4034 Effects of Rice Husk Ash on the Properties of Scrap Tyre Steel Fiber Reinforced High Performance Concrete (RHA-STSFRHAC)
Authors: Isyaka Abdulkadir, Egbe-Ngu Ntui Ogork
Abstract:
This research aims to investigate the effect of Rice Husk Ash (RHA) on Scrap Tyre Steel Fiber Reinforced High Performance Concrete (STSFRHPC). RHA was obtained by control burning of rice husk in a kiln to a temperature of 650-700oC and when cooled sieved through 75µm sieve and characterized. The effect of RHA were investigated on grade 50 STSFRHPC of 1:1.28:1.92 with water cement ratio of 0.39 at additions of Scrap Tyre Steel Fiber (STSF) of 1.5% by volume of concrete and partial replacement of cement with RHA at percentages of 0, 5, 10, 15 and 20. The fresh concrete was tested for slump while the hardened concrete was tested for compressive and splitting tensile strengths respectively at curing ages of 3, 7, 28 and 56 days in accordance with standard procedure. Results of RHA-STSFRHPC indicated a reduction in slump and compressive strength with increase in RHA content, while splitting tensile strength increased with RHA replacement up to 10% and reduction in strength above 10% RHA content. The 28 days compressive strength of RHA-STSFRHPC with up to 10% RHA attained the desired characteristic strength of 50N/mm2 and therefore up to 10% RHA is considered as the optimum replacement dosage in STSFRHPC-RHA.Keywords: compressive strength, high performance concrete, rice husk ash, scrap tyre steel fibers
Procedia PDF Downloads 3384033 Suitability of Quarry Dust as Replacement of Sand in Medium Grade Concrete
Authors: Popoola M. Oyenola
Abstract:
Concrete plays the important role and a huge percentage of concrete is being utilized in every construction practices. Natural river sand is one of the major ingredients of concrete, is becoming expensive due to excessive cost of accessibility from sources. Also large scale depletion of sources creates environmental problems. Therefore, there is a need of economic alternative materials. Quarry dust is a waste obtained during quarrying process. It has been rampantly used in different construction practices and could be used as an effective fine aggregate instead of river sand. Partial and total replacement of fine aggregate in conventional concrete with quarry dust has been empirically conducted with the view to examining primarily the compressive strength of the resulting composite and possible total utilization of quarry dust as fine aggregate in the production of medium grade concrete. The results of the study showed that its specific gravity, porosity and water absorption showed satisfactory performance. The percentage replacement of natural river sand with quarry dust for a designed strength of 25N/mm2 varied at intervals of 10% up to a maximum value of 100%. A total of 132 cubes of 150 x 150 x 150mm were cast and tested at 7, 14 and 28 days of hydration. Compressive strength increases with curing age in all the mixes. Compressive strength decreases with increase in percentage of quarry dust. Generally the compressive strength of concrete incorporating quarry dust attained strength of 22.47 N/mm2 after 28 days which makes it a suitable aggregate for the production medium grade concrete.Keywords: quarry dust, concrete, aggregates, compressive strength
Procedia PDF Downloads 2454032 Differential Effect of Technique Majors on Isokinetic Strength in Youth Judoka Athletes
Authors: Chungyu Chen, Yi-Cheng Chen, Po-Hsian Hsu, Hsin-Ying Chen, Yen-Po Hsiao
Abstract:
The purpose of this study was to assess the muscular strength performance of upper and lower extremity in isokinetic system for the youth judo players, and also to compare the strength difference between major techniques. Sixteen male and 20 female judo players (age: 16.7 ± 1.6 years old, training age: 4.5 ± 0.8 years) were served as the volunteers for this study. There were 21 players major hand techniques and 15 players major foot techniques. The Biodex S4 Pro was used to assess the strength performance of extensor and flexor of concentric action under the load condition of 30 degree/sec, 60 degree/sec, and 120 degree/sec for elbow joints and knee joints. The strength parameters were included the maximal torque, the normalized maximal torque, the average power, and the average maximal torque. A t test for independent groups was used to evaluate whether hand major and foot major differ significantly with an alpha level of .05. The result showed the maximal torque of left knee extensor in foot major players (243.5 ± 36.3 Nm) was higher significantly than hand major (210.7 ± 21.0 Nm) under the load of 30 degree/sec (p < .05). There were no differences in upper extremity strength between the hand and foot techniques major in three loads (ps < .05). It indicated that the judo player is required to develop the upper extremity strength overall to secure the execution of major techniques.Keywords: knee, elbow, power, judo
Procedia PDF Downloads 4574031 The Development of a Low Carbon Cementitious Material Produced from Cement, Ground Granulated Blast Furnace Slag and High Calcium Fly Ash
Authors: Ali Shubbar, Hassnen M. Jafer, Anmar Dulaimi, William Atherton, Ali Al-Rifaie
Abstract:
This research represents experimental work for investigation of the influence of utilising Ground Granulated Blast Furnace Slag (GGBS) and High Calcium Fly Ash (HCFA) as a partial replacement for Ordinary Portland Cement (OPC) and produce a low carbon cementitious material with comparable compressive strength to OPC. Firstly, GGBS was used as a partial replacement to OPC to produce a binary blended cementitious material (BBCM); the replacements were 0, 10, 15, 20, 25, 30, 35, 40, 45 and 50% by the dry mass of OPC. The optimum BBCM was mixed with HCFA to produce a ternary blended cementitious material (TBCM). The replacements were 0, 10, 15, 20, 25, 30, 35, 40, 45 and 50% by the dry mass of BBCM. The compressive strength at ages of 7 and 28 days was utilised for assessing the performance of the test specimens in comparison to the reference mixture using 100% OPC as a binder. The results showed that the optimum BBCM was the mix produced from 25% GGBS and 75% OPC with compressive strength of 32.2 MPa at the age of 28 days. In addition, the results of the TBCM have shown that the addition of 10, 15, 20 and 25% of HCFA to the optimum BBCM improved the compressive strength by 22.7, 11.3, 5.2 and 2.1% respectively at 28 days. However, the replacement of optimum BBCM with more than 25% HCFA have showed a gradual drop in the compressive strength in comparison to the control mix. TBCM with 25% HCFA was considered to be the optimum as it showed better compressive strength than the control mix and at the same time reduced the amount of cement to 56%. Reducing the cement content to 56% will contribute to decrease the cost of construction materials, provide better compressive strength and also reduce the CO2 emissions into the atmosphere.Keywords: cementitious material, compressive strength, GGBS, HCFA, OPC
