combined model parameters are optimized and tracked in an offline mode over the entire batteries lifespan. Based on the optimized model, a state and parameter estimation strategy based on the Extended Kalman Filter (EKF) and the relatively new Smooth Variable Structure Filter (SVSF) have been applied to estimate the SOC at various states of life.Keywords: lithium-ion batteries, genetic algorithm optimization, battery aging test, parameter identification
Procedia PDF Downloads 2684198 Using Atomic Force Microscope to Investigate the Influence of UVA Radiation and HA on Cell Behaviour and Elasticity of Dermal Fibroblasts
Authors: Pei-Hsiu Chiang, Ling Hong Huang, Hsin-I Chang
Abstract:
In this research, we used UVA irradiation, which can penetrate into dermis and fibroblasts, the most abundant cells in dermis, to investigate the effect of UV light on dermis, such as inflammation, ECM degradation and elasticity loss. Moreover, this research is focused on the influence of hyaluronic acid (HA) on UVA treated dermal fibroblasts. We aim to establish whether HA can effectively relief ECM degradation, and restore the elasticity of UVA-damaged fibroblasts. Prolonged exposure to UVA radiation can damage fibroblasts and led variation in cell morphology and reduction in cell viability. Besides, UVA radiation can induce IL-1β expression on fibroblasts and then promote MMP-1 and MMP-3 expression, which can accelerate ECM degradation. On the other hand, prolonged exposure to UVA radiation reduced collagen and elastin synthesis on fibroblasts. Due to the acceleration of ECM degradation and the reduction of ECM synthesis, Atomic force microscope (AFM) was used to analyze the elasticity reduction on UVA-damaged fibroblasts. UVA irradiation causes photoaging on fibroblasts. UVA damaged fibroblasts with HA treatment can down-regulate the gene expression of MMP-1, MMP-3, and then slow down ECM degradation. On the other hand, HA may restore elastin and collagen synthesis in UV-damaged fibroblasts. Based on the slowdown of ECM degradation, UVA-damaged fibroblast elasticity can be effectively restored by HA treatment. In summary, HA can relief the photoaging conditions on fibroblasts, but may not be able to return fibroblasts to normal, healthy state. Although HA cannot fully recover UVA-damaged fibroblasts, HA is still potential for repairing photoaging skin.Keywords: atomic force microscope, hyaluronic acid, UVA radiation, dermal fibroblasts
Procedia PDF Downloads 3914197 Standard and Processing of Photodegradable Polyethylene
Authors: Nurul-Akidah M. Yusak, Rahmah Mohamed, Noor Zuhaira Abd Aziz
Abstract:
The introduction of degradable plastic materials into agricultural sectors has represented a promising alternative to promote green agriculture and environmental friendly of modern farming practices. Major challenges of developing degradable agricultural films are to identify the most feasible types of degradation mechanisms, composition of degradable polymers and related processing techniques. The incorrect choice of degradable mechanisms to be applied during the degradation process will cause premature losses of mechanical performance and strength. In order to achieve controlled process of agricultural film degradation, the compositions of degradable agricultural film also important in order to stimulate degradation reaction at required interval of time and to achieve sustainability of the modern agricultural practices. A set of photodegradable polyethylene based agricultural film was developed and produced, following the selective optimization of processing parameters of the agricultural film manufacturing system. Example of agricultural films application for oil palm seedlings cultivation is presented.Keywords: photodegradable polyethylene, plasticulture, processing schemes
Procedia PDF Downloads 5184196 Sun-Light Driven Photocatalytic Degradation of Tetracycline Antibiotics Employing Hydrothermally Synthesized sno₂/mnv₂o₆ Heterojunction
Authors: Sandeep Kaushal
Abstract:
Tetracycline (TC) is a widespread antibiotic that is utilised in a multitude of countries, particularly China, India, and the United States of America, due to its low cost and potency in boosting livestock production. Unfortunately, certain antibiotics can be hazardous to living beings due to metal complexation and aggregation, which can lead to teratogenicity and carcinogenicity. Heterojunction photocatalysts are promising for the effective removal of pollutants like antibiotics. Herein, a simple, economical, and pollution-less hydrothermal technique was used to construct SnO₂/MnV₂O₆heterojunction with varying amounts of tin dioxide (SO₂). Various sophisticated techniques like XRD, FTIR, XPS, FESEM, HRTEM, and PLand Raman spectroscopy demonstrated the successful synthesis of SnO₂/MnV₂O₆ heterojunction