	%X This paper presents the experimental results on
ageing deterioration of silicone rubber outdoor polymer insulator
under salt water dip wheel test based on IEC 62217. In order to comparison effect of chemical contents, silicone rubber outdoor
polymer insulators having same configuration and leakage distant
from two manufactures were tested together continuously 30,000 test cycles. Many discharge activities were observed in during the test.
After 30,000 test cycles, in spite of same configuration, differences in
degree of surface aging were observed. Physical analysis such as
decreasing in hydrophobicity and increasing in hardness
measurement were measured on two-type tested specimen surface in order to confirm degree of surface ageing. Furthermore, chemical
analysis by ATR-FTIR to diagnose the chemical change of tested
specimen surface was conducted to confirm the physical analysis results.
	%P 1896 - 1903