Procedia PDF Downloads 1954030 Improvement of Compressive and Tensile Strengths of Concrete Using Polypropylene Fibers
Authors: Omar Asad Ahmad, Mohammed Awwad
Abstract:
Concrete is one of the essential elements that used in different types of construction these days, but it has many problems when interacts with environmental elements such as water, air, temperature, dust, and humidity. Also concrete made with Portland cement has certain characteristics: it is relatively strong in compression but weak in tension and tends to be brittle. These disadvantages make concrete limited to use in certain conditions. The most common problems appears on concrete are manifested by tearing, cracking, corrosion and spalling, which will lead to do some defect in concrete then in the whole construction, The fundamental objective of this research was to provide information about the hardened properties of concrete achieved by using easily available local raw materials in Jordan to support the practical work with partners in assessing the practicability of the mixes with polypropylene, and to facilitate the introduction of polypropylene fiber concrete (PFC) technology into general construction practice. Investigate the effect of the polypropylene fibers in PCC mixtures and on materials properties such as compressive strength, and tensile strength. Also to investigate the use of polypropylene fibers in plain cubes and cylindrical concrete to improve its compressive and tensile strengths to reduce early cracking and inhibit later crack growth. Increasing the hardness of concrete in this research is the main purpose to measure the deference of compressive strength and tensile strength between plain concrete and concrete mixture with polypropylene fibers different additions and to investigate its effect on reducing the early and later cracking problem. To achieve the goals of research 225 concrete test sample were prepared to measure it’s compressive strength and tensile strength, the concrete test sample were three classes (A,B,C), sub-classified to standard , and polypropylene fibers added by the volume of concrete (5%, 10%, 15%, and 20%). The investigation of polypropylene fibers mixture with concrete shows that the strengths of the cement are increased and the cracking decreased. The results show that for class A the recommended addition were 5% of polypropylene fibers additions for compressive strength and 10 % for tensile strength revels the best compressive strength that reach 26.67 Mpa and tensile strength that reach 2.548 Mpa records. Achieved results show that for classes B and C the recommend additions were 10 % polypropylene fibers revels the best compressive strength records where they reach 21.11 and 33.78 Mpa, records reach for tensile strength 2.707 and 2.65 Mpa respectively.Keywords: polypropylene, effects, compressive, tensile, strengths, concrete, construction
Procedia PDF Downloads 5474029 Relationship between Interfacial Instabilities and Mechanical Strength of Multilayer Symmetric Polymer Melts
Authors: Mohammad Ranjbaran Madiseh
Abstract:
In this research, an experimental apparatus has been developed for observing interfacial stability and deformation of multilayer pressure-driven channel flows. The interface instability of the co-extrusion flow of polyethylene and polypropylene is studied experimentally in a slit geometry. By investigating the growing interfacial wave (IW) and tensile stress of extrudate samples, a relationship between interfacial instability (II) and mechanical properties of polypropylene (PP) and high-density polyethylene (HDPE) has been established. It is shown that the mechanism of interfacial strength is related to interfacial instabilities as well as interfacial strength. It is shown that there is an ability to forecast the quality of final products in the co-extrusion process. In this study, it is found that the instability is controlled by its dominant wave number, which is associated with maximum tensile stress at the interface.Keywords: interfacial instability, interfacial strength, wave number, interfacial wave
Procedia PDF Downloads 924028 Structural Strength Potentials of Nigerian Groundnut Husk Ash as Partial Cement Replacement in Mortar
Authors: F. A. Olutoge, O.R. Olulope, M. O. Odelola
Abstract:
This study investigates the strength potentials of groundnut husk ash as partial cement replacement in mortar and also develops a predictive model using Artificial Neural Network. Groundnut husks sourced from Ogbomoso, Nigeria, was sun dried, calcined to ash in a furnace at a controlled temperature of 600⁰ C for a period of 6 hours, and sieved through the 75 microns. The ash was subjected to chemical analysis and setting time test. Fine aggregate (sand) for the mortar was sourced from Ado Ekiti, Nigeria. The cement: GHA constituents were blended in ratios 100:0, 95:5, 90:10, 85:15 and 80:20 %. The sum of SiO₂, Al₂O₃, and Fe₂O₃ content in GHA is 26.98%. The compressive strength for mortars PC, GHA5, GHA10, GHA15, and GHA20 ranged from 6.3-10.2 N/mm² at 7days, 7.5-12.3 N/mm² at 14 days, 9.31-13.7 N/mm² at 28 days, 10.4-16.7 N/mm² at 56days and 13.35- 22.3 N/mm² at 90 days respectively, PC, GHA5 and GHA10 had competitive values up to 28 days, but GHA10 gave the highest values at 56 and 90 days while GHA20 had the lowest values at all ages due to dilution effect. Flexural strengths values at 28 days ranged from 1.08 to 1.87 N/mm² and increased to a range of 1.53-4.10 N/mm² at 90 days. The ANN model gave good prediction for compressive strength of the mortars. This study has shown that groundnut husk ash as partial cement replacement improves the strength properties of mortar.Keywords: compressive strength, groundnut husk ash, mortar, pozzolanic index