photocatalysts.BET surface area analysis revealed that the as-synthesized heterojunction has a favorable surface area and surface properties for efficacious degradation of tetracycline. Under the direct sunlight exposure, the SnO₂/MnV₂O₆ heterojunction possessed superior photodegradation activity toward TC than the pristine SnO₂ and MnV2O6owing to their excellent adsorption abilities suitable band positions, large surface areas along with the effective charge-transfer ability of the heterojunction. The SnO₂/MnV₂O₆ heterojunction possessed extraordinary efficiency for the photocatalytic degradation of TC antibiotic (98% in 60 min) with an apparent rate constant of 0.092 min–1. In the degradation experiments, photocatalytic activities of as-synthesized heterojunction were studied by varying different factors such as time contact, catalyst dose, and solution pH. The role of reactive species in antibiotics was validated by radical scavenging studies, which indicated that.OH, radical has a critical role in photocatalytic degradation. Moreover, liquid chromatography-mass spectrometry (LC-MS) investigations were employed to anticipate a plausible mechanism for TC degradation.Keywords: photocatalytic degradation, tetracycline, heterojunction, LC-MS
Procedia PDF Downloads 1064195 Assessment of Collapse Potential of Degrading SDOF Systems
Authors: Muzaffer Borekci, Murat Serdar Kirçil
Abstract:
Predicting the collapse potential of a structure during earthquakes is an important issue in earthquake engineering. Many researchers proposed different methods to assess the collapse potential of structures under the effect of strong ground motions. However most of them did not consider degradation and softening effect in hysteretic behavior. In this study, collapse potential of SDOF systems caused by dynamic instability with stiffness and strength degradation has been investigated. An equation was proposed for the estimation of collapse period of SDOF system which is a limit value of period for dynamic instability. If period of the considered SDOF system is shorter than the collapse period then the relevant system exhibits dynamic instability and collapse occurs.Keywords: collapse, degradation, dynamic instability, seismic response
Procedia PDF Downloads 3784194 Development of Stability Indicating Method and Characterization of Degradation Impurity of Nirmaltrelvir in Its Self-Emulsifying Drug Delivery System
Authors: Ravi Patel, Ravisinh Solanki, Dignesh Khunt
Abstract:
A stability-indicating reverse phase high performance liquid chromatography (RP-HPLC) method was developed and validated for estimating Nirmatrelvir in its self-emulsifying drug delivery system (SEDDS). The separation of Nirmatrelvir and its degradation products was accomplished by employing an Agilent Zorbax Eclipse plus C18 (250 mm x 4.6 mm, 5 µm) column, through which the mobile phase 5 mM phosphate buffer (pH 4.0) as mobile phase A and Acetonitrile as mobile phase B in a ratio of (40:60 % v/v) was pumped at a flow rate of 1.0 mL/min, through the HPLC system. Chromatographic separation and elution were monitored by a photo-diode array detector at 210 nm. Stress studies have been employed to evaluate this method's ability to indicate stability. Nirmatrelvir was exposed to several stress conditions, such as acid, alkali, oxidative, photolytic, and thermal degradations. Significant degradation was observed during acid and alkali hydrolysis, and the resulting degradation product was successfully separated from the Nirmatrelvir peak, preventing any interference. Furthermore, the primary degradant produced under alkali degradation conditions was identified using UPLC-ESI-TQ-MS/MS. The method was validated in accordance with the International Council on Harmonization (ICH) and found to be selective, precise, accurate, linear, and robust. The apparent permeability of Nirmatrelvir SEDDS was 4.20 ± 0.21×10-6 cm/sec, and the average proportion of free drug recovered was 0.5%. The method developed in this study was feasible and accurate for routine quality control evaluation of Nirmatrelvir SEDDS.Keywords: Nirmatrelvir, SEDDS, degradation study, HPLC, LC-MS/MS
Procedia PDF Downloads 184193 Nanoceutical Intervention (Nanodrug) of Neonatal Hyperbilirubinemias Compared to Conventional Phototherapy
Authors: Samir Kumar Pal
Abstract:
