Comparison Ageing Deterioration of Silicone Rubber Outdoor Polymer Insulators in Artificial Accelerated Salt Fog Ageing Test

Authors: S.Thong-Om, W. Payakcho, J. Grasaesom, A. Oonsivilai, B. Marungsri

Abstract:

This paper presents the experimental results of silicone rubber outdoor polymer insulators in salt fog ageing test based on IEC 61109. Specimens made ofHTV silicone rubber with ATH content having three different configurations, straight shedsalternated sheds, and incline and alternate sheds, were tested continuously 1000 hrs.in artificial salt fog chamber. Contamination level, reduction of hydrophobicity and hardness measurement were used as physical damaged inspection techniques to evaluate degree of surface deterioration. In addition, chemical changing of tested specimen surface was evaluated by ATR-FTIRto confirm physical damaged inspection. After 1000 hrs.of salt fog test, differences in degree of surface deterioration were observed on all tested specimens. Physical damaged inspection and chemical analysis results confirmed the experimental results as well.

Keywords: Ageing deterioration, Silicone rubber, Polymer Insulator, Salt fog ageing test.

Digital Object Identifier (DOI): doi.org/10.5281/zenodo.1063190

Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2543

References:


[1] Han-Goo Cho, Se-Won Han and Un-Yong Lee, "Multi-Aging Test Technology for Estimating Long Time Performance of Polymer Insulators”, IEEE International Symposium on Electrical Insulation, Boston, MA USA, April 2006, pp. 232-2236.
[2] A. E. Vlastos and S. M. Gubanski, " Surface Structural Changes of Naturally Aged Silicone and EPDM Composite Insulators”, IEEE Transaction on Power Delivery, Vol. 6, No. 2, pp. 888-900, April 1991.
[3] B. Marungsri, H. Shinokubo, R. Matsuoka and S. Kumagai, "Effect of Surface Treatment of Fillers on Deterioration of Silicone Rubber Housing Materials in Salt Fog Ageing Test”, International Symposium on Electrical Insulating Materials, June 5-9, 2005, pp. 556-559.
[4] R. Sundararajan, C. Olave, E Romero and B. Trepanier, "Modified IEC 5000-h Multistress Aging of 28-kV Thermoplastic Elastomeric Insulators”, IEEE Transactions on Power Delivery, Vol. 22, No. 2, April 2007, pp. 1079-1085.
[5] B. Marungsri, H.Shinokubo, and R. Matsuoka, "Effect of Specimen Configuration on Deterioration of Silicone Rubber for Polymer Insulators in Salt Fog Ageing Test”, IEEE Transactions on Dielectrics and Electrical Insulation, Vol. 13, No. 1, 2006, pp. 129-138.
[6] S. H. Kim, E. A. Cherney, R. Hackam and K. G. Ratherford, "Chemical Changes at the Surface of RTV Silicone Rubber Coatings on Insulators during Dry Band Arcing”, IEEE Transactions on Dielectrics and Electrical Insulation, Vol. 1, 1994, pp. 106-123.
[7] Y. Koshino, I. Umeda and M. Ishiwari, "Deterioration of Silicone Rubber for Polymer Insulators by Corona Discharge and Effect of Fillers”, IEEE Conf. Electrical Insulation Dielectrics and Phenomena, 1998, pp. 72-79.
[8] S. Thong-om, W. Payakcho, J. Grasaesom and B. Marungsri, "Study of Ageing Deterioration of Silicone Rubber Housing Material for Outdoor Polymer Insulators”, World Academy of Science, Engineering and Technology, Issue 80, August 2011, pp. 533-539.
[9] J. Grasaesom, S. Thong-om, W. Payakcho and B. Marungsri, "Ageing Deterioration of Silicone Rubber Polymer Insulator under Salt Water Dip Wheel Test”, World Academy of Science, Engineering and Technology, Issue 80, August 2011, pp. 211-217.
[10] W. Payakcho, J. Grasaesom, S. Thong-om and B. Marungsri, "Artificial Accelerated Ageing Test of Silicone Rubber Housing Material for Lightning Arrester”, World Academy of Science, Engineering and Technology, Issue 80, August 2011, pp. 650-655.
[11] IEC 61109, "Composite insulators for a.c. overhead lines with a nominal voltage greater than 1000 V - Definitions, test methods and acceptance criteria”, 1992.
[12] S. Kumagai and N. Yoshimura, "Leakage Current Characterization for Estimating the Conditions of Ceramic and Polymeric InsulatingSurface”,IEEE Transactions on Dielectrics and Electrical Insulation, Vol. 11, 2004, pp. 681-690.
[13] IEC 60507, "Artificial pollution tests on high-voltage insulators to be used on AC systems”, Ed. 2 b, 1991.
[14] STRI Guide, "Hydrophobicity Classification Guide", 92/1, 1992.
[15] S. H. Kim, E. A. Cherney, R. Hackam and K. G. Ratherford, "Chemical Changes at the Surface of RTV Silicone Rubber Coatings on Insulators during Dry Band Arcing”, IEEE Transactions on Dielectrics and Electrical Insulation, Vol. 1, No. 1, pp. 106-123, 1994
[16] ISO 868, "Plastics and ebonite – Determination of indentation hardness by means of a durometer (Shore hardness)”.