3 Electrochemical Studies of the Inhibition Effect of 2-Dimethylamine on the Corrosion of Austenitic Stainless Steel Type 304 in Dilute Hydrochloric Acid

Authors: Roland Tolulope Loto, Cleophas Akintoye Loto, Abimbola Patricia Popoola

Abstract:

The inhibiting action of 2-dimethylamine on the electrochemical behaviour of austenitic stainless steel (type 304) in dilute hydrochloric was evaluated through weight-loss method, open circuit potential measurement and potentiodynamic polarization tests at specific concentrations of the organic compound. Results obtained reveal that the compound performed effectively giving a maximum inhibition efficiency of 79% at 12.5% concentration from weight loss analysis and 80.9% at 12.5% concentration from polarization tests. The average corrosion potential of -321 mV was obtained the same concentration from other tests which is well within passivation potentials on the steel thus, providing good protection against corrosion in the acid solutions. 2-dimethylamine acted through physiochemical interaction at the steel/solution interface from thermodynamic calculations and obeyed the Langmuir adsorption isotherm. The values of the inhibition efficiency determined from the three methods are in reasonably good agreement. Polarization studies showed that the compounds behaved as cathodic type inhibitor.

Keywords: corrosion, 2-dimethylamine, inhibition, adsorption, hydrochloric acid, steel

Procedia PDF Downloads 320
2 Corrosion Inhibition of Mild Steel by Calcium Gluconate in Magnesium Chloride Solution

Authors: Olaitan Akanji, Cleophas Loto, Patricia Popoola, Andrei Kolesnikov

Abstract:

Studies involving performance of corrosion inhibitors had been identified as one of the critical research needs for improving the durability of mild steel used in various industrial applications. This paper investigates the inhibiting effect of calcium gluconate against the corrosion of mild steel in 2.5M magnesium chloride using weight loss method and linear polarization technique, calculated corrosion rates from the obtained weight loss data, potentiodynamic polarization measurements are in good agreement. Results revealed calcium gluconate has strong inhibitory effects with inhibitor efficiency increasing with increase in inhibitor concentration at ambient temperature, the efficiency of the inhibitor increased in the following order of concentrations 2%g/vol,1.5%g/vol,1%g/vol,0.5%g/vol. Further results obtained from potentiodynamics experiments had good correlation with those of the gravimetric methods, the adsorption of the inhibitor on the mild steel surface from the chloride has been found to obey Langmuir, Frumkin and Freudlich adsorption isotherm. Scanning electron microscopy (SEM) observation confirmed the existence of an absorbed protective film on the metal surface.

Keywords: calcium gluconate, corrosion, magnesium chloride, mild steel

Procedia PDF Downloads 349
1 Synchrotron Based Techniques for the Characterization of Chemical Vapour Deposition Overgrowth Diamond Layers on High Pressure, High Temperature Substrates

Authors: T. N. Tran Thi, J. Morse, C. Detlefs, P. K. Cook, C. Yıldırım, A. C. Jakobsen, T. Zhou, J. Hartwig, V. Zurbig, D. Caliste, B. Fernandez, D. Eon, O. Loto, M. L. Hicks, A. Pakpour-Tabrizi, J. Baruchel

Abstract:

The ability to grow boron-doped diamond epilayers of high crystalline quality is a prerequisite for the fabrication of diamond power electronic devices, in particular high voltage diodes and metal-oxide-semiconductor (MOS) transistors. Boron and intrinsic diamond layers are homoepitaxially overgrown by microwave assisted chemical vapour deposition (MWCVD) on single crystal high pressure, high temperature (HPHT) grown bulk diamond substrates. Various epilayer thicknesses were grown, with dopant concentrations ranging from 1021 atom/cm³ at nanometer thickness in the case of 'delta doping', up 1016 atom/cm³ and 50µm thickness or high electric field drift regions. The crystalline quality of these overgrown layers as regards defects, strain, distortion… is critical for the device performance through its relation to the final electrical properties (Hall mobility, breakdown voltage...). In addition to the optimization of the epilayer growth conditions in the MWCVD reactor, other important questions related to the crystalline quality of the overgrown layer(s) are: 1) what is the dependence on the bulk quality and surface preparation methods of the HPHT diamond substrate? 2) how do defects already present in the substrate crystal propagate into the overgrown layer; 3) what types of new defects are created during overgrowth, what are their growth mechanisms, and how can these defects be avoided? 4) how can we relate in a quantitative manner parameters related to the measured crystalline quality of the boron doped layer to the electronic properties of final processed devices? We describe synchrotron-based techniques developed to address these questions. These techniques allow the visualization of local defects and crystal distortion which complements the data obtained by other well-established analysis methods such as AFM, SIMS, Hall conductivity…. We have used Grazing Incidence X-ray Diffraction (GIXRD) at the ID01 beamline of the ESRF to study lattice parameters and damage (strain, tilt and mosaic spread) both in diamond substrate near surface layers and in thick (10–50 µm) overgrown boron doped diamond epi-layers. Micro- and nano-section topography have been carried out at both the BM05 and ID06-ESRF) beamlines using rocking curve imaging techniques to study defects which have propagated from the substrate into the overgrown layer(s) and their influence on final electronic device performance. These studies were performed using various commercially sourced HPHT grown diamond substrates, with the MWCVD overgrowth carried out at the Fraunhofer IAF-Germany. The synchrotron results are in good agreement with low-temperature (5°K) cathodoluminescence spectroscopy carried out on the grown samples using an Inspect F5O FESEM fitted with an IHR spectrometer.

Keywords: synchrotron X-ray diffaction, crystalline quality, defects, diamond overgrowth, rocking curve imaging

Procedia PDF Downloads 261