Search results for: S. Teramoto
2 Effect of Ground Subsidence on Load Sharing and Settlement of Raft and Piled Raft Foundations
Authors: T.V. Tran, S. Teramoto, M. Kimura, T. Boonyatee, Le Ba Vinh
Abstract:
In this paper, two centrifugal model tests (case 1: raft foundation, case 2: 2x2 piled raft foundation) were conducted in order to evaluate the effect of ground subsidence on load sharing among piles and raft and settlement of raft and piled raft foundations. For each case, two conditions consisting of undrained (without groundwater pumping) and drained (with groundwater pumping) conditions were considered. Vertical loads were applied to the models after the foundations were completely consolidated by selfweight at 50g. The results show that load sharing by the piles in piled raft foundation (piled load share) for drained condition decreases faster than that for undrained condition. Settlement of both raft and piled raft foundations for drained condition increases more quickly than that for undrained condition. In addition, the settlement of raft foundation increases more largely than the settlement of piled raft foundation for drained condition.Keywords: Ground subsidence, Piled raft, Load sharing, Centrifugal model test.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 29261 Effect of Addition Rate of Expansive Additive on Autogenous Shrinkage and Delayed Expansion of Ultra-High Strength Mortar
Authors: Yulu Zhang, Atushi Teramoto, Taka-Aki Ohkubo
Abstract:
In this study, the effect of expansive additives on autogenous shrinkage and delayed expansion of ultra-high strength mortar was explored. The specimens made for the study were composed of ultra-high strength mortar, which was mixed with ettringite-lime composite type expansive additive. Two series of experiments were conducted with the specimens. The experimental results confirmed that the autogenous shrinkage of specimens was effectively decreased by increasing the proportion of the expansive additive. On the other hand, for the specimens, which had 7% expansive additive, and were cured for seven days at a constant temperature of 20°C, and then cured for a long time in either in an underwater, moist (Relative humidity: 100%) or dry air (Relative humidity: 60%) environment, excessively large expansion strain occurred. Specifically, typical turtle shell-like swelling expansion cracks were confirmed in the specimens that underwent long-term curing in an underwater and moist environment. According to the result of hydration analysis, the formation of expansive substances, calcium hydroxide and alumina, ferric oxide, tri-sulfate contribute to the occurrence of delayed expansion.
Keywords: Ultra-high strength mortar, expansive additive, autogenous shrinkage, delayed expansion.
Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 757