Procedia PDF Downloads 1554027 Comparative Study on Efficacy and Clinical Outcomes in Minimally Invasive Surgery Transforaminal Interbody Fusion vs Minimally Invasive Surgery Lateral Interbody Fusion
Authors: Sundaresan Soundararajan, George Ezekiel Silvananthan, Chor Ngee Tan
Abstract:
Introduction: Transforaminal Interbody Fusion (TLIF) has been adopted for many decades now, however, XLIF, still in relative infancy, has grown to be accepted as a new Minimally Invasive Surgery (MIS) option. There is a paucity of reports directly comparing lateral approach surgery to other MIS options such as TLIF in the treatment of lumbar degenerative disc diseases. Aims/Objectives: The objective of this study was to compare the efficacy and clinical outcomes between Minimally Invasive Transforaminal Interbody Fusion (TLIF) and Minimally Invasive Lateral Interbody Fusion (XLIF) in the treatment of patients with degenerative disc disease of the lumbar spine. Methods: A single center, retrospective cohort study involving a total of 38 patients undergoing surgical intervention between 2010 and 2013 for degenerative disc disease of lumbar spine at single L4/L5 level. 18 patients were treated with MIS TLIF, and 20 patients were treated with XLIF. Results: The XLIF group showed shorter duration of surgery compared to the TLIF group (176 mins vs. 208.3 mins, P = 0.03). Length of hospital stay was also significantly shorter in XLIF group (5.9 days vs. 9 days, p = 0.03). Intraoperative blood loss was favouring XLIF as 85% patients had blood loss less than 100cc compared to 58% in the TLIF group (P = 0.03). Radiologically, disc height was significantly improved post operatively in the XLIF group compared to the TLIF group (0.56mm vs. 0.39mm, P = 0.01). Foraminal height increment was also higher in the XLIF group (0.58mm vs. 0.45mm , P = 0.06). Clinically, back pain and leg pain improved in 85% of patients in the XLIF group and 78% in the TLIF group. Post op hip flexion weakness was more common in the XLIF group (40%) than in the TLIF group (0%). However, this weakness resolved within 6 months post operatively. There was one case of dural tear and surgical site infection in the TLIF group respectively and none in the XLIF group. Visual Analog Scale (VAS) score 6 months post operatively showed comparable reduction in both groups. TLIF group had Owsterty Disability Index (ODI) improvement on 67% while XLIF group showed improvement of 70% of its patients. Conclusions: Lateral approach surgery shows comparable clinical outcomes in resolution of back pain and radiculopathy to conventional MIS techniques such as TLIF. With significantly shorter duration of surgical time, minimal blood loss and shorter hospital stay, XLIF seems to be a reasonable MIS option compared to other MIS techniques in treating degenerative lumbar disc diseases.Keywords: extreme lateral interbody fusion, lateral approach, minimally invasive, XLIF
Procedia PDF Downloads 2204026 Characterization of Erodibility Using Soil Strength and Stress-Strain Indices for Soils in Some Selected Sites in Enugu State
Authors: C. C. Egwuonwu, N. A. A. Okereke, K. O. Chilakpu, S. O. Ohanyere
Abstract:
In this study, initial soil strength indices (qu) and stress-strain characteristics, namely failure strain (ϵf), area under the stress-strain curve up to failure (Is) and stress-strain modulus between no load and failure (Es) were investigated as potential indicators for characterizing the erosion resistance of two compacted soils, namely sandy clay loam (SCL) and clay loam (CL) in some selected sites in Enugu State, Nigeria. The unconfined compressive strength (used in obtaining strength indices) and stress-strain measurements were obtained as a function of moisture content in percentage (mc %) and dry density (γd). Test were conducted over a range of 8% to 30% moisture content and 1.0 g/cm3 to 2.0 g/cm3 dry density at applied loads of 20, 40, 80, 160 and 320 kPa. Based on the results, it was found out that initial soil strength alone was not a good indicator of erosion resistance. For instance, in the comparison of exponents of mc% and γd for jet index or erosion resistance index (Ji) and the strength measurements, qu and Es agree in signs for mc%, but are opposite in signs for γd. Therefore, there is an inconsistency in exponents making it difficult to develop a relationship between the strength parameters and Ji for this data set. In contrast, the exponents of mc% and γd for Ji and ϵf and Is are opposite in signs, there is potential for an inverse relationship. The measured stress-strain characteristics, however, appeared to have potential in providing useful information on erosion resistance. The models developed for the prediction of the extent or the susceptibility of soils to erosion and subjected to sensitivity test on some selected sites achieved over 90% efficiency in their functions.Keywords: characterization of erodibility, selected sites in Enugu state, soil strength, stress-strain indices
Procedia PDF Downloads 4154025 The Effect of Mineral Addition (Natural Pozzolana) on the Capillary Absorption and Compressive Strength of Environmental Mortar
Authors: W. Deboucha, M. N. Oudjit, A. Bouzid, L. Belagraa, A.Noui
Abstract:
The cement manufacturing is the one of the factors that pollutes the atmosphere in the industrial sector. The common way to reduce this pollution is using mineral additions as partial replacement of Portland cement. Particularly, natural pozzolana (NP) is component in which they can be used to decrease the rate of pollution. The main objective of this experimental work is the study of the effect of mineral addition (natural pozzolana) on the capillary water absorption and compressive-flexural strength of cement mortar. The results obtained in the present research showed that the higher dosages of natural pozzolana added could be the principal parameter of such decrease in strength at early and medium term. Further, this increase of incorporated addition has been believed to reduce the capillary water absorption.Keywords: Natural pozzolana, mortar, strength, capillary absorption
