3 Development of Mechanical Properties of Self Compacting Concrete Contain Rice Husk Ash

Authors: M. A. Ahmadi, O. Alidoust, I. Sadrinejad, M. Nayeri

Abstract:

Self-compacting concrete (SCC), a new kind of high performance concrete (HPC) have been first developed in Japan in 1986. The development of SCC has made casting of dense reinforcement and mass concrete convenient, has minimized noise. Fresh self-compacting concrete (SCC) flows into formwork and around obstructions under its own weight to fill it completely and self-compact (without any need for vibration), without any segregation and blocking. The elimination of the need for compaction leads to better quality concrete and substantial improvement of working conditions. SCC mixes generally have a much higher content of fine fillers, including cement, and produce excessively high compressive strength concrete, which restricts its field of application to special concrete only. To use SCC mixes in general concrete construction practice, requires low cost materials to make inexpensive concrete. Rice husk ash (RHA) has been used as a highly reactive pozzolanic material to improve the microstructure of the interfacial transition zone (ITZ) between the cement paste and the aggregate in self compacting concrete. Mechanical experiments of RHA blended Portland cement concretes revealed that in addition to the pozzolanic reactivity of RHA (chemical aspect), the particle grading (physical aspect) of cement and RHA mixtures also exerted significant influences on the blending efficiency. The scope of this research was to determine the usefulness of Rice husk ash (RHA) in the development of economical self compacting concrete (SCC). The cost of materials will be decreased by reducing the cement content by using waste material like rice husk ash instead of. This paper presents a study on the development of Mechanical properties up to 180 days of self compacting and ordinary concretes with rice-husk ash (RHA), from a rice paddy milling industry in Rasht (Iran). Two different replacement percentages of cement by RHA, 10%, and 20%, and two different water/cementicious material ratios (0.40 and 0.35), were used for both of self compacting and normal concrete specimens. The results are compared with those of the self compacting concrete without RHA, with compressive, flexural strength and modulus of elasticity. It is concluded that RHA provides a positive effect on the Mechanical properties at age after 60 days. Base of the result self compacting concrete specimens have higher value than normal concrete specimens in all test except modulus of elasticity. Also specimens with 20% replacement of cement by RHA have the best performance.

Keywords: Self compacting concrete (SCC), Rice husk ash(RHA), Mechanical properties.

Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 3630
2 Formulation and in vitro Evaluation of Ondansetron Hydrochloride Matrix Transdermal Systems Using Ethyl Cellulose/Polyvinyl Pyrrolidone Polymer Blends

Authors: Rajan Rajabalaya, Li-Qun Tor, Sheba David

Abstract:

Transdermal delivery of ondansetron hydrochloride (OdHCl) can prevent the problems encountered with oral ondansetron. In previously conducted studies, effect of amount of polyvinyl pyrrolidone, permeation enhancer and casting solvent on the physicochemical properties on OdHCl were investigated. It is feasible to develop ondansetron transdermal patch by using ethyl cellulose and polyvinyl pyrrolidone with dibutyl pthalate as plasticizer, however, the desired flux is not achieved. The primary aim of this study is to use dimethyl succinate (DMS) and propylene glycol that are not incorporated in previous studies to determine their effect on the physicochemical properties of an OdHCl transdermal patch using ethyl cellulose and polyvinyl pyrrolidone. This study also investigates the effect of permeation enhancer (eugenol and phosphatidylcholine) on the release of OdHCl. The results showed that propylene glycol is a more suitable plasticizer compared to DMS in the fabrication of OdHCl transdermal patch using ethyl cellulose and polyvinyl pyrrolidone as polymers. Propylene glycol containing patch has optimum drug content, thickness, moisture content and water absorption, tensile strength, and a better release profile than DMS. Eugenol and phosphatidylcholine can increase release of OdHCl from the patches. From the physicochemical result and permeation profile, a combination of 350mg of ethyl cellulose, 150mg polyvinyl pyrrolidone, 3% of total polymer weight of eugenol, and 40% of total polymer weight of propylene glycol is the most suitable formulation to develop an OdHCl patch. OdHCl release did not increase with increasing the percentage of plasticiser. DMS 4, PG 4, DMS 9, PG 9, DMS 14, and PG 14 gave better release profiles where using 300mg: 0mg, 300mg: 100mg, and 350mg: 150mg of EC: PVP. Thus, 40% of PG or DMS appeared to be the optimum amount of plasticiser when the above combination where EC: PVP was used. It was concluded from the study that a patch formulation containing 350mg EC, 150mg PVP, 40% PG and 3% eugenol is the best transdermal matrix patch compositions for the uniform and continuous release/permeation of OdHCl over an extended period. This patch design can be used for further pharmacokinetic and pharmacodynamic studies in suitable animal models.

Keywords: Ondansetron hydrochloride, dimethyl succinate, eugenol.

Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2418
1 Influence of Crystal Orientation on Electromechanical Behaviors of Relaxor Ferroelectric P(VDF-TrFE-CTFE) Terpolymer

Authors: Qing Liu, Jean-Fabien Capsal, Claude Richard

Abstract:

In this current contribution, authors are dedicated to investigate influence of the crystal lamellae orientation on electromechanical behaviors of relaxor ferroelectric Poly (vinylidene fluoride –trifluoroethylene -chlorotrifluoroethylene) (P(VDF-TrFE-CTFE)) films by control of polymer microstructure, aiming to picture the full map of structure-property relationship. In order to define their crystal orientation films, terpolymer films were fabricated by solution-casting, stretching and hot-pressing process. Differential scanning calorimetry, impedance analyzer, and tensile strength techniques were employed to characterize crystallographic parameters, dielectric permittivity, and elastic Young’s modulus respectively. In addition, large electrical induced out-of-plane electrostrictive strain was obtained by cantilever beam mode. Consequently, as-casted pristine films exhibited surprisingly high electrostrictive strain 0.1774% due to considerably small value of elastic Young’s modulus although relatively low dielectric permittivity. Such reasons contributed to large mechanical elastic energy density. Instead, due to 2 folds increase of elastic Young’s modulus and less than 50% augmentation of dielectric constant, fullycrystallized film showed weak electrostrictive behavior and mechanical energy density as well. And subjected to mechanical stretching process, Film C exhibited stronger dielectric constant and out-performed electrostrictive strain over Film B because edge-on crystal lamellae orientation induced by uniaxially mechanical stretch. Hot-press films were compared in term of cooling rate. Rather large electrostrictive strain of 0.2788% for hot-pressed Film D in quenching process was observed although its dielectric permittivity equivalent to that of pristine as-casted Film A, showing highest mechanical elastic energy density value of 359.5 J/m3. In hot-press cooling process, dielectric permittivity of Film E saw values at 48.8 concomitant with ca.100% increase of Young’s modulus. Films with intermediate mechanical energy density were obtained.

Keywords: Crystal orientation, electrostrictive strain, mechanical energy density, permittivity, relaxor ferroelectric.

Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 1624