Background: Targeted rapid degradation of bilirubin has the potential to thwart incipient bilirubin encephalopathy. Uncontrolled hyperbilirubinemia is a potential problem in developing countries, including India, because of the lack of reliable healthcare institutes for conventional phototherapy. In India, most of the rural subjects duel in the exchange limit during transport, leading to a risk of kernicterus when they arrive at the treatment centre. Thus, an alternative pharmaceutical agent is needed for the hours. Objective: Exploration of a distinct therapeutic strategy for the control of neonatal hyperbilirubinemia compared to conventional phototherapy in a clinical setting. Method: We synthesized, characterized and investigated a spinel-structured Manganese citrate nanocomplex (C-Mn₃O₄ NC, the nanodrug) along with conventional phototherapy in neonatal subjects. We have also observed BIND scores in order to assess neurological dysfunctions. Results: Our observational study clearly reveals that the rate of declination of bilirubin in neonatal subjects with nanodrug oral administration and phototherapy is faster compared to that in the case of phototherapy only. The associated neural dysfunctions were also found to be significantly lower in the case of combined therapy. Conclusion: This study demonstrates that combined therapy works better than conventional phototherapy only for the control of hyperbilirubinemia. We have observed that a significant portion of neonatal subjects requiring blood exchange has been prevented with the combined therapeutic strategy. Further compilation of a drug-safety-dossier is warranted to translate this novel therapeutic chemo preventive approach to clinical settings.Keywords: nanodrug, nanoparticle, Neonatal hyperbilirubinemia, alternative to phototherapy, redox modulation, redox medicine
Procedia PDF Downloads 594192 Modelling Kinetics of Colour Degradation in American Pokeweed (Phytolacca americana) Extract Concentration
Authors: Seyed-Ahmad Shahidi, Salemeh Kazemzadeh, Mehdi Sharifi Soltani, Azade Ghorbani-HasanSaraei
Abstract:
The kinetics of colour changes of American Pokeweed extract, due to concentration by various heating methods was studied. Three different heating/evaporation processes were employed for production of American Pokeweed extract concentrate. The American Pokeweed extract was concentrated to a final 40 °Brix from an initial °Brix of 4 by microwave heating, rotary vacuum evaporator and evaporating at atmospheric pressure. The final American Pokeweed extract concentration of 40 °Brix was achieved in 188, 216 and 320 min by using microwave, rotary vacuum and atmospheric heating processes, respectively. The colour change during concentration processes was investigated. Total colour differences, Hunter L, a and b parameters were used to estimate the extent of colour loss. All Hunter colour parameters decreased with time. The zero-order, first-order and a combined kinetics model were applied to the changes in colour parameters. All models were found to describe the L, a and b-data adequately. Results indicated that variation in TCD followed both first-order and combined kinetics models. This model implied that the colour formation and pigment destruction occurred during concentration processes of American Pokeweed extract.Keywords: American pokeweed, colour, concentration, kinetics
Procedia PDF Downloads 4984191 Biodegradation of 2,4-Dichlorophenol by Pseudomonas chlororaphis Strain Isolated from Activated Sludge Sample from a Wastewater Treatment Plant in Durban, South Africa
Authors: Boitumelo Setlhare, Mduduzi P. Mokoena, Ademola O. Olaniran
Abstract:
Agricultural and industrial activities have led to increasing production of xenobiotics such as 2,4-dichlorophenol (2,4-DCP), a derivative of 2,4-dichlorophenoxyacetic acid (2,4-D), which is a widely used herbicide. Bioremediation offers an efficient, cost-effective and environmentally friendly method for degradation of the compound through the activities of the various microbial enzymes involved in the catabolic pathway. The aim of this study was to isolate and characterize bacterial isolate indigenous to contaminated sites in Durban, South Africa for 2,4-DCP degradation. One bacterium capable of utilizing 2,4-DCP as sole carbon source was isolated using culture enrichment technique and identified as Pseudomonas chlororaphis strain UFB2 via PCR amplification and analysis of 16S rRNA gene sequence. This isolate was able to degrade up to 75.11% of 2,4-DCP in batch cultures within 10 days, with the degradation rate constant of 0.14 mg/l/d. Phylogenetic analysis revealed the relatedness of this bacterial isolate to other Pseudomonas sp. previously characterized for chlorophenol degradation. PCR amplification of the catabolic genes involved in 2,4-DCP degradation revealed the presence of the correct amplicons for phenol hydroxylase (600 bp), catechol 1,2-dioxygenase (214 bp), muconate isomerase (851 bp), cis-dienelactone hydrolase (577 bp), and trans-dienelactone hydrolase (491 bp) genes. Enzyme assays revealed activity as high as 21840 mU/mg, 15630 mU/mg, 2340 mU/mg and 1490 mU/mg obtained for phenol hydroxylase, catechol 1,2-dioxygenase, cis-dienelactone hydroxylase and trans-dienelactone hydroxylase, respectively. The absence of catechol 2,3-dioxygenase gene and the corresponding enzyme in this isolate suggests that the organism followed ortho-pathway for 2,4-DCP degradation. Furthermore, the absence of malaycetate reductase genes showed that the bacterium may not be able to completely mineralize 2,4-DCP. Further studies are required to optimize 2,4-DCP degradation by this isolate as well as to elucidate the mechanism of 2,4-DCP degradation.Keywords: biodegradation, catechol 1, 2-dioxygenase, 2, 4-dichlorophenol, phenol hydroxylase, Pseudomonas chlororaphis