Procedia PDF Downloads 3494024 Study on the Strength and Durability Properties of Ternary Blended Concrete
Authors: Athira Babu, M. Nazeer
Abstract:
Concrete is the most common and versatile construction material used in any type of civil engineering structure. The durability and strength characteristics of concrete make it more desirable among any other construction materials. The manufacture and use of concrete produces wide range of environmental and social consequences. The major component in concrete, cement accounts for roughly 5 % of global CO2 emissions. In order to improve the environmental friendliness of concrete, suitable substitutes are added to concrete. The present study deals with GGBS and silica fume as supplementary cementitious materials. The strength and durability studies were conducted in this ternary blended concrete. Several mixes were adopted with varying percentages of Silica Fume i.e., 5%, 10% and 15%. Binary mix with 50% GGBS was also prepared. GGBS content has been kept constant for the rest of mixes. There is an improvement in compressive strength with addition of Silica Fume.Maximum workability, split tensile strength, modulus of elasticity, flexural strength and impact resistance are obtained for GGBS binary blend. For durability studies, maximum sulphate resistance,carbonation resistance andresistance to chloride ion penetration are obtained for ternary blended concrete. Partial replacement of GGBS and Silica Fume reduces the environmental effects, produces economical and eco-friendly concrete. The study showed that for strength characteristics, binary blended concrete showed better performance while for durability study ternary blend performed better.Keywords: concrete, GGBS, silica fume, ternary blend
Procedia PDF Downloads 4824023 Development of Light-Weight Refractory Bricks
Authors: Liaqat Ali, Furqan Ahmad
Abstract:
The heat losses should be controlled during the high temperature processes from energy conservation point of view. For this purpose, refractories with low thermal conductivity, high porosity and good mechanical strength along with low price are desirable. In this work, various combinations of naturally occurring, locally available, cheap raw materials, namely, clay, rice husk and saw dust were used. Locally produced insulating firebricks (IFBs) cannot be used at higher than a few hundred °C and possess low strength as well. Various process parameters were studied and the refractories with desirable properties were produced, which can be used up to 1200 °C.Keywords: firebricks, mechanical strength, thermal conductivity, refractory bricks
Procedia PDF Downloads 3294022 Particle Size Effect on Shear Strength of Granular Materials in Direct Shear Test
Authors: R. Alias, A. Kasa, M. R. Taha
Abstract:
The effect of particle size on shear strength of granular materials are investigated using direct shear tests. Small direct shear test (60 mm by 60 mm by 24 mm deep) were conducted for particles passing the sieves with opening size of 2.36 mm. Meanwhile, particles passing the standard 20 mm sieves were tested using large direct shear test (300 mm by 300 mm by 200 mm deep). The large direct shear tests and the small direct shear tests carried out using the same shearing rate of 0.09 mm/min and similar normal stresses of 100, 200, and 300 kPa. The results show that the peak and residual shear strength decreases as particle size increases.Keywords: particle size, shear strength, granular material, direct shear test
Procedia PDF Downloads 4924021 Reformulation of Theory of Critical Distances to Predict the Strength of Notched Plain Concrete Beams under Quasi Static Loading
Authors: Radhika V., J. M. Chandra Kishen
Abstract:
The theory of critical distances (TCD), due to its appealing characteristics, has been successfully used in the past to predict the strength of brittle as well as ductile materials, weakened by the presence of stress risers under both static and fatigue loading. By utilising most of the TCD's unique features, this paper summarises an attempt for a reformulation of the point method of the TCD to predict the strength of notched plain concrete beams under mode I quasi-static loading. A zone of micro cracks, which is responsible for the non-linearity of concrete, is taken into account considering the concept of an effective elastic crack. An attempt is also made to correlate the value of the material characteristic length required for the application of TCD with the maximum aggregate size in the concrete mix, eliminating the need for any extensive experimentation prior to the application of TCD. The devised reformulation and the proposed power law based relationship is found to yield satisfactory predictions for static strength of notched plain concrete beams, with geometric dimensions of the beam, tensile strength, and maximum aggregate size of the concrete mix being the only needed input parameters.Keywords: characteristic length, effective elastic crack, inherent material strength, modeI loading, theory of critical distances
Procedia PDF Downloads 1004020 Flexural Strength of Alkali Resistant Glass Textile Reinforced Concrete Beam with Prestressing
Authors: Jongho Park, Taekyun Kim, Jungbhin You, Sungnam Hong, Sun-Kyu Park
Abstract:
Due to the aging of bridges, increasing of maintenance costs and decreasing of structural safety is occurred. The steel corrosion of reinforced concrete bridge is the most common problem and this phenomenon is accelerating due to abnormal weather and increasing CO2 concentration due to climate change. To solve these problems, composite members using textile have been studied. A textile reinforced concrete can reduce carbon emissions by reduced concrete and without steel bars, so a lot of structural behavior studies are needed. Therefore, in this study, textile reinforced concrete beam was made and flexural test was performed. Also, the change of flexural strength according to the prestressing was conducted. As a result, flexural strength of TRC with prestressing was increased compared and flexural behavior was shown as reinforced concrete.Keywords: AR-glass, flexural strength, prestressing, textile reinforced concrete
Procedia PDF Downloads 3314019 Bioremediation Effect on Shear Strength of Contaminated Soils
