	  author    = {A. A. Samat and  N. A. Abdullah and  M. A. M. Ishak and  N. Osman},
	  country	= {},
	  institution	= {},
	  abstract     = {Powder of La0.6Sr0.4CoO3-α (LSCO) was synthesized
by a combined citrate-EDTA method. The as-synthesized LSCO
powder was calcined, respectively at temperatures of 800, 900 and
1000 °C with different heating/cooling rates which are 2, 5, 10 and
15 °C min-1. The effects of heat treatments on the phase formation of
perovskite phase of LSCO were investigated by powder X-ray
diffraction (XRD). The XRD patterns revealed that the rate of
5 °C min-1 is the optimum heating/cooling rate to obtain a single
perovskite phase of LSCO with calcination temperature of 800 °C.
This result was confirmed by a thermogravimetric analysis (TGA) as
it showed a complete decomposition of intermediate compounds to
form oxide material was also observed at 800 °C.},
	    journal   = {International Journal of Chemical and Molecular Engineering},
	  volume    = {6},
	  number    = {10},
	  year      = {2012},
	  pages     = {963 - 967},
	  ee        = {https://publications.waset.org/pdf/6546},
	  url   	= {https://publications.waset.org/vol/70},
	  bibsource = {https://publications.waset.org/},
	  issn  	= {eISSN: 1307-6892},
	  publisher = {World Academy of Science, Engineering and Technology},
	  index 	= {Open Science Index 70, 2012},
	}