Procedia PDF Downloads 2504190 Numerical Simulation of the Effect of 1 Mev Electron Beam on the Performance of a Solar Cell of Type n+/p GaAs
Authors: Waleed Alsaidy, Mourad Mbarki
Abstract:
In this work, it have investigated the effect of electron irradiation on the output characteristics of n+/p GaAs solar cell. The studied solar cell is exposed to an electron beam with kinetic energy of 1 MeV under AM0 illumination. In this work, it have used our own software to calculate the damage caused by these energetic particles. Indeed, these particles produce severe degradation on the performances of the solar cells. The aim of this work is to investigate the effect of electronic irradiation on the J(V) characteristics upon the fluence of particles φ (electron/cm2). Thereafter, we have evaluated the degradation of its performances such as the short circuit current J_sc, the open circuit voltage V_oc the efficiency η with respect to the fluence φ of electrons. it have shown that the variation of these parameters decrease linearly with the logarithm of the fluence φ, and their degradation begins from a threshold value φ_m. To validate our calculation, we have compared our results with other theoretical and experimental results available in the literature and we have found a good agreement between them.Keywords: solar cells, GaAs, short circuit current, open circuit voltage, fluence, degradation
Procedia PDF Downloads 224189 A Framework for Incorporating Non-Linear Degradation of Conductive Adhesive in Environmental Testing
Authors: Kedar Hardikar, Joe Varghese
Abstract:
Conductive adhesives have found wide-ranging applications in electronics industry ranging from fixing a defective conductor on printed circuit board (PCB) attaching an electronic component in an assembly to protecting electronics components by the formation of “Faraday Cage.” The reliability requirements for the conductive adhesive vary widely depending on the application and expected product lifetime. While the conductive adhesive is required to maintain the structural integrity, the electrical performance of the associated sub-assembly can be affected by the degradation of conductive adhesive. The degradation of the adhesive is dependent upon the highly varied use case. The conventional approach to assess the reliability of the sub-assembly involves subjecting it to the standard environmental test conditions such as high-temperature high humidity, thermal cycling, high-temperature exposure to name a few. In order to enable projection of test data and observed failures to predict field performance, systematic development of an acceleration factor between the test conditions and field conditions is crucial. Common acceleration factor models such as Arrhenius model are based on rate kinetics and typically rely on an assumption of linear degradation in time for a given condition and test duration. The application of interest in this work involves conductive adhesive used in an electronic circuit of a capacitive sensor. The degradation of conductive adhesive in high temperature and humidity environment is quantified by the capacitance values. Under such conditions, the use of established models such as Hallberg-Peck model or Eyring Model to predict time to failure in the field typically relies on linear degradation rate. In this particular case, it is seen that the degradation is nonlinear in time and exhibits a square root t dependence. It is also shown that for the mechanism of interest, the presence of moisture is essential, and the dominant mechanism driving the degradation is the diffusion of moisture. In this work, a framework is developed to incorporate nonlinear degradation of the conductive adhesive for the development of an acceleration factor. This method can be extended to applications where nonlinearity in degradation rate can be adequately characterized in tests. It is shown that depending on the expected product lifetime, the use of conventional linear degradation approach can overestimate or underestimate the field performance. This work provides guidelines for suitability of linear degradation approximation for such varied applicationsKeywords: conductive adhesives, nonlinear degradation, physics of failure, acceleration factor model.