Authors: Samira Abbaspour
Abstract:
Soil contamination by oil industry is unavoidable issue; irrespective of environmental impact, which occurs during the process of soil contaminating and remediating. Effect of this phenomenon on the geotechnical properties of the soil has not been investigated thoroughly. Some researchers studied the environmental aspects of these phenomena more than geotechnical point of view. In this research, compaction and unconfined compression tests were conducted on samples of natural, contaminated and treated soil after 50 days of bio-treatment. The results manifest that increasing the amount of crude oil, leads to decreased values of maximum dry density and optimum water content and increased values of unconfined compression strength (UCS). However, almost 65% of this contamination terminated by using a Bioremer as a bioremediation agent. Foremost, as bioremediation takes place, values of maximum dry density, unconfined compression strength and failure strain increase.Keywords: contamination, shear strength, compaction, oil contamination
Procedia PDF Downloads 1854018 X-Bracing Configuration and Seismic Response
Authors: Saeed Rahjoo, Babak H. Mamaqani
Abstract:
Concentric bracing systems have been in practice for many years because of their effectiveness in reducing seismic response. Depending on concept, seismic design codes provide various response modification factors (R), which itself consists of different terms, for different types of lateral load bearing systems but configuration of these systems are often ignored in the proposed values. This study aims at considering the effect of different x-bracing diagonal configuration on values of ductility dependent term in R computation. 51 models were created and nonlinear push over analysis has been performed. The main variables of this study were the suitable location of X–bracing diagonal configurations, which establishes better nonlinear behavior in concentric braced steel frames. Results show that some x-bracing diagonal configurations improve the seismic performance of CBF significantly and explicit consideration of lateral load bearing systems seems necessary.Keywords: bracing configuration, concentrically braced frame (CBF), push over analyses, response reduction factor
Procedia PDF Downloads 3514017 Mechanical Behaviour of High Strength Steel Thin-Walled Profiles for Automated Rack Supported Warehouses
Authors: Agnese Natali, Francesco Morelli, Walter Salvatore, José Humberto Matias de Paula Filho, Patrick Pol
Abstract:
In the framework of the evaluation of the applicability of high strength steel to produce thin-walled elements to be used in Automated Rack Supported Warehouses, an experimental campaign is carried outto evaluate the structural performance of typical profile shapes adopted for such purposes and made of high strength steel. Numerical models are developed to fit the observed failure modes, stresses, and deformation patterns, and proper directions are proposed to simplify the numerical simulations to be used in further applications and to evaluate the mechanical behavior and performance of profiles.Keywords: Steel racks, Automated Rack Supported Warehouse, thin walled cold-formed elements, high strength steel.
Procedia PDF Downloads 1804016 Nano and Micro Silica Cooperating Effect on Ferrocement Mortar
Authors: Aziz Ibrahim Abdulla, Omar Mohanad Mahdi
Abstract:
The objective of this paper is to explore the effect of incorporating Nano-Silica with Silica-fume in ferrocement mortar to enhancing mechanical properties of it. One type of Nano silica with average diameter size 23nm and silica fume have been used with two percentage (1%, 2% Nano silica and 5%, 10% silica fume per weight of cement) and w/c with / without superplasticizer was been calculated by flow test method. Also three sand: cement ratios have been used (1.5, 2.0 and 2.5) with max. Aggregate size 0.6mm in this study for reference and other mixtures. Results reveal adding Nano silica with silica fume to ferrocement mortar enhances its physical and mechanical properties such as compressive strength and flexural strength. The SEM pictures and density with absorption ratio demonstrate that Nano silica with silica fume contributes to enhancement of mortar through yielding denser, more compact and uniform mixtures.Keywords: nano silica, ferrocement mortar, compresion strength, flexural strength
Procedia PDF Downloads 3824015 Variation of Compressive Strength of Hollow Sand Crate Block (6”) with Mix Ratio Using Locally Made Cement (Sokoto Cement)
Authors: Idris Adamu Idris
Abstract:
The Nigerian construction industry is faced with problems of failure of structures/buildings. These failures are attributed to the use of low quality construction materials of which sand crate bock is inclusive. The research was conducted to determine the compressive strength of hollow sand crate block (6”) using locally made cement (Sokoto cement). Samples were tested for 7, 14, 21 and 28 days for mix ratio of 1:3 to 1:12. From the laboratory results obtained, a mix ratio of 1:10 corresponding to a minimum compressive strength of 1.9N/mm2 at 7 days should be adopted. This satisfies the BS 2028, 1364 1986 which specified a minimum compressive strength of 1.8N/mm2 at 7 days. At 28 days of curing, the same mix ratio meets the minimum BS standard of 2.5N/mm2 .Keywords: buildings, cement, construction, hollow sand crate block, Nigeria
Procedia PDF Downloads 4074014 The Use of Palm Kernel Shell and Ash for Concrete Production
Authors: J. E. Oti, J. M. Kinuthia, R. Robinson, P. Davies
Abstract:
