Preparation and Cutting Performance of Boron-Doped Diamond Coating on Cemented Carbide Cutting Tools with High Cobalt Content
Commenced in January 2007
Frequency: Monthly
Edition: International
Paper Count: 33093
Preparation and Cutting Performance of Boron-Doped Diamond Coating on Cemented Carbide Cutting Tools with High Cobalt Content

Authors: Zhaozhi Liu, Feng Xu, Junhua Xu, Xiaolong Tang, Ying Liu, Dunwen Zuo

Abstract:

Chemical vapor deposition (CVD) diamond coated cutting tool has excellent cutting performance, it is the most ideal tool for the processing of nonferrous metals and alloys, composites, nonmetallic materials and other difficult-to-machine materials efficiently and accurately. Depositing CVD diamond coating on the cemented carbide with high cobalt content can improve its toughness and strength, therefore, it is very important to research on the preparation technology and cutting properties of CVD diamond coated cemented carbide cutting tool with high cobalt content. The preparation technology of boron-doped diamond (BDD) coating has been studied and the coated drills were prepared. BDD coating were deposited on the drills by using the optimized parameters and the SEM results show that there are no cracks or collapses in the coating. Cutting tests with the prepared drills against the silumin and aluminum base printed circuit board (PCB) have been studied. The results show that the wear amount of the coated drill is small and the machined surface has a better precision. The coating does not come off during the test, which shows good adhesion and cutting performance of the drill.

Keywords: Cemented carbide with high cobalt content, CVD boron-doped diamond, cutting test, drill.

Digital Object Identifier (DOI): doi.org/10.5281/zenodo.1100248

Procedia APA BibTeX Chicago EndNote Harvard JSON MLA RIS XML ISO 690 PDF Downloads 2720

References:


[1] Gomez H, Durham D, Xiao X, et al, “Adhesion analysis and dry machining performance of CVD diamond coatings deposited on surface modified WC–Co turning inserts,” J. Mater. Process. Technol., vol. 212, no. 2, pp. 523–533, Feb. 2012.
[2] Xu F, Xu J H, Yuen M F, et al, “Adhesion improvement of diamond coatings on cemented carbide with high cobalt content using PVD interlayer,” Diamond Relat. Mater., vol. 34,pp. 70–75, Apr. 2013.
[3] Roy P, Sarangi S K, Ghosh A , Chattopadhyay A K, “Machinability study of pure aluminum and Al–12% Si alloys against uncoated and coated carbide inserts,” Int. J. Refract. Met. Hard Mater., vol. 27, no. 3, pp. 535–544, May. 2009.
[4] Sun F H, Zhang Z M, Chen M, Shen H S, “Improvement of adhesive strength and surface roughness of diamond films on Co-cemented tungsten carbide tools,” Diamond Relat. Mater., vol. 12, no. 3-7, pp. 711–718, Mar-Jul. 2003.
[5] Zhang D, Shen B, Sun F, “Study on tribological behavior and cutting performance of CVD diamond and DLC films on Co-cemented tungsten carbide substrates,” Appl. Surf. Sci., vol. 256, no. 8, pp. 2479–2489, Feb. 2010.
[6] Sarangi S K, Chattopadhyay A, Chattopadhyay A K, “Effect of pretreatment methods and chamber pressure on morphology, quality and adhesion of HFCVD diamond coating on cemented carbide inserts,” Appl. Surf. Sci., vol. 254, no. 13, pp. 3721–3733, Apr. 2008.
[7] Y. Jamal, Sheikh-Ahmad, Machining of Polymer Composites. New York: Springer-Verlag, 2009, ch. 4.
[8] Tang Y, Li Y S, Yang Q, et al. “Deposition and characterization of diamond coatings on WC-Co cutting tools with W/Al interlayer,” Diamond Relat. Mater., vol. 19, pp 496-499, May. 2010.
[9] Juang Y, Nurhayati E, Huang C, Pan J, Huang S, “A hybrid electrochemical advanced oxidation/microfiltration system using BDD/Ti anode for acid yellow 36 dye wastewater treatment,” Sep. Purif. Technol., vol. 120, no. 13, pp. 289–295, Dec. 2013.
[10] Zhou Y L, Tian R H, Zhi J F, “Amperometric biosensor based on tyrosinase immobilized on a boron-doped diamond electrode,” Biosens. Bioelectron., vol. 22, no. 6, pp. 822–828, Jan. 2007.
[11] Haymond S, Babcock G T, Swain G M, “Direct electrochemistry of cytochrome c at nanocrystalline boron-doped diamond,” J. Am. Chem. Soc., vol. 124, no. 36, pp. 10634–10635, Aug. 2002.
[12] Haubner R, Bohr S, Lux B, “Comparison of P, N and B additions during CVD diamond deposition,” Diamond Relat. Mater., vol. 8, no. 2-5, pp. 171–178, Mar. 1999.
[13] Haubner R, “Comparison of sulfur, boron, nitrogen and phosphorus additions during low-pressure diamond deposition,” Diamond Relat. Mater., vol. 14, no. 3-7, pp. 355–363, Mar-Jul. 1999.
[14] Kalss W, Bohr S, Haubner R, et al, “Influence of boron on diamond growth on WC-Co hardmetals,” Int. J. Refract. Met. Hard Mater., vol. 14, no. 1-3, pp. 137–144, Mar. 1996.
[15] Zhang J G, Wang X C, Shen B, et al. “Effect of boron and silicon doping on improving the cutting performance of CVD diamond coated cutting tools in machining CFRP,” Int. J. Refract. Met. Hard Mater., vol. 41, pp. 285-292, Apr. 2013.
[16] Azevedo A F, Mendes de Barros R C, Serrano S H P, Ferreira N G, “SEM and Raman analysis of boron-doped diamond coating on spherical textured substrates,” Surf. Coat. Technol., vol. 200, no. 20-21, pp. 5973–5977, May. 2006.
[17] Zhao X, Li Y, “Tool Wear Pattern and Mechanics in High Speed Cutting Microwave Printed Circuit Board,” Key Eng. Mater., vol. 426-427,pp. 515–519, May. 2010.
[18] W.M. Zhang, M.H. Hao, Y. Y. Shen, “Ceramic composite materials containing carbon nanotube-infused fiber materials and methods for production,” Mechatronics, vol. 4, pp. 12–15, Mar. 2004.
[19] Ager III J W, Walukiewicz W, McCluskey M, et al, “Fano interference of the Raman phonon in heavily boron-doped diamond films grown by chemical vapor deposition,” Appl. Phys. Lett., vol. 66, no. 5, pp. 616–618, Nov. 1994.
[20] May P W, Ludlow W J, Hannaway M, et al, “Raman and conductivity studies of boron-doped microcrystalline diamond, facetted nanocrystalline diamond and cauliflower diamond films,” Diamond Relat. Mater., vol. 17, no. 2, pp. 105–117, Feb. 2008.