Procedia PDF Downloads 1354188 Identification, Isolation and Characterization of Unknown Degradation Products of Cefprozil Monohydrate by HPTLC
Authors: Vandana T. Gawande, Kailash G. Bothara, Chandani O. Satija
Abstract:
The present research work was aimed to determine stability of cefprozil monohydrate (CEFZ) as per various stress degradation conditions recommended by International Conference on Harmonization (ICH) guideline Q1A (R2). Forced degradation studies were carried out for hydrolytic, oxidative, photolytic and thermal stress conditions. The drug was found susceptible for degradation under all stress conditions. Separation was carried out by using High Performance Thin Layer Chromatographic System (HPTLC). Aluminum plates pre-coated with silica gel 60F254 were used as the stationary phase. The mobile phase consisted of ethyl acetate: acetone: methanol: water: glacial acetic acid (7.5:2.5:2.5:1.5:0.5v/v). Densitometric analysis was carried out at 280 nm. The system was found to give compact spot for cefprozil monohydrate (0.45 Rf). The linear regression analysis data showed good linear relationship in the concentration range 200-5.000 ng/band for cefprozil monohydrate. Percent recovery for the drug was found to be in the range of 98.78-101.24. Method was found to be reproducible with % relative standard deviation (%RSD) for intra- and inter-day precision to be < 1.5% over the said concentration range. The method was validated for precision, accuracy, specificity and robustness. The method has been successfully applied in the analysis of drug in tablet dosage form. Three unknown degradation products formed under various stress conditions were isolated by preparative HPTLC and characterized by mass spectroscopic studies.Keywords: cefprozil monohydrate, degradation products, HPTLC, stress study, stability indicating method
Procedia PDF Downloads 2994187 Synthesis, Characterization and Photocatalytic Applications of Ag-Doped-SnO₂ Nanoparticles by Sol-Gel Method
Authors: M. S. Abd El-Sadek, M. A. Omar, Gharib M. Taha
Abstract:
In recent years, photocatalytic degradation of various kinds of organic and inorganic pollutants using semiconductor powders as photocatalysts has been extensively studied. Owing to its relatively high photocatalytic activity, biological and chemical stability, low cost, nonpoisonous and long stable life, Tin oxide materials have been widely used as catalysts in chemical reactions, including synthesis of vinyl ketone, oxidation of methanol and so on. Tin oxide (SnO₂), with a rutile-type crystalline structure, is an n-type wide band gap (3.6 eV) semiconductor that presents a proper combination of chemical, electronic and optical properties that make it advantageous in several applications. In the present work, SnO₂ nanoparticles were synthesized at room temperature by the sol-gel process and thermohydrolysis of SnCl₂ in isopropanol by controlling the crystallite size through calculations. The synthesized nanoparticles were identified by using XRD analysis, TEM, FT-IR, and Uv-Visible spectroscopic techniques. The crystalline structure and grain size of the synthesized samples were analyzed by X-Ray diffraction analysis (XRD) and the XRD patterns confirmed the presence of tetragonal phase SnO₂. In this study, Methylene blue degradation was tested by using SnO₂ nanoparticles (at different calculations temperatures) as a photocatalyst under sunlight as a source of irradiation. The results showed that the highest percentage of degradation of Methylene blue dye was obtained by using SnO₂ photocatalyst at calculations temperature 800 ᵒC. The operational parameters were investigated to be optimized to the best conditions which result in complete removal of organic pollutants from aqueous solution. It was found that the degradation of dyes depends on several parameters such as irradiation time, initial dye concentration, the dose of the catalyst and the presence of metals such as silver as a dopant and its concentration. Percent degradation was increased with irradiation time. The degradation efficiency decreased as the initial concentration of the dye increased. The degradation efficiency increased as the dose of the catalyst increased to a certain level and by further increasing the SnO₂ photocatalyst dose, the degradation efficiency is decreased. The best degradation efficiency on which obtained from pure SnO₂ compared with SnO₂ which doped by different percentage of Ag.Keywords: SnO₂ nanoparticles, a sol-gel method, photocatalytic applications, methylene blue, degradation efficiency