This work reports the potential of using Palm Kernel (PK) ash and shell as a partial substitute for Portland Cement (PC) and coarse aggregate in the development of mortar and concrete. PK ash and shell are agro-waste materials from palm oil mills, the disposal of PK ash and shell is an environmental problem of concern. The PK ash has pozzolanic properties that enables it as a partial replacement for cement and also plays an important role in the strength and durability of concrete, its use in concrete will alleviate the increasing challenges of scarcity and high cost of cement. In order to investigate the PC replacement potential of PK ash, three types of PK ash were produced at varying temperature (350-750 degrees) and they were used to replace up to 50% PC. The PK shell was used to replace up to 100% coarse aggregate in order to study its aggregate replacement potential. The testing programme included material characterisation, the determination of compressive strength, tensile splitting strength and chemical durability in aggressive sulfate-bearing exposure conditions. The 90 day compressive results showed a significant strength gain (up to 26.2 N/mm2). The Portland cement and conventional coarse aggregate has significantly higher influence in the strength gain compared to the equivalent PK ash and PK shell. The chemical durability results demonstrated that after a prolonged period of exposure, significant strength losses in all the concretes were observed. This phenomenon is explained, due to lower change in concrete morphology and inhibition of reaction species and the final disruption of the aggregate cement paste matrix.Keywords: sustainability, concrete, mortar, palm kernel shell, compressive strength, consistency
Procedia PDF Downloads 3994013 The Research of Hand-Grip Strength for Adults with Intellectual Disability
Authors: Haiu-Lan Chin, Yu-Fen Hsiao, Hua-Ying Chuang, Wei Lee
Abstract:
An adult with intellectual disability generally has insufficient physical activity which is an important factor leading to premature weakness. Studies in recent years on frailty syndrome have accumulated substantial data about indicators of human aging, including unintentional weight loss, self-reported exhaustion, weakness, slow walking speed, and low physical activity. Of these indicators, hand-grip strength can be seen as a predictor of mortality, disability, complications, and increased length of hospital stay. Hand-grip strength in fact provides a comprehensive overview of one’s vitality. The research is about the investigation on hand-grip strength of adults with intellectual disabilities in facilities, institutions and workshops. The participants are 197 male adults (M=39.09±12.85 years old), and 114 female ones (M=35.80±8.2 years old) so far. The aim of the study is to figure out the performance of their hand-grip strength, and initiate the setting of training on hand-grip strength in their daily life which will decrease the weakening on their physical condition. Test items include weight, bone density, basal metabolic rate (BMR), static body balance except hand-grip strength. Hand-grip strength was measured by a hand dynamometer and classified as normal group ( ≧ 30 kg for male and ≧ 20 kg for female) and weak group ( < 30 kg for male, < 20 kg for female)The analysis includes descriptive statistics, and the indicators of grip strength fo the adults with intellectual disability. Though the research is still ongoing and the participants are increasing, the data indicates: (1) The correlation between hand-grip strength and degree of the intellectual disability (p ≦. 001), basal metabolic rate (p ≦ .001), and static body balance (p ≦ .01) as well. Nevertheless, there is no significant correlation between grip strength and basal metabolic rate which had been having significant correlation with hand-grip strength. (2) The difference between male and female subjects in hand-grip strength is significant, the hand-grip strength of male subjects (25.70±12.81 Kg) is much higher than female ones (16.30±8.89 Kg). Compared to the female counterparts, male participants indicate greater individual differences. And the proportion of weakness between male and female subjects is also different. (3) The regression indicates the main factors related to grip strength performance include degree of the intellectual disability, height, static body balance, training and weight sequentially. (4) There is significant difference on both hand-grip and static body balance between participants in facilities and workshops. The study supports the truth about the sex and gender differences in health. Nevertheless, the average hand-grip strength of left hand is higher than right hand in both male and female subjects. Moreover, 71.3% of male subjects and 64.2% of female subjects have better performance in their left hand-grip which is distinctive features especially in low degree of the intellectual disability.Keywords: adult with intellectual disability, frailty syndrome, grip strength, physical condition
Procedia PDF Downloads 1794012 Improvement of Ride Comfort of Turning Electric Vehicle Using Optimal Speed Control
Authors: Yingyi Zhou, Tohru Kawabe
Abstract:
With the spread of EVs (electric Vehicles), the ride comfort has been gaining a lot of attention. The influence of the lateral acceleration is important for the improvement of ride comfort of EVs as well as the longitudinal acceleration, especially upon turning of the vehicle. Therefore, this paper proposes a practical optimal speed control method to greatly improve the ride comfort in the vehicle turning situation. For consturcting this method, effective criteria that can appropriately evaluate deterioration of ride comfort is derived. The method can reduce the influence of both the longitudinal and the lateral speed changes for providing a confortable ride. From several simulation results, we can see the fact that the method can prevent aggravation of the ride comfort by suppressing the influence of longitudinal speed change in the turning situation. Hence, the effectiveness of the method is recognized.Keywords: electric vehicle, speed control, ride comfort, optimal control theory, driving support system
Procedia PDF Downloads 2154011 Analysis Rotor Bearing System Dynamic Interaction with Bearing Supports
Abstract:
Frequently, in the design of machines, some of parameters that directly affect the rotor dynamics of the machines are not accurately known. In particular, bearing stiffness support is one such parameter. One of the most basic principles to grasp in rotor dynamics is the influence of the bearing stiffness on the critical speeds and mode shapes associated with a rotor-bearing system. Taking a rig shafting as an example, this paper studies the lateral vibration of the rotor with multi-degree-of-freedom by using Finite Element Method (FEM). The FEM model is created and the eigenvalues and eigenvectors are calculated and analyzed to find natural frequencies, critical speeds, mode shapes. Then critical speeds and mode shapes are analyzed by set bearing stiffness changes. The model permitted to identify the critical speeds and bearings that have an important influence on the vibration behavior.Keywords: lateral vibration, finite element method, rig shafting, critical speed
