2 Mineral Chemistry of Extraordinary Ilmenite from the Gabbroic Rocks of Abu Ghalaga Area, Eastern Desert, Egypt: Evidence to Metamorphic Modification

Authors: Yaser Maher Abdel Aziz Hawa

Abstract:

An assemblage of Mn-bearing ilmenite, titanomagnetite (4-17 vol.%) and subordinate chalcopyrite, pyrrhptite and pyrite is present as dissiminations in gabbroic rocks of Abu Ghalaga area, Eastern Desert, Egypt. The neoproterozoic gabbroic rocks encompasses these opaques are emplaced during oceanic island arc stage which represents the Nubian shield of Egypt. However, some textural features of these opaques suggest a relict igneous. The high Mn (up to 5.8 MnO%, 1282% MnTiO3) and very low Mg contents (0.21 MgO%, 0.82 MgTiO3) are dissimilar to those of any igneous ilmenite of tholeiitic rocks. Most of these ilmenites are associated mostly with metamorphic hornblende. Hornblende thermometry estimate crystallization of about 560°C. the present study suggests that the ilmenite under consideration has been greatly metamorphically modified, having lost Mg and gained Mn by diffusion.

Keywords: titanomagnetite, Ghalaga, ilmenite, chemistry

Procedia PDF Downloads 327
1 Hydrometallurgical Treatment of Abu Ghalaga Ilmenite Ore

Authors: I. A. Ibrahim, T. A. Elbarbary, N. Abdelaty, A. T. Kandil, H. K. Farhan

Abstract:

The present work aims to study the leaching of Abu Ghalaga ilmenite ore by hydrochloric acid and simultaneous reduction by iron powder method to dissolve its titanium and iron contents. Iron content in the produced liquor is separated by solvent extraction using TBP as a solvent. All parameters affecting the efficiency of the dissolution process were separately studied including the acid concentration, solid/liquid ratio which controls the ilmenite/acid molar ratio, temperature, time and grain size. The optimum conditions at which maximum leaching occur are 30% HCl acid with a solid/liquid ratio of 1/30 at 80 °C for 4 h using ore ground to -350 mesh size. At the same time, all parameters affecting on solvent extraction and stripping of iron content from the produced liquor were studied. Results show that the best extraction is at solvent/solution 1/1 by shaking at 240 RPM for 45 minutes at 30 °C whereas best striping of iron at H₂O/solvent 2/1.

Keywords: ilmenite ore, leaching, titanium solvent extraction, Abu Ghalaga ilmenite ore