Procedia PDF Downloads 1524186 Degradation of Heating, Ventilation, and Air Conditioning Components across Locations
Authors: Timothy E. Frank, Josh R. Aldred, Sophie B. Boulware, Michelle K. Cabonce, Justin H. White
Abstract:
Materials degrade at different rates in different environments depending on factors such as temperature, aridity, salinity, and solar radiation. Therefore, predicting asset longevity depends, in part, on the environmental conditions to which the asset is exposed. Heating, ventilation, and air conditioning (HVAC) systems are critical to building operations yet are responsible for a significant proportion of their energy consumption. HVAC energy use increases substantially with slight operational inefficiencies. Understanding the environmental influences on HVAC degradation in detail will inform maintenance schedules and capital investment, reduce energy use, and increase lifecycle management efficiency. HVAC inspection records spanning 14 years from 21 locations across the United States were compiled and associated with the climate conditions to which they were exposed. Three environmental features were explored in this study: average high temperature, average low temperature, and annual precipitation, as well as four non-environmental features. Initial insights showed no correlations between individual features and the rate of HVAC component degradation. Using neighborhood component analysis, however, the most critical features related to degradation were identified. Two models were considered, and results varied between them. However, longitude and latitude emerged as potentially the best predictors of average HVAC component degradation. Further research is needed to evaluate additional environmental features, increase the resolution of the environmental data, and develop more robust models to achieve more conclusive results.Keywords: climate, degradation, HVAC, neighborhood component analysis
Procedia PDF Downloads 4314185 Enzymatic Degradation of Poly (Butylene Adipate Terephthalate) Copolymer Using Lipase B From Candida Antarctica and Effect of Poly (Butylene Adipate Terephthalate) on Plant Growth
Authors: Aqsa Kanwal, Min Zhang, Faisal Sharaf, Li Chengtao
Abstract:
The globe is facing increasing challenges of plastic pollution due to single-use of plastic-based packaging material. The plastic material is continuously being dumped into the natural environment, which causes serious harm to the entire ecosystem. Polymer degradation in nature is very difficult, so the use of biodegradable polymers instead of conventional polymers can mitigate this issue. Due to the good mechanical properties and biodegradability, aliphatic-aromatic polymers are being widely commercialized. Due to the advancement in molecular biology, many studies have reported specific microbes that can effectively degrade PBAT. Aliphatic polyesters undergo hydrolytic cleavage of ester groups, so they can be easily degraded by microorganisms. In this study, we investigated the enzymatic degradation of poly (butylene adipate terephthalate) (PBAT) copolymer using lipase B from Candida Antarctica (CALB). Results of the study displayed approximately 5.16 % loss in PBAT mass after 2 days which significantly increased to approximately 15.7 % at the end of the experiment (12 days) as compared to blank. The pH of the degradation solution also displayed significant reduction and reached the minimum value of 6.85 at the end of the experiment. The structure and morphology of PBAT after degradation were characterized by FTIR, XRD, SEM, and TGA. FTIR analysis showed that after degradation many peaks become weaker and the peak at 2950 cm-1 almost disappeared after 12 days. The XRD results indicated that as the degradation time increases the intensity of diffraction peaks slightly increases as compared to the blank PBAT. TGA analysis also confirmed the successful degradation of PBAT with time. SEM micrographs further confirmed that degradation has occurred. Hence, biodegradable polymers can widely be used. The effect of PBAT biodegradation on plant growth was also studied and it was found that PBAT has no toxic effect on the growth of plants. Hence PBAT can be employed in a wide range of applications.Keywords: aliphatic-aromatic co-polyesters, polybutylene adipate terephthalate, lipase (CALB), biodegradation, plant growth
Procedia PDF Downloads 79