Procedia PDF Downloads 3404010 Development of a Finite Element Model of the Upper Cervical Spine to Evaluate the Atlantoaxial Fixation Techniques
Authors: Iman Zafarparandeh, Muzammil Mumtaz, Paniz Taherzadeh, Deniz Erbulut
Abstract:
The instability in the atlantoaxial joint may occur due to cervical surgery, congenital anomalies, and trauma. There are different types of fixation techniques proposed for restoring the stability and preventing harmful neurological deterioration. Application of the screw constructs has become a popular alternative to the older techniques for stabilizing the joint. The main difference between the various screw constructs is the type of the screw which can be lateral mass screw, pedicle screw, transarticular screw, and translaminar screw. The aim of this paper is to study the effect of three popular screw constructs fixation techniques on the biomechanics of the atlantoaxial joint using the finite element (FE) method. A three-dimensional FE model of the upper cervical spine including the skull, C1 and C2 vertebrae, and groups of the existing ligaments were developed. The accurate geometry of the model was obtained from the CT data of a 35-year old male. Three screw constructs were designed to compare; Magerl transarticular screw (TA-Screw), Goel-Harms lateral mass screw and pedicle screw (LM-Screw and Pedicle-Screw), and Wright lateral mass screw and translaminar screw (LM-Screw and TL-Screw). Pure moments were applied to the model in the three main planes; flexion (Flex), extension (Ext), axial rotation (AR) and lateral bending (LB). The range of motion (ROM) of C0-C1 and C1-C2 segments for the implanted FE models are compared to the intact FE model and the in vitro study of Panjabi (1988). The Magerl technique showed less effect on the ROM of C0-C1 than the other two techniques in sagittal plane. In lateral bending and axial rotation, the Goel-Harms and Wright techniques showed less effect on the ROM of C0-C1 than the Magerl technique. The Magerl technique has the highest fusion rate as 99% in all loading directions for the C1-C2 segment. The Wright technique has the lowest fusion rate in LB as 79%. The three techniques resulted in the same fusion rate in extension loading as 99%. The maximum stress for the Magerl technique is the lowest in all load direction compared to other two techniques. The maximum stress in all direction was 234 Mpa and occurred in flexion with the Wright technique. The maximum stress for the Goel-Harms and Wright techniques occurred in lateral mass screw. The ROM obtained from the FE results support this idea that the fusion rate of the Magerl is more than 99%. Moreover, the maximum stress occurred in each screw constructs proves the less failure possibility for the Magerl technique. Another advantage of the Magerl technique is the less number of components compared to other techniques using screw constructs. Despite the benefits of the Magerl technique, there are drawbacks to using this method such as reduction of the C1 and C2 before screw placement. Therefore, other fixation methods such as Goel-Harms and Wright techniques find the solution for the drawbacks of the Magerl technique by adding screws separately to C1 and C2. The FE model implanted with the Wright technique showed the highest maximum stress almost in all load direction.Keywords: cervical spine, finite element model, atlantoaxial, fixation technique
Procedia PDF Downloads 3844009 Properties of Triadic Concrete Containing Rice Husk Ash and Wood Waste Ash as Partial Cement Replacement
Authors: Abdul Rahman Mohd. Sam, Olukotun Nathaniel, Dunu Williams
Abstract:
Concrete is one of the most popular materials used in construction industry. However, one of the setbacks is that concrete can degrade with time upon exposure to an aggressive environment that leads to decrease in strength. Thus, research works and innovative ways are needed to enhance the strength and durability of concrete. This work tries to look into the potential use of rice husk ash (RHA) and wood waste ash (WWA) as cement replacement material. These are waste materials that may not only enhance the properties of concrete but also can serves as a viable method of disposal of waste for sustainability. In addition, a substantial replacement of Ordinary Portland Cement (OPC) with these pozzolans will mean reduction in CO₂ emissions and high energy requirement associated with the production of OPC. This study is aimed at assessing the properties of triadic concrete produced using RHA and WWA as a partial replacement of cement. The effects of partial replacement of OPC with 10% RHA and 5% WWA on compressive and tensile strength of concrete among other properties were investigated. Concrete was produced with nominal mix of 1:2:4 and 0.55 water-cement ratio, prepared, cured and subjected to compressive and tensile strength test at 3, 7, 14, 28 and 90days. The experimental data demonstrate that concrete containing RHA and WWA produced lighter weight in comparison with OPC sample. Results also show that combination of RHA and WWA help to prolong the initial and final setting time by about 10-30% compared to the control sample. Furthermore, compressive strength was increased by 15-30% with 10% RHA and 5% WWA replacement, respectively above the control, RHA and WWA samples. Tensile strength test at the ages of 3, 7, 14, 28 and 90 days reveals that a replacement of 15% RHA and 5% WWA produced samples with the highest tensile capacity compared to the control samples. Thus, it can be concluded that RHA and WWA can be used as partial cement replacement materials in concrete.Keywords: concrete, rice husk ash, wood waste ash, ordinary Portland cement, compressive strength, tensile strength
Procedia PDF Downloads 2604008 Influence of Scrap Tyre Steel Fiber on Mechanical Properties of High Performance Concrete
Authors: Isyaka Abdulkadir, Egbe Ngu-Ntui Ogork
Abstract:
