	  title     = {Recycling of Tungsten Alloy Swarf},
	  author    = {A. A. Alhazza},
	  country	= {},
	  institution	= {},
	  abstract     = {The recycling process of Tungsten alloy (Swarf) by
oxidation reduction technique have been investigated. The reduced
powder was pressed under a pressure 20Kg/cm2 and sintered at
1150°C in dry hydrogen atmosphere. The particle size of the recycled
alloy powder was 1-3 μm and the shape was regular at a reduction
temperature 800°C. The chemical composition of the recycled alloy
is the same as the primary Swarf.},
	    journal   = {International Journal of Materials and Metallurgical Engineering},
	  volume    = {2},
	  number    = {9},
	  year      = {2008},
	  pages     = {231 - 234},
	  ee        = {https://publications.waset.org/pdf/1845},
	  url   	= {https://publications.waset.org/vol/21},
	  bibsource = {https://publications.waset.org/},
	  issn  	= {eISSN: 1307-6892},
	  publisher = {World Academy of Science, Engineering and Technology},
	  index 	= {Open Science Index 21, 2008},
	}