Computational Study and Wear Prediction of Steam Turbine Blade with Titanium-Nitride Coating Deposited by Physical Vapor Deposition Method
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 32807
Computational Study and Wear Prediction of Steam Turbine Blade with Titanium-Nitride Coating Deposited by Physical Vapor Deposition Method

Authors: Karuna Tuchinda, Sasithon Bland

Abstract:

This work investigates the wear of a steam turbine blade coated with titanium nitride (TiN), and compares to the wear of uncoated blades. The coating is deposited on by physical vapor deposition (PVD) method. The working conditions of the blade were simulated and surface temperature and pressure values as well as flow velocity and flow direction were obtained. This data was used in the finite element wear model developed here in order to predict the wear of the blade. The wear mechanisms considered are erosive wear due to particle impingement and fluid jet, and fatigue wear due to repeated impingement of particles and fluid jet. Results show that the life of the TiN-coated blade is approximately 1.76 times longer than the life of the uncoated one.

Keywords: Physical vapour deposition, steam turbine blade, titanium-based coating, wear prediction.

Digital Object Identifier (DOI): doi.org/10.5281/zenodo.1337323

Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 3102

References:


[1] Wei-Ze Wang, Fu-Zhen Xuan, Kui-Long Zhu, Shan-Tung Tu, (2007), Failure analysis of the final stage blade in steam, Engineering Failure Analysis, Volume 14, Issue 4, Pages 632-641
[2] J Dehouve, P Nardin, M Zeghmati, (1999), Erosion study of final stage blading of low pressure steam turbines, Applied Surface Science, Volumes 144–145, Pages 238-243
[3] C.R.F. Azevedo, A. Sinátora, (2009), Erosion-fatigue of steam turbine blades, Engineering Failure Analysis, Volume 16, Issue 7, Pages 2290-2303
[4] B. Staniša, V. Ivušić, (1995) Erosion behaviour and mechanisms for steam turbine rotor blades, Wear, Volumes 186–187, Part 2, Pages 395-400
[5] Zdzislaw Mazur, Rafael Garcia-Illescas, Jorge Aguirre-Romano, Norberto Perez-Rodriguez, (2008), Steam turbine blade failure analysis, Engineering Failure Analysis, Volume 15, Issues 1–2, Pages 129-141
[6] Z. Mazur, R. Campos-Amezcua, G. Urquiza-Beltrán, A. Garcı́a-Gutiérrez, (2004), Numerical 3D simulation of the erosion due to solid particle impact in the main stop valve of a steam turbine, Applied Thermal Engineering, Volume 24, Issue 13, Pages 1877-1891
[7] B.S. Mann, VivekArya, (2003), HVOF coating and surface treatment for enhancing droplet erosion resistance of steam turbine blades, Wear, Volume 254, Issues 7–8, Pages 652-667
[8] B.S Mann, (1999), Solid-particle erosion and protective layers for steam turbine blading, Wear, Volume 224, Issue 1, Pages 8-12
[9] Hugh O. Pierson, (1992), 11 - CVD in Wear-, Erosion-, and Corrosion-Resistant Applications, Handbook of Chemical Vapor Deposition, Pages 347-385
[10] Subbiah Ramalingam, (1996), Emerging applications and new opportunities with PVD Arc sources, Handbook of Vacuum Arc Science and Technology, Pages 519-551
[11] ZhengRongShui, Bu Qian Wang, Alan V. Levy, (1990), Erosion of protective coatings, Surface and Coatings Technology, Volumes 43–44, Part 2, Pages 875-887
[12] John Stringer, (1998), Coatings in the electricity supply industry: past, present, and opportunities for the future, Surface and Coatings Technology, Volumes 108–109, Pages 1-9
[13] Y.I. Oka, H. Miyata, (2009), Erosion behaviour of ceramic bulk and coating materials caused by water droplet impingement, Wear, Volume 267, Issue 11, Pages 1804-1810
[14] P. C. Jindal, A. T. Santhanam, U. Schleinkofer, A. F., (1999), Shuster, Performance of PVD TiN, TiCN, and TiAlN coated cemented carbide tools in turning ,International Journal of Refractory Metals and Hard Materials, Volume 17, Issues 1-3, Pages 163-170
[15] J. D. Bressan, R. Hesse, E. M. Silva Jr., (2001), Abrasive wear behavior of high speed steel and hard metal coated with TiAlN and TiCN, Wear, Volume 250, Issues 1-12, Pages 561-568
[16] T. Polcar, T. Kubart, R. Novák, L. Kopecký, P. Široký , (2005), Comparison of tribologicalbehaviour of TiN, TiCN and CrN at elevated temperatures, Surface and Coatings Technology, Volume 193, Issues 1-3, Pages 192-199
[17] Tunvisut, K., O’Dowd, N.P. and Busso, E.P., (2001), Use of scaling functions to determine mechanical properties of thin coatings from microindentation tests, Int. J. Solids Struct. 38 (2) pp. 335–351.
[18] Tunvisut, K., Busso, E.P., O'Dowd, N.P. and Brantner, H.P., (2002). Determination of the mechanical properties of metallic thin films and substrates from indentation tests. Philosophical Magazine A 82,, pp. 2013–2023
[19] Tuchinda, K., (2011), Determination of stress-strain relationship of hard thin films on steel substrate from indentation tests – Industrial application., To be submitted to Surface & coatings Technologyfor publication.
[20] http://www.csm-instruments.com/en/Coating_thickness
[21] Archard, J.F. (1953). Contact and Rubbing of Flat Surface. J. Appl. Phis.Vol. 24, pp. 981–988.