This research aims to investigate the use of Scrap Tyre Steel Fibers (STSF) for the production of fiber reinforced high performance concrete. The Scrap Tyre Steel Fibers (STSF) were obtained from dealers that extracted the fibers by burning the scrap tyres and were characterized. The effect of STSF was investigated on grade 50 concrete of 1:1.28:1.92 with water cement ratio of 0.39 at additions of STSF of 0, 0.5, 1.0, 1.5, 2.0 and 2.5% by volume of concrete. The fresh concrete was tested for slump while the hardened concrete was tested for compressive and splitting tensile strengths, respectively at curing ages of 3, 7, 28 and 56 days in accordance with standard procedure. The results indicate that slump decreased with increase in STSF, while compressive and splitting tensile strengths increased with increase in STSF up to 1.5% and reduction in strength with increase in STSF above 1.5%. 1.5% STSF was considered as the optimum dosage with a 28 days increase in compressive strength and splitting tensile strength of 12.3% and 43.8% respectively, of control.Keywords: compressive strength, high performance concrete, scrap tyre steel fiber, splitting tensile strength
Procedia PDF Downloads 2174007 Surgical Prep-Related Burns in Laterally Positioned Hip Procedures
Authors: B. Kenny, M. Dixon, A. Boshell
Abstract:
The use of alcoholic surgical prep was recently introduced into the Royal Newcastle Center for elective procedures. In the past 3 months there have been a significant number of burns believed to be related to ‘pooling’ of this surgical prep in patients undergoing procedures where they are placed in the lateral position with hip bolsters. The aim of the audit was to determine the reason for the burns, analyze what pre-existing factors may contribute to the development of the burns and what can be changed to prevent further burns occurring. All patients undergoing a procedure performed on the hip who were placed in the lateral position with sacral and anterior, superior iliac spine (ASIS) support with ‘bolsters’ were included in the audit. Patients who developed a ‘burn’ were recorded, details of the surgery, demographics, surgical prep used and length of surgery were obtained as well as photographs taken to document the burn. Measures were then taken to prevent further burns and the efficacy was documented. Overall 14 patients developed burns over the ipsilateral ASIS. Of these, 13 were Total Hip Arthroplasty (THA) and 1 was a removal of femoral nail. All patients had Chlorhexidine 0.5% in Alcohol 70% Tinted Red surgical preparation or Betadine Alcoholic Skin Prep (70% etoh). Patients were set up in the standard lateral decubitus position with sacral and bilateral ASIS bolsters with a valband covering. 86% of patients were found to have pre-existing hypersensitivities to various substances. There is very little literature besides a few case reports on surgical prep-related burns. The case reports that do exist are related to the use of tourniquet-related burns and there is no mention in the literature examining ‘bolster’ related burns. The burns are hypothesized to be caused by pooling of the alcoholic solution which is amplified by the use of Valband.Keywords: arthroplasty, chemical burns, wounds, rehabilitation
Procedia PDF Downloads 3004006 Undrained Shear Strength and Anisotropic Yield Surface of Diatomaceous Mudstone
Authors: Najibullah Arsalan, Masaru Akaishi, Motohiro Sugiyama
Abstract:
When constructing a structure on soft rock, adequate research and study are required concerning the shear behavior in the over-consolidation region because soft rock is considered to be in a heavily over-consolidated state. In many of the existing studies concerning the strength of soft rock, triaxial compression tests were conducted using isotropically consolidated samples. In this study, the strength of diatomaceous soft rock anisotropically consolidated under a designated consolidation pressure is examined in undrained triaxial compression tests, and studies are made of the peak and residual strengths of the sample in the over-consolidated state in the initial yield surface and the anisotropic yield surface.Keywords: diatomaceouse mudstone, shear strength, yield surface, triaxial compression test
Procedia PDF Downloads 4304005 Effect of Glass Powder and GGBS on Strength of Fly Ash Based Geopolymer Concrete
Authors: I. Ramesha Mithanthaya, N. Bhavanishankar Rao
Abstract:
In this study, the effect of glass powder (GP) and ground granulated blast furnace slag (GGBS) on the compressive strength of Fly ash based geopolymer concrete has been investigated. The mass ratio of fine aggregate (fA) to coarse aggregate (CA) was maintained constant. NAOH flakes dissolved in water was used as activating liquid and mixed with fly ash (FA) to produce geopolymer paste or cementing material. This paste was added to mixture of CA and fA to obtain geopolymer concrete. Cube samples were prepared from this concrete. The ranges of investigation parameters include GP/FA from 0% to 20%, and GGBS/ FA from 0% to 20% with constant amount of GP. All the samples were air cured inside laboratory under room temperature. Compressive strength of cube samples after 7 days and 28 days curing were determined. The test results are presented and discussed. Based on the results of limited tests a suitable composition of FA, GP and GGBS for constant quantity of CA and fA has been obtained to produce geopolymer concrete of M32. It is found that geopolymer concrete is 14% cheaper than concrete of same strength using OPC. The strength gain in the case of geo-polymer concrete is rather slow compared to that of Portland cement concrete. Tensile strength of this concrete was also determined by conducting flexure test on beam prepared using this concrete. During curing, up to 7days, greyish-white powder used to come out from all the surfaces of sample and it was found to be a mixture of Carbonates and Sulphides of Na, Mg and Fe. Detailed investigation is necessary to arrive at an optimum mixture composition for producing Geo-polymer concrete of required strength. Effect of greyish-white powder on the strength and durability of the concrete is to be studied.Keywords: geopolymer, industrial waste, green material, cost effective material, eco-friendly material
Procedia PDF Downloads 545